KR20180068263A - Method and apparatus for making a sheet adhered with an adhesive and a laminate using the same - Google Patents

Method and apparatus for making a sheet adhered with an adhesive and a laminate using the same Download PDF

Info

Publication number
KR20180068263A
KR20180068263A KR1020160170009A KR20160170009A KR20180068263A KR 20180068263 A KR20180068263 A KR 20180068263A KR 1020160170009 A KR1020160170009 A KR 1020160170009A KR 20160170009 A KR20160170009 A KR 20160170009A KR 20180068263 A KR20180068263 A KR 20180068263A
Authority
KR
South Korea
Prior art keywords
sheet
mixed adhesive
extruded
low temperature
temperature
Prior art date
Application number
KR1020160170009A
Other languages
Korean (ko)
Other versions
KR101933503B1 (en
Inventor
신원택
Original Assignee
신원택
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by 신원택 filed Critical 신원택
Priority to KR1020160170009A priority Critical patent/KR101933503B1/en
Publication of KR20180068263A publication Critical patent/KR20180068263A/en
Application granted granted Critical
Publication of KR101933503B1 publication Critical patent/KR101933503B1/en

Abstract

The present invention relates to a method and device for producing a low-temperature laminated sheet and a low-temperature laminated sheet using the same to allow a film to be laminated onto an extruded sheet at a low temperature, thereby realizing mass production, reducing defects, and recycling a defective sheet. In the process of extruding an extruded sheet (1) from an extrusion die (10), a PP mixed adhesive liquid (2a) is applied and extruded. The PP mixed adhesive liquid (2a) is cooled at a lower temperature relatively lower than an extrusion temperature by a cooling roller (30) such that a PP mixed adhesive (2) having a gel state and a low-temperature state is formed. The extruded sheet (1), to which the low-temperature PP mixed adhesive (2) is attached, and a different sheet (3) are sequentially passed between a pair of pressure rollers (20, 40) so that the extruded sheet (1) and the different sheet (3) are overlapped with each other. The different sheet (3) is pressed and adheres to the low-temperature PP mixed adhesive (2) to produce a low-temperature laminated sheet (123).

Description

저온합지시트제조방법과 장치 및 이를 이용한 저온합지시트{Method and apparatus for making a sheet adhered with an adhesive and a laminate using the same}TECHNICAL FIELD [0001] The present invention relates to a method and an apparatus for manufacturing a low temperature composite sheet, and a low temperature composite sheet using the same.

본 발명은 주로 압출시트지에 필름이 합지 되도록 하는 합지시트에 관한 것으로서, 더욱 상세하게는 저온으로 합지 되도록 하여 불량율 감소가 도모되고, 불량 발생된 합지시트를 재활용할 수 있도록 개선된 저온합지시트제조방법과 장치 및 이를 이용한 저온합지시트에 관한 것이다.The present invention relates generally to a laminated sheet in which a film is laminated on an extruded sheet, and more particularly, to an improved low-temperature laminated sheet manufacturing method capable of reducing a defective ratio by causing lamination at a low temperature and recycling a defective laminated sheet And a low-temperature laminated sheet using the same.

일반적으로 2개 이상의 시트지나 필름을 합지되게 하는데 있어서 크게 구분하면 각각 제조된 필름을 선행기술문헌의 특허문헌에 기재된 선행기술과 같이 서로 포개지게 하고 고온으로 가열 및 가압하여 상호 융착되게 하여 합지되게 하는 것이 있고, 다른 하나는 압출기의 압출다이에서 압출되는 시트지에 다른 필름이 포개지게 하여 고온 상태로 압출되는 젤 상태의 시트지에 필름이 융착되게 하는 제조 방법이 알려져 있다. 본 발명에서 이해를 돕기 위해 상기와 같이 압출기의 압출다이에서 압출되는 시트지를 압출시트지라고 명칭하고 설명하는 것으로 한다.Generally, two or more sheets or films are largely divided into laminated films. The laminated films are made to overlap each other as in the prior art described in the patent documents of the prior art documents, heated and pressed at a high temperature, And the other is a manufacturing method in which a film is extruded from an extrusion die of an extruder and another film is superimposed on the sheet to cause the film to be fused to a sheet of gel state extruded at a high temperature. In order to facilitate understanding of the present invention, the sheet to be extruded in the extrusion die of the extruder will be referred to as an extruded sheet.

따라서, 상기한 선행기술들은 시트지나 또는 필름이 고온으로 가열된 상태에서 재질 자체가 녹아서 융착 되게 합지 되는 것이기 때문에 두개 이상의 시트지나 필름이 일체가 되는 상태로 합지 되는 것이다.Therefore, the above-described prior arts are such that two or more sheets or films are joined together in a state in which the sheet itself or the film is heated to a high temperature so that the material itself is melted and fused.

그러므로 종래에는 합지 과정에 여러 가지 이유에 의해서 불량이 발생 되면 이종 시트지나 필름의 경우 서로 박리시킬 수 없게 되는 문제점이 있고, 그로 인해 재활용이 불가능하고 전부 폐기해야 하는 비경제적인 문제점이 야기 되었다.Therefore, conventionally, when defects are caused by various reasons in the lapping process, in the case of a heterogeneous sheet or film, there is a problem that they can not be peeled off from each other, and therefore, there is an uneconomical problem in that it can not be recycled and must be completely discarded.

특히, 압출시트지에 필름이 융착되어 합지되는 경우에는 압출다이에서 압출되는 압출시트지가 고온상태이기 때문에 탄화물이 발생되는 경우가 많고, 이러한 탄화물이 있는 압출시트지에 필름이 융착되므로 불순물이 있는 상태로 합지되어 불량이 발생되는 문제점이 있다. Particularly, when the film is fused to the extruded sheet, the extruded sheet extruded from the extruded die is in a high temperature condition, so that carbide is often generated. Since the film is fused to the extruded sheet having such a carbide, Thereby causing defects.

KR 10-1360182 B1 2014.02.11KR 10-1360182 B1 2014.02.11

본 발명은 압출시트지에 필름이 저온 합지 되도록 하여 양산이 도모되고 불량 감소 및 불량시트의 재활용이 도모될 수 있도록 개선된 저온합지시트제조방법과 장치 및 이를 이용한 저온합지시트를 제공하려는데 그 목적이 있다.An object of the present invention is to provide a method and apparatus for manufacturing an improved low-temperature laminated sheet and a low-temperature laminated sheet using the same, in which mass production is promoted by allowing a film to be laminated at low temperature on an extruded sheet, defects can be reduced, and a defective sheet can be recycled .

본 발명은, 압출다이에서 압출시트지가 압출되는 과정에 PP혼합접착액이 도포되어 압출되고, PP혼합접착액이 냉각로울러에 의해서 압출온도와 상대적으로 낮은 저온으로 냉각되게 하여 젤 상태이면서 저온 상태의 PP혼합접착제가 형성되게 하고, 저온 상태의 PP혼합접착제가 피착 된 압출시트지와 이종시트지가 겹치도록 한쌍의 가압로울러 사이를 연속으로 통과되게 하여 저온 상태의 PP혼합접착제에 이종시트지가 가압되게 접착되어 저온합지시트가 제조되도록 이루어지는 저온합지시트제조방법을 그 특징으로 한다.In the present invention, a PP mixed adhesive liquid is applied and extruded in the process of extruding an extruded sheet in an extrusion die, and the PP mixed adhesive liquid is cooled to a low temperature relatively lower than the extrusion temperature by a cooling roller, PP mixed adhesive is formed, and the extruded sheet subjected to the low temperature PP mixed adhesive is continuously passed between a pair of pressure rollers so that the extruded sheet overlaps with the dissimilar sheet, and the dissimilar sheet is pressed and bonded to the low temperature PP mixed adhesive And a low-temperature laminated sheet is produced.

상기 PP혼합접착제는 폴리프로필렌 40~45중량%와 본드 55~60중량%가 혼합되어 이루어지고, 110~120℃로 냉각되어 이종시트지가 접착되도록 하는 것을 다른 특징으로 한다.The PP mixed adhesive is formed by mixing 40 to 45% by weight of polypropylene with 55 to 60% by weight of a bond, and is cooled to 110 to 120 캜 to bond the dissimilar sheet.

그리고 본 발명은 압출기와 연결되는 바디부재의 중앙에 구비되고 시트용액이 통과되는 노즐공이 있는 노즐관과, 상기 노즐관에 체결되고 노즐공과 연통되는 토출공이 있는 토출팁과, 상기 바디부재에 구비되는 PP혼합접착액공급통로와 연통되고 토출팁 일측으로 형성되는 PP혼합접착액토출로를 구비하고, 상기 PP혼합접착액토출로 외측으로 형성된 이동공간 내부에서 조절볼트에 의해 이동되는 접착액두께조절부재와, 장공을 관통하는 고정볼트에 의해 접착액두께조절부재와 바디부재가 연결되도록 고정되게 하는 고정부재로 이루어지는 접착제두께조절수단을 갖도록 하거나, 또는 상기 접착액두께조절부재에 냉각수로를 더 구비하도록 하는 것 중에 어느 하나로 이루어지는 압출다이와;According to another aspect of the present invention, there is provided an extruder comprising: a nozzle tube provided at a center of a body member connected to an extruder and having a nozzle hole through which a sheet solution passes; a discharge tip having a discharge hole communicated with the nozzle hole, And a PP mixed adhesive solution discharge path communicated with the PP mixed adhesive solution supply passage and formed at one side of the discharge tip, wherein the adhesive solution thickness adjusting member, which is moved by the adjustment bolt in the movement space formed outside the PP mixed adhesive solution discharge path, And an adhesive thickness adjusting means composed of a fixing member for fixing the adhesive liquid thickness adjusting member and the body member so as to be connected by a fixing bolt passing through the long hole or having a cooling water path to the adhesive liquid thickness adjusting member An extrusion die made of any one of:

상기 토출공으로 압출되는 압출시트지에 접촉되어 가압하는 가압로울러와 압출시트지 상면에 도포된 PP혼합접착제에 접촉되어 냉각되게 하는 냉각로울러를 구비하고, 상기 가압로울러와 상대적으로 배치되는 가압로울러 사이로 저온상태로 냉각된 PP혼합접착제가 있는 압출시트지와 이종시트지가 겹치도록 통과되게 하여 PP혼합접착제에 이종시트지가 가압되어 접착되도록 구성되게 이루어지는 저온합지시트제조장치를 다른 특징으로 한다.And a cooling roller which is brought into contact with the pressurized roller which is in contact with the extruded sheet extruded by the ejection hole and which is brought into contact with the pressurized roller and the PP mixed adhesive applied on the upper surface of the extruded sheet paper to cool the pressurized roller, The present invention is characterized in that the extruded sheet having the cooled PP mixed adhesive and the dissimilar sheet are caused to pass so as to overlap each other so that the dissimilar sheet is pressed and adhered to the PP mixed adhesive.

상기 냉각로울러는, 길이방향으로 구비되어 냉매가 순환되는 냉매통로 양측에 각각 냉매공을 가진 로울러축이 있고, 상기 로울러축 외측에는 냉매공)과 연통되고 냉매관과 연결되는 출입니플이 있고, 상기 로울러축과 출입니플을 지지하는 사각수평이동부재가 기대의 이동공 내에서 조절실린더에 의해 이동 가능하도록 구성되고, 상기 냉각로울러 외주면이 평면을 이루게 하거나 또는 다수의 미세요홈부와 미세돌기부를 갖도록 하는 것 중에 어느 하나로 구성되게 이루어지는 것을 다른 특징으로 한다.Wherein the cooling roller has a roller shaft having a refrigerant hole on both sides of the refrigerant passage provided in the longitudinal direction and circulating the refrigerant, an outlet nipple communicating with the refrigerant hole on the outer side of the roller shaft and connected to the refrigerant pipe, A rectangular horizontally moving member for supporting a roller shaft and an outlet nipple is configured to be movable by a regulating cylinder in a moving hole of a base and the outer peripheral surface of the cooling roller is made flat or has a plurality of fine groove portions and fine projections The present invention is not limited thereto.

그리고 본 발명은 상기 저온합지시트제조방법이나 장치에 의해 제조되는 저온합지시트를 또 다른 특징으로 한다.Further, the present invention is characterized in that the low-temperature laminated sheet produced by the method or apparatus for producing a low-temperature laminated sheet is further characterized.

본 발명은 압출다이를 통해 압출시트지가 토출될 때 압출시트지 상면부에 압출시트지의 압출온도 보다 상대적으로 낮은 온도의 PP혼합접착액이 도포되므로 압출다이의 토출공 끝단부 온도가 과도하게 상승 되지 않게 되므로 압출시트지가 일부 타서 발생되는 카본이 발생 되지 않게 되므로 양질의 제품을 얻을 수 있게 되고 지속적인 양산이 가능하게 되는 효과가 있을 뿐만 아니라 불량 감소가 되는 효과가 있다.Since the PP mixed adhesive liquid having a temperature lower than the extrusion temperature of the extruded sheet is applied to the upper surface of the extruded sheet when the extruded sheet is discharged through the extruded die, the temperature of the extruded sheet is not excessively increased So that the carbon produced from a part of the extruded sheet is not generated, so that a high-quality product can be obtained, the continuous mass production is possible, and the defect is reduced.

그리고 불량시트가 발생 되면 압출시트지와 이종시트지가 녹아서 융착 된 것이 아니고 접착된 것이기 때문에 압출시트지로부터 이종시트지를 떼어내어서 분리시킬 수 있기 때문에 분리된 압출시트지 및 이종시트지를 재활용할 수 있게 되는 효과가 있는 것이다.In addition, since the extruded sheet and the dissimilar sheet are melted and adhered rather than fused, when the defective sheet is generated, the separated sheet can be separated from the extruded sheet and can be separated, so that the separated extruded sheet and the different sheet can be recycled It is.

도 1은 본 발명에 따른 일실시예의 제조 과정도,
도 2는 본 발명에 따른 일실시예의 압출다이의 종단면 구성도,
도 3은 본 발명에 따른 접착제두께조절수단의 구성도,
도 4는 본 발명에 따른 냉각로울러의 전체 구성도,
도 5는 본 발명에 따른 냉각로울러의 일부 단면 구성도,
도 6은 본 발명에 따른 압출다이의 다른 실시예의 종단면 구성도,
도 7은 본 발명에 따른 다른 냉각 및 접착 과정을 설명하는 제조과정도,
도 8은 본 발명에 따른 또 다른 냉각 및 접착 과정을 설명하는 제조과정도,
도 9는 본 발명의 냉각로울러의 다른 실시 구성도,
도 10의 (a),(b)는 도 9에 나타낸 냉각로울러 실시에 의한 접착상태를 나타낸 설명도이다.
1 is a diagram illustrating a manufacturing process of an embodiment according to the present invention,
2 is a longitudinal sectional view of an extrusion die according to an embodiment of the present invention,
3 is a structural view of an adhesive thickness adjusting means according to the present invention,
Fig. 4 is an overall configuration diagram of a cooling roller according to the present invention,
5 is a partial cross-sectional view of a cooling roller according to the present invention,
6 is a longitudinal sectional view of another embodiment of the extrusion die according to the present invention,
7 is a manufacturing process diagram illustrating another cooling and bonding process according to the present invention,
8 is a manufacturing process diagram illustrating another cooling and bonding process according to the present invention.
9 is a diagram showing another embodiment of the cooling roller of the present invention,
Figs. 10 (a) and 10 (b) are explanatory diagrams showing the state of adhesion by the cooling roller implementation shown in Fig. 9. Fig.

본 발명을 첨부된 바람직한 실시 도면에 의거하여 보다 상세히 설명하면 다음과 같다.DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS The present invention will be described in more detail with reference to the accompanying drawings.

도 1을 참조하면, 본 발명은 압출기(H,H')와 연결되는 압출다이(10)를 구비한다.Referring to FIG. 1, the present invention includes an extrusion die 10 connected to extruders H and H '.

상기 압출다이(10)는, 도 2에 나타낸 바와 같이 압출기(H,H')와 연결되는 바디부재(11)의 중앙에 구비되고 시트용액(1a)이 통과되는 노즐공(121)이 있는 노즐관(12)을 구비한다.2, the extrusion die 10 is provided with a nozzle hole 121 provided at the center of the body member 11 connected to the extruder H and H 'and having a nozzle hole 121 through which the sheet solution 1a passes, And a pipe (12).

또한, 상기 노즐관(12)에 체결되고 노즐공(121)과 연통되는 토출공(131)이 있는 토출팁(13)을 구비하고, 상기 바디부재(11)에 구비되는 PP혼합접착액공급통로(14)와 연통되고 토출팁(13) 일측으로 형성되는 PP혼합접착액토출로(152)를 구비한다.And a discharge tip 13 having a discharge hole 131 connected to the nozzle hole 121 and communicating with the nozzle hole 121. The PP mixed adhesive solution supply passage And a PP mixed adhesive solution discharge path (152) communicating with the discharge tip (14) and formed at one side of the discharge tip (13).

또한, 상기 PP혼합접착액토출로(152) 외측으로 형성된 이동공간(153) 내부에서 도 2 및 도 3에 나타낸 바와 같이 조절볼트(154)에 의해 이동되는 접착액두께조절부재(151) 및 장공(156)을 관통하는 고정볼트(157)에 의해 접착액두께조절부재(151)와 바디부재(11)가 연결되도록 고정되게 하는 고정부재(155)로 이루어지는 접착제두께조절수단(15)을 갖도록 구성된다.2 and 3, inside the moving space 153 formed outside the PP mixed adhesive solution discharging path 152, there are provided an adhesive liquid thickness adjusting member 151 which is moved by the adjusting bolt 154, (15) composed of a fixing member (155) for fixing the adhesive liquid thickness adjusting member (151) and the body member (11) by a fixing bolt (157) do.

따라서, 고정볼트(157)를 풀은 상태에서 조절볼트(154)를 풀거나 아니면 반대로 조이게 되면 접착액두께조절부재(151)가 상부방향 또는 하부방향으로 이동시킬 수 있게 됨으로써 PP혼합접착액토출로(152)가 넓어지거나 또는 반대로 좁아지도록 조절됨에 따라 PP혼합접착제(2)의 두께가 조절되는 것이다.Therefore, if the adjusting bolt 154 is loosened or otherwise tightened in the state where the fixing bolt 157 is being pulled, the adhesive liquid thickness adjusting member 151 can move upward or downward, The thickness of the PP mixed adhesive 2 is adjusted as the thickness of the adhesive 152 is adjusted to be widened or narrowed.

그리고 조절이 완료된 후에는 다시 고정볼트(157)를 조이게 되면 고정부재(155)에 의해서 접착액두께조절부재(151)가 고정되는 상태가 되는 것이다.After the adjustment is completed, the fixing bolt (157) is tightened again, and the fixing member (155) fixes the adhesive liquid thickness adjusting member (151).

따라서, 노즐공(121)과 토출공(131)을 통해서 시트용액(1a)이 압출되고, PP혼합접착액토출로(152)를 통해서는 PP혼합접착액(2a)이 압출되는 상태가 됨으로써 압출다이(10)로부터 압출된 상태가 되면 압출시트지(1) 상면부에 PP혼합접착제(2)가 도포되는 상태가 된다.Therefore, the sheet solution 1a is extruded through the nozzle hole 121 and the discharge hole 131, and the PP mixed adhesive liquid 2a is extruded through the PP mixed adhesive solution discharge path 152, The PP mixed adhesive 2 is applied to the upper surface of the extruded sheet 1 when the extruded sheet 1 is extruded from the die 10.

PP혼합접착제(2)는, 폴리프로필렌(polypropylene,약어:PP) 40~45중량%, 본드 55~60중량%가 혼합되어 이루어진 것으로서, 폴리프로필렌은 밀도가 작아서 본드와 잘 혼합되고, 가열된 상태에서는 액 상태가 되므로 압출다이(10) 내에서 이동이 가능하다. 상기 폴리프로필렌은 본 발명에서 PP(약어)로도 설명하기도 한다.The PP mixed adhesive 2 is a mixture of 40 to 45% by weight of polypropylene (abbreviation: PP) and 55 to 60% by weight of a bond. The polypropylene has a low density and is well mixed with the bond, It is possible to move in the extrusion die 10. The polypropylene may also be referred to as PP (abbreviation) in the present invention.

따라서, 본 발명은 압출다이(10)의 토출공(131)으로 압출되는 압출시트지(1)에 접촉되어 가압하는 가압로울러(20) 및 압출시트지(1) 상면에 도포된 PP혼합접착제(2)에 접촉되어 냉각되게 하는 냉각로울러(30)를 구비한다.Therefore, the present invention is characterized in that the pressure roller 20 which is in contact with the extruded sheet 1 to be extruded by the discharge hole 131 of the extrusion die 10 and the PP mixed adhesive 2 applied on the upper surface of the extruded sheet 1, And a cooling roller (30) for allowing the cooling roller (30) to cool.

도 4 및 도 5를 참조하면, 가압로울러(20)는 기대(50)에 고정되는 베어링보스(22)에 로울러축(21)이 지지되어 회동 가능하도록 구성된다.4 and 5, the pressure roller 20 is configured such that the roller shaft 21 is supported by the bearing boss 22 fixed to the base 50 and is rotatable.

상기 가압로울러(20)는 감속모터(23) 동력에 의해서 회전되도록 구성되고, 가압로울러(20)와 대향 되는 냉각로울러(30)도 감속모터(미도시됨) 동력이 체인기어(322)로 전달되게 하여 구동되도록 할 수도 있다.The pressure roller 20 is configured to rotate by the power of the deceleration motor 23 and the cooling roller 30 opposed to the pressure roller 20 is also transmitted to the chain gear 322 through a deceleration motor To be driven.

냉각로울러(30)는, 길이방향으로 구비되어 냉매가 순환되는 냉매통로(31) 양측에 각각 냉매공(321)을 가진 로울러축(32)이 있다.The cooling roller 30 has a roller shaft 32 having a refrigerant hole 321 on both sides of the refrigerant passage 31 in which the refrigerant is circulated.

또한, 상기 로울러축(32) 외측에는 냉매공(321)과 연통되고 냉매관(391)과 연결되는 출입니플(35)이 있다. 부호 33은 베어링이고, 부호 34는 누수 방지를 위한 패킹을 나타낸다.An outlet nipple 35 communicating with the refrigerant hole 321 and connected to the refrigerant pipe 391 is disposed outside the roller shaft 32. Reference numeral 33 denotes a bearing, and reference numeral 34 denotes a packing for preventing leakage.

냉각로울러(30) 양측에 있는 출입니플(35)에는 냉매관(391)에 의해 냉각유니트(39)과 연결된다. 상기 냉각유니트(39)는 냉매 온도를 낮추는 장치로서 이미 알려진 것이므로 상세한 설명과 도면은 생략한다.The inlet and outlet nipples 35 on both sides of the cooling roller 30 are connected to the cooling unit 39 by a refrigerant pipe 391. The cooling unit 39 is already known as a device for lowering the temperature of refrigerant, so that detailed description and drawings are omitted.

따라서, 냉각로울러(30)의 냉매통로(31)에 있는 냉매가 냉각유니트(39)에서 냉각된 상태가 되어 다시 냉매통로(31)로 유입되는 순환작용이 지속 된다.Therefore, the circulation operation in which the refrigerant in the refrigerant passage 31 of the cooling roller 30 is cooled by the cooling unit 39 and then flows into the refrigerant passage 31 is continued.

한편, 본 발명은 로울러축(32)과 출입니플(35)을 지지하는 사각수평이동부재(36)가 기대(50)의 이동공(37) 내에서 조절실린더(38)에 의해 이동 가능하도록 구성된다. The present invention is configured such that the rectangular horizontal moving member 36 supporting the roller shaft 32 and the entry and exit nipple 35 can be moved by the adjusting cylinder 38 in the moving hole 37 of the base 50 do.

그러므로 조절실린더(38)에 의해서 냉각로울러(30)가 이동되어 가압로울러(20)와의 이격 된 간격을 크게 또는 작게 조절할 수 있게 되고, 그로 인해 접착제(2)가 도포된 압출시트지(1) 두께에 따라 가압로울러(20)와 냉각로울러(30)의 간격을 조절하게 되는 것이다.Therefore, the cooling roller 30 can be moved by the adjusting cylinder 38 to adjust the spacing between the pressing roller 20 and the pressing roller 20 to be large or small so that the thickness of the extruded sheet 1 coated with the adhesive 2 The distance between the pressurizing roller 20 and the cooling roller 30 is adjusted.

본 발명은 압출다이(10)에서 압출되는 압출시트지(1) 상면부에 PP혼합접착제(2)가 도포된 상태에서 도 1에 나타낸 바와 같이 가압로울러(20)와 냉각로울러(30) 사이를 통과하게 됨으로써 PP혼합접착제(2)가 냉각되는 상태가 된다.The present invention is characterized in that the PP mixed adhesive 2 is applied on the upper face of the extruded sheet 1 to be extruded in the extrusion die 10 and passes through between the pressurizing roller 20 and the cooling roller 30 So that the PP mixed adhesive 2 is cooled.

압출시트지(1)는 압출기(H)에서 녹아서 압출될 수 있는 수지재질의 압출시트지(1)로서, 주로 1mm 이하의 두께를 갖는 것이 압출되고, PP혼합접착제(2)는 그 보다 얇은 두께를 갖게 된다.The extruded sheet 1 is an extruded sheet 1 made of a resin material which can be melted and extruded in an extruder H and is mainly extruded to have a thickness of 1 mm or less and the PP mixed adhesive 2 has a thickness do.

그러므로 PP혼합접착제(2)에 냉각로울러(30)가 접촉되면 PP혼합접착제(2)가 냉각되는 상태가 되므로 냉각로울러(30)를 통과한 상태에서는 젤 상태와 같은 상태가 된다.Therefore, when the cooling roller 30 is brought into contact with the PP mixed adhesive 2, the PP mixed adhesive 2 is in a state of being cooled, and therefore, the state is the same as that of the gel state when passing through the cooling roller 30.

따라서, 본 발명은 가압로울러(20)와 상대적으로 배치되는 가압로울러(40) 사이로 저온상태로 냉각된 PP혼합접착제(2)가 있는 압출시트지(1)와 이종시트지(3)가 겹치도록 통과되게 하여 PP혼합접착제(2)에 이종시트지(3)가 가압되어 접착되도록 구성된다. Therefore, the present invention is characterized in that the extruded sheet 1 having the PP mixed adhesive 2 cooled to a low temperature state between the pressurizing rollers 40 disposed relatively to the pressurizing roller 20 is passed through the overlapped sheet 3 in an overlapping manner So that the dissimilar sheet 3 is pressed and adhered to the PP mixed adhesive 2.

상기 이종시트지(3)는 필름이나 부직포일 수 있는 것으로서, 이종시트지롤(3a)에서 풀림되어 한쌍의 가압로울러(20,40) 사이로 끼워져 들어가면서 저온상태로 냉각된 PP혼합접착제(2)에 접착되는 상태가 됨에 따라 압출시트지(1)와 이종시트지(3)가 접착된 상태의 저온합지시트(123)가 제조되는 것이다. 부호 R은 가이드롤러이고, 부호 123a는 합지시트롤을 나타낸다.The dissimilar sheet 3 may be a film or a nonwoven fabric. The dissimilar sheet 3 may be a film or a nonwoven fabric. The dissimilar sheet 3 may be a film or a nonwoven fabric. The dissimilar sheet 3 is bonded to a PP mixed adhesive 2, The state that the extrusion sheet 1 and the heterogeneous sheet 3 are adhered to each other is produced. Reference symbol R denotes a guide roller, and reference numeral 123a denotes a trolley upon jointing.

즉, 본 발명은 압출다이(10)에서 압출시트지(1)가 압출되는 과정에 PP혼합접착액(2a)이 도포되어 압출되고, 그 이후에 냉각로울러(30)에 의해서 PP혼합접착액(2a)이 압출온도와 상대적으로 낮은 저온으로 냉각되게 하여 젤 상태의 저온 상태의 PP혼합접착제(2)가 형성되게 하고, 저온 상태의 PP혼합접착제(2)가 피착된 압출시트지(1)와 이종시트지(3)가 겹치도록 한쌍의 가압로울러(20,40) 사이를 통과되게 하여 저온 상태의 PP혼합접착제(2)에 이종시트지(3)가 가압되게 접착되어 하나의 저온합지시트(123)가 제조되는 것에 특징이 있는 것이다.That is, in the present invention, the PP mixed adhesive liquid 2a is applied and extruded in the process of extruding the extruded sheet 1 in the extruding die 10, and thereafter the PP mixed adhesive liquid 2a Is cooled to a low temperature relatively lower than the extrusion temperature to form a gel-state low-temperature PP mixed adhesive (2), and the extruded sheet (1) coated with the low-temperature PP mixed adhesive (2) The different kind of sheet 3 is pressed and adhered to the low-temperature PP mixed adhesive 2 so as to pass between the pair of pressure rollers 20 and 40 so as to overlap with each other, It is characterized by becoming.

한편, 압출온도와 상대적으로 낮은 저온으로 PP혼합접착제(2)를 냉각시켜서 이종시트지(3)가 접착되게 한 것이므로 저온상태의 PP혼합접착제(2)에 의해 합지되었다는 의미이므로 이해를 돕기 위해서 본 발명에서 얻어지는 합지를 저온합지시트(123)라고 명칭 하는 것으로 하고 설명되었다.On the other hand, since the PP mixed adhesive 2 is cooled at a low temperature relatively lower than the extrusion temperature to bond the different sheet 3, it means that the PP mixed adhesive 2 is laminated at a low temperature. Is referred to as a low-temperature laminated sheet 123. The low-

PP혼합접착제(2)의 성분혼합비율을 조절하면서 1mm 두께의 압출시트지(1)로서 PP시트지가 압출되게 하되 압출다이(10)의 압출온도 260℃로 압출하면서 PP혼합접착액(2a)을 냉각로울러(30)에 의해 압출온도와 상대적으로 저온 상태가 되도록 냉각시켜 저온 상태의 PP혼합접착제(2)가 되게 하여 이종시트지(3)로서 0.5mm 두께의 PP필름이 접착되게 하는 실험을 실시하였고, 또한 이들을 상호 분리되게 하는 실험을 [표 1]과 같이 실시하였다.The PP mixed adhesive liquid 2a was cooled while extruding the PP sheet as the extruded sheet 1 having a thickness of 1 mm while controlling the component mixing ratio of the PP mixed adhesive 2, The rollers 30 were cooled so as to be in a relatively low temperature state relative to the extrusion temperature to make the PP mixed adhesive 2 in the low temperature state to adhere the PP film having a thickness of 0.5 mm as the different sheet 3, Experiments to separate them were carried out as in [Table 1].

kg당
PP혼합접착제혼합비율(%)
per kg
PP Mixing Adhesive Mixing Ratio (%)

압출온도(℃)

Extrusion temperature (캜)
냉각된
온도(℃)
Cooled
Temperature (℃)

접착성

Adhesiveness

분리성(박리)

Separation (peeling)
PP     PP 본드    bond 25     25 75    75 260    260 150    150 우수    Great 매우 나쁨 Very bad 30     30 70    70 260    260 140    140 우수    Great 나쁨    Poor 35     35 65    65 260    260 130    130 양호    Good 저조    Low 40     40 60    60 260    260 120    120 양호    Good 비교적 양호 Relatively good 45     45 55    55 260    260 110    110 양호    Good 매우 양호 Very good 50     50 50    50 260    260 100    100 불량    Bad 좋음    good

상기 [표 1]에 의하면 PP혼합접착제(2)는 폴리프로필렌 40~45중량%, 본드 55~60중량%가 혼합되어 이루어진 것이 접착성도 양호하고 접착된 압출시트지(1)와 이종시트지(3)를 서로 분리하는데 용이한 것으로 나타났으며, PP혼합접착제(2)를 110~120℃로 냉각시켜서 이종시트지(3)가 접착되게 하는 것이 양호한 것으로 나타났다.According to the above Table 1, the PP mixed adhesive 2 is formed by mixing 40 to 45% by weight of polypropylene and 55 to 60% by weight of a bond. The result is that the extruded sheet 1 and the heterogeneous sheet 3, And it was found that it was preferable to cool the PP mixed adhesive 2 to 110 to 120 ° C to bond the heterogeneous sheet 3 to each other.

한편, 본 발명은 도 6에 나타낸 바와 같이 접착액두께조절부재(151)에 냉각수로(158)를 구비하도록 실시될 수 있다.6, the present invention can be implemented to include a cooling water path 158 in the adhesive liquid thickness control member 151. [

이 경우 압출다이(10)의 다른 구성은 이미 [실시예 1]와 동일한 것이므로 여기서의 상세한 설명은 생략하는 것으로 한다.In this case, the other structure of the extrusion die 10 is the same as that of the first embodiment, and a detailed description thereof will be omitted.

상기 냉각수로(158)은 냉각유니트(미도시됨)와 연결되는 것이므로 냉각수(W)가 순환되는 것이다.Since the cooling water path 158 is connected to a cooling unit (not shown), the cooling water W circulates.

따라서, 본 발명은 PP혼합접착액토출로(152)를 따라 토출되는 PP혼합접착액(2a)을 냉각시키게 되므로 압출시트지(1)에 도포되어 압출되는 PP혼합접착액(2a)을 더욱 신속하게 냉각시킬 수 있게 된다.Therefore, the present invention cools the PP mixed adhesive liquid 2a ejected along the PP mixed adhesive liquid ejection path 152, so that the PP mixed adhesive liquid 2a applied to the extruded sheet 1 and extruded can be ejected more rapidly Thereby allowing cooling.

그리고 도 7에 나타낸 바와 같이 PP혼합접착제(2)가 피착된 압출시트지(1)가 또 다시 냉각로울러(30)와 가압로울러(20) 사이를 통과되게 하여 2차적으로 PP혼합접착제(2)의 냉각작용이 도모되게 할 수 있다.7, the extruded sheet 1 on which the PP mixed adhesive 2 is adhered is again passed between the cooling roller 30 and the pressurizing roller 20, So that the cooling action can be promoted.

또한, 경우에 따라서는 PP혼합접착제(2)가 피착된 압출시트지(1)가 또 다시 냉각로울러(30)와 냉각로울러(30) 사이를 통과되게 하여 2차적으로 PP혼합접착제(2)의 냉각작용이 도모되게 할 수도 있는 것으로서, 더욱 확실한 PP혼합접착제(2) 냉각 작용이 도모되도록 할 수 있고, PP혼합접착제(2)가 냉각되는 온도를 정확성 있게 냉각시킬 수 있게 된다.In some cases, the extruded sheet 1 on which the PP mixed adhesive 2 is adhered is again passed between the cooling rollers 30 and the cooling rollers 30 to cool the PP mixed adhesive 2 As a result, the more reliable function of cooling the PP mixed adhesive 2 can be achieved, and the temperature at which the PP mixed adhesive 2 is cooled can be cooled accurately.

물론, 도 7에 나타낸 실시상태는 접착액두께조절부재(151)에 냉각수로(158)를 구비하지 않는 상태에서도 실시 가능하다.Of course, the embodiment shown in Fig. 7 can be implemented without providing the cooling water passage 158 in the adhesive liquid thickness adjusting member 151. Fig.

또한, 본 발명은 도 8에 나타낸 바와 같이 PP혼합접착제(2)가 피착된 압출시트지(1)가 한쌍의 냉각로울러(30) 사이를 통과되게 하여 PP혼합접착제(2)의 냉각작용이 이루어지게 한 후에 이종시트지(3)가 끼워지게 통과하게 되는 로울러도 냉각로울러(30)로 이루어지게 함으로써 더욱 효율적인 냉각 작용과 가압작용이 동시에 이루어지게 할 수도 있는 것이다.8, the extruded sheet 1 on which the PP mixed adhesive 2 is adhered is allowed to pass between the pair of cooling rollers 30 so that the cooling action of the PP mixed adhesive 2 is performed And the cooling rollers 30 that pass through the different kind of sheet paper 3 after they are passed through the cooling rollers 30 can be made to perform the cooling operation and the pressing action more efficiently at the same time.

본 발명에 실시되는 냉각로울러(30)는 도 9에 나타낸 바와 같이 외주면에 다수의 미세요홈부(30a)와 미세돌기부(30b)를 갖도록 실시될 수 있다.The cooling roller 30 according to the present invention can be implemented to have a plurality of fine groove portions 30a and fine protrusions 30b on the outer circumferential surface as shown in FIG.

이 경우에는 냉각로울러(30)에 의해서 PP혼합접착제(2)가 냉각되는 동시에 그 PP혼합접착제(2) 표면에 도 10의 (a)에 나타낸 바와 같이 요홈부(2b) 및 요철부(2c)가 형성되는 상태가 된다.In this case, the PP mixed adhesive 2 is cooled by the cooling roller 30 and the recessed portion 2b and the recessed portion 2c are formed on the surface of the PP mixed adhesive 2 as shown in Fig. 10 (a) Is formed.

그러므로 이종시트지(3)가 가압로울러(40)에 의해 PP혼합접착제(2) 표면에 가압되는 상태가 되면 도 10의 (b)에 나타낸 바와 같이 요철부(2c)가 눌리게 되면서 양 옆방향으로 퍼지게 되면서 이종시트지(3)가 접착되는 상태가 되고, 그로 인해 이종시트지(3)와 PP혼합접착제(2) 사이에는 매우 작은 공간 상태의 요홈부(2b)가 존재하는 상태가 된다.Therefore, when the sheet 3 of different kind is pressed by the pressure roller 40 to the surface of the PP mixed adhesive 2, as shown in Fig. 10 (b), the recessed / concave portions 2c are pressed, So that the heterogeneous sheet 3 is adhered to the adhesive layer 3 and the space 2b having a very small space is present between the dissimilar sheet 3 and the PP mixed adhesive 2. As a result,

그러므로 압출시트지(1)와 이종시트지(3)를 분리시킬 때에는 요홈부(2b) 부분이 접착되지 않은 상태이므로 접착면적이 적어서 보다 수월하게 분리시킬 수 있게 되는 것이다.Therefore, when separating the extruded sheet 1 and the dissimilar sheet 3 from each other, the portion of the recessed portion 2b is not adhered, so that the adhesive area is small and it can be separated more easily.

본 발명의 이해를 돕기 위해 접착제에 의해서만으로 접착되게 할 시에는 접착강도가 높아서 압출시트지(1)와 이종시트지(3)를 분리시킬 수 없거나 매우 어려우나, 본 발명은 PP혼합접착제(2)의 PP성분의 접착력이 비교적 낮으므로 이종시트지(3)를 압출시트지(1)로부터 분리시킬 수 있게 되는 것이고, 이종시트지(3)가 접착된 상태에서 요홈부(2b) 부분이 접착되지 않은 상태이므로 더욱 수월하게 분리시킬 수 있게 되는 것이다In order to facilitate understanding of the present invention, it is difficult or impossible to separate the extruded sheet 1 and the heterogeneous sheet 3 due to the high adhesive strength, but the present invention can be applied to the PP mixed adhesive 2 (PP) It is possible to separate the different sheet 3 from the extruded sheet 1 because the adhesive force of the component is relatively low and the portion of the recessed portion 2b is not adhered in the state where the different sheet 3 is adhered, As shown in Fig.

따라서, 본 발명은 압출다이(10)를 통해 압출시트지(1)가 토출될 때 압출시트지(1) 상면부에 그 압출시트지(1)의 압출온도 보다 상대적으로 낮은 온도의 PP혼합접착액이 도포되므로 압출다이(10)의 토출공 끝단부 온도가 과도하게 상승 되지 않게 되므로 압출시트지(1)가 일부 타서 발생되는 카본이 발생 되지 않게 되므로 양질의 제품을 얻을 수 있게 되고 지속적인 양산이 가능하게 되고, 그로 인해 불량 감소가 도모 되는 것이다.Therefore, the present invention is characterized in that, when the extruded sheet 1 is discharged through the extrusion die 10, a PP mixed adhesive liquid having a temperature lower than the extrusion temperature of the extruded sheet 1 is applied to the upper surface of the extruded sheet 1 The temperature of the end of the discharge hole of the extrusion die 10 is not excessively increased. As a result, carbon produced from a part of the extruded sheet 1 is not generated, so that a good quality product can be obtained and continuous mass production becomes possible, Thereby reducing defects.

그리고 불량시트가 발생 되면 압출시트지와 이종시트지가 녹아서 융착 된 것이 아니고 분리 가능하게 접착된 것이기 때문에 압출시트지로부터 이종시트지를 떼어내어서 분리시킬 수 있기 때문에 분리된 압출시트지 및 이종시트지를 재활용할 수 있게 되는 것이다.Since the extruded sheet and the dissimilar sheet are melted and not fused and detachably adhered to each other when the defective sheet is generated, the separated sheet can be separated from the extruded sheet and can be separated, so that the separated extruded sheet and the heterogeneous sheet can be recycled .

본 발명은 도면으로 도시되고 설명된 것에 반드시 국한되는 것은 아니고 본 발명이 속하는 기술분야의 통상의 지식을 가진 자에 의해서 여러 가지 형태로 변형 실시될 수 있는 것이므로 청구범위를 크게 벗어나지 않는 한 폭넓게 보호되어야 하는 것은 자명한 것이다.It is to be understood that the invention is not limited to the details shown and described herein, and that various changes and modifications may be made without departing from the scope of the invention as broadly defined by the person skilled in the art. It is self-evident.

1:압출시트지 1a:시트용액
2:PP혼합접착제 2a:PP혼합접착액
2b:요홈부 2c:요철부
3:이종시트지 3a:이종시트지롤
123:저온합지시트 123a:합지시트롤
10:압출다이 11:바디부재
12:노즐관 121:노줄공
13:토출팁 131:토출공
14:PP혼합접착액공급통로 15:접착제두께조절수단
151:접착액두께조절부재 152:접착액토출로
153:이동공간 154:조절볼트
155:고정부재 156:장공
157:고정볼트 158:냉각수로
20:가압로울러 21:로울러축
22:베어링보스 23:감속모터
30:냉각로울러 30a:미세요홈부
30b:미세요철부 31:냉매통로
32:로울러축 321:냉매공
33:베어링 34:패킹
35:출입니플 36:사각수평이동부재
37:이동공 38:조절실린더
39:냉각유니트 391:냉매관
40:가압로울러 50:기대
1: extruded sheet 1a: sheet solution
2: PP mixed adhesive 2a: PP mixed adhesive liquid
2b: recessed portion 2c: concave and convex portion
3: heterogeneous sheet 3a: heterogeneous sheet roll
123: Low temperature laminate sheet 123a:
10: extrusion die 11: body member
12: Nozzle tube 121:
13: Discharge tip 131: Discharge ball
14: PP mixed adhesive liquid supply passage 15: adhesive thickness adjusting means
151: Adhesive liquid thickness controlling member 152: Adhesive liquid discharging line
153: moving space 154: adjusting bolt
155: Fixing member 156: Long hole
157: Fixing bolt 158: With cooling water
20: pressure roller 21: roller shaft
22: Bearing boss 23: Deceleration motor
30: cooling roller 30a:
30b: not pushed forward 31: refrigerant passage
32: Roller shaft 321:
33: Bearing 34: Packing
35: entry / exit nipple 36: rectangular horizontal moving member
37: moving ball 38: regulating cylinder
39: cooling unit 391: refrigerant tube
40: pressure roller 50: expectation

Claims (5)

압출다이(10)에서 압출시트지(1)가 압출되는 과정에 PP혼합접착액(2a)이 도포되어 압출되고, PP혼합접착액(2a)이 냉각로울러(30)에 의해서 압출온도와 상대적으로 낮은 저온으로 냉각되게 하여 젤 상태이면서 저온 상태의 PP혼합접착제(2)가 형성되게 하고, 저온 상태의 PP혼합접착제(2)가 피착된 압출시트지(1)와 이종시트지(3)가 겹치도록 한쌍의 가압로울러(20,40) 사이를 연속으로 통과되게 하여 저온 상태의 PP혼합접착제(2)에 이종시트지(3)가 가압되게 접착되어 저온합지시트(123)가 제조되도록 이루어지는 것을 특징으로 하는 저온합지시트제조방법.
The PP mixed adhesive liquid 2a is applied and extruded in the process of extruding the extruded sheet 1 from the extruding die 10 and the PP mixed adhesive liquid 2a is cooled by the cooling roller 30 to a relatively low So that the PP mixed adhesive 2 in a gel state and the low temperature state is formed so that the extruded sheet 1 on which the low temperature PP mixed adhesive 2 is adhered and the dissimilar sheet 3 are overlapped with each other And the low temperature compound sheet (123) is produced by allowing the dissimilar sheet (3) to adhere to the low temperature PP mixed adhesive (2) while passing the pressure between the press rollers (20, 40) continuously. / RTI >
제 1 항에 있어서,
상기 PP혼합접착제(2)는 폴리프로필렌 40~45중량%와 본드 55~60중량%가 혼합되어 이루어지고, 110~120℃로 냉각되어 이종시트지(3)가 접착되도록 이루어지게 하는 것을 특징으로 하는 저온합지시트제조방법.
The method according to claim 1,
The PP mixed adhesive (2) is a mixture of 40 to 45% by weight of polypropylene and 55 to 60% by weight of a bond, and is cooled to 110 to 120 ° C to bond the dissimilar sheet (3) A method for manufacturing a low temperature composite sheet.
압출기(H,H')와 연결되는 바디부재(11)의 중앙에 구비되고 시트용액(1a)이 통과되는 노즐공(121)이 있는 노즐관(12)과, 상기 노즐관(12)에 체결되고 노즐공(121)과 연통되는 토출공(131)이 있는 토출팁(13)과, 상기 바디부재(11)에 구비되는 PP혼합접착액공급통로(14)와 연통되고 토출팁(13) 일측으로 형성되는 PP혼합접착액토출로(152)를 구비하고, 상기 PP혼합접착액토출로(152) 외측으로 형성된 이동공간(153) 내부에서 조절볼트(154)에 의해 이동되는 접착액두께조절부재(151)와, 장공(156)을 관통하는 고정볼트(157)에 의해 접착액두께조절부재(151)와 바디부재(11)가 연결되도록 고정되게 하는 고정부재(155)로 이루어지는 접착제두께조절수단(15)을 갖도록 하거나, 또는 접착액두께조절부재(151)에 냉각수로(158)를 더 구비하도록 하는 것 중에 어느 하나로 이루어지는 압출다이(10)와;
상기 토출공(131)으로 압출되는 압출시트지(1)에 접촉되어 가압하는 가압로울러(20)와 압출시트지(1) 상면에 도포된 PP혼합접착제(2)에 접촉되어 냉각되게 하는 냉각로울러(30)를 구비하고, 상기 가압로울러(20)와 상대적으로 배치되는 가압로울러(40) 사이로 저온상태로 냉각된 PP혼합접착제(2)가 있는 압출시트지(1)와 이종시트지(3)가 겹치도록 통과되게 하여 PP혼합접착제(2)에 이종시트지(3)가 가압되어 접착되도록 구성되게 이루어지는 것을 특징으로 하는 저온합지시트제조장치.
A nozzle tube 12 provided at the center of the body member 11 connected to the extruders H and H 'and having a nozzle hole 121 through which the sheet solution 1a passes, (13) provided with a discharge hole (13) communicating with the nozzle hole (121) and communicating with the PP mixed adhesive solution supply passage (14) provided in the body member (11) And the PP mixed adhesive solution discharging passage 152 formed in the PP mixed adhesive solution discharging passage 152 is formed in the moving space 153 formed outside the PP mixed adhesive solution discharging passage 152, And a fixing member 155 for fixing the adhesive liquid thickness adjusting member 151 and the body member 11 by means of fixing bolts 157 passing through the elongated holes 156, (15), or the adhesive liquid thickness adjusting member (151) is further provided with a cooling water path (158) (10);
A cooling roller 30 which is brought into contact with the pressurizing roller 20 which is in contact with and presses the extruded sheet 1 to be extruded by the discharge hole 131 and the PP mixed adhesive 2 applied on the upper surface of the extruded sheet 1, And the extruded sheet 1 having the PP mixed adhesive 2 cooled to a low temperature state between the pressurizing rollers 40 disposed relatively to the pressurizing roller 20 is passed So that the dissimilar sheet 3 is pressed against the PP mixed adhesive 2 so as to be adhered thereto.
제 3 항에 있어서,
상기 냉각로울러(30)는 길이방향으로 구비되어 냉매가 순환되는 냉매통로(31) 양측에 각각 냉매공(321)을 가진 로울러축(32)이 있고, 상기 로울러축(32) 외측에는 냉매공(321)과 연통되고 냉매관(391)과 연결되는 출입니플(35)이 있고, 상기 로울러축(32)과 출입니플(35)을 지지하는 사각수평이동부재(36)가 기대(50)의 이동공(37) 내에서 조절실린더(38)에 의해 이동 가능하도록 구성되고, 상기 냉각로울러(30) 외주면이 평면을 이루게 하거나 또는 다수의 미세요홈부(30a)와 미세돌기부(30b)를 갖도록 하는 것 중에 어느 하나로 구성되게 이루어지는 것을 특징으로 하는 저온합지시트제조장치.
The method of claim 3,
The cooling roller 30 is provided in the longitudinal direction and has a roller shaft 32 having refrigerant holes 321 on both sides of the refrigerant passage 31 through which the refrigerant is circulated. Outside the roller shaft 32, And a rectangular horizontally moving member 36 for supporting the roller shaft 32 and the outlet nipple 35 is connected to the refrigerant pipe 391 and connected to the refrigerant pipe 391, The cooling roller 30 is configured to be movable by the adjusting cylinder 38 in the hole 37 and the outer circumferential surface of the cooling roller 30 is made flat or has a plurality of fine groove portions 30a and fine protrusions 30b Wherein the low temperature laminate sheet is made of a single low temperature laminate sheet.
제1항 또는 제3항의 제조방법이나 장치에 의해 저온합지시트(123)가 제조되어 구성된 것을 특징으로 하는 저온합지시트제조방법과 장치를 이용한 저온합지시트.

A low temperature laminate sheet using the method and apparatus for producing a low temperature laminate sheet, characterized in that the low temperature laminate sheet (123) is manufactured by the manufacturing method or apparatus of claim 1 or 3.

KR1020160170009A 2016-12-13 2016-12-13 Method and apparatus for making a sheet adhered with an adhesive and a laminate using the same KR101933503B1 (en)