CN206789566U - A kind of lithium ion battery Soft Roll rushes shell mould - Google Patents
A kind of lithium ion battery Soft Roll rushes shell mould Download PDFInfo
- Publication number
- CN206789566U CN206789566U CN201720546966.4U CN201720546966U CN206789566U CN 206789566 U CN206789566 U CN 206789566U CN 201720546966 U CN201720546966 U CN 201720546966U CN 206789566 U CN206789566 U CN 206789566U
- Authority
- CN
- China
- Prior art keywords
- mold
- die
- guide
- punch
- ion battery
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Active
Abstract
Description
技术领域technical field
本实用新型涉及锂离子电池生产模具,特别是涉及一种锂离子电池软包冲壳模具。The utility model relates to a lithium ion battery production mold, in particular to a lithium ion battery soft package punching mold.
背景技术Background technique
目前聚合物锂离子电池在生产过程中,若铝塑膜坑深过大(≥3.9mm),则铝塑膜成型后R角位会有过度拉伸的隐患,从而导致角位铝层残留量不达标的现象;模具弹簧过少则在冲压铝塑膜过程中上下模板对铝塑膜压力不均匀,导致在铝塑膜起皱影响电池外观等问题,所以必须保证上下模板能准确并均匀压紧铝塑膜,使冲坑时4个边可以均匀拉伸,目前由于模具冲压精度不够很难达到要求。At present, in the production process of polymer lithium-ion batteries, if the pit depth of the aluminum-plastic film is too large (≥3.9mm), there will be a hidden danger of excessive stretching at the R corner after the aluminum-plastic film is formed, resulting in residual aluminum layer at the corner If the mold spring is too small, the upper and lower templates will have uneven pressure on the aluminum-plastic film in the process of stamping the aluminum-plastic film, which will cause problems such as wrinkling of the aluminum-plastic film and affecting the appearance of the battery. Therefore, it is necessary to ensure that the upper and lower templates can be pressed accurately and evenly. Tighten the aluminum-plastic film so that the four sides can be stretched evenly when punching the hole. At present, it is difficult to meet the requirements due to insufficient stamping precision of the mold.
发明内容Contents of the invention
本实用新型的目的就是针对上述问题,提供一种锂离子电池软包冲壳模具。The purpose of this utility model is to provide a kind of lithium-ion battery soft package punching mold for the above problems.
本实用新型所采用的技术方案是:一种锂离子电池软包冲壳模具,包括:上模板、下模板,上模板上设有模具冲头、模具冲头底座、模具弹簧、限高螺丝和销钉,上模板与下模板之间设有定位导向模,导向模上设有两个与下模板模腔尺寸相同的导向孔,导向孔位置与下模的模腔位置上下对应;所述的模具冲头的上端面设有导向块,导向块通过冲头底座与上模板固定连接,在冲压工作中导向块由上向下插入导向模的导向孔中上下动作;所述的导向块的四个侧边分别设有竖向的排气槽;所述的模具冲头的前侧和后侧的上模板上分别设置两行规格相同的模具弹簧,相邻的模具弹簧的间距小于弹簧的直径。The technical solution adopted by the utility model is: a lithium-ion battery soft pack punching mold, including: an upper template, a lower template, and the upper template is provided with a mold punch, a mold punch base, a mold spring, height-limiting screws and Pins, a positioning guide mold is provided between the upper template and the lower template, and two guide holes with the same size as the mold cavity of the lower template are provided on the guide mold, and the position of the guide holes corresponds to the cavity position of the lower mold up and down; the mold The upper end surface of the punch is provided with a guide block, which is fixedly connected with the upper template through the punch base, and the guide block is inserted into the guide hole of the guide die from top to bottom to move up and down during the stamping work; the four guide blocks described above Vertical exhaust grooves are respectively arranged on the sides; two rows of die springs of the same specification are respectively arranged on the front and rear upper templates of the die punch, and the distance between adjacent die springs is smaller than the diameter of the springs.
所述的模具冲头为铁氟龙冲头。The die punch is a Teflon punch.
所述的导向模的排气槽每个侧边至少设置两条排气槽。At least two exhaust grooves are arranged on each side of the exhaust grooves of the guide mold.
本实用新型的有益效果:由于设有定位导向模,可以使铝塑膜成型时拉伸更加均匀,提升铝塑膜成品质量,并且可以大幅度节省换型时的调试时间,减少了调试设备时所需报废的铝塑膜原料,从而节省成本。Beneficial effects of the utility model: due to the positioning guide mold, the stretching of the aluminum-plastic film can be made more uniform during forming, the quality of the finished product of the aluminum-plastic film can be improved, and the debugging time when changing the model can be greatly saved, and the time for debugging the equipment can be reduced. The aluminum-plastic film raw materials that need to be scrapped, thereby saving costs.
附图说明Description of drawings
图1为本实用新型其中一个实施例上下模分开展示的立体示意图。Fig. 1 is a three-dimensional schematic diagram showing the upper and lower molds separately in one embodiment of the present invention.
图2为上模板去掉模具弹簧、限高螺丝和销钉的示意图。Fig. 2 is a schematic diagram of removing the mold spring, height-limiting screw and pin from the upper formwork.
图3为模具冲头的示意图。Figure 3 is a schematic diagram of a die punch.
具体实施方式detailed description
下面将结合本实用新型实施例中的附图,对本实用新型实施例中的技术方案进行清楚、完整地描述,显然,所描述的实施例仅仅是本实用新型的一部分实施例,而不是全部的实施例。基于本实用新型中的实施例,本领域普通技术人员在没有做出创造性劳动的前提下所获得的所有其他实施例,都属于本实用新型保护的范围。The technical solutions in the embodiments of the present invention will be clearly and completely described below in conjunction with the accompanying drawings in the embodiments of the present invention. Obviously, the described embodiments are only part of the embodiments of the present invention, not all of them. Example. Based on the embodiments of the present utility model, all other embodiments obtained by persons of ordinary skill in the art without making creative efforts belong to the scope of protection of the present utility model.
如图1至图3所示,本实用新型包括:上模板1、下模板3,上模板1上设有模具冲头11、模具冲头底座12、模具弹簧13、限高螺丝14和销钉15,上模板1与下模板3之间设有定位导向模2,导向模上设有两个与模腔尺寸相同的导向孔21,导向孔位置与下模板的模腔31位置上下对应;所述的模具冲头的上端面设有导向块111,导向块通过模具冲头底座与上模板固定连接,在冲压工作中导向块由上向下插入导向孔中并且导向块水平向不晃动,此时模具冲头与导向孔内壁精密配合定位,模具冲头起到了导向的作用,使模具冲头与型腔两边的间隙保持更高的精度,在铝塑膜成型过程中四个边可以更加均匀拉伸,提升铝塑膜成品质量。所述的导向块上四个侧边分别设有两条竖向的排气槽1111;如图2所示,所述的模具冲头的前侧和后侧分别设置两行规格相同的模具弹簧,相邻的模具弹簧的间距小于弹簧的直径,两行弹簧使模具冲压时铝塑膜各个位置受力更均匀。模具冲头材料为铁氟龙,即聚四氟乙烯。铁氟龙冲头与导向孔精密配合,导向孔起导向作用,使模具冲头与型腔两边间隙保持一致,并且模具冲头与导向孔壁保证光滑度来减少冲压成型时铁氟龙冲头与内壁之间的摩擦力,从而达到了延长铁氟龙冲头寿命的作用。As shown in Figures 1 to 3, the utility model includes: an upper template 1, a lower template 3, and the upper template 1 is provided with a die punch 11, a die punch base 12, a die spring 13, height-limiting screws 14 and pins 15 , a positioning guide mold 2 is provided between the upper template 1 and the lower template 3, and the guide mold is provided with two guide holes 21 having the same size as the mold cavity, and the position of the guide holes corresponds to the position of the mold cavity 31 of the lower template; The upper end surface of the die punch is provided with a guide block 111, and the guide block is fixedly connected with the upper template through the die punch base. The mold punch and the inner wall of the guide hole are precisely positioned, and the mold punch plays a guiding role, so that the gap between the mold punch and the two sides of the cavity can be maintained with higher precision, and the four sides can be drawn more evenly during the aluminum-plastic film forming process. Stretch, improve the quality of finished aluminum-plastic film. Two vertical exhaust grooves 1111 are respectively provided on the four sides of the guide block; as shown in FIG. , the distance between adjacent mold springs is smaller than the diameter of the springs, and the two rows of springs make the force on each position of the aluminum-plastic film more uniform when the mold is stamped. The material of the die punch is Teflon, that is, polytetrafluoroethylene. The Teflon punch and the guide hole are precisely matched, and the guide hole acts as a guide to keep the gap between the mold punch and the two sides of the cavity consistent, and the mold punch and the guide hole wall ensure smoothness to reduce the Teflon punch during stamping. The friction between the inner wall and the inner wall, thus achieving the effect of prolonging the life of the Teflon punch.
工作时,上摸板销钉穿过定位导向模的销钉孔22和下模板的销钉孔32,During work, the last template pin passes through the pin hole 22 of the positioning guide mold and the pin hole 32 of the lower template,
铝塑膜在导向模的销钉孔和下模板的销钉孔之间均匀压紧,通过气缸,将上摸板下压,铁氟龙冲头对铝塑膜进行冲压成型。上摸板1与导向模2之间连接有限高螺钉,使用限高螺丝可以使两块模板在非工作状态下保持平行,各个弹簧受力相等,延长弹簧寿命。The aluminum-plastic film is evenly pressed between the pin holes of the guide die and the pin holes of the lower template, and the upper template is pressed down through the cylinder, and the Teflon punch punches the aluminum-plastic film. The height-limiting screw is connected between the upper template 1 and the guide mold 2. Using the height-limiting screw can keep the two templates parallel in the non-working state, and the force of each spring is equal to prolong the life of the spring.
Claims (3)