RU2486143C1 - Mixture for making porous aggregate - Google Patents
Mixture for making porous aggregate Download PDFInfo
- Publication number
- RU2486143C1 RU2486143C1 RU2012106567/03A RU2012106567A RU2486143C1 RU 2486143 C1 RU2486143 C1 RU 2486143C1 RU 2012106567/03 A RU2012106567/03 A RU 2012106567/03A RU 2012106567 A RU2012106567 A RU 2012106567A RU 2486143 C1 RU2486143 C1 RU 2486143C1
- Authority
- RU
- Russia
- Prior art keywords
- mixture
- porous aggregate
- dolomite
- coal
- sieved
- Prior art date
Abstract
Description
Изобретение относится к производству пористых заполнителей для бетонов.The invention relates to the production of porous aggregates for concrete.
Известна шихта для производства пористого заполнителя, содержащая, мас.%: глина монтмориллонитовая 35,0-38,0; уголь 5,0-6,0; доломит 36,0-50,0 [1].A known mixture for the production of porous aggregate, containing, wt.%: Clay montmorillonite 35,0-38,0; coal 5.0-6.0; dolomite 36.0-50.0 [1].
Задачей изобретения является повышение прочности пористого заполнителя, полученного из шихты.The objective of the invention is to increase the strength of the porous aggregate obtained from the mixture.
Технический результат достигается тем, что шихта для производства пористого заполнителя, содержащая глину монтмориллонитовую, уголь, доломит, дополнительно содержит древесные опилки и карбоксиметилцеллюлозу при следующем соотношении компонентов, мас.%: глина монтмориллонитовая 96,5-97,5; размолотый и просеянный через сетку №014 уголь 0,5-1,0; размолотый и просеянный через сетку №014 доломит 0,5-1,0; просеянные через сетку №5 древесные опилки 0,5-1,0; карбоксиметилцеллюлоза 0,5-1,0.The technical result is achieved by the fact that the mixture for the production of porous aggregate containing montmorillonite clay, coal, dolomite, additionally contains sawdust and carboxymethyl cellulose in the following ratio of components, wt.%: Montmorillonite clay 96.5-97.5; coal 0.5–1.0 milled and sifted through mesh No. 014; milled and sifted through mesh No. 014, dolomite 0.5-1.0; wood sawdust sieved through mesh No. 5 0.5-1.0; carboxymethyl cellulose 0.5-1.0.
В таблице приведены составы шихты для производства пористого заполнителя.The table shows the composition of the mixture for the production of porous aggregate.
В составе шихты для производства пористого заполнителя используют глины монтмориллонитовые, включающие Al-монтмориллонит и Fe-монтмориллонит (нонтронит).Montmorillonite clays, including Al-montmorillonite and Fe-montmorillonite (nontronite) are used in the mixture for the production of porous aggregate.
Компоненты сырьевой смеси дозируют в требуемых количествах. Уголь и доломит размалывают до порошкообразного состояния, просеивают через сетку №014, добавляют глину монтмориллонитовую, просеянные через сетку №5 древесные опилки, карбоксиметилцеллюлозу и смешивают. Полученную шихту увлажняют до 18-24% и формуют из нее гранулы размером 20-40 мм, которые сушат до влажности 3-6% и обжигают при температуре 1000-1100°С.The components of the raw mix are dosed in the required quantities. The coal and dolomite are ground to a powder state, sieved through mesh No. 014, montmorillonite clay is added, sawdust sifted through mesh No. 5, carboxymethyl cellulose and mixed. The resulting mixture is moistened to 18-24% and granules of 20-40 mm in size are formed from it, which are dried to a moisture content of 3-6% and fired at a temperature of 1000-1100 ° C.
Источник информацииThe source of information
1. SU 1161500, С04В 31/00, 1985.1. SU 1161500, C04B 31/00, 1985.
Claims (1)