JP2012189946A - Pseudo adhesive label - Google Patents

Pseudo adhesive label Download PDF

Info

Publication number
JP2012189946A
JP2012189946A JP2011055340A JP2011055340A JP2012189946A JP 2012189946 A JP2012189946 A JP 2012189946A JP 2011055340 A JP2011055340 A JP 2011055340A JP 2011055340 A JP2011055340 A JP 2011055340A JP 2012189946 A JP2012189946 A JP 2012189946A
Authority
JP
Japan
Prior art keywords
pseudo
base material
label
surface base
adhesive layer
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Pending
Application number
JP2011055340A
Other languages
Japanese (ja)
Inventor
Daisuke Tomita
大介 冨田
Shinobu Takano
忍 高野
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Lintec Corp
Original Assignee
Lintec Corp
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Lintec Corp filed Critical Lintec Corp
Priority to JP2011055340A priority Critical patent/JP2012189946A/en
Publication of JP2012189946A publication Critical patent/JP2012189946A/en
Pending legal-status Critical Current

Abstract

PROBLEM TO BE SOLVED: To provide a pseudo adhesive label in which breakage is rarely generated on a surface substrate at places other than a cutting line when peeling the surface substrate from a pseudo adhesive layer, and which has good workability.SOLUTION: A pseudo adhesive label 10 is configured by laminating a surface base material 11, a pseudo adhesive layer artificially joined to the surface base material 11, and an adhesive agent layer in this order. The surface base material 11 can be peeled from the pseudo adhesive layer so as to be separated along a cutting line 20 as label portions 18 and 19. In the cutting line 20, a plurality of streaks 20x are formed at intervals. The cutting line 20 has a shape in which intermediate portions 20b are tilted to linear portions 20a and 20c on both sides.

Description

本発明は、物品の搬送や管理等に使用される配送伝票、各種の保険やチケットの申し込み等に使用される記録票等に適用される擬似接着ラベルに関する。   The present invention relates to a pseudo-adhesive label applied to a delivery slip used for transportation and management of articles, a record slip used for application for various insurances and tickets, and the like.

例えば、郵便、宅配便、通信販売などにおいて、商品の受注、発送、顧客の受け取り等からなる流通過程を管理するために、配送伝票等が用いられる。広く用いられる配送伝票の1つとして、感圧紙が複数枚重ね合わされた伝票がある。このような配送伝票では、商品名、送り先等の情報を記入する際、一番下の伝票まで情報を書き込むために、強い圧力を加えなければならず、ボールペン、タイプライター、ドットプリンター等が必要とされる。しかし、ボールペン、タイプライターを用いての書き込みは、煩雑な手作業であり、また誤字、脱字、写し間違いなどによって、誤配送の原因となる。また、ドットプリンターを用いる場合、印字に時間がかかるという欠点がある。さらに、感圧紙が複数枚重ね合わされた配送伝票は、その一部が流通過程で破れたり、剥がれ落ちたりすることもある。   For example, a delivery slip or the like is used in order to manage a distribution process including ordering of goods, shipping, receipt of a customer, etc. in mail, parcel delivery, mail order sales, and the like. As one of widely used delivery slips, there is a slip in which a plurality of pressure sensitive papers are overlapped. In such a delivery slip, when filling in information such as product name and destination, it is necessary to apply a strong pressure to write the information down to the bottom slip, and a ballpoint pen, typewriter, dot printer, etc. are required. It is said. However, writing with a ballpoint pen or a typewriter is a cumbersome manual operation, and causes erroneous delivery due to typographical errors, omissions, or copying errors. In addition, when using a dot printer, there is a drawback that printing takes time. Furthermore, a part of a delivery slip in which a plurality of pressure sensitive papers are stacked may be broken or peeled off during the distribution process.

上記問題点を解決するために、例えば、表面基材、擬似接着層、粘着剤層、及び剥離シートがこの順に積層されてなり、表面基材と擬似接着層との間が剥離可能なように擬似接着された擬似接着ラベルが配送伝票に使用される。擬似接着ラベルは、剥離シートが剥離された後、粘着剤層が配送物に貼付されて、配送伝票として使用される(例えば、特許文献1参照)。   In order to solve the above problems, for example, a surface base material, a pseudo-adhesive layer, a pressure-sensitive adhesive layer, and a release sheet are laminated in this order so that the surface base material and the pseudo-adhesive layer can be peeled off. The pseudo-adhesive label that is pseudo-adhered is used for the delivery slip. The pseudo-adhesive label is used as a delivery slip after the release sheet is peeled off, and an adhesive layer is affixed to the delivery (see, for example, Patent Document 1).

このような擬似接着ラベルの配送伝票には、種々の印刷が施された表面基材の表面に断裁線が入れられており、1枚の表面基材が2つのラベル部として分離して剥離可能となっている。そして、例えば、一方のラベル部が配達票として使用されると共に、他方のラベル部が、受領票として使用され、捺印・サイン後に剥がされて持ち帰られ、伝票整理等に使用される。   In the delivery slip of such a pseudo-adhesive label, a cut line is put on the surface of the surface base material on which various printings are applied, and one surface base material can be separated and separated as two label portions. It has become. For example, one label portion is used as a delivery slip, the other label portion is used as a receipt slip, peeled off after stamping / signing, and taken home, and used for slip arrangement.

擬似接着ラベルを用いれば、郵便、宅配便、通信販売などにおいて商品の受注から顧客の受け取りまで1枚のシートで流通過程を管理することが可能であり、さらに流通過程における伝票の破れや紛失等も防止することができる。また、レーザープリンター、熱転写等による情報の書き込みが可能であるため、記入が迅速に行えると共に、誤字・脱字等も低減させることができる。   By using pseudo-adhesive labels, it is possible to manage the distribution process with a single sheet from the order of goods to the receipt of customers in mail, courier, mail order, etc. Furthermore, slips and loss of slips in the distribution process, etc. Can also be prevented. In addition, since information can be written by laser printer, thermal transfer, etc., it is possible to fill in quickly and to reduce typographical errors and omissions.

特公昭55−15035号公報Japanese Patent Publication No.55-15035

しかし、擬似接着ラベルにおいて断裁線がミシン目の場合には、切れ目が断続的であるため、ラベル部が引き剥がされる際、断裁線の途中の意図しない部分で表面基材が破れるおそれがある。   However, when the cut line is perforated in the pseudo-adhesive label, the cut is intermittent, and therefore, when the label portion is peeled off, the surface base material may be broken at an unintended portion in the middle of the cut line.

そこで、本発明は、表面基材をミシン目の断裁線で分離して剥離する際に、断裁線以外の箇所で表面基材に破れが発生することなく擬似接着層から剥離することができる擬似接着ラベルを提供することを目的とする。   Therefore, the present invention provides a pseudo-pseudo material that can be peeled off from the pseudo-adhesive layer without tearing the surface base material at a place other than the cut line when the surface base material is separated and peeled at the perforation line. An object is to provide an adhesive label.

本発明に係る擬似接着ラベルは、表面基材と、表面基材に擬似接着される擬似接着層と、粘着剤層とがこの順に積層された積層構造を備え、粘着剤層が被着物に貼着された状態で、表面基材を擬似接着層から剥離可能な擬似接着ラベルであって、表面基材は、少なくとも2以上のラベル部に分離して擬似接着層から剥離可能とするためのミシン目状の断裁線を備え、断裁線における中途部は、その両側の線状部に対して傾斜した形状を有することを特徴とする。   The pseudo-adhesive label according to the present invention has a laminated structure in which a surface base material, a pseudo-adhesive layer pseudo-adhered to the surface base material, and an adhesive layer are laminated in this order, and the adhesive layer is attached to an adherend. A pseudo-adhesive label capable of peeling a surface base material from a pseudo-adhesive layer in a worn state, wherein the surface base material is separated into at least two or more label portions so as to be peelable from the pseudo-adhesive layer It is characterized by comprising a grid-like cutting line, and the midway part in the cutting line has a shape inclined with respect to the linear parts on both sides thereof.

中途部は、その両側の線状部に対して鈍角で連接することが好ましい。また、中途部は、傾斜した直線状であっても良い。さらに、両側の線状部は、互いに平行な直線状となっていても良い。   The midway part is preferably connected to the linear parts on both sides thereof at an obtuse angle. Further, the midway part may be an inclined straight line. Furthermore, the linear portions on both sides may be linear parallel to each other.

本発明では、表面基材をミシン目の断裁線で分離して剥離する際に、断裁線以外の箇所で表面基材に破れが発生することなく擬似接着層から剥離することができる擬似接着ラベルを提供することができる。   In the present invention, when the surface base material is separated by a perforated cut line and peeled off, the pseudo adhesive label can be peeled off from the pseudo adhesive layer without tearing the surface base material at a place other than the cut line. Can be provided.

本発明の実施形態に係る擬似接着ラベルを模式的に示す断面図である。It is sectional drawing which shows typically the pseudo | simulation adhesive label which concerns on embodiment of this invention. 本発明の実施形態に係る擬似接着ラベルを模式的に示す平面図である。It is a top view which shows typically the pseudo adhesive label which concerns on embodiment of this invention.

以下、図面を参照しつつ本発明の実施形態について説明する。図1は、本発明の実施形態に係る擬似接着ラベルを模式的に示す断面図であり、図2はその平面図である。   Hereinafter, embodiments of the present invention will be described with reference to the drawings. FIG. 1 is a cross-sectional view schematically showing a pseudo-adhesive label according to an embodiment of the present invention, and FIG. 2 is a plan view thereof.

図1に示すように、本発明の実施形態に係る擬似接着ラベル10は、表面基材11、表面基材11に擬似接着される擬似接着層12、擬似接着層12に接着された粘着剤層13がこの順に積層された積層構造を備え、更に、剥離基材14が粘着剤層13に貼着されている。擬似接着ラベル10は、剥離基材14が粘着剤層13から剥離され、露出した粘着剤層13によって、被着物(図示せず)に貼着されて使用される。   As shown in FIG. 1, a pseudo-adhesive label 10 according to an embodiment of the present invention includes a surface base material 11, a pseudo-adhesion layer 12 that is pseudo-adhered to the surface base material 11, and an adhesive layer that is adhered to the pseudo-adhesion layer 12. 13 has a laminated structure in which the layers are laminated in this order, and a peeling substrate 14 is attached to the pressure-sensitive adhesive layer 13. The pseudo-adhesive label 10 is used after the release substrate 14 is peeled off from the pressure-sensitive adhesive layer 13 and is adhered to an adherend (not shown) by the exposed pressure-sensitive adhesive layer 13.

擬似接着層12は、表面基材11に剥離可能に擬似接着されており、擬似接着ラベル10が被着物に貼着された状態で、表面基材11が擬似接着層12から剥離される。擬似接着ラベル10には、表面基材11の表面から多数の切れ目20xが切り込まれており、切れ目20xによってミシン目状の断裁線20(図2参照)が構成される。切れ目20xは、図1に示すように、表面基材11の表面から切り込まれて、表面基材11、擬似接着層12、及び粘着剤層13を貫通するものである。なお、切れ目20xは、表面基材11の裏面まで貫通していれば、擬似接着層12及び粘着剤層13は切り込まれていなくても良い。ただし、表面基材11がその裏面に、後述する熱可塑性樹脂層や離型剤層を備える場合には、それらも切り込まれる。   The pseudo-adhesion layer 12 is pseudo-adhered to the surface base material 11 so as to be peeled off, and the surface base material 11 is peeled from the pseudo-adhesion layer 12 in a state where the pseudo-adhesive label 10 is attached to the adherend. In the pseudo-adhesive label 10, a large number of cuts 20x are cut from the surface of the surface base material 11, and the cut line 20x forms a perforated cutting line 20 (see FIG. 2). As shown in FIG. 1, the cut 20 x is cut from the surface of the surface base material 11 and penetrates the surface base material 11, the pseudo adhesive layer 12, and the pressure-sensitive adhesive layer 13. Note that the pseudo adhesive layer 12 and the pressure-sensitive adhesive layer 13 do not have to be cut as long as the cut 20x penetrates to the back surface of the surface base material 11. However, when the surface base material 11 is provided with a thermoplastic resin layer or a release agent layer, which will be described later, on the back surface thereof, they are also cut.

表面基材11としては、例えば上質紙、熱転写用紙、クラフト紙、グラシン紙、感熱紙、合成紙、又はプラスティックフィルムが使用される。表面基材11の厚みは、例えば15〜120μm、好ましくは20〜110μmであり、更に好ましくは30〜100μmである。表面基材11の表面は、例えば文字等の情報が表示されるための面に使用される。   As the surface base material 11, for example, high-quality paper, thermal transfer paper, craft paper, glassine paper, thermal paper, synthetic paper, or plastic film is used. The thickness of the surface base material 11 is 15-120 micrometers, for example, Preferably it is 20-110 micrometers, More preferably, it is 30-100 micrometers. The surface of the surface substrate 11 is used as a surface for displaying information such as characters.

擬似接着層12は、表面基材11に剥離可能に擬似接着されるものであれば、特に限定されないが、熱可塑性樹脂層であることが好ましい。熱可塑性樹脂層は、例えば、加熱溶融された熱可塑性樹脂が表面基材11の裏面に押出積層されることにより形成される。熱可塑性樹脂層を形成するための熱可塑性樹脂としては、例えば、ポリエチレン、ポリプロピレン、ポリメチルペンテン等が単独で又は2種類以上混合されて使用される。熱可塑性樹脂層の厚さは、特に限定されないが、例えば3〜70μm、好ましくは5〜50μmである。   The pseudo adhesive layer 12 is not particularly limited as long as it is pseudo-adhered to the surface substrate 11 so as to be peeled off, but is preferably a thermoplastic resin layer. The thermoplastic resin layer is formed, for example, by extrusion laminating a heat-melted thermoplastic resin on the back surface of the surface base material 11. As the thermoplastic resin for forming the thermoplastic resin layer, for example, polyethylene, polypropylene, polymethylpentene and the like are used alone or in admixture of two or more. Although the thickness of a thermoplastic resin layer is not specifically limited, For example, it is 3-70 micrometers, Preferably it is 5-50 micrometers.

表面基材11の裏面には、擬似接着層12から表面基材11を容易に剥離できるように、離型剤層が被膜されていても良い。離型剤層は、特に限定されないが、スチレン−アクリル共重合体、ポリスチレン、スチレン−ブタジエン共重合体、エチレン酢酸ビニル共重合体、アクリル酸エステル、アクリル酸エステル共重合体、エチレン・アクリル酸共重合体などからなる離型剤によって形成される。なお、表面基材11は、離型剤層が設けられる場合には、擬似接着層12と離型剤層との界面で剥離される。また、表面基材11は、その裏面にさらに上記熱可塑性樹脂で形成された熱可塑性樹脂層と、離型剤層とがこの順に設けられたものであっても良い。   A release agent layer may be coated on the back surface of the surface base material 11 so that the surface base material 11 can be easily peeled off from the pseudo adhesive layer 12. The release agent layer is not particularly limited, but styrene-acrylic copolymer, polystyrene, styrene-butadiene copolymer, ethylene vinyl acetate copolymer, acrylic acid ester, acrylic acid ester copolymer, ethylene / acrylic acid copolymer. It is formed by a mold release agent made of a polymer or the like. In addition, the surface base material 11 peels in the interface of the pseudo adhesion layer 12 and a mold release agent layer, when a mold release agent layer is provided. Moreover, the surface base material 11 may be further provided with a thermoplastic resin layer formed of the thermoplastic resin and a release agent layer in this order on the back surface.

粘着剤層13は、擬似接着層12の裏面側に設けられ、擬似接着ラベル10を被着物に粘着させるための層であって、アクリル系粘着剤、天然ゴム系粘着剤、合成ゴム系粘着剤、シリコーン系粘着剤等の従来公知の粘着剤から形成される。粘着剤層13の厚さは、特に限定されないが、例えば5〜50μm、好ましくは10〜40μmである。剥離基材14は、粘着剤層13に貼着されるための表面がシリコーン系剥離剤等によって離型処理された剥離シート等である。   The pressure-sensitive adhesive layer 13 is provided on the back side of the pseudo-adhesive layer 12 and is a layer for adhering the pseudo-adhesive label 10 to an adherend, and is an acrylic pressure-sensitive adhesive, natural rubber-based pressure-sensitive adhesive, and synthetic rubber-based pressure-sensitive adhesive. It is formed from a conventionally known adhesive such as a silicone-based adhesive. Although the thickness of the adhesive layer 13 is not specifically limited, For example, 5-50 micrometers, Preferably it is 10-40 micrometers. The release substrate 14 is a release sheet or the like whose surface to be attached to the pressure-sensitive adhesive layer 13 is subjected to a release treatment with a silicone release agent or the like.

粘着剤層13は、例えば、剥離基材14に粘着剤が塗布されて形成される。そして、その剥離基材14の上に形成された粘着剤層13に、表面基材11に積層された擬似接着層12が貼り合わされることにより、擬似接着ラベル10が得られる。但し、粘着剤層13は、表面基材11に積層されている擬似接着層12の上に直接塗布して形成され、その上に剥離基材14が貼り合わされて擬似接着ラベル10が形成されても良い。   The pressure-sensitive adhesive layer 13 is formed, for example, by applying a pressure-sensitive adhesive to the peeling substrate 14. And the pseudoadhesion label 10 is obtained by bonding the pseudoadhesion layer 12 laminated | stacked on the surface base material 11 to the adhesive layer 13 formed on the peeling base material 14 together. However, the pressure-sensitive adhesive layer 13 is formed by directly coating the pseudo-adhesive layer 12 laminated on the surface base material 11, and the pseudo-adhesive label 10 is formed by pasting the release base material 14 thereon. Also good.

図2に示すように、本発明の実施形態に係る擬似接着ラベル10は、打ち抜き加工が施されることにより、表面基材11、擬似接着層12、及び粘着剤層13が打ち抜き切断された後、カス上げによって不要部分が剥離基材14から取り除かれ、下辺10A及び上辺10Bを長辺とし、左右の側辺10C、10Dを短辺とする略矩形のラベルに形成される。擬似接着ラベル10は、打ち抜き加工と共に略中央部にミシン目加工が施され、表面基材11の略中央部に断裁線20が形成される。打ち抜き加工及びミシン目加工は、例えば、ダイカッタが用いられて行われるが、レーザー照射等によって行われても良い。   As shown in FIG. 2, the pseudo-adhesive label 10 according to the embodiment of the present invention is obtained by punching and cutting the surface base material 11, the pseudo-adhesive layer 12, and the pressure-sensitive adhesive layer 13 by performing a punching process. Unnecessary portions are removed from the peeling base material 14 by raising the residue, and a substantially rectangular label having the lower side 10A and the upper side 10B as long sides and the left and right side sides 10C and 10D as short sides is formed. The pseudo-adhesive label 10 is perforated at a substantially central portion together with the punching process, and a cutting line 20 is formed at a substantially central portion of the surface base material 11. The punching and perforation are performed using, for example, a die cutter, but may be performed by laser irradiation or the like.

図2に示すように、断裁線20は、表面基材11の下辺10Aから上辺10Bまで延在する。表面基材11は、断裁線20によって右左の略矩形のシート(これらをラベル部18、19という。)に分離して擬似接着層12から剥離可能である。   As shown in FIG. 2, the cutting line 20 extends from the lower side 10 </ b> A to the upper side 10 </ b> B of the surface base material 11. The surface base material 11 can be separated from the pseudo-adhesive layer 12 by being separated into right and left substantially rectangular sheets (referred to as label portions 18 and 19) by a cutting line 20.

断裁線20は、中途部20bがその両側の線状部20a、20cに対して傾斜しており、平面視でクランク状の折り曲がり線状となる。線状部20a、20cは、互いに平行でかつ縦方向に延在する直線であり、それぞれ表面基材11の外縁である下辺10A及び上辺10Bまで延在する。中途部20bは、線状部20a、20cの上端及び下端に鈍角(好ましくは95°〜165°、より好ましくは100°〜145°。)に連接する直線状の傾斜部である。中途部20bは、断裁線20の略中央位置に配置される。   In the cutting line 20, the midway part 20 b is inclined with respect to the linear parts 20 a and 20 c on both sides thereof, and has a crank-like bent line shape in plan view. The linear portions 20 a and 20 c are straight lines that are parallel to each other and extend in the vertical direction, and extend to the lower side 10 </ b> A and the upper side 10 </ b> B that are the outer edges of the surface base material 11, respectively. The midway portion 20b is a linear inclined portion connected to the upper and lower ends of the linear portions 20a and 20c at an obtuse angle (preferably 95 ° to 165 °, more preferably 100 ° to 145 °). The midway portion 20 b is disposed at a substantially central position of the cutting line 20.

このように、断裁線20は、上側の線状部20cが、中途部20bを介して下側の線状部20aに対して横方向にずれた折り曲がり線状となる。そして、断裁線20全体の幅Xは、2本の線状部20a、20cの横方向における離間距離(すなわち、折れ曲がり幅)となる。幅Xは、2mm〜20mmであることが好ましく、3mm〜10mmであることがより好ましい。幅Xが大きすぎるとラベルの形状上好ましくなく、小さすぎると表面基材11に破れが生じやすくなる。   As described above, the cutting line 20 has a bent line shape in which the upper linear portion 20c is shifted laterally with respect to the lower linear portion 20a via the midway portion 20b. The width X of the entire cutting line 20 is the distance between the two linear portions 20a and 20c in the lateral direction (that is, the bending width). The width X is preferably 2 mm to 20 mm, and more preferably 3 mm to 10 mm. If the width X is too large, it is not preferable in terms of the shape of the label, and if it is too small, the surface substrate 11 is easily broken.

また、断裁線20が上記したような折り曲がり線状となることにより、ラベル部18の下側部分は、ラベル部19側に張り出した形状となり、その張り出した部分に、後述するように剥離開始部となる角部18Aがある。ラベル部19の上側部分も同様に、ラベル部18側に張り出した形状となり、剥離開始部となる角部19Bがある。   Further, since the cutting line 20 has a bent line shape as described above, the lower part of the label portion 18 has a shape protruding to the label portion 19 side, and peeling starts on the protruding portion as described later. There is a corner 18A to be a part. Similarly, the upper portion of the label portion 19 has a shape protruding to the label portion 18 side, and has a corner portion 19B that becomes a peeling start portion.

断裁線20を構成する複数の切れ目20xは、下辺10Aから上辺10Bまで間隔dをおいて連続的に設けられる。断裁線20の最下端及び最上端に配置された切れ目20x、20xは、下辺10A及び上辺10Bに接続される。   The plurality of cuts 20x constituting the cutting line 20 are continuously provided with a distance d from the lower side 10A to the upper side 10B. The cuts 20x and 20x arranged at the lowermost end and the uppermost end of the cutting line 20 are connected to the lower side 10A and the upper side 10B.

切れ目20xの長さは、切れ目20x、20xの離間距離dより長いことが好ましい。切れ目20xの長さが離間距離dより短くなると、断裁線20に沿って表面基材11が分離されにくくなり、破れが生じやすくなる。切れ目20xの長さは、例えば0.2〜15mm、好ましくは0.4〜10mmであり、各切れ目20xの離間距離dは、例えば、0.1〜1mm、好ましくは0.2〜0.8mmである。切れ目20xの長さ及び離間距離が上記範囲から外れると、ラベル部18、19を剥離する際、断裁線20に沿って表面基材11が分離されにくくなり、破れが生じやすくなる。   The length of the cut 20x is preferably longer than the distance d between the cuts 20x and 20x. When the length of the cut 20x is shorter than the separation distance d, the surface base material 11 is not easily separated along the cutting line 20, and tearing is likely to occur. The length of the cut 20x is, for example, 0.2 to 15 mm, preferably 0.4 to 10 mm, and the separation distance d of each cut 20x is, for example, 0.1 to 1 mm, preferably 0.2 to 0.8 mm. It is. When the length and the separation distance of the cut 20x are out of the above ranges, the surface base material 11 is difficult to be separated along the cutting line 20 when the label portions 18 and 19 are peeled off, and breakage is likely to occur.

次に、疑似接着ラベル10における表面基材11の剥離方法について説明する。表面基材11のラベル部18の切り離しは、例えば、下辺10Aと断裁線20が交差する位置にあるラベル部18の角部18Aを剥離開始部として摘まんで、表面基材11を剥離方向Aに引き剥がすことにより行われる。このとき、ラベル部18は、ラベル部19側を残すように、断裁線20に沿って表面基材11を断裁しつつ擬似接着層12から剥離される。   Next, the peeling method of the surface base material 11 in the pseudo adhesive label 10 is demonstrated. For example, the label portion 18 of the surface base material 11 is separated by, for example, picking the corner portion 18A of the label portion 18 at the position where the lower side 10A intersects the cutting line 20 as a peeling start portion and placing the surface base material 11 in the peeling direction A. This is done by peeling off. At this time, the label portion 18 is peeled from the pseudo adhesive layer 12 while cutting the surface base material 11 along the cutting line 20 so as to leave the label portion 19 side.

本実施形態では、角部18Aからラベル部18が剥離されるとき、その剥離方向Aは、縦方向に対して、中途部20bと同じ向きに傾斜するものである。したがって、ラベル部18が剥離方向Aに引き剥がされるときに表面基材11に作用される力は、断裁線20に沿って伝わりやすくなり、それにより、断裁線20の途中の意図しない位置から表面基材11が破れるのが防止される。また、断裁線20は、意図しない破れが生じやすい断裁線20の中央付近で傾斜するため、より有効に表面基材11の破れが防止される。   In the present embodiment, when the label portion 18 is peeled from the corner portion 18A, the peeling direction A is inclined in the same direction as the midway portion 20b with respect to the vertical direction. Therefore, when the label portion 18 is peeled off in the peeling direction A, the force applied to the surface base material 11 is easily transmitted along the cutting line 20, and thereby the surface is moved from an unintended position in the middle of the cutting line 20. It is prevented that the base material 11 is torn. Moreover, since the cutting line 20 inclines near the center of the cutting line 20 in which unintended tearing is likely to occur, the surface base material 11 is more effectively prevented from being torn.

また、ラベル部18、19は断裁線20に沿って容易に切れるため、断裁線20が流れ方向やフィルムの延伸方向に対して垂直に形成されている場合であっても表面基材11が破れにくくなる。さらに、断裁線20における最下端の切れ目20xは、下辺10Aに接続するため、ラベル部18の剥離が角部18Aから開始しやすくなる。   Further, since the label portions 18 and 19 are easily cut along the cutting line 20, even if the cutting line 20 is formed perpendicular to the flow direction or the film stretching direction, the surface substrate 11 is torn. It becomes difficult. Furthermore, since the lowermost cut 20x in the cutting line 20 is connected to the lower side 10A, peeling of the label portion 18 can easily start from the corner portion 18A.

なお、以上の説明では、2つのラベル部のうち、ラベル部18が先に剥離されるときの動作について説明したが、ラベル部19が、上辺10Bと断裁線20が交差する位置にある角部19Bを剥離開始部として、先に剥離される際にも同様の作用によりラベル部19の破れが防止される。さらに、一方のラベル部が剥がされた後、残ったラベル部は、擬似剥離層12から適宜剥離される。   In the above description, of the two label portions, the operation when the label portion 18 is peeled first has been described. However, the label portion 19 is located at a position where the upper side 10B and the cutting line 20 intersect. When 19B is used as the peeling start portion, tearing of the label portion 19 is prevented by the same action when peeling off first. Further, after the one label portion is peeled off, the remaining label portion is appropriately peeled off from the pseudo peeling layer 12.

なお、本実施形態では、上記したように、中途部20bが剥離方向Aと同じ向きに傾斜していなければ、破れを生じさせることなくラベル部18を剥離するのが難しい。すなわち、上記実施形態では、上辺10Bと断裁線20が交差する位置にあるラベル部18の角部18Bを剥離開始部として、ラベル部18を剥離することは難しい。そのため、表面基材11等にマーク等が付されて、例えば、角部18Aがラベル部18の剥離開始部であることが示されていても良い。また、表面基材11上に剥離方向Aを示した矢印が付されても良い。同様に、角部19Bが剥離開始部であることが示されても良い。ただし本実施形態では、マーク等が付されなくても、角部18A、19Bは、ラベル部18、19それぞれの張り出した部分にあるため、使用者に剥離開始部として認識されやすくなる。   In the present embodiment, as described above, unless the midway portion 20b is inclined in the same direction as the peeling direction A, it is difficult to peel off the label portion 18 without causing tearing. That is, in the said embodiment, it is difficult to peel off the label part 18 by making the corner | angular part 18B of the label part 18 in the position where the upper side 10B and the cutting line 20 cross | intersect into a peeling start part. Therefore, a mark or the like may be attached to the surface base material 11 or the like, for example, indicating that the corner portion 18A is a peeling start portion of the label portion 18. An arrow indicating the peeling direction A may be attached on the surface base material 11. Similarly, it may be indicated that the corner portion 19B is a peeling start portion. However, in this embodiment, even if a mark or the like is not added, the corners 18A and 19B are located on the protruding portions of the label portions 18 and 19, respectively, so that it is easy for the user to recognize the peeling start portion.

なお、擬似接着ラベル10は、2つのラベル部のうち、いずれのラベル部が先に剥離されるかが予め決まっている場合がある。例えば、擬似接着ラベルが配送伝票に使用され、ラベル部18が受領票、ラベル部19が配達票とされると、ラベル部18が先に剥離されることとなる。このような場合、ラベル部18を角部18Aから剥離しやすくするために、断裁線20の最下端における切れ目20xは、下辺10Aに接続する必要があるが、最上端における切れ目は、上辺10Bに接続する必要はない。   In some cases, the pseudo-adhesive label 10 has a predetermined one of the two label portions to be peeled first. For example, when a pseudo-adhesive label is used for a delivery slip, the label portion 18 is a receipt slip and the label portion 19 is a delivery slip, the label portion 18 is peeled first. In such a case, in order to make it easy to peel off the label portion 18 from the corner portion 18A, the cut 20x at the lowermost end of the cutting line 20 needs to be connected to the lower side 10A, but the cut at the uppermost end is connected to the upper side 10B. There is no need to connect.

また、中途部20bは、直線で形成されたが、直線に限定されずに、曲線を含んでいても良い。また、中途部20bには、複数の傾斜部が設けられて階段状となっていても良い。同様に、線状部20a、20cも曲線を含んでいても良い。さらには、線状部20a、20cにはさらに別の線状部が接続され、その線状部が下辺10A、10Bに接続しても良い。   Moreover, although the midway part 20b was formed in the straight line, it is not limited to a straight line, The curve may be included. Further, the midway portion 20b may be provided with a plurality of inclined portions and have a stepped shape. Similarly, the linear portions 20a and 20c may include curves. Furthermore, another linear part may be connected to the linear parts 20a and 20c, and the linear part may be connected to the lower sides 10A and 10B.

また、断裁線20の各切れ目20x間の間隔は、表面基材11の裏面まで完全に貫通しないように、ハーフカットされ、あるいは、筋押しにより筋状の窪みが形成されても良い。   Moreover, the space | interval between each cut | interruption 20x of the cutting line 20 may be half-cut so that it may not penetrate completely to the back surface of the surface base material 11, or a streak-like hollow may be formed by muscle pushing.

なお、上記実施形態において、ラベル部18、19は略矩形であったが、その形状は矩形に限定されず、例えば三角形等他の多角形でも良いし、円形等であっても良い。また、擬似接着ラベル10の構造や材質は、上記実施形態に限定されない。例えば、表面基材11、擬似接着層12、粘着剤層13以外の層を備えたものであっても構わない。また、各断裁線の間隔や切れ目の長さは、均等でも非均等であっても構わない。更に、擬似接着ラベル10の構造や材質は、上記実施形態に限定されない。例えば、表面基材11、擬似接着層12、粘着剤層13以外の層を備えたものであっても構わない。   In the above-described embodiment, the label portions 18 and 19 are substantially rectangular. However, the shape is not limited to a rectangle, and may be another polygon such as a triangle or a circle. Further, the structure and material of the pseudo-adhesive label 10 are not limited to the above embodiment. For example, you may provide layers other than the surface base material 11, the pseudo adhesion layer 12, and the adhesive layer 13. Further, the intervals between the cutting lines and the lengths of the cut lines may be uniform or non-uniform. Furthermore, the structure and material of the pseudo-adhesive label 10 are not limited to the above embodiment. For example, you may provide layers other than the surface base material 11, the pseudo adhesion layer 12, and the adhesive layer 13.

次に、本発明について、以下実施例を用いて説明するが、本発明は以下の実施例の構成に限定されない。   Next, the present invention will be described below using examples, but the present invention is not limited to the configurations of the following examples.

[実施例1]
表面基材として、タック原紙(ユポ・コーポレーション社製、商品名:ユポタック原紙 60SGS)を使用した。擬似接着層を形成するための熱可塑性樹脂として、ポリプロピレン(サンアロマー社製、商品名:サンアロマーPHA03A)を使用した。熱可塑性樹脂は、押出温度290℃、厚さ20μmとなるようにTダイにて押し出し、タック原紙の裏面に熱可塑性樹脂を積層して擬似接着シートとした。次に、シリコーン系剥離紙の離型剤面にアクリル系粘着剤を厚さ25μmになるように塗工して粘着剤層を形成し、先に形成した擬似接着シートの擬似接着層に貼り合わせた。その後、打ち抜き加工及びミシン目加工、カス上げを行って図2に示すような擬似接着ラベルを得た。
[Example 1]
Tack base paper (manufactured by YUPO Corporation, trade name: YUPO TACK base paper 60SGS) was used as the surface substrate. Polypropylene (manufactured by Sun Allomer, trade name: Sun Allomer PHA03A) was used as the thermoplastic resin for forming the pseudo adhesive layer. The thermoplastic resin was extruded with a T-die so that the extrusion temperature was 290 ° C. and the thickness was 20 μm, and a thermoplastic resin was laminated on the back surface of the tack base paper to obtain a pseudo-adhesive sheet. Next, an acrylic pressure-sensitive adhesive is applied to the release agent surface of the silicone release paper to a thickness of 25 μm to form a pressure-sensitive adhesive layer, which is then bonded to the pseudo-adhesive layer of the previously formed pseudo-adhesive sheet. It was. Thereafter, punching, perforation, and scrap removal were performed to obtain a pseudo-adhesive label as shown in FIG.

擬似接着ラベルは、横150mm、縦100mmであって、横方向の中央に断裁線を設けた。断裁線20を構成する切れ目20xの長さは、それぞれ1mm、切れ目間の離間距離dは0.3mmとした。また、線状部20a、20cの長さは46mm、中途部20bの長さは10mmとし、中途部20bは、線状部20a、20cに120度で連接した。さらに、断裁線の幅Xは5mmとした。なお、切れ目は表面基材、擬似接着層及び粘着層を貫通する深さとした。   The pseudo-adhesive label was 150 mm wide and 100 mm long, and a cut line was provided at the center in the horizontal direction. The lengths of the cuts 20x constituting the cutting line 20 were each 1 mm, and the separation distance d between the cuts was 0.3 mm. The length of the linear portions 20a and 20c was 46 mm, the length of the midway portion 20b was 10 mm, and the midway portion 20b was connected to the linear portions 20a and 20c at 120 degrees. Further, the width X of the cutting line was 5 mm. In addition, the cut was made into the depth which penetrates a surface base material, a pseudo adhesion layer, and an adhesion layer.

[比較例1]
断裁線を、擬似接着ラベルの略中央部に、直線的に縦方向に延在するように形成した以外は、実施例1と同様に実施した。
[Comparative Example 1]
The cutting line was carried out in the same manner as in Example 1 except that the cutting line was formed so as to extend linearly in the longitudinal direction in the approximate center of the pseudo-adhesive label.

[評価方法: 擬似側剥離試験]
実施例及び比較例で得られた擬似接着ラベルの剥離基材を引き剥がして除去し、被着物である台紙に粘着剤層を貼着した。この状態で、図2に示す角部18Aから表面基材11のラベル部18を矢印A方向に剥離角度180°で剥離する試験を10回行い、表面基材を破かずに剥がすことができるかを評価した。表面基材の破れが発生した回数を、剥離不良率(破れが発生した回数/試験回数×100)で表し、剥離不良率20%未満を良好、剥離不良率20%以上を不良として評価した。
[Evaluation method: Pseudo-side peeling test]
The peeling base material of the pseudo-adhesive label obtained in Examples and Comparative Examples was peeled off and removed, and an adhesive layer was stuck on a mount as an adherend. In this state, can the test be performed 10 times to peel the label portion 18 of the surface base material 11 from the corner 18A shown in FIG. 2 in the direction of arrow A at a peeling angle of 180 °, and the surface base material can be peeled without breaking? Evaluated. The number of occurrences of tearing of the surface base material was expressed as a peel failure rate (number of breaks generated / number of tests × 100).

表1に、実施例及び比較例で得られた擬似接着ラベルの評価試験の結果を示す。

Figure 2012189946
Table 1 shows the results of the evaluation test of the pseudo-adhesive labels obtained in the examples and comparative examples.
Figure 2012189946

断裁線を直線状にした比較例1では、断裁線に沿って表面基材を切り難く、ラベル部を剥離する際に表面基材の破れが発生しやすかったため、剥離不良率20%以上であった。   In Comparative Example 1 in which the cutting line was linear, it was difficult to cut the surface base material along the cutting line, and the surface base material was easily broken when the label part was peeled off. It was.

これに対し、実施例1では、剥離する際に表面基材に破れが発生することなく擬似接着層から剥離することができたため、剥離不良率が20%未満と良好だった。このように、断裁線を平面視で折れ曲がり線状に形成したことにより、表面基材を断裁線で分離して剥離する際に、表面基材に破れが発生することなく擬似接着層から剥離することができ、作業性の良い擬似接着ラベルを得ることができた。   On the other hand, in Example 1, since it was possible to peel from the pseudo-adhesive layer without tearing the surface base material at the time of peeling, the peel failure rate was good at less than 20%. Thus, by forming the cutting line into a bent line shape in plan view, when the surface base material is separated by the cutting line and peeled off, the surface base material is peeled off from the pseudo-adhesive layer without being broken. Thus, a pseudo-adhesive label with good workability was obtained.

10 擬似接着ラベル
11 表面基材
12 擬似接着層
13 粘着剤層
14 剥離基材
18、19 ラベル部
20 断裁線
20a、20c 線状部
20b 中途部
DESCRIPTION OF SYMBOLS 10 Pseudo-adhesive label 11 Surface base material 12 Pseudo-adhesion layer 13 Adhesive layer 14 Peeling base material 18, 19 Label part 20 Cutting line 20a, 20c Linear part 20b Midway part

Claims (4)

表面基材と、前記表面基材に擬似接着される擬似接着層と、粘着剤層とがこの順に積層された積層構造を備え、前記粘着剤層が被着物に貼着された状態で、前記表面基材を前記擬似接着層から剥離可能な擬似接着ラベルであって、
前記表面基材は、少なくとも2以上のラベル部に分離して前記擬似接着層から剥離可能とするためのミシン目状の断裁線を備え、
前記断裁線における中途部は、その両側の線状部に対して傾斜した形状を有することを特徴とする擬似接着ラベル。
A surface base material, a pseudo-adhesive layer that is pseudo-adhered to the surface base material, and a pressure-sensitive adhesive layer are provided in this order, and the pressure-sensitive adhesive layer is attached to an adherend, A pseudo-adhesive label capable of peeling the surface substrate from the pseudo-adhesive layer,
The surface base material is provided with a perforated cut line for separating into at least two or more label portions and making the peelable peelable layer peelable.
The pseudo-adhesive label characterized in that the midway part in the cutting line has a shape inclined with respect to the linear parts on both sides thereof.
前記中途部は、その両側の線状部に対して鈍角で連接することを特徴とする請求項1に記載の擬似接着ラベル。   The pseudo-adhesive label according to claim 1, wherein the midway part is connected to the linear parts on both sides thereof at an obtuse angle. 前記中途部は、傾斜した直線状であることを特徴とする請求項1に記載の擬似接着ラベル。   The pseudo-adhesive label according to claim 1, wherein the midway part is an inclined straight line. 前記両側の線状部は、互いに平行な直線状となることを特徴とする請求項1に記載の擬似接着ラベル。   The pseudo-adhesive label according to claim 1, wherein the linear portions on both sides are linearly parallel to each other.
JP2011055340A 2011-03-14 2011-03-14 Pseudo adhesive label Pending JP2012189946A (en)