CN205653900U - Waterproof construction of basement bottom plate - Google Patents
Waterproof construction of basement bottom plate Download PDFInfo
- Publication number
- CN205653900U CN205653900U CN201620365120.6U CN201620365120U CN205653900U CN 205653900 U CN205653900 U CN 205653900U CN 201620365120 U CN201620365120 U CN 201620365120U CN 205653900 U CN205653900 U CN 205653900U
- Authority
- CN
- China
- Prior art keywords
- waterproof
- layer
- basement bottom
- construction
- bottom board
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Expired - Fee Related
Abstract
The present case is a waterproof construction of basement bottom plate, from including in proper order on and down: foundation soil, the C15 concrete cushion, the coiled material waterproof layer, the isolation layer, the C20 pea gravel concreten, cement base infiltration crystallization type waterproof layer, waterproof reinforced concrete bottom plate, the surface course, wherein, infiltration crystallization type waterproof layer is not less than 1mm's cement base infiltration crystallization type waterproof layer coating for thickness, the coiled material waterproof layer adopts thickness to be not less than 1.5mm's senior compound S type self -adhered waterproofing membrane. The waterproof construction of present case exist the waterproof system that never lost efficacy, certainly heal performance, back side workability remarkable, solve a large amount of basement leakage problem, nontoxic, environmental protection, anticorrosive, acid and alkali -resistance, can improve concrete intensity, need not advantages such as screed -coat and protective layer, and save the time limit for a project for the project progress, construction comprehensive cost greatly reduced.
Description
Technical field
This utility model relates to building waterproofing technique field, is specifically related to the waterproof knot of a kind of basement bottom board
Structure structure.
Background technology
Way at basement bottom board routine waterproof roll has: hot melt, from bonding, wet-laid process etc..?
After waterproof roll paving is complete, it is generally required to do waterproof slab protective layer, prevent the waterproof layer of finished product in the later stage
Base plate assembling reinforcement, destruction during casting concrete.Waterproof slab interface protective layer routine uses at present
Way is that the prior art that 50mm thickness C15 pea gravel concreten routine waterproof roll interface protective layer uses all is wrapped
, there is cost high, shortcoming long in time limit in cement mortar cover, it is impossible to meets project duration very well and want
Ask, because construction environment is moist moisture, out-of-flatness, clean, so wanting to reach qualified waterproof
Effect, also will face the pressure of duration cost.
Utility model content
For overcoming the deficiencies in the prior art, the purpose of this utility model is to provide simple in construction, waterproof effect
The waterproof construction of the best basement bottom board.
For achieving the above object, this utility model is achieved through the following technical solutions:
The waterproof construction of a kind of basement bottom board, includes the most successively: foundation soil 8, C15 concrete
Bed course 7, coil waterproof layer 6, sealing coat 5, C20 pea gravel concreten 4, cement-base infiltration crystallization type is prevented
Water layer 3, waterproof reinforced concrete floor 2, surface layer 1, wherein, described infiltration crystallization type water-proof layer is thick
The degree cement-base infiltration crystallization type water-proof coating not less than 1mm, described coil waterproof layer uses thickness not
Senior composite S type adhesive waterproof coil less than 1.5mm.
Preferably, the waterproof construction of described basement bottom board, wherein, described C20 pea gravel concreten
Thickness is 50mm.
Preferably, the waterproof construction of described basement bottom board, wherein, described senior composite S type is certainly
Viscous waterproof roll fabric width is 1m, a length of 15m-20m.
Preferably, the waterproof construction of described basement bottom board, wherein, described composite high-molecular self-adhesion
Waterproof roll fabric width is 1m, a length of 15m-20m.
Preferably, the waterproof construction of described basement bottom board, wherein, described C15 concrete cushion
Thickness is 100mm-150mm.
The beneficial effects of the utility model: the waterproof construction of this case adds coil waterproof layer, sealing coat,
C20 pea gravel concreten, cement-base infiltration crystallization type water-proof layer, waterproof material uses coil waterproof layer,
Cement-base infiltration crystallization type water-proof layer, wherein cement-base infiltration crystallization type water-proof layer is inorganic material, exists
The waterproof system that never lost efficacy, self-healing performance, back side workability are remarkable, solve a large amount of basement
Leakage problems, nontoxic, environmental protection, anticorrosion, acid and alkali-resistance, concrete strength can be improved, without screed-coat
With the advantage such as protective layer, and saving the duration, speed up the work, construction integrated cost is substantially reduced, when
Other waterproof systems can work on after losing efficacy, and has infiltration function, can be penetrated into by chemical reaction mixed
The raw crystalline solid of the internal ginseng of solidifying soil blocks the pore of concrete;The DWKDS senior composite S waterproof volume of type self-adhesion
Material can use executes laid process or the construction of dry-laid method, and rainy weather is preferentially selected wet application, executed severe
Construct under work environment, still possess preferable water resistance.
Accompanying drawing explanation
Fig. 1 is the structural representation of the waterproof construction of the basement bottom board described in this utility model one embodiment
Figure.
Wherein, 1-surface layer, the waterproof reinforced concrete floor of 2-, 3-cement-base infiltration crystallization type water-proof layer,
4-C20 pea gravel concreten, 5-sealing coat, 6-coil waterproof layer, 7-C15 concrete cushion, 8-foundation soil.
Detailed description of the invention
Below in conjunction with the accompanying drawings this utility model is described in further detail, to make those skilled in the art
Can implement according to this with reference to description word.
The waterproof construction of a kind of basement bottom board, refers to accompanying drawing 1, includes the most successively: ground
Soil 8, C15 concrete cushion 7, coil waterproof layer 6, sealing coat 5, C20 pea gravel concreten 4, cement
Base infiltration crystallization type water-proof layer 3, waterproof reinforced concrete floor 2, surface layer 1, wherein, described infiltration knot
Crystal formation waterproof layer is the cement-base infiltration crystallization type water-proof coating that thickness is not less than 1mm, and described coiled material is prevented
Water layer uses the thickness DWKDS senior composite S type adhesive waterproof coil not less than 1.5mm.
Further, described C20 pea gravel concreten thickness is 50mm.
Further, described DWKDS senior composite S type adhesive waterproof coil fabric width is 1m, a length of
15m-20m。
Further, described DWPVS composite high-molecular adhesive waterproof coil fabric width is 1m, a length of
15m-20m。
Further, described C15 concrete mats layer thickness is 100mm-150mm.
DWKDS senior composite S type adhesive waterproof coil can use executes laid process or the construction of dry-laid method, overcast and rainy
Gas preferentially selects wet application.
Although embodiment of the present utility model is disclosed as above, but it is not restricted to description and reality
Executing listed in mode utilization, it can be applied to various applicable field of the present utility model completely, for
For those skilled in the art, it is easily achieved other amendment, therefore without departing substantially from claim
And under the general concept that limited of equivalency range, this utility model is not limited to specific details and shows here
The legend gone out and describe.
Claims (5)
1. the waterproof construction of a basement bottom board, it is characterised in that include the most successively: ground
Soil, C15 concrete cushion, coil waterproof layer, sealing coat, C20 pea gravel concreten, cement-based penetrant is tied
Crystal formation waterproof layer, waterproof reinforced concrete floor, surface layer, wherein, described infiltration crystallization type water-proof layer is
The thickness cement-base infiltration crystallization type water-proof coating not less than 1mm, described coil waterproof layer uses thickness
Senior composite S type adhesive waterproof coil not less than 1.5mm.
2. the waterproof construction of basement bottom board as claimed in claim 1, it is characterised in that described C20
Pea gravel concreten thickness is 50mm.
3. the waterproof construction of basement bottom board as claimed in claim 2, it is characterised in that described senior
Composite S type adhesive waterproof coil fabric width is 1m, a length of 15m-20m.
4. the waterproof construction of basement bottom board as claimed in claim 3, it is characterised in that described compound
High-polymer self-adhesion waterproof coiled material fabric width is 1m, a length of 15m-20m.
5. the waterproof construction of basement bottom board as claimed in claim 4, it is characterised in that described C15
Concrete mats layer thickness is 100mm-150mm.