KR960002714A - 반도체소자의 소자분리절연막 형성방법 - Google Patents

반도체소자의 소자분리절연막 형성방법 Download PDF

Info

Publication number
KR960002714A
KR960002714A KR1019940013236A KR19940013236A KR960002714A KR 960002714 A KR960002714 A KR 960002714A KR 1019940013236 A KR1019940013236 A KR 1019940013236A KR 19940013236 A KR19940013236 A KR 19940013236A KR 960002714 A KR960002714 A KR 960002714A
Authority
KR
South Korea
Prior art keywords
insulating film
isolation insulating
forming
device isolation
semiconductor device
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Ceased
Application number
KR1019940013236A
Other languages
English (en)
Inventor
홍상기
여태정
이우봉
고재완
구영모
김세정
Original Assignee
김주용
현대전자산업 주식회사
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by 김주용, 현대전자산업 주식회사 filed Critical 김주용
Priority to KR1019940013236A priority Critical patent/KR960002714A/ko
Publication of KR960002714A publication Critical patent/KR960002714A/ko
Ceased legal-status Critical Current

Abstract

본 발명은 반도체소자의 소자분리 절연막 형성방법에 관한 것으로, 종래기술로 소자분리 절연막을 형성함으로써 고집적 반도체소자 형성시 발생되는 문제점을 해결하기 위하여, 반도체기판을 식각하여 트랜치를 형성하고 채널스토퍼를 형성한 다음, 열산화 공정으로 소자분리절연막을 형성함으로써 반도체소자의 신뢰성을 향상시키고 반도체 소자의 고집적화를 가능하게 하는 기술이다.

Description

반도체 소자의 소자분리절연막 형성방법
본 내용은 요부공개 건이므로 전문내용을 수록하지 않았음
제2A도 내지 제2E도는 본 발명의 실시예로서 반도체소자의 소자분리 절연막 형성공정을 도시한 단면도.

Claims (2)

  1. 반도체 소자의 소자분리절연막 형성방법에 있어서, 반도체기판 상부에 패드산화막과 질화막을 순차적으로 증착하고 그 상부에 감광막패턴을 형성한 다음, 상기 감광막패턴을 마스크로하여 상기 질화막 및 패드산화막을 순차적으로 식각한 다음, 상기 감광막패턴을 제거하는 공정과, 상기 질화막을 식각장벽으로 하여 상기 반도체기판의 일정깊이를 식각하여 트렌치를 형성하는 공정과, 상기 질화막을 마스크로 하여 반도체기판에 불순물이온을 주입하여 채널스토퍼를 형성하는 공정과, 열산화 공정으로 소자분리절연막을 형성하는 공정을 포함하는 반도체소자의 소자분리절연막 형성방법.
  2. 제1항에 있어서, 상기 트랜티의 깊이는 예정된 소자분리절연막의 두께의 50-60%로 하는 것을 특징으로 하는 반도체소자의 소자분리절연막 형성방법.
    ※ 참고 사항 : 최초출원 내용에 의하여 공개하는 것임.
KR1019940013236A 1994-06-13 1994-06-13 반도체소자의 소자분리절연막 형성방법 Ceased KR960002714A (ko)