JPH0410885B2 - - Google Patents
Info
- Publication number
- JPH0410885B2 JPH0410885B2 JP59096197A JP9619784A JPH0410885B2 JP H0410885 B2 JPH0410885 B2 JP H0410885B2 JP 59096197 A JP59096197 A JP 59096197A JP 9619784 A JP9619784 A JP 9619784A JP H0410885 B2 JPH0410885 B2 JP H0410885B2
- Authority
- JP
- Japan
- Prior art keywords
- emulsion
- vinyl acetate
- pva
- modified pva
- polymerization
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Expired - Lifetime
Links
Landscapes
- Polymerisation Methods In General (AREA)
- Addition Polymer Or Copolymer, Post-Treatments, Or Chemical Modifications (AREA)
Priority Applications (1)
Application Number | Priority Date | Filing Date | Title |
---|---|---|---|
JP9619784A JPS60240710A (ja) | 1984-05-14 | 1984-05-14 | 乳化重合方法 |
Applications Claiming Priority (1)
Application Number | Priority Date | Filing Date | Title |
---|---|---|---|
JP9619784A JPS60240710A (ja) | 1984-05-14 | 1984-05-14 | 乳化重合方法 |
Publications (2)
Publication Number | Publication Date |
---|---|
JPS60240710A JPS60240710A (ja) | 1985-11-29 |
JPH0410885B2 true JPH0410885B2 (enrdf_load_stackoverflow) | 1992-02-26 |
Family
ID=14158562
Family Applications (1)
Application Number | Title | Priority Date | Filing Date |
---|---|---|---|
JP9619784A Granted JPS60240710A (ja) | 1984-05-14 | 1984-05-14 | 乳化重合方法 |
Country Status (1)
Country | Link |
---|---|
JP (1) | JPS60240710A (enrdf_load_stackoverflow) |
Families Citing this family (3)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
JP5934274B2 (ja) * | 2014-03-26 | 2016-06-15 | デンカ株式会社 | 変性ポリ酢酸ビニルの製造方法 |
JP6550908B2 (ja) * | 2015-05-08 | 2019-07-31 | 国立大学法人福井大学 | アルケニルエーテル系重合体の製造方法 |
JP6638930B2 (ja) | 2015-05-08 | 2020-02-05 | 国立大学法人福井大学 | アルケニルエーテル−ビニルエステル共重合体 |
Family Cites Families (1)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
JPS54135882A (en) * | 1978-04-13 | 1979-10-22 | Kuraray Co Ltd | Emulsion polymerization |
-
1984
- 1984-05-14 JP JP9619784A patent/JPS60240710A/ja active Granted
Also Published As
Publication number | Publication date |
---|---|
JPS60240710A (ja) | 1985-11-29 |
Similar Documents
Publication | Publication Date | Title |
---|---|---|
JPS6015429A (ja) | 水性ポリマ−分散液の製法 | |
JPH0322917B2 (enrdf_load_stackoverflow) | ||
JPH04272902A (ja) | 湿潤粘着特性が改善された酢酸ビニル/エチレン共重合体エマルジョン | |
JPH0410885B2 (enrdf_load_stackoverflow) | ||
JPH086003B2 (ja) | 酢酸ビニル樹脂エマルジョン組成物 | |
JPH11106727A (ja) | 紙管用接着剤およびこれを用いた紙管 | |
JPS59179605A (ja) | アルコキシル基と結合したシリル基を有する変性ポリビニルアルコ−ルの製造法 | |
JP2657600B2 (ja) | 初期接着性に優れたエマルジョン接着剤及びその製造方法 | |
JP3441187B2 (ja) | 水性エマルジョン | |
JPH0160485B2 (enrdf_load_stackoverflow) | ||
JPS6411643B2 (enrdf_load_stackoverflow) | ||
JPS6344768B2 (enrdf_load_stackoverflow) | ||
JP4151950B2 (ja) | 接着剤組成物 | |
JP2916190B2 (ja) | 合成ゴムラテックス系接着剤の製造方法 | |
JP2515655B2 (ja) | ホットメルト接着方法 | |
JP3210712B2 (ja) | 乳化重合用分散安定剤 | |
JP2757113B2 (ja) | 紙管用接着剤 | |
JPS58162611A (ja) | アクリル系重合体エマルジヨンの製法 | |
JP2001072952A (ja) | 紙工用接着剤及びその製法 | |
JPH0160484B2 (enrdf_load_stackoverflow) | ||
JPH093424A (ja) | 接着剤 | |
JP2515654B2 (ja) | 合板の製造方法 | |
JPH07102007A (ja) | ビニル化合物系乳化重合物の製造方法 | |
JPS6333483B2 (enrdf_load_stackoverflow) | ||
JPH07247400A (ja) | 水性エマルジョン |