CN203929507U - 组合式金属圆棒低温拉伸试验夹具 - Google Patents
组合式金属圆棒低温拉伸试验夹具 Download PDFInfo
- Publication number
- CN203929507U CN203929507U CN201420360235.7U CN201420360235U CN203929507U CN 203929507 U CN203929507 U CN 203929507U CN 201420360235 U CN201420360235 U CN 201420360235U CN 203929507 U CN203929507 U CN 203929507U
- Authority
- CN
- China
- Prior art keywords
- sample
- fixture
- tensile test
- metal pole
- combined metal
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Expired - Fee Related
Abstract
本实用新型公开了一种组合式金属圆棒低温拉伸试验夹具,包括上下两端均设有伸长杆的低温箱,其特征在于:所述两根伸长杆相对的一端均与试样固定座上的拉杆连接头连接,所述试样固定座内均设有与拉伸试样安装头配合的试样固定槽,所述每个试样固定座均由两个半圆柱型的夹块构成。本实用新型夹具将低温拉伸试样直接嵌入夹具中,通过插销杆组合左右两个夹具,无锁紧式夹具的旋转螺纹缝隙,不会因为缝隙结冰而无法旋紧或松开夹具,试样不会因为夹具冻结而无法卸除,装卸试样轻松方便;试验过程更加顺畅,省时省力,试验成功率也更高;通过试样固定槽弧面卡住哑铃状试样头部进行拉伸,不存在锁紧式夹具中常见的打滑现象。
Description
技术领域
本实用新型涉及金属材料力学性能测试技术领域,具体地指一种组合式金属圆棒低温拉伸试验夹具。
背景技术
随着压力容器、船舶、桥梁用钢的发展,为适应这类钢材的使用环境,对于其所有钢材的低温性能提出了很高的要求,金属圆棒试样低温拉伸试验是测试金属材料在低温环境下使用时的抗拉强度、屈服强度、断后伸长率等力学性能指标的试验。目前,金属圆棒试样低温拉伸试验使用较多的夹具为弹簧自动锁紧式的夹具,它主要通过自锁力及装夹表面的锯齿产生的摩擦力将试样两端夹紧,从而与试验机连接完成拉伸试验,该夹具在低温环境下使用存在以下缺点:1.低温下楔形夹块与夹具母体接触坡面处大量结冰冻住,无法自由上下滑动,装卸试样困难,试样也很难夹紧。2.夹具手柄旋转松紧处螺纹缝隙在低温下结冰,手柄无法旋转到最紧,试样夹紧力不够,拉伸时容易打滑。3.试样夹紧后低温下保温一段时间后,手柄旋转处及夹块与夹具母体接触面结冰冻住,导致试样拉断后因夹具无法打开而无法卸除试样。需升温环境箱,再保温一段时间,使夹具解冻,再换下一件试样继续试验,严重影响试验效率,且大大增高了液氮介质以及电能的损耗。
发明内容
本实用新型的目的就是要提供一种装卸方便、可避免打滑的组合式金属圆棒低温拉伸试验夹具。
为实现上述目的,本实用新型所设计的组合式金属圆棒低温拉伸试验夹具,包括上下两端均设有伸长杆的低温箱,其特征在于:所述两根伸长杆相对的一端均与试样固定座上的拉杆连接头连接,所述试样固定座内均设有与拉伸试样安装头配合的试样固定槽,所述每个试样固定座均由两个半圆柱型的夹块构成。
进一步地,所述夹块的接触面一边设有凸销,另一边设有与凸销配合的凸销槽。
进一步地,它还包括用于固定两个夹块的插销杆,所述夹块另一边沿轴向设有供插销杆穿过的插销孔,所述凸销上也设有供插销孔穿过的孔,插销杆穿过插销孔和孔并通过螺栓限位可避免因结冰而不易拆卸的问题。
再进一步地,它还包括用于固定伸长杆和拉杆连接头的固定销,所述拉杆连接头上设有与固定销配合的固定销连接孔。
本实用新型的优点在于:本实用新型夹具将低温拉伸试样直接嵌入夹具中,通过插销杆组合左右两个夹具,无锁紧式夹具的旋转螺纹缝隙,不会因为缝隙结冰而无法旋紧或松开夹具,试样不会因为夹具冻结而无法卸除,装卸试样轻松方便;试验过程更加顺畅,省时省力,试验成功率也更高;通过试样固定槽弧面卡住哑铃状试样头部进行拉伸,不存在锁紧式夹具中常见的打滑现象;其结构简单,制造成本低,使用方便,易于推广。
附图说明
图1为组合式金属圆棒低温拉伸试验夹具的使用状态结构示意图。
图2为夹块与拉杆连接头的连接示意图。
具体实施方式
以下结合附图和具体实施例对本实用新型作进一步的详细描述。
图中所示组合式金属圆棒低温拉伸试验夹具,包括上下两端均设有伸长杆1a的低温箱1,两个拉杆连接头3分别伸入两根伸长杆1a内,固定销5穿过两个拉杆连接头3上的孔和固定销连接孔3a将试样固定座2与伸长杆1a连接,试样固定座2内均设有与拉伸试样安装头配合的试样固定槽2b,每个试样固定座2均由两个半圆柱型的夹块2a构成,夹块2a的接触面一边设有凸销2c,另一边设有与凸销2c配合的凸销槽2d,它还包括用于固定两个夹块2a的插销杆4,夹块2a另一边沿轴向设有供插销杆4穿过的插销孔2e,凸销2c上也设有供插销杆4穿过的孔2f。
使用时,试样6的两端分别放入一个夹块2a中,将另一个夹块2a的凸销2c插入其凸销槽2d中,再将四个插销杆4均插入插销孔2e内并用螺帽固定,再将两个拉杆连接头3伸入伸长杆1a内并通过固定销5将其固定;将两个伸长杆1a分别与试验机横梁及底座连接,然后关闭低温环境箱,做好密封,开启降温程序,降温至设定温度后,达到一定保温时间即可开始低温拉伸试验。
Claims (4)
1.一种组合式金属圆棒低温拉伸试验夹具,包括上下两端均设有伸长杆(1a)的低温箱(1),其特征在于:所述两根伸长杆(1a)相对的一端均与试样固定座(2)上的拉杆连接头(3)连接,所述试样固定座(2)内均设有与拉伸试样安装头配合的试样固定槽(2b),所述每个试样固定座(2)均由两个半圆柱型的夹块(2a)构成。
2.根据权利要求1所述组合式金属圆棒低温拉伸试验夹具,其特征在于:所述夹块(2a)的接触面一边设有凸销(2c),另一边设有与凸销(2c)配合的凸销槽(2d)。
3.根据权利要求2所述组合式金属圆棒低温拉伸试验夹具,其特征在于:它还包括用于固定两个夹块(2a)的插销杆(4),所述夹块(2a)另一边沿轴向设有供插销杆(4)穿过的插销孔(2e),所述凸销(2c)上也设有供插销杆(4)穿过的孔(2f)。
4.根据权利要求1-3中任一项所述组合式金属圆棒低温拉伸试验夹具,其特征在于:它还包括用于固定伸长杆(1a)和拉杆连接头(3)的固定销(5),所述拉杆连接头(3)上设有与固定销(5)配合的固定销连接孔(3a)。