TWI663006B - Method for forming blank of wrench tool - Google Patents

Method for forming blank of wrench tool Download PDF

Info

Publication number
TWI663006B
TWI663006B TW105130545A TW105130545A TWI663006B TW I663006 B TWI663006 B TW I663006B TW 105130545 A TW105130545 A TW 105130545A TW 105130545 A TW105130545 A TW 105130545A TW I663006 B TWI663006 B TW I663006B
Authority
TW
Taiwan
Prior art keywords
section
head
blank
forging
wrench tool
Prior art date
Application number
TW105130545A
Other languages
Chinese (zh)
Other versions
TW201811459A (en
Inventor
賴傳榮
Original Assignee
賴傳榮
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by 賴傳榮 filed Critical 賴傳榮
Priority to TW105130545A priority Critical patent/TWI663006B/en
Publication of TW201811459A publication Critical patent/TW201811459A/en
Application granted granted Critical
Publication of TWI663006B publication Critical patent/TWI663006B/en

Abstract

一種扳手工具胚料的成型方法,包含一備料步驟、一擠壓拉伸步驟、一第一鍛頭步驟,及一第二鍛頭步驟。在該備料步驟中,準備一圓柱狀的桿材。在該擠壓拉伸步驟中,將該桿材擠壓拉伸為一呈板狀的胚品。該胚品包括一板柄部,及分別位於該板柄部的兩相反端的一第一端部與一第二端部。在該第一鍛頭步驟中,將該第一端部鍛壓成型出一第一頭部。在該第二鍛頭步驟中,將該第二端部鍛壓成型出一第二頭部而製得一扳手工具胚料。該成型方法不需經加熱、冷卻,及除料等步驟,因此可簡化工序並節省電力及工時,亦可避免因產生廢料而相對提升成本及避免資源浪費之情事。A method for forming a blank of a wrench tool includes a material preparation step, an extrusion drawing step, a first forging head step, and a second forging head step. In this preparation step, a cylindrical rod is prepared. In the pressing and stretching step, the rod is squeezed into a plate-shaped blank. The embryo includes a plate shank, and a first end portion and a second end portion respectively located at two opposite ends of the plate shank portion. In the first forging step, a first head is forged and formed into a first end. In the second forging head step, a second head is forged and formed into a second head to obtain a wrench tool blank. The molding method does not require steps such as heating, cooling, and material removal, so it can simplify the process and save electricity and man-hours. It can also avoid the relative increase in costs and waste of resources due to the generation of waste.

Description

扳手工具胚料的成型方法Method for forming blank of wrench tool

本發明是有關於一種成型方法,特別是指一種用於製成扳手工具的胚料之成型方法。The invention relates to a forming method, in particular to a forming method for making blanks of wrench tools.

扳手工具是十分普及的手工具之一,使用時是先以扳手工具的頭部來夾制螺帽,接著對扳手工具的手柄部分施力,從而讓使用者可省力地擰緊或扭鬆螺帽及螺桿。而扳手工具的頭部可為概呈U字形的開口,也可為封閉式且具有內鋸齒的封閉式開孔,甚至是可讓使用者在進行擰緊或扭鬆動作時,不需將頭部由螺帽或螺桿移開的棘輪結構。由於扳手工具具有兩個相反端,因此常會在扳手工具兩端搭配不同類型的頭部,以增加功能性。The wrench tool is one of the very popular hand tools. When using it, first use the head of the wrench tool to clamp the nut, and then apply force to the handle part of the wrench tool, so that the user can easily tighten or loosen the nut. And screw. The head of the wrench tool can be a generally U-shaped opening, or it can be a closed type with a closed hole with internal serrations. It can even allow the user to tighten the head without loosening the head. A ratchet structure removed by a nut or screw. Because the wrench tool has two opposite ends, different types of heads are often used at both ends of the wrench tool to increase functionality.

參閱圖1,上述的扳手工具製作時,是先將未加工的金屬製的原料11成型為一胚料12,再透過切削、打磨,或精整等後處理程序,以將胚料12製成扳手工具。而一般胚料12的成型方法是包含一備料步驟、一加熱步驟、一沖壓步驟、一冷卻步驟,及一除料步驟。在該備料步驟中,是先取一金屬圓桿作為原料11並裁切至適當長度。在該加熱步驟中,是以加熱裝置對該原料11施以固定高溫進行加熱軟化處理。在該沖壓步驟中,是以模具對高溫軟化後的原料11進行沖壓,以將圓柱狀的原料11成型為扁平狀態。在該冷卻步驟中,是等待該原料11冷卻以確保定型。在該除料步驟中,是以除料機根據所需的輪廓進行廢料切除作業,從而製得所需的扳手工具胚料12。Referring to FIG. 1, when the aforementioned wrench tool is manufactured, the raw metal material 11 is first formed into a blank 12, and then the blank 12 is made through a post-processing procedure such as cutting, grinding, or finishing. Wrench tool. The forming method of the blank 12 generally includes a material preparation step, a heating step, a stamping step, a cooling step, and a material removing step. In this preparation step, a metal round rod is first taken as the raw material 11 and cut to an appropriate length. In this heating step, the raw material 11 is subjected to a heating and softening treatment at a fixed high temperature by a heating device. In this pressing step, the raw material 11 that has been softened at a high temperature is punched with a mold to form the cylindrical raw material 11 into a flat state. In this cooling step, the raw material 11 is waited for cooling to ensure the setting. In this removal step, the waste removal operation is performed by the removal machine according to the required contour, thereby obtaining the required wrench tool blank 12.

然而前述的胚料12成型方法不但需要使用加熱裝置對原料進行加熱軟化,還需將該原料11靜置一段時間以進行冷卻定型,工序繁瑣且須耗費大量電力及工時。此外,該除料步驟是以切削等方式去除多餘的料件,因此會產生廢料而造成成本的增加及資源的浪費。However, the aforementioned method for forming the blank 12 not only requires heating and softening the raw material by using a heating device, but also requires the raw material 11 to stand for a period of time for cooling and setting. In addition, the material removal step is to remove excess materials by cutting or the like, so waste will be generated, which will increase cost and waste resources.

因此,本發明之目的,即在提供一種不需經加熱、冷卻,及除料等工序的扳手工具胚料的成型方法。Therefore, an object of the present invention is to provide a method for forming a blank of a wrench tool without the steps of heating, cooling, and removing materials.

於是,本發明扳手工具胚料的成型方法,包含一備料步驟、一擠壓拉伸步驟、一第一鍛頭步驟,及一第二鍛頭步驟。Therefore, the method for forming a blank of a wrench tool according to the present invention includes a material preparation step, an extrusion drawing step, a first forging head step, and a second forging head step.

在該備料步驟中,準備一圓柱狀且由金屬製成的桿材。在該擠壓拉伸步驟中,將該桿材擠壓拉伸為一呈板狀且長度大於該桿材長度的胚品。該胚品包括一板柄部,及分別位於該板柄部的兩相反端的一第一端部與一第二端部。在該第一鍛頭步驟中,將該胚品之第一端部鍛壓成型出一第一頭部,該第一頭部具有二相間隔設置的第一外圓角。在該第二鍛頭步驟中,將該胚品之第二端部鍛壓成型出一第二頭部而製得一扳手工具胚料,該第二頭部具有二相間隔設置的外表面,及一連接於該等外表面間的弧面。In this preparation step, a cylindrical rod made of metal is prepared. In the extrusion and stretching step, the rod is extruded into a blank having a plate shape and a length greater than the length of the rod. The embryo includes a plate shank, and a first end portion and a second end portion respectively located at two opposite ends of the plate shank portion. In the first forging step, a first head is formed by forging the first end of the embryo, and the first head has first outer rounded corners arranged at two intervals. In the second forging head step, a second head is formed by forging the second end of the embryo to form a wrench tool blank, the second head has an outer surface spaced two phases apart, and A curved surface connected between the outer surfaces.

本發明之功效在於:藉由該擠壓拉伸步驟、該第一鍛頭步驟與該第二鍛頭步驟的配合,使該成型方法不需經高溫加熱、冷卻定型,及除料等步驟,因此可簡化工序並節省電力及工時,亦可避免因產生廢料而相對提升成本及避免資源浪費之情事。The effect of the present invention is: through the cooperation of the extrusion stretching step, the first forging head step and the second forging head step, the forming method does not need to be subjected to high-temperature heating, cooling, setting, and material removal steps, Therefore, the process can be simplified, power and man-hours can be saved, and the relative increase in costs and waste of resources due to waste generation can be avoided.

參閱圖2及圖3,本發明扳手工具胚料2的成型方法之一實施例,包含一備料步驟31、一擠壓拉伸步驟32、一第一鍛頭步驟33,及一第二鍛頭步驟34。在該備料步驟31中,準備一圓柱狀且由金屬製成的桿材4。Referring to FIGS. 2 and 3, an embodiment of a forming method of the wrench tool blank 2 according to the present invention includes a material preparation step 31, an extrusion drawing step 32, a first forging head step 33, and a second forging head. Step 34. In this preparation step 31, a cylindrical rod 4 made of metal is prepared.

參閱圖2、圖3,及圖4,在該擠壓拉伸步驟32中,將該桿材4以滾軋等方式擠壓拉伸為一呈板狀的胚品5。該胚品5包括一個沿一第一方向A長向延伸的板柄部51,及分別位於該板柄部51的兩相反端的一第一端部52與一第二端部53。定義一垂直該第一方向A的第二方向B,及一同時垂直該第一方向A及該第二方向B的第三方向C,在本實施例所述的第三方向C是指進入紙面的方向,該第一端部52沿該第二方向B延伸的尺寸,以及沿該第三方向C的尺寸皆大於該板柄部51及該第二端部53。該第一端部52具有一連接該板柄部51的內端段521、一個一端連接該內端段521的中身段522,及一連接該中身段522之另一端且朝遠離該板柄部51的方向延伸的外端段523。在本實施例中,該胚品5的橫截面為矩形,該內端段521沿該第二方向B的尺寸是往遠離該板柄部51的方向逐漸增加,該中身段522沿該第二方向B的尺寸是保持相同,而該外端段523沿該第二方向B的尺寸,是往遠離該中身段522的方向逐漸減少。該第二端部53與該板柄部51沿該第二方向B的尺寸相同。Referring to FIG. 2, FIG. 3, and FIG. 4, in the extrusion stretching step 32, the rod material 4 is extruded into a plate-shaped blank 5 by rolling or the like. The blank 5 includes a plate shank portion 51 extending longitudinally along a first direction A, and a first end portion 52 and a second end portion 53 respectively located at two opposite ends of the plate shank portion 51. Define a second direction B that is perpendicular to the first direction A, and a third direction C that is perpendicular to both the first direction A and the second direction B. The third direction C described in this embodiment refers to entering the paper surface. The dimensions of the first end portion 52 extending along the second direction B and the dimensions along the third direction C are larger than the plate handle portion 51 and the second end portion 53. The first end portion 52 has an inner end portion 521 connected to the plate handle portion 51, a middle body portion 522 connected to the inner end portion 521 at one end, and a second end connected to the middle body portion 522 and facing away from the plate handle portion. The outer end section 523 extends in the direction of 51. In this embodiment, the cross section of the embryo 5 is rectangular, and the size of the inner end section 521 along the second direction B gradually increases away from the plate handle 51, and the middle body section 522 follows the second direction. The size of the direction B remains the same, and the size of the outer end section 523 along the second direction B gradually decreases in a direction away from the middle body section 522. The second end portion 53 has the same size as the plate handle portion 51 along the second direction B.

參閱圖2、圖3,及圖5,在該第一鍛頭步驟33中,先將該第一端部52鍛壓成一第一雛形部54。該第一雛形部54具有兩個相間隔且彼此相互傾斜設置的斜側面541,每一斜側面541的延伸面D與一參考面E之間的夾角為15度。參閱圖2、圖3,及圖6,接著再將該第一雛形部54鍛壓成一第一頭部55。該第一頭部55具有一連接該板柄部51的第一接頭段551、二相間隔地設置於該第一接頭段551的兩相反側的第一內圓角552、一由該第一接頭段551朝遠離該板柄部51的方向延伸的扳手加工段553,及二相間隔地形成於該扳手加工段553的兩相反側的第一外圓角554。在本實施例中,該第一頭部55的橫截面同樣為矩形。Referring to FIG. 2, FIG. 3, and FIG. 5, in the first forging head step 33, the first end portion 52 is first forged into a first prototype portion 54. The first prototype 54 has two oblique side surfaces 541 spaced from each other and disposed obliquely to each other. An included angle between the extension surface D of each oblique side surface 541 and a reference plane E is 15 degrees. Referring to FIG. 2, FIG. 3, and FIG. 6, the first prototype 54 is then forged into a first head 55. The first head 55 has a first joint section 551 connected to the plate handle 51, two first fillets 552 disposed on two opposite sides of the first joint section 551 at two intervals, and a first A spanner processing section 553 extending in a direction away from the plate handle 51 and a joint section 551 and first outer fillets 554 formed on two opposite sides of the spanner processing section 553 at two intervals. In this embodiment, the cross section of the first head 55 is also rectangular.

參閱圖2、圖3,及圖7,在該第二鍛頭步驟34中,先將該第二端部53鍛壓成型為一第二雛形部56。該第二雛形部56具有一個一端連接該板柄部51的連接段561、二相間隔地形成於該連接段561上且連接該板柄部51的第二內圓角562、一連接於該連接段561另一端的承接段563、一由該承接段563朝遠離該連接段561的方向延伸的延伸段564,及二相間隔地形成於該承接段563上且分別連接該延伸段564及該等第二內圓角562的第二外圓角565。在本步驟中,該連接段561沿該第二方向B的尺寸是朝遠離該板柄部51的方向逐漸增加。該承接段563沿該第二方向B的尺寸是朝遠離該連接段561的方向逐漸減少。該延伸段564沿該第二方向B的尺寸是維持相同。Referring to FIG. 2, FIG. 3, and FIG. 7, in the second forging head step 34, the second end portion 53 is first forged and formed into a second prototype portion 56. The second prototype 56 has a connecting section 561 connected to the plate handle 51 at one end, a second inner fillet 562 formed at two intervals on the connecting section 561 and connected to the plate handle 51, and a second The receiving section 563 at the other end of the connecting section 561, an extending section 564 extending from the receiving section 563 in a direction away from the connecting section 561, and two extending at intervals on the receiving section 563 and connecting the extending section 564 and A second outer fillet 565 of the second inner fillets 562. In this step, the size of the connecting section 561 along the second direction B is gradually increased in a direction away from the plate handle portion 51. The size of the receiving section 563 along the second direction B gradually decreases toward the direction away from the connecting section 561. The size of the extension 564 along the second direction B remains the same.

參閱圖2、圖3,及圖8,最後將該第二雛形部56鍛壓成一第二頭部57,從而製得如圖8所示的一個扳手工具胚料2。該第二頭部57具有一由連接段561成型出而形成有該等第二內圓角562的第二接頭段571,及一由該承接段563及該延伸段564成型出的棘輪加工段572。參閱圖8及圖9,該第二接頭段571維持與該連接段561相同之外型,該棘輪加工段572具有二沿該第三方向C相間隔設置的外表面573,及一連接於該等外表面573間的弧面574。參閱圖3、圖8,及圖10,藉由上述步驟,可將該桿材4在不需高溫加熱、冷卻定型,及額外切削除料的情況下,完全以鍛造方式製得如圖8所示的扳手工具胚料2。本實施例的扳手工具胚料2再經後續加工後即可製成如圖10所示的一個棘輪扳手工具6,其中,該扳手工具胚料2之第一頭部55被加工成該棘輪扳手工具6的一個扳手結構61,該板柄部51被加工成該棘輪扳手工具6的一個把手62,而該第二頭部57被加工成該棘輪扳手工具6的一個棘輪結構63。由於該棘輪扳手工具6具有特定結構,為配合其結構,本發明製作出的該扳手工具胚料2亦必須具備特定結構,因此本發明透過各鍛造過程之配合,使成型出該第一頭部55具有該等第一外圓角554,以對應該扳手結構61,該第二頭部57具有該等外表面573與該弧面574以對應該棘輪結構63。由於該成型方法全程不需以高溫來軟化該桿材4,因此不需額外設置加熱裝置,也不用等待工件冷卻,可節省電力及工時並簡化工序。此外,該成型方法以鍛造方式製得該扳手工具胚料2,因此能取適量桿材4材料鍛造出,亦不需進行切削除料而可節省用料及成本。Referring to FIG. 2, FIG. 3, and FIG. 8, the second prototype portion 56 is finally forged into a second head 57 to obtain a wrench tool blank 2 as shown in FIG. 8. The second head 57 has a second joint section 571 formed from the connecting section 561 to form the second fillets 562, and a ratcheting section formed from the receiving section 563 and the extension section 564. 572. Referring to FIG. 8 and FIG. 9, the second joint section 571 maintains the same shape as the connecting section 561, the ratcheting section 572 has two outer surfaces 573 spaced apart from each other along the third direction C, and a connection to the Arc surface 574 between outer surfaces 573. Referring to FIG. 3, FIG. 8, and FIG. 10, through the above steps, the rod 4 can be completely forged as shown in FIG. 8 without the need for high-temperature heating, cooling, and additional cutting and removal. Show the wrench tool blank 2. The wrench tool blank 2 of this embodiment can be made into a ratchet wrench tool 6 as shown in FIG. 10 after subsequent processing. The first head 55 of the wrench tool blank 2 is processed into the ratchet wrench. A wrench structure 61 of the tool 6, the plate handle 51 is processed into a handle 62 of the ratchet wrench tool 6, and the second head 57 is processed into a ratchet structure 63 of the ratchet wrench tool 6. Because the ratchet wrench tool 6 has a specific structure, in order to match the structure, the wrench tool blank 2 produced by the present invention must also have a specific structure, so the present invention enables the first head to be formed through the cooperation of various forging processes. 55 has the first outer rounded corners 554 to correspond to the wrench structure 61, and the second head 57 has the outer surfaces 573 and the curved surface 574 to correspond to the ratchet structure 63. Since the molding method does not need to soften the rod material 4 at a high temperature throughout the process, there is no need to provide an additional heating device, and there is no need to wait for the workpiece to cool, which can save power and man-hours and simplify the process. In addition, in the forming method, the wrench tool blank 2 is prepared by forging, so that an appropriate amount of rod material 4 can be forged, and cutting and material removal are not required, which can save materials and costs.

綜上所述,藉由該擠壓拉伸步驟32、該第一鍛頭步驟33與該第二鍛頭步驟34的配合,使本發明的成型方法不需進行高溫加熱、冷卻定型,及除料等步驟,因此可簡化工序並節省電力及工時,亦可避免因傳統製法的除料步驟產生廢料而造成成本提高及資源浪費之情事,故本發明還能節省用料成本、避免材料浪費,確實能達成本發明之目的。In summary, the cooperation of the extrusion stretching step 32, the first forging head step 33, and the second forging head step 34 makes the forming method of the present invention unnecessary to perform high-temperature heating, cooling setting, and removal. Material and other steps, so it can simplify the process and save electricity and man-hours. It can also avoid the cost increase and waste of resources caused by the waste produced by the traditional material removal step. Therefore, the invention can also save the cost of materials and avoid waste of materials. , Can indeed achieve the purpose of cost invention.

惟以上所述者,僅為本發明之實施例而已,當不能以此限定本發明實施之範圍,凡是依本發明申請專利範圍及專利說明書內容所作之簡單的等效變化與修飾,皆仍屬本發明專利涵蓋之範圍內。However, the above are only examples of the present invention. When the scope of implementation of the present invention cannot be limited in this way, any simple equivalent changes and modifications made in accordance with the scope of the patent application and the content of the patent specification of the present invention are still Within the scope of the invention patent.

2‧‧‧扳手工具胚料 2‧‧‧ wrench tool blank

31‧‧‧備料步驟 31‧‧‧ preparation steps

32‧‧‧擠壓拉伸步驟 32‧‧‧Extrusion step

33‧‧‧第一鍛頭步驟 33‧‧‧First forging head step

34‧‧‧第二鍛頭步驟 34‧‧‧Second forging head step

4‧‧‧桿材 4‧‧‧ rod

5‧‧‧胚品 5‧‧‧ embryo

51‧‧‧板柄部 51‧‧‧ plate handle

52‧‧‧第一端部 52‧‧‧first end

521‧‧‧內端段 521‧‧‧inner end

522‧‧‧中身段 522‧‧‧ middle body

523‧‧‧外端段 523‧‧‧outer end

53‧‧‧第二端部 53‧‧‧ second end

54‧‧‧第一雛形部 54‧‧‧First prototype

541‧‧‧斜側面 541‧‧‧ oblique side

55‧‧‧第一頭部 55‧‧‧first head

551‧‧‧第一接頭段 551‧‧‧First joint section

552‧‧‧第一內圓角 552‧‧‧first fillet

553‧‧‧扳手加工段 553‧‧‧Wrench processing section

554‧‧‧第一外圓角 554‧‧‧First Fillet

56‧‧‧第二雛形部 56‧‧‧Second prototype

561‧‧‧連接段 561‧‧‧connection section

562‧‧‧第二內圓角 562‧‧‧Second Fillet

563‧‧‧承接段 563‧‧‧ Undertake section

564‧‧‧延伸段 564‧‧‧extended

565‧‧‧第二外圓角 565‧‧‧Second Fillet

57‧‧‧第二頭部 57‧‧‧Second Head

571‧‧‧第二接頭段 571‧‧‧Second joint section

572‧‧‧棘輪加工段 572‧‧‧ Ratchet Processing Section

573‧‧‧外表面 573‧‧‧outer surface

574‧‧‧弧面 574‧‧‧arc

6‧‧‧棘輪扳手工具 6‧‧‧ Ratchet wrench tool

61‧‧‧扳手結構 61‧‧‧ wrench structure

62‧‧‧把手 62‧‧‧handle

63‧‧‧棘輪結構 63‧‧‧Ratchet structure

A‧‧‧第一方向 A‧‧‧ first direction

B‧‧‧第二方向 B‧‧‧ Second direction

C‧‧‧第三方向 C‧‧‧ Third direction

D‧‧‧延伸面 D‧‧‧Extended surface

E‧‧‧參考面 E‧‧‧reference surface

本發明之其他的特徵及功效,將於參照圖式的實施方式中清楚地呈現,其中: 圖1是一習知扳手工具之胚料的成型方法的一示意圖; 圖2是本發明扳手工具胚料的成型方法之一實施例的一流程圖; 圖3是該實施例的一示意圖; 圖4是該實施例之一擠壓拉伸步驟的一示意圖; 圖5及圖6皆是該實施例之一第一鍛頭步驟的示意圖; 圖7及圖8皆是該實施例之一第二鍛頭步驟的示意圖; 圖9是該實施例之一扳手工具胚料的側視圖;及 圖10是以該實施例所製成之一扳手工具的一立體圖。Other features and effects of the present invention will be clearly presented in the embodiment with reference to the drawings, in which: FIG. 1 is a schematic diagram of a conventional method for forming a blank of a wrench tool; FIG. 2 is a blank of a wrench tool according to the present invention FIG. 3 is a schematic diagram of the embodiment; FIG. 4 is a schematic diagram of the extrusion and stretching step of the embodiment; FIG. 5 and FIG. 6 are the embodiment A schematic diagram of a first forging head step; FIGS. 7 and 8 are schematic diagrams of a second forging head step of this embodiment; FIG. 9 is a side view of a wrench tool blank of this embodiment; and FIG. 10 is A perspective view of a wrench tool made in this embodiment.

Claims (4)

一種扳手工具胚料的成型方法,包含:一備料步驟,準備一圓柱狀且由金屬製成的桿材;一擠壓拉伸步驟,利用滾軋方式將該桿材擠壓拉伸為一呈板狀且長度大於該桿材長度的胚品,該胚品包括一板柄部,及分別位於該板柄部的兩相反端的一第一端部與一第二端部;一第一鍛頭步驟,先將該第一端部鍛壓成一第一雛形部,該第一雛形部具有兩個相間隔且彼此相互傾斜設置的斜側面,再將該第一雛形部鍛壓成該第一頭部,該第一頭部具有二相間隔設置且由該等斜側面成型而成的第一外圓角、一連接該板柄部的第一接頭段、二相間隔地設置於該第一接頭段上的第一內圓角,及一由該第一接頭段朝遠離該板柄部的方向延伸且形成有該等第一外圓角的扳手加工段;及一第二鍛頭步驟,先將該第二端部鍛壓成型為一第二雛形部,該第二雛形部具有二相間隔設置且連接該板柄部的第二內圓角、一個一端連接該板柄部的連接段、一連接於該連接段另一端的承接段,及一由該承接段朝遠離該連接段的方向延伸的延伸段,該等第二內圓角是形成於該連接段上,接著將該第二雛形部鍛壓成型出一第二頭部而製得一扳手工具胚料,該第二頭部具有二相間隔設置的外表面、一連接於該等外表面間的弧面、一由該第二雛形部之連接段成型出而形成有該等第二內圓角的第二接頭段,及由該承接段及該延伸段成型出並具有該等外表面及該弧面的棘輪加工段。A method for forming a blank of a wrench tool, including: a material preparation step, preparing a cylindrical rod made of metal; a squeezing step, using a rolling method to extrude the rod into a shape A plate-shaped embryo with a length greater than the length of the rod, the embryo including a plate shank, and a first end and a second end respectively located at two opposite ends of the plate shank; a first forging head Step, first forging the first end part into a first prototype part, the first prototype part having two oblique sides spaced and inclined to each other, and then forging the first prototype part into the first head part, The first head has two outer phases, which are spaced apart and formed from the oblique sides, a first joint segment connected to the plate handle, and two phases spaced on the first joint segment. A first inner rounded corner, and a wrench processing segment extending from the first joint section in a direction away from the plate handle and forming the first outer rounded corners; and a second forging step, first The second end portion is forged and formed into a second prototype portion, and the second prototype portion has two phases spaced apart from each other. And a second fillet connected to the plate handle, a connecting section connected to the plate handle at one end, a receiving section connected to the other end of the connecting section, and a extending section extending away from the connecting section from the receiving section The second fillet is formed on the connecting section, and then the second prototype is forged into a second head to obtain a wrench tool blank. The second head has two Outer surfaces disposed at intervals, an arc surface connected between the outer surfaces, a second joint section formed from the connecting sections of the second prototype to form the second fillets, and The receiving section and the extended section are formed with ratcheting sections having the outer surface and the arc surface. 如請求項1所述的扳手工具胚料的成型方法,其中,在該第二鍛頭步驟中,該第二雛形部還具有二形成於該承接段上且分別連接該延伸段及該等第二內圓角的第二外圓角。The method for forming a blank of a wrench tool according to claim 1, wherein in the second forging step, the second prototype portion further has two formed on the receiving section and connected to the extension section and the first section respectively. The second outer fillet of two fillets. 如請求項1所述的扳手工具胚料的成型方法,其中,在該擠壓拉伸步驟中,該第一端部的尺寸大於該第二端部的尺寸。The method for forming a blank of a wrench tool according to claim 1, wherein in the pressing and stretching step, a size of the first end portion is larger than a size of the second end portion. 如請求項1所述的扳手工具胚料的成型方法,其中,在該擠壓拉伸步驟中,該第一端部具有一連接該板柄部的內端段、一個一端連接該內端段的中身段,及一連接該中身段之另一端且朝遠離該板柄部的方向延伸的外端段。The method for forming a blank of a wrench tool according to claim 1, wherein in the extrusion and stretching step, the first end portion has an inner end portion connected to the plate shank portion, and one end connected to the inner end portion A middle body section and an outer end section connected to the other end of the middle body section and extending in a direction away from the plate handle.
TW105130545A 2016-09-22 2016-09-22 Method for forming blank of wrench tool TWI663006B (en)