JP2007100870A5 - - Google Patents

Download PDF

Info

Publication number
JP2007100870A5
JP2007100870A5 JP2005292717A JP2005292717A JP2007100870A5 JP 2007100870 A5 JP2007100870 A5 JP 2007100870A5 JP 2005292717 A JP2005292717 A JP 2005292717A JP 2005292717 A JP2005292717 A JP 2005292717A JP 2007100870 A5 JP2007100870 A5 JP 2007100870A5
Authority
JP
Japan
Prior art keywords
rolling
inner member
zinc coating
rolling device
less
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Pending
Application number
JP2005292717A
Other languages
Japanese (ja)
Other versions
JP2007100870A (en
Filing date
Publication date
Application filed filed Critical
Priority to JP2005292717A priority Critical patent/JP2007100870A/en
Priority claimed from JP2005292717A external-priority patent/JP2007100870A/en
Publication of JP2007100870A publication Critical patent/JP2007100870A/en
Publication of JP2007100870A5 publication Critical patent/JP2007100870A5/ja
Pending legal-status Critical Current

Description

さらに、本発明に係る請求項3の転動装置は、請求項1又は請求項2に記載の転動装置において、前記亜鉛被膜の厚さが0.1μm以上8μm以下であることを特徴とする。
さらに、本発明に係る請求項4の転動装置は、請求項1又は請求項2に記載の転動装置において、前記亜鉛被膜の厚さが0.5μm以上8μm以下であることを特徴とする。
亜鉛被膜の厚さが0.1μm未満であると、十分且つ持続的な防錆効果が得られないおそれがある。一方、亜鉛被膜の厚さが8μm超過であると、亜鉛被膜の脱落が生じやすくなり、転動装置にとって異物となるおそれがある。
Furthermore, the rolling device according to claim 3 according to the present invention is the rolling device according to claim 1 or 2, wherein the zinc coating has a thickness of 0.1 μm or more and 8 μm or less. To do.
Furthermore, the rolling device according to claim 4 according to the present invention is the rolling device according to claim 1 or 2, wherein the thickness of the zinc coating is 0.5 μm or more and 8 μm or less. .
If the thickness of the zinc coating is less than 0.1 μm, there is a possibility that a sufficient and sustained rust prevention effect cannot be obtained. On the other hand, if the thickness of the zinc coating is more than 8 μm, the zinc coating is likely to fall off, which may be a foreign matter for the rolling device.

さらに、本発明に係る請求項5の転動装置は、請求項1〜4のいずれか一項に記載の転動装置において、前記内方部材の表面,前記外方部材の表面,及び前記転動体の表面のうち少なくとも前記亜鉛被膜が備えられた部分に、深さ0.1μm以上5μm以下のディンプルを設けたことを特徴とする。
ディンプルにより亜鉛被膜と母材との密着性が向上する。また、転動装置の駆動時に脱落した亜鉛被膜がディンプル内にトラップされるので、防錆効果が長く維持される。このような効果を得るためには、ディンプルの深さを0.1μm以上とすることが好ましい。ただし、ディンプルの深さを5μm超過としても、それ以上の効果は期待できないので、ディンプルの深さは5μm以下とすることが好ましい。
Furthermore, the rolling device according to a fifth aspect of the present invention is the rolling device according to any one of the first to fourth aspects, wherein the surface of the inner member, the surface of the outer member, and the rolling device. A dimple having a depth of 0.1 μm or more and 5 μm or less is provided on at least a portion of the surface of the moving body provided with the zinc coating.
The dimple improves the adhesion between the zinc coating and the base material. In addition, since the zinc coating that has fallen off when the rolling device is driven is trapped in the dimples, the antirust effect is maintained for a long time. In order to obtain such an effect, the depth of the dimple is preferably set to 0.1 μm or more. However, even if the dimple depth exceeds 5 μm, no further effect can be expected. Therefore, the dimple depth is preferably 5 μm or less.

さらに、本発明に係る請求項6の転動装置は、請求項1〜5のいずれか一項に記載の転動装置において、前記亜鉛被膜の表面の中心線平均粗さRaが0.1μm以上0.5μm以下であることを特徴とする。
このような構成であれば、防錆効果が得られるとともに、転動装置の音響特性が良好である。特に、内方部材の軌道面,外方部材の軌道面,及び転動体の転動面に亜鉛被膜を形成する場合には、亜鉛被膜の表面の中心線平均粗さRaを上記範囲内とすることが好ましい。亜鉛被膜の表面の中心線平均粗さRaが0.5μm超過であると、音響特性が不十分となるおそれがある。一方、中心線平均粗さRaを0.1μm未満とすると、転動装置が高価となってしまうおそれがある。
Furthermore, the rolling device of Claim 6 which concerns on this invention is a rolling device as described in any one of Claims 1-5. The centerline average roughness Ra of the surface of the said zinc coating is 0.1 micrometer or more. It is 0.5 μm or less.
With such a configuration, an antirust effect is obtained and the acoustic characteristics of the rolling device are good. In particular, when a zinc coating is formed on the raceway surface of the inner member, the raceway surface of the outer member, and the rolling surface of the rolling element, the center line average roughness Ra of the surface of the zinc coating is within the above range. It is preferable. If the center line average roughness Ra of the surface of the zinc coating is more than 0.5 μm, the acoustic characteristics may be insufficient. On the other hand, if the center line average roughness Ra is less than 0.1 μm, the rolling device may be expensive.

Claims (6)

外面に軌道面を有する内方部材と、該内方部材の軌道面に対向する軌道面を有し前記内方部材の外方に配された外方部材と、前記両軌道面間に転動自在に配された複数の転動体と、を備える転動装置において、
前記内方部材,前記外方部材,及び前記転動体のうち少なくとも一つは、その表面の少なくとも一部に、機械的エネルギーにより形成された亜鉛被膜を備えていることを特徴とする転動装置。
An inner member having a raceway surface on the outer surface, an outer member having a raceway surface opposite to the raceway surface of the inner member, and arranged on the outer side of the inner member, and rolling between the both raceway surfaces In a rolling device comprising a plurality of freely arranged rolling elements,
At least one of the inner member, the outer member, and the rolling element includes a zinc coating formed by mechanical energy on at least a part of the surface thereof. .
外面に軌道面を有する内方部材と、該内方部材の軌道面に対向する軌道面を有し前記内方部材の外方に配された外方部材と、前記両軌道面間に転動自在に配された複数の転動体と、を備える転動装置において、
前記内方部材,前記外方部材,及び前記転動体のうち少なくとも一つは、その表面の少なくとも一部に、亜鉛粉末のショットピーニングにより形成された亜鉛被膜を備えていることを特徴とする転動装置。
An inner member having a raceway surface on the outer surface, an outer member having a raceway surface opposite to the raceway surface of the inner member, and arranged on the outer side of the inner member, and rolling between the both raceway surfaces In a rolling device comprising a plurality of freely arranged rolling elements,
At least one of the inner member, the outer member, and the rolling element includes a zinc coating formed by shot peening of zinc powder on at least a part of the surface thereof. Moving device.
前記亜鉛被膜の厚さが0.1μm以上8μm以下であることを特徴とする請求項1又は請求項2に記載の転動装置。 The rolling device according to claim 1 or 2, wherein a thickness of the zinc coating is 0.1 µm or more and 8 µm or less. 前記亜鉛被膜の厚さが0.5μm以上8μm以下であることを特徴とする請求項1又は請求項2に記載の転動装置。The rolling device according to claim 1 or 2, wherein a thickness of the zinc coating is 0.5 µm or more and 8 µm or less. 前記内方部材の表面,前記外方部材の表面,及び前記転動体の表面のうち少なくとも前記亜鉛被膜が備えられた部分に、深さ0.1μm以上5μm以下のディンプルを設けたことを特徴とする請求項1〜4のいずれか一項に記載の転動装置。Of the surface of the inner member, the surface of the outer member, and the surface of the rolling element, dimples having a depth of 0.1 μm or more and 5 μm or less are provided at least in a portion provided with the zinc coating. The rolling device according to any one of claims 1 to 4. 前記亜鉛被膜の表面の中心線平均粗さRaが0.1μm以上0.5μm以下であることを特徴とする請求項1〜5のいずれか一項に記載の転動装置。The rolling device according to any one of claims 1 to 5, wherein a center line average roughness Ra of the surface of the zinc coating is 0.1 µm or more and 0.5 µm or less.
JP2005292717A 2005-10-05 2005-10-05 Rolling device Pending JP2007100870A (en)