CN207124235U - 一种负极片折片结构 - Google Patents
一种负极片折片结构 Download PDFInfo
- Publication number
- CN207124235U CN207124235U CN201720747140.4U CN201720747140U CN207124235U CN 207124235 U CN207124235 U CN 207124235U CN 201720747140 U CN201720747140 U CN 201720747140U CN 207124235 U CN207124235 U CN 207124235U
- Authority
- CN
- China
- Prior art keywords
- section
- coated
- negative plate
- substrate
- plate flap
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Active
Abstract
一种负极片折片结构,包括基片(1),所述的基片(1)包括涂设段(1.1)和基片本体段(1.2),所述的涂设段(1.1)于基片(1)上涂设负极材料以形成所述的涂设段,所述的基片本体段(1.2)由涂设段(1.1)上的基片(1)自端部延伸以形成所述的基片本体段,所述的基片本体段(1.2)经折叠形成不易起皱变形的折叠段。本实用新型的负极片折片结构不易起皱变形,在操作时便于插入。
Description
技术领域
本实用新型涉及锂离子电池制作领域,具体讲是指一种负极片折片结构。
背景技术
在锂离子电池的制作过程中所形成的负极片,因负极片的端部段上没有涂覆负极材料,而没有涂负极材料的负极片端部段质地较软,在进行后续工序时,如进行插入动作时容易起皱,不便于实际操作。
实用新型内容
本实用新型要解决的技术问题是,提供一种不易起皱变形,便于插入动作的负极片折片结构。
为解决上述技术问题,本实用新型提供的技术方案为:包括基片,所述的基片包括涂设段和基片本体段,所述的涂设段于基片上涂设负极材料以形成所述的涂设段,所述的基片本体段由涂设段上的基片自端部延伸以形成所述的基片本体段,所述的基片本体段经折叠形成不易起皱变形的折叠段。
优选地,所述的负极材料为铜箔。
优选地,所述的基片为长条状片体。
在一个实施例中,所述的折叠段包括基体部和折叠部,所述的基体部与涂设段连接,所述的折叠部折叠在基体部上,易于折叠操作。
优选地,所述的基体部与折叠部上下对齐,插入时顺畅。
在另一个实施例中,所述的折叠段包括多个折叠部,所述的多个折叠部经卷绕折叠后整体扁平,强度增加,防皱效果显著。
本实用新型的一种负极片折片结构,因基片本体段为折叠段,整体强度增加,不易起皱变形,便于后续的插入动作。
附图说明
图1是本实用新型的一种负极片折片结构的一个实施例的结构示意图(折叠状态)。
图2是本实用新型的一种负极片折片结构的一个实施例的结构示意图(展开状态)。
图3是本实用新型的一种负极片折片结构的又一实施例的结构示意图(折叠状态)。
本实用新型图中所示:
1基片,1.1涂设段,1.2基片本体段,1.21基体部,1.22折叠部。
具体实施方式
下面结合附图对本实用新型做进一步的详细说明。
如图所示,本实用新型的一种负极片折片结构,包括基片1,所述的基片1包括涂设段 1.1和基片本体段1.2。其中所述的涂设段1.1于基片1上涂设负极材料以形成所述的涂设段。所述的基片本体段1.2由涂设段1.1上的基片1自端部延伸以形成所述的基片本体段。所述的基片本体段1.2经折叠形成不易起皱变形的折叠段。
作为负极材料的一种选择,所述的负极材料为铜箔。
作为基片1,所述的基片1可以采用长条状片体。
在一个实施例中,所述的折叠段包括基体部1.21和折叠部1.22,所述的基体部1.21与涂设段1.1连接,所述的折叠部1.22折叠在基体部1.21上。参考图1和图2。
此时,所述的基体部1.21与折叠部1.22上下对齐。
在另一个实施例中,所述的折叠段包括多个折叠部1.22,所述的多个折叠部1.22经卷绕折叠后整体呈扁平状态。参考图3。
Claims (6)
1.一种负极片折片结构,包括基片(1),其特征在于:所述的基片(1)包括涂设段(1.1)和基片本体段(1.2),所述的涂设段(1.1)于基片(1)上涂设负极材料以形成所述的涂设段,所述的基片本体段(1.2)由涂设段(1.1)上的基片(1)自端部延伸以形成所述的基片本体段,所述的基片本体段(1.2)经折叠形成不易起皱变形的折叠段。
2.根据权利要求1所述的一种负极片折片结构,其特征在于:所述的负极材料为铜箔。
3.根据权利要求1所述的一种负极片折片结构,其特征在于:所述的基片(1)为长条状片体。
4.根据权利要求1或3所述的一种负极片折片结构,其特征在于:所述的折叠段包括基体部(1.21)和折叠部(1.22),所述的基体部(1.21)与涂设段(1.1)连接,所述的折叠部(1.22)折叠在基体部(1.21)上。
5.根据权利要求4所述的一种负极片折片结构,其特征在于:所述的基体部(1.21)与折叠部(1.22)上下对齐。
6.根据权利要求1所述的一种负极片折片结构,其特征在于:所述的折叠段包括多个折叠部(1.22),所述的多个折叠部(1.22)经卷绕折叠后整体呈扁平状态。