JPH0790241B2 - Rolling method of steel bars - Google Patents

Rolling method of steel bars

Info

Publication number
JPH0790241B2
JPH0790241B2 JP22716389A JP22716389A JPH0790241B2 JP H0790241 B2 JPH0790241 B2 JP H0790241B2 JP 22716389 A JP22716389 A JP 22716389A JP 22716389 A JP22716389 A JP 22716389A JP H0790241 B2 JPH0790241 B2 JP H0790241B2
Authority
JP
Japan
Prior art keywords
mill
rolling
trough
long
rolled material
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Expired - Lifetime
Application number
JP22716389A
Other languages
Japanese (ja)
Other versions
JPH0390201A (en
Inventor
大海保 小杉
義一 松尾
久雄 矢入
明宏 野村
Original Assignee
日本鋼管株式会社
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by 日本鋼管株式会社 filed Critical 日本鋼管株式会社
Priority to JP22716389A priority Critical patent/JPH0790241B2/en
Publication of JPH0390201A publication Critical patent/JPH0390201A/en
Publication of JPH0790241B2 publication Critical patent/JPH0790241B2/en
Anticipated expiration legal-status Critical
Application status is Expired - Lifetime legal-status Critical

Description

【発明の詳細な説明】 [産業上の利用分野] この発明は、冷却床への条鋼搬入トラフまたは搬入ローラーテーブル入口で圧延材にトラブルが発生した時、トラブルを自動的に検知し、圧延材をコブルカッティングして圧延機への圧延材の噛込みを中断してミスロールの発生量を低減させる条鋼の圧延方法に関する。 DETAILED DESCRIPTION OF THE INVENTION [Field of the Industrial] This invention, when a trouble occurs in the rolled material in long products carrying trough or carrying roller table entrance to the cooling bed, automatically detect problems, rolled material the related rolling method of long steel to reduce the generation amount of Misuroru to interrupt inclusive bite of the rolled material to Cobble cutting to mill.

[従来技術] 条鋼の圧延は、通常第5図のような設備配置にて行なわれる。 Rolling PRIOR ART long products is carried out in a usual equipment arrangement shown in Figure 5. すなわち、条鋼圧延用のビレットは、加熱炉21で加熱される。 That is, the billet for long product rolling is heated in a heating furnace 21. そして、加熱されたビレットは、粗圧延機 The heated billets, roughing mill
22、中間圧延機23および仕上圧延機24の順に圧延されて最終製品の断面形状となる。 22, is rolled in the order of the intermediate mill 23 and the finishing mill 24 with the final product of the cross-sectional shape. 次いで仕上圧延機24の後方に配置した分割シヤー25で100m程度の長さごとに切断された後、冷却床26に搬入される。 Then, after being cut for each length of about 100m in a split shear 25 provided behind the finishing mill 24, it is carried into the cooling bed 26. 冷却床26において前記切断された長尺条鋼27は、レッヘン28により冷却床26の出口方向に移送され、アラインメントローラ29により長さ方向に送られて、ストッパ30に衝突させられ、長尺条鋼27の先端が揃えられる。 Long long steel 27 which is the cutting in the cooling bed 26 is transported in the exit direction of the cooling bed 26 by Rehhen 28, is sent in the longitudinal direction by the alignment roller 29 are brought into collision with the stopper 30, the long steel bars 27 the tip of the are aligned. そして、冷却床26の搬出口に設けたドライブローラ31により、長尺条鋼27は5〜100 Then, by the drive roller 31 provided on the carry-out port of the cooling bed 26, the long steel bars 27 5-100
本毎に冷却床26から搬出され、コールドシヤー32によりまとめて切断され、長さの揃った短尺条鋼33となる。 Is carried out to each present a cooling bed 26, they are collectively cut by Korudoshiya 32, a short long steel 33 with uniform length. なお、粗圧延機22、中間圧延機23および仕上圧延機24の間には、コブル切断用のフライングシヤー34を設けて、トラブル発生時にコブルカッティングを行ない、圧延材の圧延機への噛込みを中断して、大量のミスロール材が発生しないようにしている。 Incidentally, rough rolling mill 22, between the intermediate mill 23 and finishing mill 24, provided with a flying shear 34 for Cobble cutting performs Cobble cutting when trouble occurs, the biting of the rolling mill of the rolled material is interrupted, a large amount of Misuroru material is not to occur.

ところで、冷却床26の入口には条鋼を冷却床26に搬入するための搬入テーブルまたは搬入トラフ35が設けられいるが、搬入トラフ35を設けている設備においては、条鋼は自動的に複数の搬入トラフ35に振り分けられて、搬入トラフ35内を進み全長が搬入トラフ35内に納まったタイミングで搬入トラフ35の回転軸が回転し、搬入トラフ35 By the way, carrying the table or loading trough 35 for carrying the long products to cooling beds 26 to the inlet of the cooling bed 26 is provided in the equipment is provided with a loading trough 35, long products are automatically plurality of loading It is distributed to the trough 35, to rotate the rotary shaft of the loading trough 35 at the timing when the full-length advances the loading trough 35 is accommodated in the loading trough 35, loading trough 35
内の長尺条鋼27は搬入トラフ35から落下し、冷却床26に設けたレッヘン28により冷却床26に搬入されるようになっている。 Long long products 27 of the inner will fall from the loading trough 35 is adapted to be carried into the cooling bed 26 by Rehhen 28 provided in the cooling bed 26. また、搬入テーブルは傾斜した多数のローラーからなり、比較的低速度で搬入される条鋼の場合に使用される。 Also, carry-table consists of a number of rollers which are inclined, are used in the case of long steel being transported at a relatively low speed.

[発明が解決しようとする課題] 上記した搬入トラフ35に条鋼が突入するとき、長尺条鋼 When long products rushes to the carrying trough 35 as described above [0007], long long products
27の先端の切断面に切断時に発生した切断ばりが付着していると、この切断ばりが搬入トラフ35の縁に当たって、長尺条鋼27が搬入トラフ35にうまく導かれず、搬入トラフ35の前でくしゃくしゃに折れ曲がって後続の長尺条鋼27の進行を妨害することになり、圧延を中断しなければならない自体が発生することがある。 The cutting burrs generated during cutting are attached on the cut surface of the tip 27, when the edge of the cutting burr is carried trough 35, not guided well to long long products 27 conveyed trough 35, in front of the loading trough 35 crumpled the bent would interfere the progress of the subsequent long steel bars 27, itself must be interrupted rolling may occur.

上記したような状態が発生した場合、従来は作業員が目視でその状態を確認し、電話等で圧延機の運転者に連絡して、条鋼の圧延を中断するようにしていた。 When the state as described above occurs, conventional checks its state visually worker, contact the operator of the mill on the phone, etc., it had to be interrupted rolling long products. しかしながら、このような方法で圧延を中断するのでは、トラブルの発生から圧延を中断するまでに時間がかかりすぎ、 However, this way of aborting the rolling in a way, too much time from troubles occur before aborting the rolling,
その間中条鋼が圧延されしかもそのすべてが搬入トラフ前で折れ曲がってしまうので、ほとんどビレット1本分のスクラップが発生し、そのスクラップを除去するために30分もの時間を要するので、条鋼圧延の稼働率を著しく低下させるという問題点があった。 Since all the addition is between in long products are rolled will bent before carrying trough, almost billet one roll of scrap generated, it takes 30 minutes of time in order to remove the scrap, the operation rate of long product rolling was a problem that significantly reduces.

この発明は、従来技術の上述のような問題点を解消し、 This invention is to solve the aforementioned problems of the prior art,
搬入トラフ前でトラブルが発生したとき、自動的に異常を検出して圧延材をコブルカッティングして、圧延材の圧延機への噛込みを中断することにより、スクラップの発生を極力減少させる条鋼の圧延方法を提供することを目的としている。 When trouble occurs in the previous loading trough, automatically abnormality detection by the rolled material and Cobble cutting by the by interrupting biting into the rolling mill of the rolled material, of long products that reduce the occurrence of scrap utmost and its object is to provide a rolling method.

[課題を解決するための手段] この発明に係る条鋼の圧延方法は、条鋼圧延機群に後続する冷却床入口の搬入トラフまたは搬入ローラーテーブルの中間に圧延材検出装置を設け、圧延機群と冷却床の間に配置された走行分割シヤーからの切断信号が発せられてから所定の時間内に前記圧延材検出装置が圧延材を検出しない場合、圧延機群の間に設けたフライングシヤーにて圧延材をコブルカッティングして圧延機への圧延材の噛込みを中断する条鋼の圧延方法である。 [Means for Solving the Problems] rolling method of long products according to the invention, a rolled material detecting device provided in the middle of the cooling bed inlet of the loading trough or carrying roller table following the long products mill group, and the mill group If the rolled material detecting device disconnection signal from disposed in the cooling beds traveling divided shears from is issued within a predetermined time it does not detect the rolled material, the rolled material at a flying shears provided between the mill group which is a rolling method of interrupting long products a lump bite of the rolled material to the Cobble cutting to the rolling mill.

[作用] この発明に係る条鋼の圧延方法においては、条鋼圧延機群に後続する冷却床入口の搬入トラフまたは搬入ローラーテーブルの中間に圧延材検出装置を設け、圧延機群と冷却床の間に配置された走行分割シヤーからの切断信号が発せられてから所定の時間内に前記圧延材検出装置が圧延材を検出しない場合、圧延機群の間に設けたフライングシヤーにて圧延材をコブルカッティングして圧延機への圧延材の噛込みを中断するようにしている。 [Operation] In the rolling method of long products according to the invention is provided with a rolled material detecting apparatus in the middle of the cooling bed inlet of the loading trough or carrying roller table following the long products mill group are disposed in the cooling alcove and mill group and when the running dividing the rolled material detection device disconnected from the signal is issued within a predetermined time from the shear does not detect the rolled material, and Cobblestone cutting the rolled material at a flying shears provided between the mill group and so as to interrupt the biting of the strip into the rolling mill. このようにして圧延しているので、搬入トラフまたは搬入ローラーテーブルに条鋼がうまく導かれずにトラブルが発生した場合、圧延材検出装置は走行分割シヤーからの切断信号が発せられてから所定時間内に条鋼を検出できないので、これに基づく警報信号を圧延機運転室に送る。 Since the rolled this way, if trouble occurs without long products are directed well to carry trough or carrying roller table, the rolled material detection device within a predetermined from being issued is disconnect signal from the traveling dividing shears time can not detect long products, it sends an alarm signal based on this mill cab. この警報信号に基づき、圧延機の間に設けられているコブルカッティング用のフライングシヤーが自動的に作動して、圧延材のコブルカッティングを行ない、圧延機への圧延材の噛込みを中断させる。 Based on this alarm signal, the rolling mill a flying shears for Cobble cutting is provided is operated automatically during performs Cobble cutting of the rolled material, to interrupt the biting of the strip into the rolling mill. 前記圧延材検出装置は、 The rolled material detecting apparatus,
異常発生から短時間で異常を検出できるので、異常発生から圧延中断までの時間も短くなり、その間に発生するスクラップの発生量は少なくてすむ。 Because a short time can be detected abnormality from the abnormality occurs, is shortened time from the abnormality occurrence to the rolling interruptions, fewer generation amount of scrap generated therebetween. したがって、異常発生に伴うスクラップ除去作業も短時間で行なえるので圧延機の稼働率を高めることができる。 Therefore, it is possible to increase the operation rate of a rolling mill so performed in a short time even scrap removal operation accompanying the occurrence of abnormality. 合わせてスクラップの減少に伴い圧延歩留が向上する。 Rolling yield with decreasing scrap combined is improved.

[実施例] 本発明の1実施例の条鋼の圧延方法を第1図〜第4図により説明する。 EXAMPLES be described by FIG. 1-FIG. 4 the rolling method of long products of one embodiment of the present invention. 本発明の1実施例の鋼材の直送圧延方法においては、条鋼圧延設備の粗圧延機1の入口に粗圧延機材料検出器2を、中間圧延機3の入口に中間圧延機材料検出器4を、仕上圧延機5の入口には仕上圧延機材料検出器6を、また冷却床7の入口に連結するトラフライン8の中間に冷却床入口部材料検出器9を設けている。 In one direct rolling method of steel of Example of the present invention, the roughing mill material detector 2 to the inlet of the rough rolling mill 1 long product rolling equipment, the intermediate rolling mill material detector 4 to an inlet of the intermediate rolling mill 3 , and a rolling mill material detector 6 finish at the entrance of the finishing mill 5 and the intermediate cooling bed inlet section material detector 9 of the trough line 8 connected to the inlet of the cooling bed 7 is provided.
トラフライン8の中間に設けた冷却床入口部材料検出器9について詳述すると次のようになる。 More specifically the cooling bed inlet section material detector 9 provided in the middle of the trough line 8 as follows. 第2図はトラフライン8の一部側面図であるが、圧延された条鋼は第1 Although FIG. 2 is a partial side view of the trough line 8, it is rolled long products first
図に示すトラフライン8の入口に設置されている振分装置10により振り分けられ、第2図に示す上下方向に4段に並んで配置されたトラフ11に導入される。 Sorted by the sorting apparatus 10 which is installed at the entrance of the trough line 8 shown in FIG., It is introduced into the trough 11 that is arranged in four stages in the vertical direction shown in Figure 2. このトラフ This trough
11は、ラッパ状の口を有する300mm程度の短尺トラフ12 11, the short trough 12 of approximately 300mm with a trumpet-shaped mouth
を20mm程度の間隔をあけて多数連続して配置したものであり、直径30mm程度の内部空間を有している。 The are those arranged many continuously at intervals of about 20 mm, and has an internal space having a diameter of about 30 mm. このトラフ11の中間に、トラフ11内を搬送されている条鋼を検出するための冷却床入口部材料検出器9を各トラフ11に設けている。 In the middle of the trough 11 is provided with a cooling bed inlet section material detector 9 for detecting the long products being conveyed in the trough 11 in the trough 11. 第3図は第2図のA−A矢視図であるが、この冷却床入口部材料検出器9は、短尺トラフ12と短尺トラフ12の間の隙間から光学的に条鋼を検出するようになっている。 Although FIG. 3 is an A-A arrow view of FIG. 2, the cooling bed inlet section material detector 9 to detect optically long products from the gap between the short trough 12 and the short troughs 12 going on. そして、検出した信号はケーブル13を通して、制御器14に伝えられる。 Then, the detected signal through the cable 13, is transmitted to the controller 14.

本発明の1実施例の条鋼の圧延方法においては、上述した各材料検出器を使用して、トラフ11に条鋼がうまく誘導されず、トラフ11の入口で折れ曲がってミスロールとなった場合、後続の条鋼の進行を妨げて、連続してミスロール材が発生するのを防止するようにしている。 In one rolling method of long products in the embodiment of the present invention, using the materials detectors mentioned above, long products to the trough 11 is not successfully induced, when a Misuroru bent at the inlet of the trough 11, the subsequent preventing the progression of long products, Misuroru material continuously is to be prevented. その方法は、第1図に示す仕上圧延機5の後方の分割シヤー The method of the mill 5 finish shown in Figure 1 the rear of the split shears
15で条鋼が切断されてから所定時間内に冷却床入口部材料検出器9が条鋼を検知しない時には、その信号に基づき粗圧延機と中間圧延機の間に設けたNo.1フライングシヤー16、および中間圧延機と仕上圧延機の間に設けたN When 15 long products are cutting in the cooling within a predetermined time bed inlet material detector 9 does not detect the long products are, No.1 flying shears 16 provided between the roughing mill and the intermediate rolling mill on the basis of the signal, N and provided between the intermediate rolling mill and finish rolling mill
o.2フライングシヤー17を作動させ、圧延材をコブルカッティングして圧延材の圧延機への噛込みを中断させて、ミスロール材の多量発生を防止するというものである。 o.2 actuating the flying shear 17 and the rolled material is interrupted biting into the rolling mill of the Cobble cutting to rolled material, is that of preventing a large amount occurrence of Misuroru material.

第4のブロック図により、本発明の1実施例のミスロール材を多量に発生させない条鋼の圧延方法を説明する。 The fourth block diagram, illustrating a rolling method of long steel which does not heavily generate Misuroru material of one embodiment of the present invention.
分割シヤーの切断信号と検出された仕上圧延機の最終圧延スタンドの回転数の信号を演算器に送り、切断された条鋼が、導入さるべきトラフに配置した冷却床入口部材料検出器9で検出される到達予定時間を演算し、その結果を演算タイマーに送り、条鋼の到達予定時間を設定する。 The rotational speed signal of the last rolling stand of the disconnect signal and the detected finish rolling mill of split shear feed to the calculator, the cut long products are detected in the cooling bed inlet material detector 9 disposed in the trough should leave introduced is the calculated arrival scheduled time, sends the result to the arithmetic timer, sets the estimated arrival time of the long products. 冷却床入口部材料検出器9が予定到達時間内に条鋼を検知した時には、制御器14からNo.1およびNo.2フライングシヤー対して正常状態保持指令、すなわち作動しなくてもよいという指令が発せられる。 When cooling bed inlet section material detector 9 detects the long products in the expected arrival time, the normal state hold command for the controller 14 No.1 and No.2 flying shears, that is, a command that may not work It emitted. 冷却床入口部材料検出器9が予定到達時間内に条鋼を検知せず、かつ粗圧延機材料検出器2、中間圧延機材料検出器4および仕上圧延機材料検出器6が圧延材料を検出している時には、 Without detecting the long products in the cooling bed inlet section material detector 9 scheduled arrival time, and the roughing mill material detector 2, intermediate rolling mill material detector 4 and the finishing mill material detector 6 detects the rolled material when is is,
No.1フライングシヤー16およびNo.2フライングシヤー17 No.1 flying shear 16 and No.2 flying shear 17
に対して連続カット指令、すなわちコブルカッティング指令が発せられ、圧延材料はコブルカッティングされる。 Continuous cut command, i.e. Cobble cutting command is issued with respect to the rolling material is Cobble cutting. そして、コブルカッティングが完了して、No.1フライングシヤー16およびNo.2フライングシヤー17に設けた材料検出器が材料を検知しなくなった時には、一定時間経過後No.1フライングシヤー16およびNo.2フライングシヤー17に対して連続カット停止指令が発せられ、No.1フライングシヤー16およびNo.2フライングシヤー17は作動を停止する。 Then, Cobble cutting is completed, No.1 flying when shear 16 and No.2 material detector provided on the flying shears 17 does not detect the material, and a predetermined time has elapsed after the No.1 flying shear 16 No. 2 continuous cut stop command to the flying shears 17 is issued, No.1 flying shear 16 and No.2 flying shears 17 stops operating. 冷却床入口部材料検出器9が予定到達時間内に条鋼を検知しなくても、粗圧延機材料検出器2、中間圧延機材料検出器4および仕上圧延機材料検出器6が圧延材料を検出していない時には、連続カット指令は発せられない。 Also cooling bed inlet section material detector 9 is not detecting the long products in the expected arrival time, the roughing mill material detector 2, intermediate rolling mill material detector 4 and the finishing mill material detector 6 detects a rolled material when you are not, the continuous cut instruction is not issued.

本発明の1実施例の条鋼の圧延方法においては、上述したように、トラフラインでのトラブルをいち早く検出して、自動的にコブルカッティングして、圧延材の圧延機への噛込みを中断するようにしているので、トラブル発生時のミスロール材の除去処理に時間を要しないとともに、圧延歩留も向上する。 In the long products rolling method of an embodiment of the present invention, as described above, to quickly detect a trouble in the trough line, automatically Cobblestone cutting suspends inclusive bite into the rolling mill of the rolled material since the way, with no need to time the removal process Misuroru material when trouble occurred is also improved rolling yield.

なお、本発明の1実施例の条鋼の圧延方法を搬入トラフの場合で説明したが、搬入ローラーテーブルの場合にも、本圧延方法が適用可能であるのは当然である。 Although a rolling method of long products in the embodiment of the invention has been described in the case of carrying trough, in the case of carrying roller table, the present rolling method is applicable is a matter of course.

[発明の効果] この発明により、トラフラインでのトラブル発生時のミスロール材の除去処理に時間を要しないとともに、圧延歩留も向上する。 [Effect of the Invention] This invention, together with not requiring the time the removal process Misuroru material troubles during development in the trough line is also improved rolling yield.

【図面の簡単な説明】 BRIEF DESCRIPTION OF THE DRAWINGS

第1図は本発明の1実施例の条鋼の圧延方法を実施する圧延ラインの設備配置を示す平面図、第2図はトラフの側面図、第3図は第2図のA−A矢視図、第4図は本発明の1実施例の条鋼の圧延方法を示すブロック図、第5 Plan view showing the equipment arrangement of the rolling line carrying out the rolling method of the long products in the first embodiment of Figure 1 the present invention, FIG. 2 is a side view of the trough, Figure 3 is A-A arrow view of FIG. 2 Figure, Figure 4 is a block diagram illustrating a rolling process of long products of one embodiment of the present invention, the fifth
図は従来の圧延ラインの設備配置を示す平面図である。 Figure is a plan view showing the equipment arrangement of a conventional rolling line. 2……粗圧延機材料検出器、4……中間圧延機材料検出器、6……仕上圧延機材料検出器、9……冷却床入口部材料検出器、11……トラフ、15……分割シヤー、16…… 2 ...... roughing mill material detector, 4 ...... intermediate mill material detector, 6 ...... finishing mill material detector, 9 ...... cooling bed inlet section material detector, 11 ...... trough, 15 ...... divided shear, 16 ......
No.1フライングシヤー、17……No.2フライングシヤー。 No.1 flying shear, 17 ...... No.2 flying shear.

フロントページの続き (56)参考文献 特開 昭49−93251(JP,A) 特開 昭60−92010(JP,A) 特公 昭53−34675(JP,B2) Of the front page Continued (56) Reference Patent Sho 49-93251 (JP, A) JP Akira 60-92010 (JP, A) Tokuoyake Akira 53-34675 (JP, B2)

Claims (1)

    【特許請求の範囲】 [The claims]
  1. 【請求項1】条鋼圧延機群に後続する冷却床入口の搬入トラフまたは搬入ローラーテーブルの中間に圧延材検出装置を設け、圧延機群と冷却床の間に配置された分割シヤーからの切断信号が発せられてから所定の時間内に前記圧延材検出装置が圧延材を検出しない場合、圧延機群の間に設けたフライングシヤーにて圧延材をコブルカッティングして圧延機への圧延材の噛込みを中断することを特徴とする条鋼の圧延方法。 1. A long product rolled material detection device provided in the middle of subsequent cooling bed inlet of the loading trough or carrying roller table mill group, issued the disconnect signal from the arranged split shear cooling alcove and mill group If being the rolled material detection device within a predetermined time after does not detect the rolled material, the biting of the strip of rolled material to Cobble cutting to mill at a flying shears provided between the mill group rolling method of long steel, characterized in that the interruption.
JP22716389A 1989-09-01 1989-09-01 Rolling method of steel bars Expired - Lifetime JPH0790241B2 (en)