CN202464419U - 一种密封良好且方便撕裂的聚合物复合薄膜 - Google Patents

一种密封良好且方便撕裂的聚合物复合薄膜 Download PDF

Info

Publication number
CN202464419U
CN202464419U CN2012200821391U CN201220082139U CN202464419U CN 202464419 U CN202464419 U CN 202464419U CN 2012200821391 U CN2012200821391 U CN 2012200821391U CN 201220082139 U CN201220082139 U CN 201220082139U CN 202464419 U CN202464419 U CN 202464419U
Authority
CN
China
Prior art keywords
tearing
layer
composite film
polymer composite
utility
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Expired - Fee Related
Application number
CN2012200821391U
Other languages
English (en)
Inventor
李波
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Individual
Original Assignee
Individual
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Individual filed Critical Individual
Priority to CN2012200821391U priority Critical patent/CN202464419U/zh
Application granted granted Critical
Publication of CN202464419U publication Critical patent/CN202464419U/zh
Anticipated expiration legal-status Critical
Expired - Fee Related legal-status Critical Current

Abstract

本实用新型涉及一种密封良好且方便撕裂的聚合物复合薄膜,包括由内到外的聚合物薄膜层、黏胶层、油墨层和硅油层,所述黏胶层、油墨层和硅油层设置有撕裂缝,所述撕裂缝的外部设置有装饰涂层,本实用新型的油墨层通过黏胶层和聚合物薄膜相连,外部覆盖有一层较难撕裂的硅油层,通过这样的复合结构,既加大了本实用新型的撕裂难度,又可以满足包装的需要,在外三层上设置有撕裂缝,撕裂缝外部设置有装饰涂层,既可很方便的找到撕裂缝的位置,又美观,且方便撕开。

Description

一种密封良好且方便撕裂的聚合物复合薄膜
技术领域
本实用新型涉及一种密封良好且方便撕裂的聚合物复合薄膜。 
背景技术
现有的需要包装食品等的薄膜材料基本都是一种软性材料,因此,很容易被不小心撕裂,很不方便,而那种硬性材料,不适合用来包装食品等,即使可包装,由于其硬度大的问题,也会带来难以撕裂的问题,使其在打开时,需要额外的工具。 
而那种既有一定硬度,又方便撕开,而且可用于食品包装的薄膜材料的价格却很贵,因此,一种满足上述要求的复合材料是很有市场前景的。 
实用新型内容
本实用新型要解决的技术问题是提供一种密封良好且方便撕裂的聚合物复合薄膜。 
本实用新型的内容是其包括由内到外的聚合物薄膜层、黏胶层、油墨层和硅油层,所述黏胶层、油墨层和硅油层设置有撕裂缝,所述撕裂缝的外部设置有装饰涂层。 
所述撕裂缝的数目为1个或2个。 
所述装饰涂层的厚度为0.01-0.5mm。 
本实用新型的有益效果是,本实用新型的聚合物薄膜层是一层可食用材料制成的,撕裂力小,通常作为内部包装放置在最里面,但是由于较易撕裂,因此,外部需要涂盖其他材料的薄膜层。 
油墨层通过黏胶层和聚合物薄膜相连,外部覆盖有一层较难撕裂的硅油层,通过这样的复合结构,既加大了本实用新型的撕裂难度,又可以满足包装的需 要。但同时也带来了一个问题,就是难以撕裂的问题,因此,在外三层上设置有撕裂缝,撕裂缝外部设置有装饰涂层,既可很方便的找到撕裂缝的位置,又美观。 
本实用新型的撕裂缝的数目可为1或2个,方便撕开;厚度为0.01-0.5mm。 
附图说明
附图是本实用新型的结构示意图。 
在图中,1聚合物薄膜层、2黏胶层、3油墨层、4硅油层、5装饰涂层、6撕裂缝。 
具体实施方式
如附图所示,本实用新型包括由内到外的聚合物薄膜层1、黏胶层2、油墨层3和硅油层4,所述黏胶层2、油墨层3和硅油层4设置有撕裂缝6,所述撕裂缝6的外部设置有装饰涂层5。 
所述撕裂缝6的数目为1个或2个。 
所述装饰涂层5的厚度为0.01-0.5mm。 
本实用新型的聚合物薄膜层1是一层可食用材料制成的,撕裂力小,通常作为内部包装放置在最里面,但是由于较易撕裂,因此,外部需要涂盖其他材料的薄膜层。 
油墨层3通过黏胶层2和聚合物薄膜层1相连,外部覆盖有一层较难撕裂的硅油层4,通过这样的复合结构,既加大了本实用新型的撕裂难度,又可以满足包装的需要。但同时也带来了一个问题,就是难以撕裂的问题,因此,在外三层上设置有撕裂缝6,撕裂缝6外部设置有装饰涂层5,既可很方便的找到撕裂缝6的位置,又美观。 
本实用新型的撕裂缝6的数目可为1或2个,方便撕开;厚度为0.01-0.5mm。 

Claims (3)

1.一种密封良好且方便撕裂的聚合物复合薄膜,其特征是,包括由内到外的聚合物薄膜层(1)、黏胶层(2)、油墨层(3)和硅油层(4),所述黏胶层(2)、油墨层(3)和硅油层(4)设置有撕裂缝(6),所述撕裂缝(6)的外部设置有装饰涂层(5)。
2.根据权利要求1所述的密封良好且方便撕裂的聚合物复合薄膜,其特征是,所述撕裂缝(6)的数目为1个或2个。
3.根据权利要求1所述的密封良好且方便撕裂的聚合物复合薄膜,其特征是,所述装饰涂层(5)的厚度为0.01-0.5mm。
CN2012200821391U 2012-02-29 2012-02-29 一种密封良好且方便撕裂的聚合物复合薄膜 Expired - Fee Related CN202464419U (zh)