JP2577064Y2 - Time indicator - Google Patents

Time indicator

Info

Publication number
JP2577064Y2
JP2577064Y2 JP1992010300U JP1030092U JP2577064Y2 JP 2577064 Y2 JP2577064 Y2 JP 2577064Y2 JP 1992010300 U JP1992010300 U JP 1992010300U JP 1030092 U JP1030092 U JP 1030092U JP 2577064 Y2 JP2577064 Y2 JP 2577064Y2
Authority
JP
Japan
Prior art keywords
sample
fading
time indicator
different degrees
colorant
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Expired - Lifetime
Application number
JP1992010300U
Other languages
Japanese (ja)
Other versions
JPH0571792U (en
Inventor
輝男 中川
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Dai Nippon Printing Co Ltd
Original Assignee
Dai Nippon Printing Co Ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Dai Nippon Printing Co Ltd filed Critical Dai Nippon Printing Co Ltd
Priority to JP1992010300U priority Critical patent/JP2577064Y2/en
Publication of JPH0571792U publication Critical patent/JPH0571792U/en
Application granted granted Critical
Publication of JP2577064Y2 publication Critical patent/JP2577064Y2/en
Anticipated expiration legal-status Critical
Expired - Lifetime legal-status Critical Current

Description

【考案の詳細な説明】[Detailed description of the invention]

【0001】[0001]

【産業上の利用分野】本考案は、試料部の退色によって
概略の経過時間を表示するタイムインジケータに関す
る。
BACKGROUND OF THE INVENTION 1. Field of the Invention The present invention relates to a time indicator for displaying an approximate elapsed time by fading a sample portion.

【0002】[0002]

【従来の技術】概略の経過時間を検出するタイムインジ
ケータとしては、試料の変色を利用したものが知られて
いる。これは特定の物質が特定のガス、特に酸素、によ
り化学変化を起こして変色する性質を応用したものであ
る。
2. Description of the Related Art As a time indicator for detecting an approximate elapsed time, an indicator utilizing discoloration of a sample is known. This is an application of the property that a specific substance undergoes a chemical change by a specific gas, particularly oxygen, to change color.

【0003】[0003]

【考案が解決しようとする課題】上記のものでは、使用
開始までは試料が酸素に触れないように脱酸素剤などと
共に密封しておく必要があって、構造が複雑になると共
に取り扱いも煩雑となる上、材料が高価でコストが高く
つく等の問題があった。本考案はこのような点に着目
し、取り扱いが容易で安価なタイムインジケータを得る
ことを課題としてなされたものである。
In the above method, it is necessary to seal the sample with an oxygen scavenger so that the sample does not come into contact with oxygen until the start of use, so that the structure becomes complicated and handling becomes complicated. In addition, there are problems that the material is expensive and the cost is high. The present invention focuses on such a point, and has been made to provide an inexpensive time indicator that is easy to handle.

【0004】[0004]

【課題を解決するための手段】上記の課題を解決するた
めに、本考案では、耐光性の弱い着色剤からなる1つの
試料部又は退色の度合いを異ならせた複数の試料部を基
材の表面に形成し、上面を遮光保護層で覆った構造とし
ている。基材の表面には、1つの試料部又は退色の度合
いを異ならせた複数の試料部の退色を示す基準色部を設
けてもよい。また、試料部の設けられている基材の裏面
には粘着剤層を介して離型紙を積層した構造としてもよ
い。
In order to solve the above-mentioned problems, according to the present invention, one sample portion made of a colorant having low light resistance or a plurality of sample portions having different degrees of fading is used as a base material. It is formed on the surface and the upper surface is covered with a light-shielding protective layer. On the surface of the base material, a reference color portion indicating the fading of one sample portion or a plurality of sample portions having different degrees of fading may be provided. Further, a structure in which release paper is laminated on the back surface of the substrate on which the sample portion is provided via an adhesive layer may be employed.

【0005】[0005]

【作用】光線の当たる場所に放置しておくことにより試
料部が退色するので、その退色の状態によって概略の経
過時間を知ることができる。また、試料部とともに耐光
性の強い着色剤からなる基準色部を基材の表面に設ける
ことにより、試料部の退色状態の判断が容易となる。ま
た、試料部の設けられている基材の裏面に粘着剤層を介
して離型紙を積層した構造とすることにより、貼着ラベ
ルとしての機能をも有することが可能である。
The sample portion is discolored by leaving it in a place where a light beam hits, so that the approximate elapsed time can be known from the discoloration state. Further, by providing a reference color portion made of a colorant having high light resistance together with the sample portion on the surface of the base material, it is easy to determine the fading state of the sample portion. In addition, by having a structure in which release paper is laminated via a pressure-sensitive adhesive layer on the back surface of the substrate on which the sample section is provided, it is possible to have a function as an adhesive label.

【0006】[0006]

【実施例】以下、図示の一実施例について説明する。図
1は厚さ方向を拡大して示した断面図であり、1は紙、
アルミ箔、合成樹脂フィルム等からなる基材、2a,2b,
2cは基材1の表面に形成された試料部、3はこれらの
試料部が設けられている基材1の表面に形成された透光
性の離型剤層、4は紙、アルミ箔、着色合成樹脂フィル
ムあるいはこれらの積層体からなる遮光層5の片面に粘
着剤層6を形成した保護層であり、この保護層4は少な
くとも各試料部2a,2b,2cを覆うように基材1の表面
の貼着されている。また、基材1の裏面には、粘着剤層
7を介して離型紙8が積層されている。
BRIEF DESCRIPTION OF THE DRAWINGS FIG. FIG. 1 is an enlarged cross-sectional view in the thickness direction.
Substrates made of aluminum foil, synthetic resin film, etc., 2a, 2b,
2c is a sample portion formed on the surface of the substrate 1, 3 is a translucent release agent layer formed on the surface of the substrate 1 provided with these sample portions, 4 is paper, aluminum foil, A protective layer in which a pressure-sensitive adhesive layer 6 is formed on one side of a light-shielding layer 5 made of a colored synthetic resin film or a laminate thereof, and the protective layer 4 covers at least the sample portions 2a, 2b, and 2c. The surface is stuck. A release paper 8 is laminated on the back surface of the base material 1 via an adhesive layer 7.

【0007】9は上述した各層の積層体で構成された薄
片状のタイムインジケータであり、全体の形状は例えば
図2に示すような長方形など、用途に応じた適宜の形状
が可能である。試料部2a,2b,2cは染料などの耐光性
の弱い着色剤を使用し、しかも退色の度合いを異ならせ
て形成されたものであり、使用する際には裏面の離型紙
8を剥がして検体に貼り付け、試料部2a,2b,2cに光
が当たるように表面の保護層4を剥がしておくのであ
る。試料部2a,2b,2cは時間の経過とともに次第に退
色して行くので、例えば色がほとんど消えるまでの所要
日数が、試料部2aは10日、2bは20日、2cは30
日となるように設計しておくことにより、各試料部の色
の消え具合と相互間の比較から概略の経過時間を知るこ
とができる。また色が消えるまで待たなくても、途中の
退色の進行状態によっても概略の経過時間を知ることが
でき、場合によっては試料部が1個のみでもその退色の
進行状態から概略の経過時間を知ることができる。
Reference numeral 9 denotes a flaky time indicator composed of a laminate of the above-mentioned layers. The overall shape of the time indicator can be any suitable shape such as a rectangle as shown in FIG. The sample portions 2a, 2b, and 2c are formed by using a colorant having low light resistance such as a dye and having a different degree of fading, and when used, release the release paper 8 on the back surface and remove the sample. And the protective layer 4 on the surface is peeled off so that the sample portions 2a, 2b and 2c are exposed to light. Since the sample sections 2a, 2b, and 2c gradually fade with time, for example, the number of days required until the color almost disappears is 10 days for the sample section 2a, 20 days for 2b, and 30 days for 2c.
By designing so as to be days, the approximate elapsed time can be known from the degree of disappearance of the color of each sample portion and a comparison between them. Even without waiting for the color to disappear, the approximate elapsed time can be known from the progress of fading in the middle, and in some cases, even if only one sample part is used, the approximate elapsed time can be known from the progress of fading. be able to.

【0008】このように、各試料部2a,2b,2cの退色
状態から経過時間が分かるのであるが、試料部の色を比
較できる何らかの基準があれば判断が容易となる。図2
の10a,10b,10cはこのために設けられた基準色部
であり、各試料部の退色後や途中の色の状態を示すよう
に耐光性の強い着色剤を使用して形成されている。な
お、上述のように試料部を1個のみとした場合には、退
色の進行状態に応じた色調の基準色部を複数個設けてお
くことにより比較判断が容易となる。
As described above, the elapsed time can be determined from the fading state of each of the sample portions 2a, 2b, 2c. However, if there is some reference that can compare the colors of the sample portions, the judgment can be made easily. FIG.
Reference numerals 10a, 10b, and 10c are reference color portions provided for this purpose. The reference color portions are formed using a colorant having strong light resistance so as to show a color state after or in the middle of each sample portion. In the case where only one sample portion is provided as described above, comparison judgment is facilitated by providing a plurality of reference color portions having a color tone corresponding to the progress of fading.

【0009】次に、試料部2a,2b,2cの形成例につい
て説明する。染料としては耐光性の弱いものが使用さ
れ、一例を挙げると青色ではメチレンブルー FZ(M
ETHYLENE BLUE FZ)が、赤色ではアス
トラフロキシン FF コンク(ASTRAPHLOX
INE FF CONC)が使用可能である。これらの
染料をフレキソ用メジウム(水性)に溶解したインクを用
い、例えば印刷によって試料部を形成する。この印刷の
際に染料の濃度を変化させたり、印刷厚さを変化させた
りすることによって各試料部の退色の度合いを異ならせ
るのであり、印刷厚さは印刷の回数を変えたり、グラビ
ア方式の印刷であれば版深を変えたりすることで変化さ
せることができる。
Next, an example of forming the sample portions 2a, 2b, 2c will be described. Dyes having low light fastness are used. For example, methylene blue FZ (M
ETHYLENE BLUE FZ) is red and Astraphloxin FF Conch (ASTRAPHLOX)
INE FF CONC) can be used. A sample part is formed by, for example, printing using an ink in which these dyes are dissolved in a medium for flexo (aqueous). At the time of this printing, the degree of fading of each sample portion is changed by changing the concentration of the dye or changing the printing thickness, and the printing thickness is changed by changing the number of times of printing or using a gravure method. For printing, it can be changed by changing the plate depth.

【0010】具体的には、例えば150L/inch、版深
40μmのグラビア印刷において、インクの濃度を0.1
%、0.2%、0.3%のように3段階に変えることによ
って、各試料部10a,10b,10cの耐光性を段階的に
変化させることができ、この場合にはインク濃度が高く
なるほど退色しにくくなって色が消えるまでの所要時間
が長くなる。また同じ150Lのものにおいて、インク
濃度は変えないで試料部ごとに版深を40μm、60μ
m、80μmのように変化させてもよく、更に例えば15
0L、版深40μm、インク濃度0.1%という同一の条
件において、1回刷、2回刷、3回刷のように印刷の回
数を変えることもでき、この場合には印刷厚さが大きく
なるほど退色しにくくなって色が消えるまでの所要時間
が長くなる。なお、基準色部10a,10b,10cは顔料
などの耐光性の強い着色剤を使用したインクにより、所
定の色調で適宜印刷される。
Specifically, for example, in gravure printing at 150 L / inch and a plate depth of 40 μm, the density of the ink is set at 0.1.
%, 0.2%, and 0.3%, the light resistance of each of the sample portions 10a, 10b, and 10c can be changed stepwise. In this case, the ink density is high. It becomes difficult to fade, and the time required for the color to disappear becomes longer. In the same 150L, the plate depth was set to 40 μm and 60 μm for each sample without changing the ink density.
m, 80 μm.
Under the same conditions of 0 L, plate depth of 40 μm, and ink concentration of 0.1%, the number of times of printing can be changed, such as one-time printing, two-time printing, and three-time printing. It becomes difficult to fade, and the time required for the color to disappear becomes longer. The reference color portions 10a, 10b, and 10c are appropriately printed in a predetermined color tone using an ink using a colorant having high light resistance such as a pigment.

【0011】[0011]

【考案の効果】上述の説明から明らかなように、本考案
は、耐光性の弱い着色剤、例えば染料を使用して1つ又
は退色の度合いの異なる複数の試料部を基材の表面に形
成し、上面を遮光保護層で覆った構造としたものであ
る。従って、例えば芳香剤や脱臭剤のように有効期間が
限られているものを光線の当たる場所で使用する場合に
併用すれば、光線による試料部の退色状態から概略の経
過時間を知ることができるのであり、簡単なタイムイン
ジケータを低コストで得ることができる。また試料部の
色と比較できる基準色部を設けたものでは、経過時間の
判断が容易となり、また、基材の裏面に粘着剤層を介し
て離型紙を積層した貼着ラベル型のものでは、使用時の
取り扱いが容易で商品価値の高いタイムインジケータが
得られる。
As is clear from the above description, the present invention forms one or a plurality of sample portions having different degrees of fading on the surface of a substrate by using a colorant having low light resistance, for example, a dye. In addition, the upper surface is covered with a light-shielding protective layer. Therefore, when used together with a light source that has a limited effective period, such as a fragrance or a deodorant, in a place where the light beam hits, it is possible to know the approximate elapsed time from the discoloration state of the sample portion due to the light beam. Therefore, a simple time indicator can be obtained at low cost. In addition, in the case of providing a reference color portion that can be compared with the color of the sample portion, the elapsed time can be easily determined, and in the case of a sticking label type in which release paper is laminated via an adhesive layer on the back surface of the base material. In addition, a time indicator that is easy to handle during use and has high commercial value can be obtained.

【図面の簡単な説明】[Brief description of the drawings]

【図1】 本考案の一実施例の厚さ方向を拡大して示し
た断面図である。
FIG. 1 is an enlarged cross-sectional view of one embodiment of the present invention in a thickness direction.

【図2】 同実施例の斜視図である。FIG. 2 is a perspective view of the embodiment.

【符号の説明】[Explanation of symbols]

1 基材 2a,2b,2c 試
料部 3 離型材層 4 遮光保護層 5 遮光層 6 粘着剤層 7 粘着剤層 8 離型紙 9 タイムインジケータ 10a,10b,10c
基準色部
DESCRIPTION OF SYMBOLS 1 Base material 2a, 2b, 2c Sample part 3 Release material layer 4 Light shielding protective layer 5 Light shielding layer 6 Adhesive layer 7 Adhesive layer 8 Release paper 9 Time indicator 10a, 10b, 10c
Standard color part

Claims (3)

(57)【実用新案登録請求の範囲】(57) [Scope of request for utility model registration] 【請求項1】 耐光性の弱い着色剤からなる1つの試料
部又は退色の度合いを異ならせた複数の試料部(2a,2
b,2c)を基材(1)の表面に形成し、上面を遮光保護層
(4)で剥離自在に覆ったことを特徴とするタイムインジ
ケータ。
1. A sample section made of a colorant having weak lightfastness or a plurality of sample sections (2a, 2a) having different degrees of fading.
b, 2c) are formed on the surface of the substrate (1), and the upper surface is formed of a light-shielding protective layer.
A time indicator characterized in that it is detachably covered with (4).
【請求項2】 1つの試料部又は退色の度合いを異なら
せた複数の試料部(2a,2b,2c)の退色状態を示す基準
色部(10a,10b,10c)を耐光性の強い着色剤を使用
して基材(1)の表面に併設した請求項1記載のタイムイ
ンジケータ。
2. A reference color part (10a, 10b, 10c) showing a fading state of one sample part or a plurality of sample parts (2a, 2b, 2c) having different degrees of fading is provided with a colorant having strong light resistance. 2. The time indicator according to claim 1, wherein the time indicator is provided along with the surface of the base material (1).
【請求項3】 1つの試料部又は退色の度合いを異なら
せた複数の試料部(2a,2b,2c)が設けられている基材
(1)の裏面に粘着剤層(7)を介して離型紙(8)を積層し
た請求項1または請求項2記載のタイムインジケータ。
3. A substrate provided with one sample portion or a plurality of sample portions (2a, 2b, 2c) having different degrees of fading.
3. The time indicator according to claim 1, wherein a release paper (8) is laminated on the back surface of (1) via an adhesive layer (7).
JP1992010300U 1992-03-03 1992-03-03 Time indicator Expired - Lifetime JP2577064Y2 (en)