KR20100128856A - Fire prevention it bites and the frame production production frame which it bites - Google Patents

Fire prevention it bites and the frame production production frame which it bites Download PDF

Info

Publication number
KR20100128856A
KR20100128856A KR1020090047508A KR20090047508A KR20100128856A KR 20100128856 A KR20100128856 A KR 20100128856A KR 1020090047508 A KR1020090047508 A KR 1020090047508A KR 20090047508 A KR20090047508 A KR 20090047508A KR 20100128856 A KR20100128856 A KR 20100128856A
Authority
KR
South Korea
Prior art keywords
mold
bending
fire door
frame
protrusion
Prior art date
Application number
KR1020090047508A
Other languages
Korean (ko)
Inventor
김홍기
김동주
Original Assignee
엔에이취케이주식회사
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by 엔에이취케이주식회사 filed Critical 엔에이취케이주식회사
Priority to KR1020090047508A priority Critical patent/KR20100128856A/en
Publication of KR20100128856A publication Critical patent/KR20100128856A/en

Abstract

PURPOSE: A mold frame for manufacturing a fire door frame, capable of mass production regardless of the length of a metal plate is provided to independently form a metal plate curved. CONSTITUTION: A mold frame for manufacturing a fire door frame comprises a press punch(20), a lower mold(50), an upper mold(30), an intermediate mold(40) and a bend mold(60). The lower mold is installed in the lower part of the bend mold. The lower mold comprises a lower part bending groove. The lower part bending groove is corresponded to a mold bend protrusion. The upper mold is installed in the lower part of the press punch. The intermediate mold is installed in the lower part of the upper mold. The bend mold is installed in the lower part of the intermediate mold.

Description

방화문 문틀 제작용 금형틀{Fire prevention it bites and the frame production production frame which it bites}Fire prevention it bites and the frame production production frame which it bites}

본 발명은 방화문 문틀 제작용 금형틀에 관한 것으로서, 더욱 상세하게는 방화문을 구성하는 금속판을 길이에 구애 없이 절곡성형할 수 있도록 한 방화문 문틀 제작용 금형틀에 관한 것이다. The present invention relates to a metal mold for producing a fire door, and more particularly, to a metal mold for producing a fire door, so that the metal plate constituting the fire door can be bent without regard to length.

일반적으로 아파트나 상가 등의 대규모 거주건물이 증가하면서 거주공간을 외부로부터 견고하게 차단하고, 화재 등으로부터 내부거주자를 보호하기 위해서 방화문이 주로 사용된다.In general, as a large number of residential buildings such as apartments and shopping malls increase, fire doors are mainly used to block living spaces from the outside and protect internal residents from fire.

그리고 이러한 방화문을 설치하기 위해서는 방화문을 지지해주는 문틀(프레임)이 반드시 필요하다.And in order to install such a fire door is required a door frame (frame) that supports the fire door.

이때, 상기 방화문의 문틀 중 방화문의 하부를 지지하는 하부 문틀인 경우에는 외부에서 내부로 또는 내부에서 외부로 사람 등의 중량체가 지나다니게 되므로 견고해야할 뿐만 아니라 외부의 충격에도 쉽게 변형되지 않고, 녹도 슬지 않으며 중량체가 하부 문틀을 타고 내, 외부로 쉽게 이동될 수 있어야하며, 문의 밀폐를 완벽하게 하기 위해 소정의 돌출편이 형성되도록 구성되고 있다.At this time, in the case of the lower door frame of the door frame of the fire door to support the lower portion of the fire door, from the outside to the inside or from the inside to the outside of the weight, such as a person to pass, not only need to be strong, but also not easily deformed to the external impact, rust sludge In addition, the weight should be able to easily move in and out of the lower door frame, it is configured to form a predetermined protrusion to perfect the door seal.

상기와 같은 문틀을 제작하기 위한 종래의 금형틀 및 제작방법으로는 타 출원인으로 부터 선출원 된바 있는 특허등록 제10-0264526호 및 특허등록 제10-0347551호의 것이 알려져 있으며 여기서 상기 특허등록 제10-0347551호의 경우에는 금형다이 내부에 다수의 절곡부를 가진 금형을 내장하고 그 상단에 펀치프레스를 구성하여 금속판을 절곡하여 형성된다.Conventional molds and manufacturing methods for manufacturing the door frame as described above are known in the Patent Registration No. 10-0264526 and Patent Registration No. 10-0347551 that has been previously filed from other applicants, the patent registration No. 10-0347551 In the case of the arc, a metal plate is formed by embedding a metal mold having a plurality of bent portions inside the die die and forming a punch press at the upper end thereof.

그러나 이러한 금형틀은 금형구조가 매우 복잡하고 금속판의 제작시 금속판이 길어지게 되면 금형틀의 구조에 간섭을 받게 되어 금속판을 원하는 형태로 가공을 할 수 없는 문제점 있었다.However, such a mold frame has a problem that the mold structure is very complicated and the metal plate is lengthened during the manufacture of the metal plate, which causes interference with the structure of the mold frame, thereby preventing the metal plate from being processed into a desired shape.

또한, 금속판의 길이가 한정되어야만 제작할 수 있어 제작이 어려우며 이로 인해 일부만 가공하고 또 다른 일부는 별도로 가공하여 용접해야하는 문제점이 있었다.In addition, the length of the metal plate can be produced only if the length is limited, making it difficult to produce a problem because only a part of the processing and another part to be processed separately and welded.

그리고 이러한 부위별로 금속판을 가공하고 이를 용접하여 제작된 문틀이 방화문의 문틀로 이용시에는 문틀에 중량체가 지나다니면 하중에 위해 문틀이 파손 및 변형되는 문제가 발생하였으며 문틀을 보수 및 교체하는 비용이 이중으로 들어가는 문제점이 있었다.In addition, when the door frame manufactured by processing metal plate for each part and welding it is used as the door frame of fire door, the door frame is broken and deformed for the load when the weight passes through the door frame, and the cost of repairing and replacing the door frame is doubled. There was a problem entering.

본 발명은 상기와 같은 문제점을 해결하기 위하여 안출된 것으로서, 금속판의 길이에 구애 없이 방화문의 후면을 제작할 수 있을 뿐만 아니라 후면의 제작과정을 간소하여 대량 생산과 더불어 생산비를 줄일 수 있도록 하는데 그 목적이 있다. The present invention has been made to solve the above problems, it is possible not only to manufacture the back of the fire door without regard to the length of the metal plate, but also to simplify the manufacturing process of the back to reduce the mass production and production costs have.

상기와 같은 목적을 달성하기 위하여, 방화문의 제작을 위해 상부로 프레스펀치가 장착되고 상기 프레스펀치의 하부로는 절곡 형상이 형성된 하부 금형이 장착되는 방화문 문틀 제작용 금형틀에 있어서 상기 프레스펀치의 하부에 위치한 절곡돌기와 대응하는 각도를 가지는 절곡홈을 상면에 함몰형성하고 저면에는 소정의 간격을 두고 경사절곡홈과 경사면을 형성하는 상부 금형을 상기 프레스펀치의 하부에 설치하며, 상기 경사절곡홈과 경사면이 맞닿는 상면에 경사절곡돌기와 경사면을 대응되게 형성하고 저면에는 가압경사면과 함몰부를 형성하는 중간 금형을 상기 상부 금형의 하부에 설치하며, 상부에 사각형 형상의 결합부를 형성하여 상기 함몰부에 삽입장착하고, 저면에는 마름모 형상의 금형절곡돌기를 돌출형성하면서 상기 절곡 경사면과 대응하는 부분으로 절곡 경사면을 대응되게 형성하는 절곡 금형을 상기 중간 금형의 하부에 설치하고, 상기 절곡 금형의 하부에 설치되고 상면에 상기 금형절곡돌기와 대응하는 하부 절곡홈을 형성하는 하부 금형을 포함하여 이루어진 것을 특징으로 한다. In order to achieve the above object, the press punch is mounted to the top for the manufacture of the fire door and the lower mold of the fire door door frame manufacturing mold is installed in the lower die of the bent shape is mounted to the lower portion of the press punch the lower portion of the press punch The upper groove forming a bent groove having an angle corresponding to the bent protrusion located in the upper surface and forming an inclined bent groove and an inclined surface at a predetermined interval on the bottom thereof is installed in the lower portion of the press punch, and the inclined bent groove and the inclined surface An intermediate mold is formed at the lower side of the upper mold to form an inclined bent projection and an inclined surface corresponding to the upper surface of the abutment, and a pressing inclined surface and a depression are formed at the bottom of the upper mold. On the bottom surface, while forming a rhombus-shaped die bending protrusion and the bending inclined surface Including a lower mold for installing a bending die corresponding to the corresponding inclined surface formed in the lower portion of the intermediate mold, the lower mold is installed in the lower portion of the bending mold and forming a lower bending groove corresponding to the mold bending protrusion on the upper surface Characterized in that made.

본 발명에 따르면, 금속판의 길이에 구애 없이 방화문의 후면을 대량 제작 및 생산할 수 있는 효과가 있다. According to the present invention, there is an effect that can mass-produce and produce the rear surface of the fire door regardless of the length of the metal plate.

또한, 방화문의 후면 제작과정을 간소하여 생산비를 줄일 수 있는 효과가 있다. In addition, there is an effect that can reduce the production cost by simplifying the rear fabrication process of the fire door.

또한, 방화문 문틀 제작용 금형틀을 이용해서 방화문의 절곡성형과 별도로 일반적으로 사용되는 금속판을 절곡성형할 수 있는 효과가 있다. In addition, there is an effect that can be used to bend the metal plate generally used separately from the bending molding of the fire door by using a mold for manufacturing a fire door door frame.

이하, 본 발명의 구성을 첨부된 도면을 참조로 설명하면, 도 1은 본 발명에 따른 방화문 문틀 제작용 금형틀을 나타낸 구성도이다. Hereinafter, with reference to the accompanying drawings, the configuration of the present invention, Figure 1 is a block diagram showing a mold for manufacturing a fire door door frame according to the present invention.

본 발명인 방화문 문틀 제작용 금형틀(10)은 금속판(90)을 절곡하는 프레스펀치(20)와, 상기 프레스펀치(20)의 하부에 설치되고 방화문과 더불어 일반 금속판을 절곡하는 상부 금형(30)과, 상기 상부 금형(30)의 하부에 설치되고 방화문의 가장 자리 부분과 측면을 상부 금형(30)과 함께 절곡하는 중간 금형(40)과, 상기 중간 금형(40)의 하부에 장착되는 절곡 금형(60)과, 상기 절곡 금형(60)의 하부에 설치되고 가장 자리부분, 측면, 후면을 절곡 금형(60)과 함께 절곡하는 하부 금 형(50)으로 구성된다. The mold 10 for the fire door door frame of the present invention is the press punch 20 for bending the metal plate 90, the upper die 30 is installed in the lower portion of the press punch 20 and bending the general metal plate with the fire door. And an intermediate mold 40 installed at the lower portion of the upper mold 30 and bending the edge portion and side surfaces of the fire door together with the upper mold 30, and a bending mold mounted at the lower portion of the intermediate mold 40. 60 and a lower mold 50 installed at the lower portion of the bending mold 60 and bending the edge, side, and rear side together with the bending mold 60.

금속판(90)을 절곡하는 프레스펀치(20)는 금속판(90)을 절곡할 수 있도록 하부 끝단에 소정의 각도로 절곡돌기(22)를 돌출형성하되, 상기 절곡돌기(22)는 제작하고자 하는 부품에 따라 다른 경사각과 형상을 가지고 형성될 수 있다. The press punch 20 for bending the metal plate 90 protrudes the bending protrusion 22 at a predetermined angle at the lower end so that the metal plate 90 can be bent, and the bending protrusion 22 is a part to be manufactured. It can be formed with different inclination angles and shapes.

상기 프레스펀치(20)의 하부에 설치되는 상부 금형(30)은 상면(31)에 상기 프레스펀치(20)의 절곡돌기(22)와 대응하는 각도를 가지는 절곡홈(32)이 형성되고 저면(33)에는 소정의 간격을 두고 경사절곡홈(34)과 경사면(35)이 형성된다. The upper die 30, which is installed below the press punch 20, has a bending groove 32 having an angle corresponding to the bending protrusion 22 of the press punch 20 on the upper surface 31 and the bottom surface ( 33, the inclined bent groove 34 and the inclined surface 35 are formed at predetermined intervals.

여기서, 상기 절곡홈(32)은 방화문을 절곡할 뿐만 아니라 일반 금속판을 절곡하는 용도로도 사용된다. Here, the bending groove 32 is used not only to bend the fire door but also to bend a general metal plate.

또한, 상기 경사절곡홈(34)은 수직면과 경사면을 연속하여 형성되고 상기 경사면(35)은 소정의 각도를 가지고 경사지게 형성된다. In addition, the inclined bent groove 34 is formed in a vertical plane and the inclined surface in succession, the inclined surface 35 is formed to be inclined at a predetermined angle.

그리고 상기와 같이 형성되는 상부 금형(30)은 도시된 도면과 같이 다르게 구성될 수 있는데 즉, 상기 상부 금형(30)의 상부 일측을 절개하여 절개부(36)를 형성하고 상기 절개부(36)에는 끼움 돌기(73)가 형성되는 상부 보조 금형(70)을 장착한 것이다. And the upper mold 30 formed as described above may be configured differently as shown in the figure, that is, to cut the upper side of the upper mold 30 to form the cutout 36 and the cutout 36 The upper auxiliary mold 70 is fitted with a fitting protrusion 73 is formed.

여기서, 상기 상부 보조 금형(70)은 상면(71)에 프레스펀치(20)의 절곡돌기(22)와 대응하는 형상을 가진 보조 절곡홈(72)이 형성되고 내측에는 끼움 돌기(73)가 형성되어 상기 절개부(36)의 삽입부(37)에 끼움 삽입되는 것이다. Here, the upper auxiliary mold 70 has an auxiliary bending groove 72 having a shape corresponding to the bending protrusion 22 of the press punch 20 is formed on the upper surface 71 and the fitting protrusion 73 is formed inside. It is inserted into the insertion portion 37 of the cutout 36.

상기 상부 금형(30)의 하부에 설치되는 중간 금형(40)은 상기 경사절곡홈(34)과 경사면(35)이 맞닿는 상면(41)에 경사절곡돌기(42)와 경사면(43)이 대응 되게 형성되고, 저면(44)에는 소정의 각도를 가지고 가압경사면(45)이 형성되면서 상기 가압경사면(45)의 끝단 부분으로 상부를 향해 사각형 형상의 함몰부(46)가 형성된다. The intermediate mold 40 installed below the upper mold 30 has an inclined bent protrusion 42 and an inclined surface 43 on the upper surface 41 where the inclined bent groove 34 and the inclined surface 35 abut. The bottom surface 44 has a predetermined angle at which the pressure inclined surface 45 is formed, and the depression 46 having a quadrangular shape is formed toward an upper end of the pressure inclined surface 45.

여기서, 상기 가압경사면(45)은 경사절곡홈(34)과 경사절곡돌기(42)의 일차 가공을 통해 절곡된 부분을 다시 한번 가압하여 형상을 완성하게 되는 것이다. Here, the pressure inclined surface 45 is to complete the shape by pressing the bent portion once again through the primary processing of the inclined bending groove 34 and the inclined bending protrusion 42.

또한, 상기 함몰부(46)은 사각형 형상으로 상기 절곡 금형(60)이 삽입될 수 있도록 내부를 향해 소정구간 함몰형성된다. In addition, the depression 46 is formed into a predetermined section toward the inside so that the bending mold 60 can be inserted into a rectangular shape.

상기 중간 금형(40)의 하부에 장착되는 절곡 금형(60)은 상부에 사각형 형상의 결합부(61)가 돌출형성되고, 저면에는 마름모 형상의 금형절곡돌기(62)가 돌출형성되며, 절곡 경사면(43)과 대응하는 부분에는 같은 각도로 절곡 경사면(63)이 형성된다. The bending mold 60 mounted on the lower portion of the intermediate mold 40 has a rectangular coupling portion 61 protruding from the upper portion, and a die bending protrusion 62 having a rhombus shape protrudes from the bottom thereof, and has a bending slope. The inclined surface 63 bent at the same angle is formed at the portion corresponding to 43.

여기서, 상기 금형절곡돌기(62)는 45°각도로 대칭형성될 뿐만 아니라 상기 절곡 경사면(63)과 금형절곡돌기(62)도 45°각도로 대칭형성된다. Here, the mold bending protrusion 62 is not only symmetrically formed at a 45 ° angle, but also the bending slope 63 and the mold bending protrusion 62 are symmetrically formed at a 45 ° angle.

상기 절곡 금형(60)의 하부에 설치되는 하부 금형(50)은 상면(51)에 상기 금형절곡돌기(62)와 대응하는 하부 절곡홈(52)이 형성된다. The lower mold 50 installed below the bending mold 60 has a lower bending groove 52 corresponding to the mold bending protrusion 62 on the upper surface 51.

그리고 상기 하부 금형(50)의 저면에는 승, 하강 작동 및 완충을 위한 유·공압 실린더(80)가 장착된다. The lower surface of the lower mold 50 is equipped with a hydraulic and pneumatic cylinder 80 for raising, lowering and buffering.

상기와 같이 구성되는 방화문 문틀 제작용 금형틀(10)의 실시 예를 첨부된 도면을 참조로 설명하면, 도 2 내지 도 4는 본 발명에 따른 방화문 문틀 제작용 금 형틀의 작동상태와 방화문의 제작공정을 나타낸 정면도이고, 도 5는 본 발명에 따른 방화문 문틀 제작용 금형틀을 통해 제작되는 방화문을 나타낸 단면도이다. Referring to the accompanying drawings, an embodiment of a mold for manufacturing a fire door door frame is configured as described above with reference to the accompanying drawings, Figures 2 to 4 is the operation state of the fire mold door frame manufacturing frame according to the present invention and the production of a fire door Figure 5 is a front view showing the process, Figure 5 is a cross-sectional view showing a fire door to be manufactured through a mold for producing a fire door door frame according to the present invention.

먼저, 절곡돌기(22)가 형성되는 프레스펀치(20)를 설치한 후 상기 프레스펀치(20)의 하부로 상면(31)에 절곡홈(32)이 형성되고 저면(33)에는 소정의 간격을 두고 경사절곡홈(34)과 경사면(35)이 형성되는 상부 금형(30)을 설치한다. First, after installing the press punch 20 in which the bending protrusions 22 are formed, a bending groove 32 is formed in the upper surface 31 under the press punch 20 and a predetermined interval is formed in the bottom surface 33. Place the upper mold 30 is formed inclined bending groove 34 and the inclined surface 35.

이때, 상기 상부 금형(30)의 상부 일측에는 보조 절곡홈(72)이 형성되는 상부 보조 금형(70)을 설치한다. At this time, the upper auxiliary mold 70 in which the auxiliary bending groove 72 is formed on an upper side of the upper mold 30.

그리고 상기 상부 금형(30)의 하부로 상면(41)에 경사절곡돌기(42)와 경사면(43)이 형성되고 저면(44)에는 가압경사면(45)과 함몰부(46)가 형성되는 중간 금형(40)을 설치한다. An intermediate mold having an inclined bent protrusion 42 and an inclined surface 43 formed on an upper surface 41 and a lowered surface 44 having a pressure inclined surface 45 and a depression 46 formed below the upper mold 30. Install (40).

다음으로 상기 중간 금형(40)의 하부로 상부에 결합부(61)가 돌출형성되고 저면에는 마름모 형상의 금형절곡돌기(62)와 절곡 경사면(63)이 형성되는 절곡 금형(60)을 설치한다. Next, the coupling part 61 is protruded to the upper part of the lower part of the intermediate mold 40, and at the bottom, a bending mold 60 having a rhombus-shaped mold bending protrusion 62 and a bending inclined surface 63 is formed. .

이때, 상기 중간 금형(40)은 상부 금형(30)의 함몰부(46)에 결합부(61)를 끼움 삽입되어 결합되는 것이다. At this time, the intermediate mold 40 is to be coupled by inserting the coupling portion 61 to the depression 46 of the upper mold 30.

다음으로 상기 절곡 금형(60)의 하부로 상면(51)에 상기 금형절곡돌기(62)와 대응하는 하부 절곡홈(52)이 형성되고 하부에 유·공압 실린더(80)가 장착되는 하부 금형(50)을 장착하면 방화문 문틀 제작용 금형틀(10)의 조립은 완료되는 것이다. Next, a lower die (50) having a lower bending groove (52) corresponding to the mold bending protrusion (62) is formed on the upper surface (51) below the bending mold (60) and the hydraulic / pneumatic cylinder (80) is mounted on the lower portion ( When 50) is installed, the assembly of the mold frame 10 for the manufacture of a fire door door frame is completed.

상기와 같은 상태에서 방화문 문틀 제작용 금형틀(10)을 이용해서 방화문의 후면을 제작하고자 할 경우에는 다음과 같다. When the rear door of the fire door is to be manufactured using the mold 10 for the fire door door frame manufacturing in the above state, it is as follows.

먼저, 상기 상부 금형(30)과 중간 금형(40) 사이에 금속판(90)을 삽입한 후 상기 상부 금형(30)을 가압하여 금속판(90)을 절곡성형한다. (도시된 도 2)First, the metal plate 90 is inserted between the upper mold 30 and the intermediate mold 40, and then the metal plate 90 is bent by pressing the upper mold 30. (Shown in Figure 2)

이때, 상기 금속판(90)은 상부 금형(30)의 저면(33)과 중간 금형(40)의 상면(41)에 형성되는 경사절곡홈(34)과 경사절곡돌기(42)에 의해 곡면절곡부(91)가 형성되고 상기 경사면(35)과 경사면(43)에 의해 경사면(93)을 형성하게 되는 것이다. In this case, the metal plate 90 is curved by a bent groove 34 and an inclined bent protrusion 42 formed on the bottom surface 33 of the upper mold 30 and the top surface 41 of the intermediate mold 40. A 91 is formed and the inclined surface 93 is formed by the inclined surface 35 and the inclined surface 43.

그리고 상기 금속판(90)은 상기 곡면절곡부(91)와 경사면(93)은 사이에 형성되는 수평부를 통해서 측면(92)을 형성하게 되는 것이다. The metal plate 90 forms a side surface 92 through a horizontal portion formed between the curved portion 91 and the inclined surface 93.

다음으로 상기 곡면절곡부(91)와 경사면(93)이 형성되는 금속판(90)을 상기 중간 금형(40)과 하부 금형(50) 사이에 삽입한 후 중간 금형(40)을 가압하여 금속판(90)을 절곡성형한다. (도시된 도 3)Next, the metal plate 90 having the curved portion 91 and the inclined surface 93 is inserted between the intermediate mold 40 and the lower mold 50, and then pressurizes the intermediate mold 40 to form the metal plate 90. Bend). (Shown in Figure 3)

이때, 상기 금속판(90)은 상기 중간 금형(40)의 가압경사면(45)과 중간금형(60)의 절곡 경사면(63)에 의해 곡면절곡부(91)를 다시 한번 가압하여 형상을 완성하면서 금형절곡돌기(62)와 하부 절곡홈(52)에 의해 측면(92)과 경사면(93)을 90°각도로 절곡형성하게 되는 것이다.At this time, the metal plate 90 presses the curved surface 91 again by the pressure inclined surface 45 of the intermediate mold 40 and the bent inclined surface 63 of the intermediate mold 60 to complete the mold while completing the shape. The side surface 92 and the inclined surface 93 are bent at 90 ° by the bending protrusion 62 and the lower bending groove 52.

다음으로 상기 금속판(90)은 곡면절곡부(91)의 반대 방향을 상부 금형(30)의 절곡홈(32)에 삽입한 상태에서 상기 프레스펀치(20)를 가압하여 절곡돌기(22)가 금속판(90)을 절곡하여 측면 절곡부(94)를 형성하면 방화문 후면의 조립은 완료되는 것이다. (도시된 도 4)Next, the metal plate 90 presses the press punch 20 in a state in which the opposite direction of the curved portion 91 is inserted into the bending groove 32 of the upper mold 30 so that the bending protrusion 22 presses the metal plate. When the 90 is bent to form the side bent portion 94, the assembly of the rear door is completed. (Shown in Figure 4)

이때, 상기 방화문 문틀 제작용 금형틀(10)과 금속판(90)은 하부에 위치하는 유·공압 실린더(80)의 작용을 통해 충격흡수와 더불어 금속판(90)에 가해지는 충격에 따라 형상의 변형하는 것을 방지할 수 있는 것이다. At this time, the mold frame 10 for manufacturing the fire door door frame and the metal plate 90 is deformed in accordance with the impact applied to the metal plate 90 in addition to the shock absorption through the action of the oil-pneumatic cylinder 80 located in the lower portion. You can prevent that.

이와 같이 본 발명인 방화문 문틀 제작용 금형틀(10)을 통해 방화문의 후면을 간단하고 쉽게 제작할 수 있을 뿐만 아니라 대량생산에 따른 생산비를 줄일 수 있는 효과도 얻을 수 있는 것이다. Thus, through the mold frame 10 for producing a fire door door frame of the present invention can not only easily and easily produce the back of the fire door, it is also possible to obtain the effect of reducing the production cost according to mass production.

도 1은 본 발명에 따른 방화문 문틀 제작용 금형틀을 나타낸 구성도. 1 is a block diagram showing a mold for producing a fire door door frame according to the present invention.

도 2 내지 도 4는 본 발명에 따른 방화문 문틀 제작용 금형틀의 작동상태와 방화문의 제작공정을 나타낸 정면도. 2 to 4 is a front view showing the operation state of the mold frame for producing a fire door door frame according to the present invention and the manufacturing process of the fire door.

도 5는 본 발명에 따른 방화문 문틀 제작용 금형틀을 통해 제작되는 방화문을 나타낸 단면도. Figure 5 is a cross-sectional view showing a fire door manufactured through a mold for producing a fire door door frame according to the present invention.

※ 도면의 주요부분에 대한 부호의 설명. ※ Explanation of symbols for main part of drawing.

10 : 방화문 문틀 제작용 금형틀, 20 : 프레스펀치, 10: mold frame for fire door door frame, 20: press punch,

22 : 절곡돌기, 30 : 상부 금형, 22: bending protrusion, 30: upper mold,

31 : 상면, 32 : 절곡홈, 31: upper surface, 32: bending groove,

33 : 저면, 34 : 경사절곡홈, 33: bottom, 34: inclined bending groove,

35 : 경사면, 40 : 중간 금형, 35: slope, 40: middle mold,

41 : 상면, 42 : 경사절곡돌기, 41: upper surface, 42: inclined bending protrusion,

43 : 경사면, 44 : 저면, 43: slope, 44: bottom,

45 : 가압경사면, 46 : 함몰부, 45: pressurized slope, 46: depression,

50 : 하부 금형, 51 : 상면, 50: lower mold, 51: upper surface,

52 : 금형절곡돌기, 60 : 중간 금형, 52: mold bending protrusion, 60: the middle mold,

61 : 결합부, 62 : 금형절곡돌기, 61: coupling portion, 62: mold bending protrusion,

70 : 상부 보조 금형, 80 : 유·공압 실린더. 70: upper auxiliary mold, 80: hydraulic / pneumatic cylinder.

Claims (3)

방화문의 제작을 위해 상부로 프레스펀치(20)가 장착되고 상기 프레스펀치(20)의 하부로는 절곡 형상이 형성된 하부 금형(50)이 장착되는 방화문 문틀 제작용 금형틀(10)에 있어서,In the mold 10 for manufacturing a fire door door frame in which the press punch 20 is mounted to the top for the production of a fire door, and the lower mold 50 having a bent shape is mounted to the bottom of the press punch 20, 상기 프레스펀치(20)의 하부에 위치한 절곡돌기(22)와 대응하는 각도를 가지는 절곡홈(32)을 상면(31)에 함몰형성하고 저면(33)에는 소정의 간격을 두고 경사절곡홈(34)과 경사면(35)을 형성하는 상부 금형(30)을 상기 프레스펀치(20)의 하부에 설치하며, A recessed groove 32 having an angle corresponding to the bending protrusion 22 positioned below the press punch 20 is recessed on the upper surface 31 and the inclined bending groove 34 has a predetermined interval on the bottom surface 33. ) And the upper mold 30 forming the inclined surface 35 is installed below the press punch 20, 상기 경사절곡홈(34)과 경사면(35)이 맞닿는 상면(41)에 경사절곡돌기(42)와 경사면(43)을 대응되게 형성하고 저면(44)에는 가압경사면(45)과 함몰부(46)를 형성하는 중간 금형(40)을 상기 상부 금형(30)의 하부에 설치하며, The inclined bending protrusion 42 and the inclined surface 43 are formed on the upper surface 41 where the inclined bending groove 34 and the inclined surface 35 abut, and the inclined surface 45 and the depression 46 are formed on the bottom surface 44. ) Is installed in the lower portion of the upper mold 30 to form an intermediate mold 40, 상부에 사각형 형상의 결합부(61)를 형성하여 상기 함몰부(46)에 삽입장착하고, 저면에는 마름모 형상의 금형절곡돌기(62)를 돌출형성하면서 상기 절곡 경사면(43)과 대응하는 부분으로 절곡 경사면(63)을 대응되게 형성하는 절곡 금형(60)을 상기 중간 금형(40)의 하부에 설치하고, A rectangular coupling portion 61 is formed on the upper portion and inserted into the recessed portion 46, and the bottom surface is formed to correspond to the bending inclined surface 43 while protruding a die bending protrusion 62 having a rhombus shape. A bending mold 60 for forming the bending inclined surface 63 correspondingly is provided below the intermediate mold 40; 상기 절곡 금형(60)의 하부에 설치되고 상면(51)에 상기 금형절곡돌기(62)와 대응하는 하부 절곡홈(52)을 형성하는 하부 금형(50)을 포함하여 이루어진 것을 특징으로 하는 방화문 문틀 제작용 금형틀.Fire door door frame is characterized in that it comprises a lower mold 50 is installed on the lower portion of the bending mold 60 and the upper surface 51 to form a lower bending groove 52 corresponding to the mold bending protrusion 62. Mold for manufacturing. 제 1항에 있어서, The method of claim 1, 상기 상부 금형(30)의 상부 일측을 절개하여 절개부(36)를 형성하고, 상기 절개부(36)에는 상부 보조 금형(70)을 설치하되, The upper one side of the upper mold 30 is cut to form the cutout 36, and the cutout 36 is provided with an upper auxiliary mold 70, 상기 상부 보조 금형(70)은 상면(71)에 프레스펀치(20)의 절곡돌기(22)와 대응하는 보조 절곡홈(72)를 형성하고 내측 저면에 상기 상부 금형(30)에 형성되는 삽입부(37)에 끼움 고정되는 끼움 돌기(73)를 형성한 것을 특징으로 하는 방화문 문틀 제작용 금형틀.The upper auxiliary mold 70 forms an auxiliary bending groove 72 corresponding to the bending protrusion 22 of the press punch 20 on the upper surface 71 and is formed in the upper mold 30 on the inner bottom surface. A mold frame for manufacturing a fire door door frame, characterized in that a fitting protrusion (73) is formed to be fitted to the (37). 제 1항에 있어서, The method of claim 1, 상기 금형(30)의 하부에 유·공압 실린더(80)를 장착한 것을 특징으로 하는 방화문 문틀 제작용 금형틀.A mold door for manufacturing a fire door door frame, characterized in that a hydraulic / pneumatic cylinder (80) is attached to a lower portion of the mold (30).
KR1020090047508A 2009-05-29 2009-05-29 Fire prevention it bites and the frame production production frame which it bites KR20100128856A (en)