Hong-Tai Cai
Original Assignee
Star Royal Co Ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Star Royal Co Ltd filed Critical Star Royal Co Ltd
Priority to TW97103873A priority Critical patent/TW200934923A/zh
Publication of TW200934923A publication Critical patent/TW200934923A/zh

Links

Landscapes

  • Paper (AREA)

Description

200934923 九、發明說明: 、 【發明所屬之技術領域】 本發明係為一種紙漿製造方法,尤指一種利用礦物纖維製成之 紙漿,可部分的替代目前造紙所使用之木漿來製造紙製品,俾達到 更能符合環保意識,並有助於降低造紙成本之紙漿製造方法。 【先前技術】 按,目前造紙所使用之紙漿,皆取之於大自然之林木為原料來 ®製成木漿,而隨著工業與科、技的進步,紙製品(如:紙張、紙箱)之 使用量逐日遽增,為滿足紙製品之需求,林木也被大量砍伐,甚至 已到濫伐之地步’而大量石欠伐林木之結果,除了嚴重破壞大自然生 祕境外’並已危害動、植物生命安全;有鑑於此,為倾地球之 生態環境免於繼續惡化,在環保意識日趨高漲之情形下,林木原料 之取得已日趨不易,因此也促使木漿成本之高漲者。 S纟以木I製成之紙製品,&於木I纖維不耐潮濕,因此很 ❹容易受潮或遇水而損壞者;又,由於木衆纖維係屬易燃物,因此很 容易遇火燃燒,在使用上亦有其不安全之缺失者。 【發明内容】 本么月之目的,即在於改善上述以木漿製成紙製品所具有之缺 失’提供-種_礦物纖維製造之㈣,可部分的替代目前造紙所 使用之木聚來製造紙製品,俾達到更符合環保意識,並有助於降低 造紙成本之紙漿製造方法。 s 為達到上述目的,本發明之紙漿製造方法,包含有:將擴物纖 200934923 維與適量的水放入碎聚機中,利用碎衆機之高速麟將礦物纖維 碎解成適量長度之短纖維並與水搜拌形成料聚之步驟;將經上述步 驟所升/成之料毁以除砂n去除重雜質之步驟·,將經上述步驟所完成 之料漿進行二次碎解與分離,使料製内之雜質分離並提高料聚疏 解,之步驟’將經上述步驟完成之㈣進行脫除水分,去除料默中 P伤水刀’使料聚濃縮到所需預定濃度之步驟;藉自上述之步驟, ❺.種_礦物纖維製造之纟樣,可與目前造紙所姻之木浆混 -1製造紙製品’俾達到更符合環保意識,並有助於降低造紙成本 【實施方式】 合第=發目的所運用之技術手段及其構造,茲謹再配 弟圖所不之流程圖,詳細說明如下: 如第-圖所示’本發明之紙漿製造方法,包含有: 步鄉一 礦物纖維與適量的水放入碎職中,利用碎漿機之高速 携拌,將鑛物纖維碎解成適量長度之短纖維並與水勝形 成枓漿;其中,該褒料之含水率約為90%為佳;又其中 ^物纖維係為—種以爐石或粉煤灰經高雜絲所製 成之無機纖維。 步驟二 步驟三 .將經步驟-卿成之鄕赠剌去除重雜質; 將九步驟—所完成之料舰行二次碎解與分離,使料衆内 之雜質分離’並提高料漿之疏解率; e ο 200934923 '步驟四:將經步驟三所完成之料漿進行脫除水分,去除料製中之部 伤水分,使賴濃铜所需之預定濃度以完成—種利 礦物纖維製成紙漿之方法。 藉由上述方法製成之紙、浆,其可依所造紙張之用途需求而以 適當之比例與木聚原料混合來製造紙製品;嗣,由於本發明係利用 爐石或粉煤灰經高溫熔融抽絲所形成之礦物纖維為主要原料而於 煤灰乃為火力發電廠發電過程所產生之副產物,爐石乃為練鋼過^ I所產生之副產物,因此除了可減少林木之開採,有效維護生態環 境外’並可將原為廢棄物之粉煤灰與爐石再糊,達到資源回收再 _ ’及有效的降低造紙料漿之成本n由於礦物纖維耐濕性 南’且非屬易燃物’因此可邊高製成紙製品之耐水性,及·性者。 由是,本發明確具有顯著之進步性,且確為未曾有過,誠已符合發 7專利之要件,爰依法提出專辦請,並祈賜專利為禱,至感德便。 【圖式簡單說明】 第一圖係本發明之流程圖。

Claims (1)

  1. 200934923 -十、申請專剎範園: 1. 一種紙漿製造方法,包含有: 步驟一:將#物纖維與適量的水放入碎漿機中,利用碎漿機之高 速攪拌,將礦物纖維碎解成適量長度之短纖維並與水攪 拌形成料漿; 步驟二:將經步驟一所形成之料漿以除砂器去除重雜質; 步驟三:將經步驟二所完成之料漿進行二次碎解與分離使料漿 β 内之雜質分離,並提高料漿之疏解率; ; 步驟四:將經步驟三所完成之料漿進行脫除水分,去除料漿中之 雜水分,使料聚濃縮到所需之預定遭度,以完成-種 利用礦物纖維製成紙漿之方法。 2·如申w專她㈣丨項所述之紙賴造方法’其中步驟—所形成之 料漿含水率約為90%為佳、。 ❹3. 凊,範圍第1項所述之紙衆製造方法,其中該礦物纖維係為 粉駄經高溫縣減㈣狀無機纖維。
TW97103873A 2008-02-01 2008-02-01 Manufacturing method of paper pulp TW200934923A (en)

Priority Applications (1)

Application Number Priority Date Filing Date Title
TW97103873A TW200934923A (en) 2008-02-01 2008-02-01 Manufacturing method of paper pulp

Applications Claiming Priority (1)

Application Number Priority Date Filing Date Title
TW97103873A TW200934923A (en) 2008-02-01 2008-02-01 Manufacturing method of paper pulp

Publications (1)

Publication Number Publication Date
TW200934923A true TW200934923A (en) 2009-08-16

Family

ID=44866396

Family Applications (1)

Application Number Title Priority Date Filing Date
TW97103873A TW200934923A (en) 2008-02-01 2008-02-01 Manufacturing method of paper pulp

Country Status (1)

Country Link
TW (1) TW200934923A (zh)

Cited By (1)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
CN106235936A (zh) * 2016-07-28 2016-12-21 义乌市义南纸业有限公司 一种环保无荧光剂原纸面巾纸及其制备方法

Cited By (1)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
CN106235936A (zh) * 2016-07-28 2016-12-21 义乌市义南纸业有限公司 一种环保无荧光剂原纸面巾纸及其制备方法

Similar Documents

Publication Publication Date Title
CN101666129B (zh) 建筑垃圾烧结砖及其生产方法
CN101244906B (zh) 一种高活性矿物掺合料的制备方法及应用
CN101691700B (zh) 一种促进纤维帚化的磨浆方法及其在造纸中的应用
CN106587783B (zh) 利用废弃物制备混凝土材料的方法
CA2764551C (en) Method of making particulate material
US10329505B2 (en) Method for producing biofuel and use of biofuel
CN106930133A (zh) 一种用甘蔗渣造纸的方法及其制成的水杯
CN107032683A (zh) 一种节能环保砖及制备方法
CN101818091A (zh) 秸秆复合燃料制造方法及秸秆复合燃料
CN107651897A (zh) 一种碳化植物纤维增强煤矸石砖及其生产方法
TW200934923A (en) Manufacturing method of paper pulp
CN102690698B (zh) 污泥燃料及其制造方法
Anandaraj et al. Experimental investigation on sugarcane bagasse fiber reinforced concrete using bottom ash as sand replacement
CN1995538A (zh) 在废纸板中加入蕉藕渣生产瓦楞纸的制备方法
US20090169811A1 (en) Building board
CN107973941B (zh) 可降解甘蔗渣地膜及其制备方法
TW201200653A (en) Method of reproducing discarded rock wool
CN101338534A (zh) 一种工业尾矿或固废物纤维纸浆及其为原料的造纸方法
CN105568677A (zh) 一种造纸用微细无机纤维的柔性改性方法
CN112551882A (zh) 一种处理废弃农用岩棉再利用的方法及农用岩棉
CN101830024B (zh) 用制浆造纸含纤维固体废弃物制备无醛木塑复合板的方法
JP2006256909A (ja) ロックウール製造方法及び製造装置
CN103785668A (zh) 一种处理造纸废渣的方法
JPH0829969B2 (ja) 耐火性建築材料の製造方法
CN108824061A (zh) 一种基于无机纤维纸浆生产纸产品的方法