JPS5736056A - Centrifugally cast composite roll - Google Patents
Centrifugally cast composite rollInfo
- Publication number
- JPS5736056A JPS5736056A JP11118880A JP11118880A JPS5736056A JP S5736056 A JPS5736056 A JP S5736056A JP 11118880 A JP11118880 A JP 11118880A JP 11118880 A JP11118880 A JP 11118880A JP S5736056 A JPS5736056 A JP S5736056A
- Authority
- JP
- Japan
- Prior art keywords
- specified
- composition
- yields
- hardness
- composite roll
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Pending
Abstract
PURPOSE:To obtain a roll which is highly resistant to abrasion and cracking and is resistant to accidents by combining shell cast iron of good abrasion resistance of specified component composition and core material gray cast iron of small residual stress and of required mechanical strength. CONSTITUTION:The composition of a shell material is specified at 3.0-3.6 T.C by %, 0.1-1.1 G.C, 0.5-0.9 Si, 0.4-1.3 Mn, 3.0-5.0 Ni, 0.8-2.2 Cr, 0.2-0.6 Mo, <=0.3 other trace elements, and the balance substantially Fe. This yields 70-85 hardness H, 0.5-8% graphite areas and 30-50% cementite areas. Next, the composition of a core material is specified at 2.9-3.7 T.C by %, 1.6-2.3 G.C, 0.7- 1.5 Si, 0.4-1.0 Mn, 0.3-2.0 Ni, 0.4-1.1 Cr, 0.05-0.4 Mo, <=0.4 other trace elements, and the balance substantially Fe. This yields 30-60 hardness H, and 8,000-16,000kgmm.<2> Young's modulus.
Priority Applications (1)
Application Number | Priority Date | Filing Date | Title |
---|---|---|---|
JP11118880A JPS5736056A (en) | 1980-08-12 | 1980-08-12 | Centrifugally cast composite roll |
Applications Claiming Priority (1)
Application Number | Priority Date | Filing Date | Title |
---|---|---|---|
JP11118880A JPS5736056A (en) | 1980-08-12 | 1980-08-12 | Centrifugally cast composite roll |
Publications (1)
Publication Number | Publication Date |
---|---|
JPS5736056A true JPS5736056A (en) | 1982-02-26 |
Family
ID=14554720
Family Applications (1)
Application Number | Title | Priority Date | Filing Date |
---|---|---|---|
JP11118880A Pending JPS5736056A (en) | 1980-08-12 | 1980-08-12 | Centrifugally cast composite roll |
Country Status (1)
Country | Link |
---|---|
JP (1) | JPS5736056A (en) |
Cited By (1)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
US7200935B2 (en) * | 2000-06-23 | 2007-04-10 | Novelis, Inc. | Work roll |
-
1980
- 1980-08-12 JP JP11118880A patent/JPS5736056A/en active Pending
Cited By (1)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
US7200935B2 (en) * | 2000-06-23 | 2007-04-10 | Novelis, Inc. | Work roll |
Similar Documents
Publication | Publication Date | Title |
---|---|---|
EP0098536A3 (en) | Wear-resistant sintered ferrous alloy and method of producing same | |
JPS5736056A (en) | Centrifugally cast composite roll | |
DE3572696D1 (en) | Non-magnetic steel having high corrosion resistance and high strength for use as material of drill collar, and drill collar made of the steel | |
AU678107B2 (en) | Corrosion and wear-resistant chill casting | |
JPS5616653A (en) | Soft magnetic material having superior workability and machinability | |
ATE225866T1 (en) | STEEL TO MAKE A BEARING | |
JPS5638452A (en) | Corrosion resistant sendust alloy and preparation of the same | |
JPS5798625A (en) | Nonmagnetic stainless steel and its manufacture | |
JPS5524931A (en) | Tool steel for hot processing | |
JPS57210954A (en) | Alloy steel for piston ring | |
JPS55128563A (en) | Cast iron excellent in wear and seizure resistance | |
JPS55145158A (en) | Free cutting bearing steel and its manufacture | |
JPS57101644A (en) | Composite sleeve roll for rolling h-steel and preparation thereof | |
JPS53140218A (en) | Wear resistant white pig iron | |
JPS6428342A (en) | Cast iron for cylinder block | |
ES2033761T3 (en) | PROCEDURE FOR THE PREPARATION OF A HIGHLY RESISTANT SINTERED ALLOY. | |
JPS54130427A (en) | Manufacture of rocker arm | |
JPS54118323A (en) | Heat crack resistant steel for use as metal mold | |
JPS57149456A (en) | Dendritic fe-cr-co magnet alloy | |
JPS57100809A (en) | Composite sleeve roll for rolling h-steel and its production | |
JPS645608A (en) | Hot rolling roll | |
JPS57123960A (en) | Corrosion resistant alloy for die casting | |
Bertrand et al. | Ferritic Spheroidal-Graphite Iron for Casting Thick Sections Without Segregation | |
Primerov | Complex Modifiers for Steel | |
JPS5456020A (en) | Amorphous alloy with superior formability |