JPS5778777A - Sodium-sulfur battery - Google Patents

Sodium-sulfur battery

Info

Publication number
JPS5778777A
JPS5778777A JP55154391A JP15439180A JPS5778777A JP S5778777 A JPS5778777 A JP S5778777A JP 55154391 A JP55154391 A JP 55154391A JP 15439180 A JP15439180 A JP 15439180A JP S5778777 A JPS5778777 A JP S5778777A
Authority
JP
Japan
Prior art keywords
tube
case
solid electrolyte
space
molten
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Pending
Application number
JP55154391A
Other languages
Japanese (ja)
Inventor
Hiroshi Kagawa
Takashi Nakabayashi
Sumitada Iwabuchi
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Yuasa Corp
Original Assignee
Yuasa Corp
Yuasa Battery Corp
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Yuasa Corp, Yuasa Battery Corp filed Critical Yuasa Corp
Priority to JP55154391A priority Critical patent/JPS5778777A/en
Publication of JPS5778777A publication Critical patent/JPS5778777A/en
Pending legal-status Critical Current

Abstract

PURPOSE:To secure the safety of a sodium-sulfur battery even when the solid electrolyte tube is broken by placing a double negative component, which consists of an inner case filled with Na and an outer case, inside a solid electrolyte tube so that a space is formed between the outer case and the solid electrolyte tube, and connecting the spaces of the inner and the outer cases. CONSTITUTION:Since the space between a solid electrolyte tube 1 and an outer case 13 is under reduced pressure, molten Na contained in an inner case 12 is passed through a negative terminal tube 4', is introduced from the upper hole of the tube 4' into the former space for moistening the surface of the tube 1. After that, molten Na moistening the surface of the tube 1 permeates through the tube 1 into a positive active material 8, and reacts with the material 8 to discharge electricity. When any crack or the like develops in the tube 1, the material 8 directly reacts with a negative active material 2 to generate reaction heat, which causes the outer case 13 to be broken earlier than a battery case 10. As a result, the pressure inside the case 13 and that inside the space between the tube 1 and the case 13 are equalized, and molten Na comes not to be sucked through the tube 4'. Consequently, the safety of a sodium-sulfur battery is secured by limiting the amount of the direct reaction.
JP55154391A 1980-10-31 1980-10-31 Sodium-sulfur battery Pending JPS5778777A (en)

Priority Applications (1)

Application Number Priority Date Filing Date Title
JP55154391A JPS5778777A (en) 1980-10-31 1980-10-31 Sodium-sulfur battery

Applications Claiming Priority (1)

Application Number Priority Date Filing Date Title
JP55154391A JPS5778777A (en) 1980-10-31 1980-10-31 Sodium-sulfur battery

Publications (1)

Publication Number Publication Date
JPS5778777A true JPS5778777A (en) 1982-05-17

Family

ID=15583105

Family Applications (1)

Application Number Title Priority Date Filing Date
JP55154391A Pending JPS5778777A (en) 1980-10-31 1980-10-31 Sodium-sulfur battery

Country Status (1)

Country Link
JP (1) JPS5778777A (en)

Cited By (1)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
JPS5951482A (en) * 1982-09-17 1984-03-24 Yuasa Battery Co Ltd Sodium-sulfur battery

Cited By (1)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
JPS5951482A (en) * 1982-09-17 1984-03-24 Yuasa Battery Co Ltd Sodium-sulfur battery

Similar Documents

Publication Publication Date Title
JPS5661766A (en) Pasted lead acid battery
DE3376786D1 (en) Metal halogen battery
JPS5778777A (en) Sodium-sulfur battery
GB2140967A (en) Sealed nickel-zinc cell
JPS57124866A (en) Closed type lead storage battery
JPS57174857A (en) Sealed electrochemical battery with pressure releasing vent hole
JPS5521868A (en) Enclosed lead battery
JPS56114288A (en) Sealed lead battery and its manufacture
JPS5578476A (en) Lead battery
JPS57145278A (en) Electrochemical battery including liquid sodium as cathode material
JPS5636858A (en) Sealed lead storage battery
JPS56156673A (en) Lithium solid battery
JPS5581471A (en) Air-lithium battery
JPS5778775A (en) Sealed lead battery
GB2021305A (en) Nickel oxide-hydrogen cells
JPS57162259A (en) Pasted lead battery
JPS57128466A (en) Silver dioxide battery
JPS56107473A (en) Lead acid battery
JPS5717557A (en) Sealed alkaline battery
JPS56160761A (en) Alkaline battery
JPS56114282A (en) Pasted lead acid battery
JPS5769666A (en) Battery
JPS5553060A (en) Alkaline cell
JPS5727567A (en) Manufacture of battery
JPS5723468A (en) Button-type battery