CN202486040U - 金属表面涂层界面结合强度测试用试样 - Google Patents

金属表面涂层界面结合强度测试用试样 Download PDF

Info

Publication number
CN202486040U
CN202486040U CN2012200897808U CN201220089780U CN202486040U CN 202486040 U CN202486040 U CN 202486040U CN 2012200897808 U CN2012200897808 U CN 2012200897808U CN 201220089780 U CN201220089780 U CN 201220089780U CN 202486040 U CN202486040 U CN 202486040U
Authority
CN
China
Prior art keywords
sample
coating
metal surface
bond strength
matrix
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Expired - Fee Related
Application number
CN2012200897808U
Other languages
English (en)
Inventor
王利国
朱世杰
任晨星
关绍康
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Zhengzhou University
Original Assignee
Zhengzhou University
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Zhengzhou University filed Critical Zhengzhou University
Priority to CN2012200897808U priority Critical patent/CN202486040U/zh
Application granted granted Critical
Publication of CN202486040U publication Critical patent/CN202486040U/zh
Anticipated expiration legal-status Critical
Expired - Fee Related legal-status Critical Current

Abstract

本实用新型涉及一种金属表面涂层界面结合强度测试用试样。所述试样,包括涂覆涂层的基体,所述的试样还包括与基体垂直连接的拉力加载部。本实用新型金属表面涂层界面结合强度测试用试样避免了试样横向拉断的缺陷,同时有利于更准确地检测出涂层和基体之间的剪切力。

Description

金属表面涂层界面结合强度测试用试样
技术领域
本实用新型涉及一种金属表面涂层界面结合强度测试用试样。
背景技术
目前,金属表面涂层界面结合强度测试多是根据ASTM F 1044-05标准,利用Hitachi AG-IS万能实验机来测试表面涂层与金属基体之间的剪切强度。测试前,先用粘结剂譬如环氧树脂等将有涂层试样粘接在一起,粘接面积1cm2,然后将粘好的试样在室温下用夹子固定36h。利用现有试样测试的过程如图1所示。目前的试样存在一个缺点:拉伸过程中由于上下两个夹头的加载力方向不在同一轴线,因此很容易造成试样横向拉断。
实用新型内容
本实用新型的目的在于提供一种金属表面涂层界面结合强度测试用试样,可以克服目前测试时试样容易横向拉断的缺陷。
本实用新型采用的技术方案如下:
金属表面涂层界面结合强度测试用试样,包括涂覆涂层的基体,所述的试样还包括与基体垂直连接的拉力加载部。
所述的基体横截面为长方形、正方形或半圆形。
本实用新型对试样进行了改进,试样由基体与加载部共同构成,且基体与加载部垂直形成L型。原来的试样是只有涂覆涂层的基体,因此测试时拉伸过程中由于上下两个夹头的加载力方向不在同一轴线,因此很容易造成试样横向拉断,而改进后的试样由于加设了与基体垂直的拉力加载部,因此,拉伸时可以拉力同时加载在各自的加载部位,保证了上下两个加载力在同一轴线上,避免了试样横向拉断的缺陷,也有利于更准确地检测出涂层和基体之间的剪切力。
本实用新型相对于现有技术,有以下优点:
本实用新型金属表面涂层界面结合强度测试用试样避免了试样横向拉断的缺陷,同时有利于更准确地检测出涂层和基体之间的剪切力。
附图说明
图1为利用传统试样测试的示意图,其中,1为试样,2为涂层,3为粘结剂;
图2为利用本实用新型试样测试的示意图,其中,1为试样,11为试样涂覆涂层的部位即基体,12为试样接受拉伸测试时的加载部,2为涂层,3为粘结剂。
具体实施方式
   以下以具体实施例来说明本实用新型的技术方案,但本实用新型的保护范围不限于此:
实施例1
如图2所示,金属表面涂层界面结合强度测试用试样1,包括涂覆涂层2的基体11,所述的试样1还包括与基体11垂直连接的拉力加载部12。
试样的表面涂覆及胶粘处理与传统试样处理相同,但在拉伸测试时,拉力同时加载在各自的加载部12,这样既保证了上下两个加载力在同一轴线上,避免了试样横向拉断,也有利于更准确地检测出涂层界面结合的剪切力。
所述的试样横截面(A-A横截面)为长方形。当然,也可以采用正方形或半圆形。
上述实施例为本实用新型优选的实施方式,但本实用新型的实施方式并不受上述实施例的限制,其他的任何未背离本实用新型所作的改变均应为等效的置换方式,都包含在本实用新型的保护范围之内。

Claims (2)

1. 金属表面涂层界面结合强度测试用试样,包括涂覆涂层的基体,其特征在于,所述的试样还包括与基体垂直连接的拉力加载部。
2.如权利要求1所述的金属表面涂层界面结合强度测试用试样,其特征在于,所述的基体横截面为长方形、正方形或半圆形。
CN2012200897808U 2012-03-12 2012-03-12 金属表面涂层界面结合强度测试用试样 Expired - Fee Related CN202486040U (zh)