CN211250419U - Core board for impregnated bond paper facing laminated wood board - Google Patents
Core board for impregnated bond paper facing laminated wood board Download PDFInfo
- Publication number
- CN211250419U CN211250419U CN201921943803.5U CN201921943803U CN211250419U CN 211250419 U CN211250419 U CN 211250419U CN 201921943803 U CN201921943803 U CN 201921943803U CN 211250419 U CN211250419 U CN 211250419U
- Authority
- CN
- China
- Prior art keywords
- veneer
- core
- board
- core board
- blockboard
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Active
Abstract
Description
技术领域technical field
本实用新型属于浸渍胶膜纸饰面细木工板技术领域,具体地说是一种用于浸渍胶膜纸饰面细木工板上的芯板。The utility model belongs to the technical field of impregnated plastic film paper facing blockboards, in particular to a core board used for impregnating plastic film paper facing blockboards.
背景技术Background technique
目前,浸渍胶膜纸饰面细木工板已被广泛应用于家具、车厢、船舶、建筑等领域。浸渍胶膜纸饰面细木工板是指在胶合板生产基础上,以木板条拼接或空心板作芯板,两面覆盖两层或多层胶合板,经胶压制成的一种特殊胶合板。浸渍胶膜纸饰面细木工板的性能主要由芯板结构决定,芯板的结构及制作方法对于浸渍胶膜纸饰面细木工板的横向静曲强度、表面平整度、厚度偏差等主要用于评价浸渍胶膜纸饰面细木工板性能的技术参数起着重要作用。At present, the impregnated film paper veneer blockboard has been widely used in furniture, carriages, ships, construction and other fields. Impregnated film paper veneer blockboard refers to a special kind of plywood made by glue pressing on the basis of plywood production, with wood slats spliced or hollow board as the core board, covered with two or more layers of plywood on both sides. The performance of the impregnated film paper veneer blockboard is mainly determined by the structure of the core board. The structure and production method of the core board are mainly used for the transverse static bending strength, surface flatness and thickness deviation of the impregnated film paper veneer blockboard. The technical parameters for evaluating the performance of impregnated film paper veneer blockboards play an important role.
现有技术中,在制作芯板的芯条时多层单板组坯热压后,通常将单板的叠合方向置于芯条的厚度方向上、单板的顺纹方向位于芯条的长度方向上。由于这种芯板结构中单板的叠合方向不能限制单板沿顺纹方向的变形,所获得的芯板及芯板应用的浸渍胶膜纸饰面细木工板,很容易沿单板顺纹方向发生翘曲,影响芯板及芯板所应用的浸渍胶膜纸饰面细木工板的横向静曲强度及表面平整度,不仅使得浸渍胶膜纸饰面细木工板的使用寿命降低、外部美观性变差,而且也会影响浸渍胶膜纸饰面细木工板的市场销售,降低企业的生产效益。In the prior art, after the multi-layer veneer group blank is hot-pressed when making the core strip of the core board, the stacking direction of the veneer is usually placed in the thickness direction of the core strip, and the grain direction of the veneer is located in the core strip. lengthwise. Since the superposition direction of the veneer in this core board structure cannot limit the deformation of the veneer along the grain direction, the obtained core board and the impregnated film paper veneer blockboard applied to the core board are easy to follow along the veneer direction. The warpage in the grain direction affects the transverse static bending strength and surface flatness of the core board and the impregnated film paper veneer blockboard applied to the core board, which not only reduces the service life of the impregnated film paper veneer blockboard, The external aesthetics will become poor, and it will also affect the market sales of impregnated film paper-faced blockboards, reducing the production efficiency of enterprises.
实用新型内容Utility model content
为解决现有技术中存在的以上不足,本实用新型旨在提供一种用于浸渍胶膜纸饰面细木工板上的芯板,以达提高芯板所应用的浸渍胶膜纸饰面细木工板抗变形能力、保证浸渍胶膜纸饰面细木工板表面平整的目的。In order to solve the above deficiencies in the prior art, the present utility model aims to provide a core board for impregnating film paper veneer blockboard, so as to improve the fineness of the dipping film paper veneer applied to the core board. The purpose of the anti-deformation ability of the wood board and to ensure the smooth surface of the block board with the impregnated film paper veneer.
为实现上述目的,本实用新型所采用的技术方案如下:用于浸渍胶膜纸饰面细木工板上的芯板,用于浸渍胶膜纸饰面细木工板上的芯板由多个芯条粘接拼制而成,每个芯条由N层单板组坯后热压而成,且单板的叠合方向位于芯条的宽度方向上、单板的顺纹方向位于芯条的长度方向上,其中N≥2。In order to achieve the above purpose, the technical scheme adopted by the present utility model is as follows: the core board used for impregnating the plastic film paper facing blockboard, the core board used for impregnating the plastic film paper facing blockboard is composed of a plurality of cores. The strips are bonded and assembled, and each core strip is made of N layers of veneer blanks and then hot-pressed. In the length direction, where N≥2.
作为本实用新型的限定,芯条的长度为500mm,宽度为45mm,厚度为12mm。As a limitation of the present invention, the length of the core strip is 500mm, the width is 45mm, and the thickness is 12mm.
由于采用了上述的技术方案,本实用新型与现有技术相比,所取得的有益效果是:Owing to adopting the above-mentioned technical scheme, compared with the prior art, the beneficial effects obtained by the present utility model are:
本实用新型改变了芯条中单板的放置方向,使单板的顺纹方向与芯条的变形方向相错,从而使芯板中的内应力发生变化,避免芯板沿单板顺纹方向发生变形,所获得芯板应用的浸渍胶膜纸饰面细木工板横向静曲强度提升至35~50MPa,平整度偏差不大于0.9%,厚度偏差为±0.2mm,从而提升浸渍胶膜纸饰面细木工板的使用寿命、美观度,提高单板的使用率及应用价值,增加企业的经济效益。The utility model changes the placement direction of the veneer in the core strip, so that the direction of the veneer along the grain is different from the deformation direction of the core strip, so that the internal stress in the core board changes, and the core board is prevented from running along the grain direction of the veneer. Deformation occurs, and the transverse static bending strength of the impregnated film paper facing blockboard applied to the core board is increased to 35-50MPa, the flatness deviation is not more than 0.9%, and the thickness deviation is ±0.2mm, thereby improving the impregnated film paper decoration. Improve the service life and aesthetics of the surface blockboard, improve the utilization rate and application value of the veneer, and increase the economic benefits of the enterprise.
本实用新型中制作方法中单板含水率、热压单位压力、热压时间、热压温度值相互配合,能够获得具有一定胶合强度、结构稳定、防止单板表面崩裂的板方。In the production method of the utility model, the moisture content of the veneer, the unit pressure of hot pressing, the hot pressing time, and the hot pressing temperature value cooperate with each other, so that a board with certain bonding strength, stable structure and preventing the surface of the veneer from cracking can be obtained.
本实用新型适用于家具、车厢、船舶、建筑等领域,特别是衣柜、橱柜、门扇等柜门上使用。The utility model is suitable for the fields of furniture, carriages, ships, buildings and the like, especially for use on cabinet doors such as wardrobes, cabinets, door leaves and the like.
附图说明Description of drawings
下面结合附图及具体实施例对本实用新型作更进一步详细说明。The present utility model will be described in further detail below in conjunction with the accompanying drawings and specific embodiments.
图1为本实用新型实施例1的芯板结构示意图;1 is a schematic diagram of a core board structure according to
图2为本实用新型实施例1的芯条放大结构示意图。FIG. 2 is a schematic view of the enlarged structure of the core strip according to
图中:1、单板;2、芯条。In the picture: 1. Veneer; 2. Core strip.
具体实施方式Detailed ways
以下结合附图对本实用新型的优选实施例进行说明。应当理解,此处所描述的优选实施例仅用于说明和理解本实用新型,并不用于限定本实用新型。The preferred embodiments of the present utility model will be described below with reference to the accompanying drawings. It should be understood that the preferred embodiments described herein are only used to illustrate and understand the present invention, but not to limit the present invention.
实施例1 一种用于浸渍胶膜纸饰面细木工板上的芯板Example 1 A core board for impregnating adhesive film paper veneer blockboard
本实施例通过改变芯条中单板1的放置方向,使芯板的变形方向与单板1的木纹方向相错,以使芯板中的内应力发生变化,从而提高芯板的抗变形能力及表面平整度。In this embodiment, by changing the placement direction of the
如图1至图2所示,本实施例中用于浸渍胶膜纸饰面细木工板上的芯板由多个芯条2粘接拼制而成,芯条由多个单板1胶合拼制而成。As shown in Fig. 1 to Fig. 2 , in this embodiment, the core board used to impregnate the adhesive film paper veneer blockboard is made of a plurality of
将单板1的上下两平面分别涂胶,按照由上而下的顺序叠加N层,完成单板1的组坯。其中,N≥2,本实施例中,N=14。组坯后,由浸渍胶膜纸饰面细木工板生产通用热压机将单板层热压获得板方,按规定尺寸裁切板方后形成芯条2,芯条2的长度为500mm,宽度为45mm,厚度为12mm。本文所指的多个为两个以上。Apply glue to the upper and lower planes of the
在拼合芯条2时,芯条2的长度大于芯条2宽度,需保证单板1的叠合方向位于芯条2的宽度方向上、单板1的顺纹方向位于芯条2的长度方向上。即单板层叠加厚度为芯条2宽度,单板1的延伸长度为芯条2的延伸长度,这样,单板1的顺纹方向与芯板的变形方向相错。When splicing the
放置好芯条2后,将芯条2的侧面通过胶粘剂与另一个芯条2粘接,根据制板要求,将芯条2拼制成芯板。After the
本实施例的制作方法参照实施例2、实施例3中所述。For the preparation method of this embodiment, refer to the description in
实施例2 一种用于浸渍胶膜纸饰面细木工板上的芯板制作方法Embodiment 2 A kind of core board manufacturing method for impregnating adhesive film paper veneer blockboard
本实施例用于制作实施例1中用于浸渍胶膜纸饰面细木工板上的芯板2,包括以下步骤:The present embodiment is used to manufacture the
(一)单板1组坯热压形成芯条2(1) Hot pressing of
将单板1与单板1之间涂胶粘合,按照由上而下的顺序叠加N层,完成单板1的组坯。其中,N≥2,本实施例中,N=14。The
组坯后,由热压机将单板层热压,热压单位压力为8~12公斤/平方厘米,热压时间为15~30分钟,热压温度为115~120℃,获得规定尺寸的芯条2。After assembling the blanks, the veneer layer is hot-pressed by a hot-pressing machine, the unit pressure of hot-pressing is 8-12 kg/
需保证,N层单板1的叠合方向位于芯条2的宽度方向上,且单板1的顺纹方向位于芯条2的长度方向上,即单板层叠加的厚度为芯条2的宽度,单板1的延伸长度为芯条2的延伸长度。也就是说,将由上而下依次叠加的单板层,旋转90°后,使单板层呈由左往右依次叠加,可参考图2所示。这样,所形成的芯条2的长度为500mm,宽度(即单板1层的叠加厚度)为45mm±0.2 mm,厚度为12mm。It should be ensured that the stacking direction of the N-
(二)拼合芯条2(2) Split
将芯条2的侧面通过胶粘剂与另一个芯条2粘接,根据制板要求,将芯条2拼制成芯板。The side of the
实施例3 一种用于浸渍胶膜纸饰面细木工板上的芯板制作方法Embodiment 3 A kind of core board manufacturing method for impregnating adhesive film paper veneer blockboard
本实施例用于制作实施例1中用于浸渍胶膜纸饰面细木工板上的芯板,包括以下步骤:The present embodiment is used to manufacture the core board used to impregnate the adhesive film paper facing blockboard in Example 1, including the following steps:
(一)将木段切削成单板1(1) Cutting wood segments into
将木段通过旋切或刨切成单板1,且切削方向与单板1顺纹方向垂直,所获得的单板1顺纹方向与单板1长度方向一致。木段为杨木、樟木、杉木中的任意一种。所获得的单板1长度为1265mm,宽度为650mm,厚度为3mm。经烘干后,单板1含水率小于8%。The wood segment is cut into
(二)由单板1组坯热压后形成板方(2) After hot pressing of 1 group of veneer blanks, the plate square is formed
将单板1与单板1之间涂胶粘合,按照由上而下的顺序叠加N层,完成单板1的组坯。其中,N≥2,本实施例中,N=14。The
组坯后,由热压机将单板层热压,热压单位压力为8~12公斤/平方厘米,热压时间为15~30分钟,热压温度为115~120℃,获得长度为1265mm,宽度为650mm,厚度(即单板层的叠加厚度)为45mm±0.2 mm的板方,风冷后待用。After assembling the blanks, the veneer layer is hot-pressed by a hot-pressing machine, the unit pressure of hot-pressing is 8-12 kg/
(三)由板方裁切成芯条2(3) Cut from the board into
按规定尺寸将板方锯成芯条2。需保证,N层单板1的叠合方向位于芯条2的宽度方向上,且单板1的顺纹方向位于芯条2的长度方向上,即单板层叠加的厚度为芯条2的宽度,单板1的延伸长度为芯条2的延伸长度。也就是说,将由上而下依次叠加的单板层,旋转90°后,使单板层呈由左往右依次叠加,可参考图2所示。这样,所形成的芯条2的长度为500mm,宽度(即单板层的叠加厚度)为45mm±0.2 mm,厚度为12mm。Saw the board square into
(四)拼合芯条2(4)
将芯条的侧面通过胶粘剂与另一个芯条2粘接,根据制板要求,将芯条2拼至成芯板。The side of the core strip is bonded to another
实施例4~8 一种用于浸渍胶膜纸饰面细木工板上的芯板制作方法Embodiment 4-8 A kind of core board manufacturing method for impregnating adhesive film paper veneer blockboard
所述制备方法与实施例2的制备步骤相同,不同之处在于各步骤中所涉及到的参数有区别,具体见表1。The preparation method is the same as the preparation step of Example 2, except that the parameters involved in each step are different, as shown in Table 1 for details.
所获得的用于浸渍胶膜纸饰面细木工板上的芯板应用在浸渍胶膜纸饰面细木工板上,即浸渍胶膜纸饰面细木工板由上而下包括相互粘接的上浸渍胶覆膜纸、上科技木皮、上单板、用于浸渍胶膜纸饰面细木工板上的芯板、下单板、下科技木皮以及下浸渍胶覆膜纸,浸渍胶膜纸饰面细木工板的性能优于普通浸渍胶膜纸饰面细木工板性能,具体见表2。其中,横向静曲强度的测定采用中华人民共和国国家标准GB/T 17657-2013,平整度及厚度测量采用中华人民共和国国家标准GB/T 19367-2009,且横向静曲强度、平整度偏差、厚度偏差均满足中华人民共和国国家标准GB/T 34722-2017中的要求。The obtained core board for the impregnated adhesive film paper facing blockboard is applied on the impregnated adhesive film paper facing blockboard, that is, the impregnated adhesive film paper facing blockboard is from top to bottom including mutually bonded Top impregnated laminated paper, top technical veneer, top veneer, core board for impregnated laminated paper veneer blockboard, bottom veneer, bottom technical veneer and bottom impregnated laminated paper, impregnated laminated paper The performance of the veneer blockboard is better than that of the common impregnated film paper veneer blockboard, see Table 2 for details. Among them, the measurement of transverse static bending strength adopts the national standard of the People's Republic of China GB/T 17657-2013, the measurement of flatness and thickness adopts the national standard of the People's Republic of China GB/T 19367-2009, and the transverse static bending strength, flatness deviation, thickness The deviations all meet the requirements in the National Standard of the People's Republic of China GB/T 34722-2017.
实施例9~13 一种用于浸渍胶膜纸饰面细木工板上的芯板制作方法Embodiments 9-13 A method for making core boards for impregnating adhesive film paper veneer blockboards
所述制备方法与实施例3的制备步骤相同,不同之处在于各步骤中所涉及到的参数有区别,具体见表3。The preparation method is the same as the preparation step of Example 3, except that the parameters involved in each step are different, as shown in Table 3 for details.
所获得的用于浸渍胶膜纸饰面细木工板上的芯板应用在浸渍胶膜纸饰面细木工板上,即浸渍胶膜纸饰面细木工板由上而下包括相互粘接的上浸渍胶覆膜纸、上科技木皮、上单板、用于浸渍胶膜纸饰面细木工板上的芯板、下单板、下科技木皮以及下浸渍胶覆膜纸,浸渍胶膜纸饰面细木工板的性能优于普通浸渍胶膜纸饰面细木工板性能,具体见表4。其中,横向静曲强度的测定采用中华人民共和国国家标准GB/T 17657-2013,平整度及厚度测量采用中华人民共和国国家标准GB/T 19367-2009,且横向静曲强度、平整度偏差、厚度偏差均满足中华人民共和国国家标准GB/T 34722-2017中的要求。The obtained core board for the impregnated adhesive film paper facing blockboard is applied on the impregnated adhesive film paper facing blockboard, that is, the impregnated adhesive film paper facing blockboard is from top to bottom including mutually bonded Top impregnated laminated paper, top technical veneer, top veneer, core board for impregnated laminated paper veneer blockboard, bottom veneer, bottom technical veneer and bottom impregnated laminated paper, impregnated laminated paper The performance of the veneer blockboard is better than that of the ordinary impregnated film paper veneer blockboard, as shown in Table 4. Among them, the measurement of transverse static bending strength adopts the national standard of the People's Republic of China GB/T 17657-2013, the measurement of flatness and thickness adopts the national standard of the People's Republic of China GB/T 19367-2009, and the transverse static bending strength, flatness deviation, thickness The deviations all meet the requirements in the National Standard of the People's Republic of China GB/T 34722-2017.
需要说明的是,以上所述仅为本实用新型的优选实施例而已,并不用于限制本实用新型,尽管参照上述实施例对本实用新型进行了详细的说明,对于本领域技术人员来说,其依然可以对上述各实施例所记载的技术方案进行修改,或者对其中部分技术特征进行等同替换。凡在本实用新型的精神和原则之内,所作的任何修改、等同替换、改进等,均应包含在本实用新型的保护范围之内。It should be noted that the above are only preferred embodiments of the present invention, and are not intended to limit the present invention. Although the present invention has been described in detail with reference to the above embodiments, those skilled in the art will The technical solutions described in the above embodiments can still be modified, or some technical features thereof can be equivalently replaced. Any modification, equivalent replacement, improvement, etc. made within the spirit and principle of the present invention shall be included in the protection scope of the present invention.
Claims (2)