JPS5837663U - flat battery - Google Patents
flat batteryInfo
- Publication number
- JPS5837663U JPS5837663U JP13191681U JP13191681U JPS5837663U JP S5837663 U JPS5837663 U JP S5837663U JP 13191681 U JP13191681 U JP 13191681U JP 13191681 U JP13191681 U JP 13191681U JP S5837663 U JPS5837663 U JP S5837663U
- Authority
- JP
- Japan
- Prior art keywords
- ceramic
- terminal plate
- flat battery
- thermal conductivity
- thermal expansion
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Pending
Abstract
(57)【要約】本公報は電子出願前の出願データであるた
め要約のデータは記録されません。(57) [Summary] This bulletin contains application data before electronic filing, so abstract data is not recorded.
Description
第1図は従来の扁平形電池の断面図、第2図ないし第5
図は本考案の実施例に係る扁平形電池を説明するための
もので、第2図は電池組立中の状態を示す断面図、第3
図は電池組立完了の状態を示す断面図、第4図は端子板
とセラミックスとの接合状態を示す拡大断面図、第5図
はその扁平形電池に用いる陽極端子板の平面図である。
1・・・・・・陽極端子板、2・・・・・田つ材、3・
・・・・・セラミックス、4・・・・・・陽極、5・・
・・・・固体電解質層、6・・・・・・陰極、7・・・
・・・陰極端子板。Figure 1 is a cross-sectional view of a conventional flat battery, Figures 2 to 5
The figures are for explaining a flat battery according to an embodiment of the present invention, and FIG. 2 is a cross-sectional view showing the state during battery assembly, and FIG.
4 is an enlarged sectional view showing the state of bonding between the terminal plate and ceramics, and FIG. 5 is a plan view of the anode terminal plate used in the flat battery. 1... Anode terminal plate, 2... Rice wood, 3...
...Ceramics, 4...Anode, 5...
...Solid electrolyte layer, 6...Cathode, 7...
...Cathode terminal plate.
Claims (2)
電要素をリング状のセラミックス内に挿入し、そのセラ
ミックスの上方開口部および下方開口部をそれぞれ端子
板で封口して、各端子板とセラミックスとの間をロウ材
で溶着してなる扁平形電池において、前記端子板の熱膨
張係数が前記セラミックスの熱膨張係数以下で、かつ端
子板の熱伝導率がセラミックスの熱伝導率以下であるこ
とを特徴とする扁平形電池。(1) Insert a power generation element in which a cathode and an anode are stacked together via a separator into a ring-shaped ceramic, seal the upper and lower openings of the ceramic with a terminal plate, and connect each terminal plate and the ceramic. In a flat battery formed by welding the terminal plate with a brazing material, the thermal expansion coefficient of the terminal plate is less than or equal to the thermal expansion coefficient of the ceramic, and the thermal conductivity of the terminal plate is less than or equal to the thermal conductivity of the ceramic. A flat battery featuring:
記セラミックスが90%以上のアルミナを含有する緻密
構造体からなり、一方、端子板がニッケルとクロムと鉄
との合金鋼板からなり、この端子板の熱膨張係数ならび
に熱伝導率が前記セラミックスの熱膨張係数ならびに熱
伝導率とほぼ等しいことを特徴とする扁平形電池。(2) Utility model registration In claim (1), the ceramic is made of a dense structure containing 90% or more alumina, while the terminal plate is made of an alloy steel plate of nickel, chromium, and iron, A flat battery characterized in that the coefficient of thermal expansion and thermal conductivity of the terminal plate are approximately equal to the coefficient of thermal expansion and thermal conductivity of the ceramic.