CN204174277U - 一种防止钢管白锈产生的涂覆装置 - Google Patents

一种防止钢管白锈产生的涂覆装置 Download PDF

Info

Publication number
CN204174277U
CN204174277U CN201420624806.3U CN201420624806U CN204174277U CN 204174277 U CN204174277 U CN 204174277U CN 201420624806 U CN201420624806 U CN 201420624806U CN 204174277 U CN204174277 U CN 204174277U
Authority
CN
China
Prior art keywords
passivator
vessel
steel pipe
white rust
coating unit
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Expired - Fee Related
Application number
CN201420624806.3U
Other languages
English (en)
Inventor
温朝福
王立宏
路彪
王长良
李志强
沈永华
苗立贤
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
HENGSHUI JINGHUA STEEL PIPE Co Ltd
Original Assignee
HENGSHUI JINGHUA STEEL PIPE Co Ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by HENGSHUI JINGHUA STEEL PIPE Co Ltd filed Critical HENGSHUI JINGHUA STEEL PIPE Co Ltd
Priority to CN201420624806.3U priority Critical patent/CN204174277U/zh
Application granted granted Critical
Publication of CN204174277U publication Critical patent/CN204174277U/zh
Expired - Fee Related legal-status Critical Current
Anticipated expiration legal-status Critical

Abstract

本实用新型属于钢管热镀锌制备技术领域,公开了一种防止钢管白锈产生的涂覆装置。构成该装置的技术方案:包括构成涂覆层的钝化剂容器,在钝化剂容器上设置有与其连通的喷淋箱,在该喷淋箱的两侧对应设置有钢管通道孔,该通道孔的侧部设置有对应的支撑环;喷淋箱定中设置有钝化剂喷头,该钝化剂喷头通过循环泵和管线与钝化剂容器连通。该装置能够实现对刚由镀锌锅完成镀锌的高温钢管的直接喷涂涂覆层,大大缩短涂覆层的涂覆时间,降低涂覆工序的成本。

Description

一种防止钢管白锈产生的涂覆装置
技术领域
本实用新型涉及钢管热镀锌制备技术领域,特别是涉及一种防止钢管白锈产生的涂覆装置。
背景技术
热镀锌钢管的镀锌镀层是目前最为有效的防腐涂层之一,大气环境中使用寿命一般可达15~20年,即被用作防止钢管锈蚀的防护涂层,可增加钢管的抗腐蚀能力,延长使用寿命。所以,热镀锌管的用途很广,除作输水、煤气、油等一般低压力流体的管线管外,还用作石油工业特别是海洋油田的油井管、输油管,化工焦化设备的油加热器、冷凝冷却器、煤馏洗油交换器用管,以及栈桥管桩、矿山坑道的支撑架用管等各个国民经济建设领域。但是金属锌是非常活泼的金属,锌镀层在大气环境中使用时化学稳定性不高,尤其是热镀锌钢管在储存、运输过程中遇到潮湿空气、闷热环境和与腐蚀气体、介质的接触浸蚀,其表面极易发生化学变化,产生白锈和灰色斑点,直接影响其镀层的耐腐蚀性和外观,影响镀锌钢管的使用寿命。
为了保护热镀锌镀层,需要对镀锌层进行表面处理来避免镀锌层“白锈”、灰暗色的“锌锈”的产生,传统的钢管防“白锈”、“锌锈”处理方法是:在钢管热镀锌后经过内、外镀层喷吹掉余锌、水冷却后,直接浸入铬酸盐钝化水溶液中来镀锌管的外表面形成涂覆层,但该直接浸泡形成涂覆层不仅其效率低,而且难于控制该涂覆层的厚度。
实用新型内容
本实用新型的目的就是提供一种生产效率高并且能够控制涂覆层厚度的防止钢管白锈产生的涂覆装置。
为实现上述目的,本实用新型采用的技术方案为:
一种防止钢管白锈产生的涂覆装置,包括构成涂覆层的钝化剂容器,其特征在于,在所述的钝化剂容器上设置有与其连通的喷淋箱,在该喷淋箱的两侧对应设置有钢管通道孔,该通道孔的侧部设置有对应的支撑环;所述喷淋箱定中设置有钝化剂喷头,该钝化剂喷头通过循环泵和管线与所述钝化剂容器连通。
构成上述防止钢管白锈产生的涂覆装置的附加技术特征包括:
——所述钝化剂容器顶部设置有放气孔;
——在所述钝化剂容器的内侧设置有与所述钢管通道孔对应的吹气机构;
——在所述钝化剂容器中部设置有挡板机构;
    ——在所述钝化剂容器中部设置有与所述挡板机构对应抹片机构。
本实用新型所提供的防止钢管白锈产生的涂覆装置与现有技术相比,具有以下优点:其一,由于该装置能够实现对刚由镀锌锅完成镀锌的高温钢管的直接喷涂涂覆层,不仅可以大大缩短涂覆层的涂覆时间,而且可以大大降低涂覆工序的成本;其二,由于构成该装置的钢管通道孔侧设置有对应的吹气机构,因此能够将喷涂在钢管上多余的钝化剂吹掉控制其厚度。
附图说明
图1为防止钢管白锈产生的涂覆装置的结构示意图。
具体实施方式
下面结合附图对本实用新型提供的防止钢管白锈产生的涂覆装置的结构做进一步详细说明。
如图1所示为本实用新型提供的防止钢管白锈产生的涂覆装置的结构示意图。构成该装置的结构包括盛装有构成涂覆层的钝化剂容器1,在容器上设置有与其连通的喷淋箱2,在喷淋箱的两侧对应设置有左、右钢管通道孔3、4,该通道孔的侧部设置有对应的用于将钢管穿过喷淋箱的左、右支撑环5、6;在喷淋箱的顶部设置有通过管线7和循环泵8与钝化剂容器1连通的钝化剂喷头9以及放气孔13。
其工作原理为,启动循环泵8,喷淋头实现钝化剂的喷淋,此时热镀锌后的钢管10在输送托辊旋转力的作用下,通过右支撑环6和右钢管通道孔4进入喷淋箱2中,钝化剂通过喷头喷淋在钢管上,后由钢管通道孔3和左支撑环5穿出完成镀锌钢管防止“白锈”钝化处理的钢管表面涂覆过程。
在构成上述防止钢管白锈产生的涂覆装置的结构中,
——在上述钝化剂容器的内侧设置有与钢管通道孔对应的斜向左、右吹气嘴环11、12,构成的相互对应的吹气机构,当钝化剂喷淋在钢管表面时右侧的吹气嘴环12通过设置于周圈的与其轴线X呈锐角角度的气眼16可以将钝化剂吹得更加均匀;而与右侧的吹气嘴环12结构相同的左侧吹气嘴环11不仅可以将多余的钝化剂沿箭头T的方向从钢管表面吹掉、而且通过压力为0.15MPa,温度为65~75℃的压缩空气,使钝化剂在钢管表面涂覆的均匀,同时起到防止钝化液顺着镀锌钢管带出,带有温度的压缩空气起到喷吹干钝化膜层的作用;
——在钝化剂容器中部设置有挡板机构14可以防止左侧吹气嘴环的气流对正在喷涂的喷头喷淋产生影响;
——在钝化剂容器中部设置有与挡板机构对应抹片机构15,可以将喷涂在钢管表面上的多余的钝化剂先行抹除,以减轻左侧的吹气嘴环的吹气压力。

Claims (5)

1.一种防止钢管白锈产生的涂覆装置,包括构成涂覆层的钝化剂容器,其特征在于,在所述的钝化剂容器上设置有与其连通的喷淋箱,在该喷淋箱的两侧对应设置有钢管通道孔,该通道孔的侧部设置有对应的支撑环;所述喷淋箱定中设置有钝化剂喷头,该钝化剂喷头通过循环泵和管线与所述钝化剂容器连通。
2.根据权利要求1所述的一种防止钢管白锈产生的涂覆装置,其特征在于:所述钝化剂容器顶部设置有放气孔。
3.根据权利要求1所述的一种防止钢管白锈产生的涂覆装置,其特征在于:在所述钝化剂容器的内侧设置有与所述钢管通道孔对应的吹气机构。
4.根据权利要求1所述的一种防止钢管白锈产生的涂覆装置,其特征在于:在所述钝化剂容器中部设置有挡板机构。
5.根据权利要求4所述的一种防止钢管白锈产生的涂覆装置,其特征在于:在所述钝化剂容器中部设置有与所述挡板机构对应抹片机构。
CN201420624806.3U 2014-10-27 2014-10-27 一种防止钢管白锈产生的涂覆装置 Expired - Fee Related CN204174277U (zh)