CN2793499Y - 新型内衬聚四氟乙烯钢制防腐活接 - Google Patents

新型内衬聚四氟乙烯钢制防腐活接 Download PDF

Info

Publication number
CN2793499Y
CN2793499Y CN 200520020967 CN200520020967U CN2793499Y CN 2793499 Y CN2793499 Y CN 2793499Y CN 200520020967 CN200520020967 CN 200520020967 CN 200520020967 U CN200520020967 U CN 200520020967U CN 2793499 Y CN2793499 Y CN 2793499Y
Authority
CN
China
Prior art keywords
joint
end socket
locking cap
lock cap
flexible joint
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Expired - Fee Related
Application number
CN 200520020967
Other languages
English (en)
Inventor
李永昌
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Individual
Original Assignee
Individual
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Individual filed Critical Individual
Priority to CN 200520020967 priority Critical patent/CN2793499Y/zh
Application granted granted Critical
Publication of CN2793499Y publication Critical patent/CN2793499Y/zh
Anticipated expiration legal-status Critical
Expired - Fee Related legal-status Critical Current

Abstract

本实用新型公开了一种新型内衬聚四氟乙烯钢制防腐活接,该活接包括锁紧帽(1)、左接头(2)和右接头(3),其特征在于:锁紧帽(1)的外部形状为4-8角形;左、右接头(2、3)均有变径,并在变径处分为内、外端头;左接头(2)内端头部分外侧有螺纹,外端头部分为扁形(4),左接头(2)与锁紧帽(1)的接合部位螺纹连接。本实用新型将左接头(2)的外端头部分设计成扁形,锁紧帽为多角形,角对管钳形成阻力,使管钳在拧紧的过程中不打滑。这样安装后的活接,密封效果好。解决了原用活接密封效果不好,输送管线内的腐蚀性介质容易泄漏的问题。

Description

新型内衬聚四氟乙烯钢制防腐活接
技术领域:
本实用新型属于防腐管道连接件,具体是内衬聚四氟乙烯钢制防腐活接。
背景技术:
在油田、化工等行业中使用的内衬聚四氟乙烯钢管及管件等防腐管道之间的连接,多数都是采用法兰式连接,而在埋地管线的连接中,其连接方式是采用接头(活接)连接。在内衬聚四氟乙烯钢制防腐活接构件中,包括锁紧帽、左接头和右接头,活接的外形均为圆柱状。尤其是锁紧帽、左接头的外形是圆柱状,因此在实际使用中由于外形为圆形、光滑,安装时管钳打滑,拧不紧,使左右接头的接触面不能贴紧,达不到密封效果,管道输送的腐蚀性介质易渗出腐蚀锁紧帽,严重时会使管线穿孔,影响生产。
发明内容:
本实用新型的目的是针对上述问题对活接的外形进行改进而设计的一种新型内衬聚四氟乙烯钢制防腐活接。
本实用新型的技术方案是这样实现的:新型内衬聚四氟乙烯钢制防腐活接包括锁紧帽、左接头和右接头;锁紧帽的外部形状为4-8角形;左、右接头均有变径,并在变径处分为内、外端头;左接头内端头部分外侧有螺纹,外端头部分为扁形,左接头与锁紧帽的接合部位螺纹连接。
本实用新型的有益效果:本实用新型将左接头2的外端头部分设计成扁形,锁紧帽为多角形,角对管钳形成阻力,使管钳在拧紧的过程中不打滑,这样安装后的活接,密封效果好,输送管线内的腐蚀性介质不泄漏。
附图说明:
图1是本实用新型的连接状态结构剖视图;
图2是本实用新型中锁紧帽的结构示意图;
图3是图2A向结构示意图;
图4是本实用新型中左接头的结构示意图;
图5是图4B向结构示意图。
图中:1锁紧帽、2左接头、3右接头、4扁形。
具体实施方式:
图1提供的是本实用新型安装状态的结构剖视图,图中所述的新型内衬聚四氟乙烯钢制防腐活接包括锁紧帽1、左接头2和右接头3;锁紧帽1的外部形状为4-8角形;在实际生产中锁紧帽1的外部形状以6角形为最佳,参阅图2,图3为图2中A向结构视图。左、右接头2、3均有变径,在变径处分成内端头和外端头两部分。左接头2内端头部分外侧有螺纹,内端头的螺纹部分与锁紧帽1螺纹连接,左接头2的外端头部分为扁形4,参阅图4,图5为图4中B向结构视图。使用时,先将左右接头分别焊接在钢管或管件上,在管内或管件内衬入聚四氟乙烯管,并将聚四氟乙烯管经扩口、翻边等工艺处理后,是其紧贴于左右接头的密封面上。安装时,用管钳分别卡住左接头2外端头的扁形4和锁紧帽1,此时,右接头3是戴在与锁紧帽1内,随着管钳的不断拧紧,左右接头逐渐靠拢、贴近,最后形成密封。安装好后,对锁紧帽1、左右接头2、3外表面进行沥青特加强防腐处理。

Claims (2)

1、一种新型内衬聚四氟乙烯钢制防腐活接,该活接包括锁紧帽(1)、左接头(2)和右接头(3),其特征在于:锁紧帽(1)的外部形状为4-8角形;左、右接头(2、3)均有变径,并在变径处分为内、外端头;左接头(2)内端头部分外侧有螺纹,外端头部分为扁形(4),左接头(2)与锁紧帽(1)的接合部位螺纹连接。
2、根据权利要求1所述的新型内衬聚四氟乙烯钢制防腐活接,其特征在于:锁紧帽(1)的外部形状为6角形。
CN 200520020967 2005-06-07 2005-06-07 新型内衬聚四氟乙烯钢制防腐活接 Expired - Fee Related CN2793499Y (zh)