JP2011168469A - 廃石膏再生処理物 - Google Patents
廃石膏再生処理物 Download PDFInfo
- Publication number
- JP2011168469A JP2011168469A JP2010051051A JP2010051051A JP2011168469A JP 2011168469 A JP2011168469 A JP 2011168469A JP 2010051051 A JP2010051051 A JP 2010051051A JP 2010051051 A JP2010051051 A JP 2010051051A JP 2011168469 A JP2011168469 A JP 2011168469A
- Authority
- JP
- Japan
- Prior art keywords
- waste gypsum
- coupling agent
- composite material
- resin
- waste
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Pending
Abstract
【課題】環境汚染廃棄物の廃石膏を薬剤で処理して無害化して樹脂で結合することにより無害な透水物{板、管}に再利用する。
【解決手段】廃石膏の粉砕物をシランカップリング剤0.02〜1%使用の加水分解水溶液でコーティング乾燥、または0.5〜4%の未加水分解のカップリング剤を樹脂混合してなる不飽和ポリエステル樹脂を10〜30%添加して一体の複合材料を成形硬化、複合材料体からフッ素の水溶出量を環境基準の0.8ppm以下にする。
【選択図】なし
【解決手段】廃石膏の粉砕物をシランカップリング剤0.02〜1%使用の加水分解水溶液でコーティング乾燥、または0.5〜4%の未加水分解のカップリング剤を樹脂混合してなる不飽和ポリエステル樹脂を10〜30%添加して一体の複合材料を成形硬化、複合材料体からフッ素の水溶出量を環境基準の0.8ppm以下にする。
【選択図】なし
Description
本発明は廃石膏の無害化処理及びその再利用に関する。
本発明は用途が無い環境汚染物質である廃石膏を処理して無害で再利用が可能となる材料を開発したものである。
本発明は廃石膏から溶出するフッ素化合物などの環境汚染物を無公害化、安定化することと工業材料として再利用するために、種々の薬剤で処理して、有用な廃石膏処理物を製造することにある。
本発明は廃石膏をシランカップリング剤、不飽和ポリエステル樹脂で処理して、環境基準のフッソ溶出量を0.8ppm以下にすることにある
本発明で得られる処理物は透水物{板、管}などに好適に再利用される。
廃石膏を100−1000ミクロンに粉砕したものと希薄酢酸水溶液にシランカップリング剤を加水分解したものを混合した。撹拌しながら加熱乾燥する(以下ポリ石膏という)その後ポリエステル樹脂をポリ石膏に対して10−40%添加し少量の硬化剤0.1−0.5%を同時に添加混合して、バッチ式の乾燥釜またはロータリーキルン乾燥機で加熱乾燥する。廃石膏表面と樹脂との結合を行うカップリング剤としてはシリコン系や脂肪酸系など何でもよいが例えば下記が挙げられる。一般式RSi(OR’)でRは官能基でアミノプロピル基、グリシドシ、メタクリロシキ基、N−ヘニルアミノプロビル基、メルカト基、ビニル基他R’はメチル基、エチル基シランカップリング剤は水と接すると加水分解してシラノ−ル基を生成する。
シラノ−ル基は自己縮合によって高分子化すると同時に金属表面のOH基と酸塩基塩反応で化学結合する。一方官能基Rは塗料成分と化学結合又は架橋して強固に結合する。シランカップリング剤の利点は水/メタノ−ル溶液に溶解し1%以下でも有効に単独コート使用できる。具体例としては信越化学のKBM−13メチルメトキシシランKBE22ジメチルジエトキシシラン、KBM503アクリルシランなど多数ある。不飽和ポリエステル樹脂は通常ポリ廃石膏に対して少なくとも10−40%程度添加し、廃石膏表面を覆う必要があり、樹脂には硬化剤硬化促進剤を適量添加する。得られる廃石膏処理物は、10%添加で水溶出フッソが0.8ppm以下({排出基準)、添加量が増加すればさらに溶出量が減少する。
100−1000ミクロンの廃石膏40KGにKBM575を0.01kg加水分解したものを散布し撹拌しながら加熱乾燥する。シランカップリングされたポリ石膏に不飽和ポリエステル樹脂{たとえばポロホ−プR4701}20KG,硬化剤[たとえばパ−メックN]0.2KG硬化促進剤[たとえばナフテン酸コバルト)0.1KGを混合して遠心成形機の回転型に注入する。その後加熱乾燥[110℃前後)して透水管を得る。得られた透水管は、フッ素化合物の溶出量は0.1ppmで基準の0.8ppm以下で、250mm径の肉厚約25〜30mmである目的管の形状を維持し、コンクリート管並みの強度で透水性能約1L/m2・分の性能が得られた。
100−1000ミクロンの廃石膏40KGに不飽和ポリエステル樹脂{たとえばポロホ−プR4701}20KG、硬化剤[たとえばパ−メックN]0.2KG硬化促進剤[たとえばナフテン酸コバルト)0.1KGにKMB403を0.4kg加水分解せずに添加混合して拡散樹脂を混合してなる粒子分散複合材を、遠心成形機の回転型に注入遠心成形する。その後加熱乾燥[110℃前後)して透水管を得る。得られた透水管は、フッ素化合物の溶出量は0.2ppmで基準の0.8ppm以下で、250mm径の肉厚約25〜30mmである目的管の形状を維持し、コンクリート管並みの強度で透水性能約1L/m2・分の性能が得られた。
Claims (2)
- 廃石膏の粉砕物をシランカップリング剤0.02%〜1%使用の加水分解水溶液を表面コーティング乾燥、または0.5〜4%の未加水分解のカップリング剤を樹脂混合してなる不飽和ポリエステル樹脂を10〜30%添加して一体の複合材料体を成形硬化、複合材料体からフッ素の水溶出量を環境基準の0.8ppm以下にした廃石膏からなる再生処理物。
- 請求項1記載の廃石膏を用いて、複合材料体間に連通する多数の気道を有するように充填材料の樹脂添加量と成形圧力を調整して、一体化してなる構造体化に、気道を透水目的に使用する透水物の板または管。