JPS5719396A - Formation of heating surface on aluminum material - Google Patents
Formation of heating surface on aluminum materialInfo
- Publication number
- JPS5719396A JPS5719396A JP9295980A JP9295980A JPS5719396A JP S5719396 A JPS5719396 A JP S5719396A JP 9295980 A JP9295980 A JP 9295980A JP 9295980 A JP9295980 A JP 9295980A JP S5719396 A JPS5719396 A JP S5719396A
- Authority
- JP
- Japan
- Prior art keywords
- treating soln
- wetness
- silicate
- superior
- formation
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Granted
Links
Landscapes
- Electrochemical Coating By Surface Reaction (AREA)
Priority Applications (1)
| Application Number | Priority Date | Filing Date | Title |
|---|---|---|---|
| JP9295980A JPS5719396A (en) | 1980-07-07 | 1980-07-07 | Formation of heating surface on aluminum material |
Applications Claiming Priority (1)
| Application Number | Priority Date | Filing Date | Title |
|---|---|---|---|
| JP9295980A JPS5719396A (en) | 1980-07-07 | 1980-07-07 | Formation of heating surface on aluminum material |
Publications (2)
| Publication Number | Publication Date |
|---|---|
| JPS5719396A true JPS5719396A (en) | 1982-02-01 |
| JPS6259198B2 JPS6259198B2 (https=) | 1987-12-09 |
Family
ID=14068977
Family Applications (1)
| Application Number | Title | Priority Date | Filing Date |
|---|---|---|---|
| JP9295980A Granted JPS5719396A (en) | 1980-07-07 | 1980-07-07 | Formation of heating surface on aluminum material |
Country Status (1)
| Country | Link |
|---|---|
| JP (1) | JPS5719396A (https=) |
Cited By (3)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| JPS59136498A (ja) * | 1983-01-26 | 1984-08-06 | Kobe Steel Ltd | Al又はAl合金の表面処理方法 |
| JPS60111843U (ja) * | 1983-12-30 | 1985-07-29 | 株式会社 桂精機製作所 | 瞬間蒸発式ベ−パ−ライザ |
| JPH01184296A (ja) * | 1988-01-15 | 1989-07-21 | Internatl Business Mach Corp <Ibm> | アルミニウムまたはアルミニウム合金上への陽極酸化被膜の形成方法 |
-
1980
- 1980-07-07 JP JP9295980A patent/JPS5719396A/ja active Granted
Cited By (3)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| JPS59136498A (ja) * | 1983-01-26 | 1984-08-06 | Kobe Steel Ltd | Al又はAl合金の表面処理方法 |
| JPS60111843U (ja) * | 1983-12-30 | 1985-07-29 | 株式会社 桂精機製作所 | 瞬間蒸発式ベ−パ−ライザ |
| JPH01184296A (ja) * | 1988-01-15 | 1989-07-21 | Internatl Business Mach Corp <Ibm> | アルミニウムまたはアルミニウム合金上への陽極酸化被膜の形成方法 |
Also Published As
| Publication number | Publication date |
|---|---|
| JPS6259198B2 (https=) | 1987-12-09 |
Similar Documents
| Publication | Publication Date | Title |
|---|---|---|
| IT8124156A0 (it) | Procedimento ed installazione per la conversione termica dei pneumatici usati o di scarto in materie utilizzabili in particolare come combustibili. | |
| IT7928019A0 (it) | Procedimento per la produzione d'acido metacrilico e catalizzatore in esso impiegato. | |
| JPS5719396A (en) | Formation of heating surface on aluminum material | |
| JPS5410234A (en) | Desmutting method | |
| JPS5719381A (en) | Formation of heating surface on aluminum material | |
| JPS5729595A (en) | Formation of colored film of aluminum | |
| Markert et al. | The Influence of Alumina on the Reduction of Silica in Liquid Iron Containing Manganese, Silicon and Aluminium | |
| JPS5515976A (en) | Corrosiveness controlling method for fluorine-containing solution | |
| GILL et al. | ADVANTAGES IN THE USE OF VACUUM TAR-IMPREGNATED BRICKS AND INDIGENOUS MANUFACTURING POSSIBILITY | |
| JPS5293069A (en) | Elevating apparatus of fork lift to be used above and below road surfa ce | |
| SU672305A1 (ru) | Изол ци железобетонной емкости | |
| JPS5780907A (en) | Adhesion increasing slider for wheel tread | |
| JPS52128577A (en) | Electric insulating conductor | |
| JPS5687001A (en) | Formation of fog resistant film | |
| JPS54121262A (en) | Manufacture of steel structure with excellent hydrogen embrittlement resistance | |
| Sukhotin et al. | Iron Passivity in Oxalate Solutions | |
| Tomita | Treating Aluminum Workpiece to Simulate Appearance of Porcelain | |
| Surganov | BEHAVIOR OF VANADIUM IN ANODIZATION OF A THREE-LAYER FILM STRUCTURE, ALUMINUM-VANADIUM-ALUMINUM | |
| GB2085654B (en) | Anodic oxidation and etching of semiconductor material to form mesa structures | |
| JPS54128452A (en) | Chemically treating method for aluminum foil | |
| JPS5320269A (en) | Control system for operation of battery-driven fork lifts | |
| JPS52152049A (en) | Elevator safety device | |
| JPS57159540A (en) | Oxidizing catalyst | |
| Zlobin et al. | The Effect of the Composition of the Surface Layer of 08 Kh 14 MF Steel on the Anodic Polarization Curves | |
| JPS5735379A (en) | Semiconductor device |