CN205673740U - Automatic TIG stud welding system - Google Patents
Automatic TIG stud welding system Download PDFInfo
- Publication number
- CN205673740U CN205673740U CN201620302362.0U CN201620302362U CN205673740U CN 205673740 U CN205673740 U CN 205673740U CN 201620302362 U CN201620302362 U CN 201620302362U CN 205673740 U CN205673740 U CN 205673740U
- Authority
- CN
- China
- Prior art keywords
- welding
- tig
- fixed
- turntable
- mandrel
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Expired - Lifetime
Abstract
Description
技术领域technical field
本实用新型专利涉及焊接领域,具体为一种自动TIG螺柱焊接系统。The utility model patent relates to the welding field, specifically an automatic TIG stud welding system.
背景技术Background technique
螺柱焊是将金属螺柱或其他紧固件焊接在工件上的方法。实现螺柱焊接的方法有多种,如:拉弧式螺柱焊、储能式螺柱焊、搅拌摩擦焊、手工电弧焊等。螺柱焊接工艺用途非常广,在建筑、铁路、桥梁、汽车、军事等都有广泛应用。在某些重型车辆中,车体内部的各种零部件均需要固定在车体框架上,如目前我国装甲车辆内部零部件一般是采用螺柱固定,而螺柱都是采用焊接方式固定于车体内部。由于装甲车辆的装甲材料厚度50~100mm,强度高,同时螺柱与母材结构不对称,若采用传统的电容储能螺柱焊和电弧螺柱焊,易产生未溶合及成型不良的缺陷,同时车体厚大装甲钢材料碳当量一般为0.7~0.9,拘束度大,易出现脆性组织,焊接过程中易产生冷裂纹。尽管现有的螺柱焊接技术可以焊接的最大螺柱直径达到31.8mm,但却不能应用在装甲车辆车体装甲材料的焊接,采用摩擦焊虽然是固相焊,但焊接过程中不形成溶池,并且在焊接最后阶段顶锻挤出摩擦界面的夹杂物、氧化膜、脆性相,获得良好的接头性能,适合大直径、高碳当量螺柱的焊接。摩擦焊结构复杂,设备笨重,不利于重型车辆制造的自动化与智能化。采用手工电弧焊存在的问题是焊接效率慢,焊接质量不稳定,劳动强度大等。Stud welding is the method of welding metal studs or other fasteners to workpieces. There are many ways to realize stud welding, such as: drawn arc stud welding, energy storage stud welding, friction stir welding, manual arc welding, etc. The stud welding process is very versatile and is widely used in construction, railways, bridges, automobiles, military and so on. In some heavy-duty vehicles, various parts inside the car body need to be fixed on the car body frame. For example, the internal parts of armored vehicles in my country are generally fixed by studs, and the studs are fixed on the car body by welding. body interior. Since the thickness of the armor material of the armored vehicle is 50-100mm, the strength is high, and the structure of the stud and the base material is asymmetrical, if the traditional capacitor energy storage stud welding and arc stud welding are used, defects such as incomplete fusion and poor forming are likely to occur. At the same time, the carbon equivalent of thick and large armor steel materials for the car body is generally 0.7 to 0.9, with a high degree of restraint, and brittle structures are prone to occur, and cold cracks are prone to occur during welding. Although the existing stud welding technology can weld a maximum stud diameter of 31.8 mm, it cannot be applied to the welding of armored vehicle body armor materials. Although friction welding is solid-phase welding, no molten pool is formed during the welding process. , and in the final stage of welding, the inclusions, oxide film, and brittle phase of the friction interface are extruded by upsetting to obtain good joint performance, which is suitable for welding studs with large diameter and high carbon equivalent. The friction welding structure is complex and the equipment is heavy, which is not conducive to the automation and intelligence of heavy vehicle manufacturing. The problems of manual arc welding are slow welding efficiency, unstable welding quality and high labor intensity.
现有的焊接装置只能针对管板进行焊接,需要通过气动夹紧装置对管板进行定位,使得焊接装置只能对管板或者短管进行焊接,且现有的焊接装置对管壁厚度也有要求;现有的焊接装置不能对大部分螺柱焊接螺柱进行定位,特别是对于高度不等的螺柱满足不了定位需要,所以无法满足不同规格螺柱的焊接要求。The existing welding device can only weld the tube sheet, and the tube sheet needs to be positioned by a pneumatic clamping device, so that the welding device can only weld the tube sheet or short tube, and the existing welding device also has limitations on the thickness of the tube wall. Requirements: The existing welding device cannot locate most of the stud welding studs, especially the studs with different heights cannot meet the positioning requirements, so it cannot meet the welding requirements of studs of different specifications.
实用新型内容Utility model content
针对重型车辆螺柱熔化焊接易出现焊偏、未熔合、裂纹等问题,摩擦焊机结构复杂,设备笨重的问题,本实用新型充分利用TIG焊接头性能好焊缝美观可焊直径范围大等优点,研发出了全位置自动TIG螺柱焊接系统。Aiming at problems such as welding deviation, lack of fusion and cracks in the fusion welding of heavy-duty vehicle studs, the friction welding machine has a complex structure and heavy equipment, the utility model makes full use of the advantages of good performance of the TIG welding head, beautiful weld seam and large diameter range of welding. , developed an all-position automatic TIG stud welding system.
本实用新型采用的技术方案是:The technical scheme that the utility model adopts is:
该装置包括弹簧夹头、TIG焊枪(TIG焊指的是tungsten inert gas welding)、偏心支撑柱、转动副、垂直活动导轨、送丝电机、燕尾形滑块、丝盘盒、动力驱动装置、芯轴、 转盘;弹簧夹头固连于芯轴,芯轴穿过转盘的轴心且固定在转盘上,三个偏心支撑柱固定在转盘上且均布在以转盘为圆心的圆周上,垂直活动导轨、送丝电机和丝盘盒均固定在转盘上且设置在芯轴与偏心支撑柱之间;所述的TIG焊枪连接于转动副,转动副固定在燕尾形滑块上,燕尾形滑块固定于垂直活动导轨;所述的转盘的底部固连动力驱动装置。The device includes collet, TIG welding gun (TIG welding refers to tungsten inert gas welding), eccentric support column, rotating pair, vertical movable guide rail, wire feeding motor, dovetail slider, wire reel box, power drive device, core Shaft and turntable; the spring collet is fixed to the mandrel, the mandrel passes through the axis of the turntable and is fixed on the turntable, and the three eccentric support columns are fixed on the turntable and evenly distributed on the circle centered on the turntable, moving vertically The guide rail, the wire feeding motor and the wire reel box are all fixed on the turntable and arranged between the mandrel and the eccentric support column; the TIG welding torch is connected to the rotating pair, and the rotating pair is fixed on the dovetail slider, and the dovetail slider It is fixed on the vertical movable guide rail; the bottom of the turntable is fixedly connected with the power drive device.
进一步的,弹簧夹头1通过螺纹连接在芯轴上;该弹簧夹头的直径为10~40mm;Further, the collet 1 is connected to the mandrel by threads; the diameter of the collet is 10-40mm;
进一步的,三个偏心支撑柱通过螺纹连接固定在转盘;Further, the three eccentric support columns are fixed on the turntable through threaded connections;
进一步的,TIG焊枪上设有送丝嘴;且送丝嘴送丝管连接于丝盘盒;Further, a wire feeding nozzle is provided on the TIG welding torch; and the wire feeding tube of the wire feeding nozzle is connected to the wire reel box;
进一步的,转动副通过螺栓连接于燕尾形滑块;TIG焊枪通过螺栓连接转动副;Further, the rotating pair is connected to the dovetail slider through bolts; the TIG welding torch is connected to the rotating pair through bolts;
进一步的,TIG焊枪采用小直径的陶瓷喷嘴,喷嘴直径小于9mm;Further, the TIG welding torch adopts a small-diameter ceramic nozzle, and the diameter of the nozzle is less than 9mm;
优选的,弹簧夹头和偏心支撑柱顶部高度差12mm。Preferably, the height difference between the spring collet and the top of the eccentric support column is 12mm.
本实用新型相对于现有技术相比具有如下显著优点:Compared with the prior art, the utility model has the following significant advantages:
1、本实用新型的TIG焊接头性能好、焊缝美观、可焊直径范围大等优点,能够解决常规螺柱焊易出现的焊偏、未熔合、裂纹等问题,以及设备结构复杂、笨重等不足。1. The TIG welding head of the utility model has the advantages of good performance, beautiful weld seam, and a wide range of weldable diameters, and can solve the problems of welding deviation, lack of fusion, cracks, etc. that are easy to occur in conventional stud welding, as well as complex and bulky equipment structures, etc. insufficient.
2、本实用新型通过采用弹簧夹头对螺柱焊接位置的精确定位,保证了焊枪的行走路径和螺柱相匹配。2. The utility model ensures that the walking path of the welding torch matches the stud by adopting the collet to precisely locate the welding position of the stud.
3、该系统通过偏心支撑柱固定焊接平面,保证了螺柱紧贴于待焊试板,不会出现缝隙,确保焊接质量。3. The system fixes the welding plane through the eccentric support column, which ensures that the stud is close to the test plate to be welded, and there will be no gaps to ensure the welding quality.
4、该系统通过设置小直径的陶瓷喷嘴解决了焊枪进行螺柱角焊时的限位问题。4. The system solves the limit problem when the welding torch performs stud fillet welding by setting a small-diameter ceramic nozzle.
附图说明Description of drawings
图1是螺柱焊焊机整体的右视图;Fig. 1 is the whole right view of stud welding machine;
图2是螺柱焊焊机整体的斜视图;Fig. 2 is an oblique view of the stud welding machine as a whole;
图3是固定螺柱不同规格的弹簧夹头;Fig. 3 shows collets of different specifications for fixing studs;
图4是固定TIG焊枪转动副的前视图;Fig. 4 is the front view of the revolving pair of fixed TIG welding torch;
图5是固定TIG焊枪转动副的右视图;Fig. 5 is the right side view of the revolving pair of the fixed TIG welding torch;
图6是螺柱焊焊接时定位的偏心支撑柱示意图;Fig. 6 is a schematic diagram of an eccentric support column positioned during stud welding;
图7是螺柱焊机水平位置焊接的示意图;Fig. 7 is a schematic diagram of welding in a horizontal position of a stud welding machine;
图8是螺柱焊机垂直位置焊接的示意图;Fig. 8 is a schematic diagram of welding in a vertical position of a stud welding machine;
其中:1、弹簧夹头;2、螺柱;3、待焊试板;4、TIG焊枪;5、偏心支撑柱;6、 转动副;7、垂直活动导轨;8、送丝电机;9、燕尾形滑块;10、丝盘盒;11、动力驱动装置;12、芯轴;13、转盘。Among them: 1. Spring collet; 2. Stud; 3. Test plate to be welded; 4. TIG welding torch; 5. Eccentric support column; 6. Rotating pair; 7. Vertical movable guide rail; Dovetail slider; 10, wire reel box; 11, power drive device; 12, mandrel; 13, turntable.
具体实施方式detailed description
下面结合附图和实施例对本实用新型进一步说明:Below in conjunction with accompanying drawing and embodiment the utility model is further described:
如图1和图2所示,该装置包括弹簧夹头1、TIG焊枪4、偏心支撑柱5、转动副6、垂直活动导轨7、送丝电机8、燕尾形滑块9、丝盘盒10、动力驱动装置11、芯轴12、转盘13;弹簧夹头1固连于芯轴12,芯轴12穿过转盘13的轴心且固定在转盘13上,三个偏心支撑柱5固定在转盘13上且均布在以转盘13为圆心的圆周上,垂直活动导轨7、送丝电机8和丝盘盒10均固定在转盘上且设置在芯轴12与偏心支撑柱5之间;所述的TIG焊枪4连接于转动副6,转动副6固定在燕尾形滑块9上,燕尾形滑块9固定于垂直活动导轨7;所述的转盘13的底部固连动力驱动装置11。As shown in Figure 1 and Figure 2, the device includes a collet 1, a TIG welding torch 4, an eccentric support column 5, a rotating pair 6, a vertically movable guide rail 7, a wire feeding motor 8, a dovetail slider 9, and a wire reel box 10 , a power drive device 11, a mandrel 12, and a turntable 13; the collet 1 is fixedly connected to the mandrel 12, the mandrel 12 passes through the axis of the turntable 13 and is fixed on the turntable 13, and three eccentric support columns 5 are fixed on the turntable 13 and evenly distributed on the circumference with the turntable 13 as the center of the circle, the vertical movable guide rail 7, the wire feeding motor 8 and the wire reel box 10 are all fixed on the turntable and arranged between the mandrel 12 and the eccentric support column 5; The TIG welding gun 4 is connected to the rotating pair 6, and the rotating pair 6 is fixed on the dovetail slider 9, and the dovetail slider 9 is fixed on the vertical movable guide rail 7; the bottom of the turntable 13 is fixedly connected with the power drive device 11.
上述装置中,弹簧夹头1通过螺纹连接在芯轴12上;三个偏心支撑柱5通过螺纹连接固定在转盘13;转动副6通过螺栓连接于燕尾形滑块9。In the above device, the spring collet 1 is screwed to the mandrel 12; the three eccentric support columns 5 are fixed to the turntable 13 through screw connections; the rotating pair 6 is connected to the dovetail slider 9 through bolts.
本实用新型中使用的弹簧夹头耐高温弹性好、散热性能好,在焊接结束对粘丝粘钨后续处理过程焊枪的摆动有良好的缓冲空间。对不同直径的螺柱2,采用不同的弹簧夹头1,如图3所示是适合不同螺柱直径的弹簧夹头1,弹簧夹头的直径为10~40mm。The spring collet used in the utility model has good high temperature resistance, good elasticity and good heat dissipation performance, and has a good buffer space for the swing of the welding torch in the follow-up process of sticking wire and tungsten after welding. For studs 2 of different diameters, different collets 1 are used. As shown in FIG. 3 , collets 1 suitable for different diameters of studs are used. The diameter of the collets is 10-40 mm.
该系统的TIG焊枪4上设有送丝嘴;且送丝嘴送丝管连接于丝盘盒10;TIG焊枪4通过螺栓连接转动副6;该TIG焊枪4采用小直径的陶瓷喷嘴,喷嘴直径小于9mm,可以在角焊缝焊接过程中使钨极伸出长度减小,增加保护效果。The TIG welding torch 4 of the system is provided with a wire feeding nozzle; and the wire feeding nozzle and the wire feeding tube are connected to the wire reel box 10; the TIG welding torch 4 is connected to the revolving pair 6 by bolts; the TIG welding torch 4 adopts a ceramic nozzle with a small diameter, and the diameter of the nozzle is Less than 9mm, it can reduce the protruding length of the tungsten electrode during the welding process of the fillet weld and increase the protective effect.
将该系统中的弹簧夹头1和偏心支撑柱5顶部高度差设置为12mm,弹簧夹头1和待焊试板3有恰当的高度差可以避免因为焊接热输入过高导致弹簧夹头的变形,还有因为弹簧夹头有一定厚度,高度差使焊接过程中螺柱裸露出来便于焊缝成型和焊枪有良好的调整空间。The height difference between the collet 1 and the top of the eccentric support column 5 in this system is set to 12mm, and the collet 1 and the test plate 3 to be welded have an appropriate height difference to avoid deformation of the collet due to excessive welding heat input , Also because the spring collet has a certain thickness, the height difference makes the stud exposed during the welding process, which is convenient for the welding seam forming and the welding torch to have a good adjustment space.
在焊接过程中,螺柱2紧固于弹簧夹头1,通过偏心支撑柱5使螺柱保持和板的水平接触,垂直焊接时,施加一个垂直待焊试板的力来保持紧贴,如图6、8所示;将螺柱2紧贴于待焊试板3,然后通过垂直活动导轨7和燕尾形滑块9调节焊枪4位置,TIG焊枪4通过燕尾形滑块9手动调整焊枪离螺柱2的横向距离,垂直方向由电机驱动垂直活动导轨7调整焊枪4离待焊试板3的距离,该系统还通过转动副6调节焊枪4的焊接角度,如图4和图5所示;焊接时,由送丝电机8驱动丝盘盒10中的焊丝进行送丝, 焊接过程中焊枪4由动力驱动部分11以焊前调试焊速驱动焊枪4绕螺柱进行焊接。During the welding process, the stud 2 is fastened to the collet 1, and the stud is kept in horizontal contact with the plate through the eccentric support column 5. When welding vertically, a force perpendicular to the test plate to be welded is applied to maintain close contact, such as As shown in Figures 6 and 8; the stud 2 is closely attached to the test plate 3 to be welded, and then the position of the welding torch 4 is adjusted through the vertical movable guide rail 7 and the dovetail slider 9, and the TIG welding torch 4 is manually adjusted through the dovetail slider 9. The horizontal distance of the stud 2 and the vertical direction are driven by the motor and the vertical movable guide rail 7 adjusts the distance between the welding torch 4 and the test plate 3 to be welded. The system also adjusts the welding angle of the welding torch 4 through the rotating pair 6, as shown in Figure 4 and Figure 5 During welding, the welding wire in the wire reel box 10 is driven by the wire feeding motor 8 to feed the wire, and the welding torch 4 is driven by the power drive part 11 to weld the welding torch 4 around the stud with the pre-welding debugging welding speed in the welding process.
在本实用新型的焊接过程还涉及到焊接电源以及辅助设备和保护气、冷却水系统等均为焊接领域内的常规技术。The welding process of the present invention also involves welding power supply, auxiliary equipment, shielding gas, cooling water system, etc., which are conventional technologies in the welding field.
实施例Example
以碳钢板和直径为32mm碳钢螺柱平焊为例,焊接方式如图7所示,首先焊前先对螺柱和待焊试板3进行清理,清除其表面的氧化膜和进行表面平整处理,保证焊接时螺柱和待焊试板3充分接触,然后采用32mm的弹簧夹头1,将32mm的螺柱2紧固于弹簧夹头1,保证螺柱2伸出弹簧夹头1长度大于12mm,然后将螺柱焊接系统垂直放置在待焊试板3上,保证三个偏心支撑柱5和螺柱处于一个平面上且紧贴于待焊试板3,然后用燕尾形滑块9和垂直活动导轨7调整TIG焊枪4的位置,然后用转动副6调整焊枪4焊接角度为35o,然后接通焊接电源输入焊接电流,设定送丝速度,转盘13旋转速度等参数,打开保护气,开始进行焊接,在焊接过程中,可以根据熔池形成情况用线控器手动调整焊接电流,从而完成整个焊接过程。Taking the flat welding of carbon steel plate and carbon steel stud with a diameter of 32 mm as an example, the welding method is shown in Figure 7. First, the stud and the test plate 3 to be welded are cleaned before welding, the oxide film on the surface is removed and the surface is smoothed. Processing, to ensure that the studs are in full contact with the test plate 3 to be welded during welding, and then use a 32mm spring collet 1 to fasten a 32mm stud 2 to the spring collet 1 to ensure that the stud 2 extends out of the spring collet 1 length greater than 12mm, then place the stud welding system vertically on the test plate 3 to be welded, ensure that the three eccentric support columns 5 and the studs are on the same plane and close to the test plate 3 to be welded, and then use the dovetail slider 9 Adjust the position of the TIG welding torch 4 with the vertical movable guide rail 7, then use the rotating pair 6 to adjust the welding angle of the welding torch 4 to 35°, then turn on the welding power supply to input the welding current, set the wire feeding speed, the rotation speed of the turntable 13 and other parameters, and turn on the shielding gas , start welding, during the welding process, the wire controller can be used to manually adjust the welding current according to the formation of the molten pool, so as to complete the entire welding process.
Claims (7)