CN201810170U - Wooden fire-proof door made of flame-retardant veneer laminated material - Google Patents

Wooden fire-proof door made of flame-retardant veneer laminated material Download PDF

Info

Publication number
CN201810170U
CN201810170U CN2010205671391U CN201020567139U CN201810170U CN 201810170 U CN201810170 U CN 201810170U CN 2010205671391 U CN2010205671391 U CN 2010205671391U CN 201020567139 U CN201020567139 U CN 201020567139U CN 201810170 U CN201810170 U CN 201810170U
Authority
CN
China
Prior art keywords
door
door leaf
flame
laminated
fire
Prior art date
Application number
CN2010205671391U
Other languages
Chinese (zh)
Inventor
王宝金
印胜和
朱典想
王军
丁建文
Original Assignee
宿迁新缘林木业有限公司
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by 宿迁新缘林木业有限公司 filed Critical 宿迁新缘林木业有限公司
Priority to CN2010205671391U priority Critical patent/CN201810170U/en
Application granted granted Critical
Publication of CN201810170U publication Critical patent/CN201810170U/en

Abstract

The utility model relates to a wooden fire-proof door made of flame-retardant veneer laminated material. A flame-retardant veneer laminated material is produced with low-quality fast-growing wood at first, and then a door frame and a door leaf skeleton is manufactured with the flame-retardant veneer laminated material. The door frame is formed by combining a vertical frame and horizontal frame through tenons, and the door leaf skeleton is formed by combining two side horizontal keels, two side vertical keels, a plurality of middle vertical keels and a plurality of middle horizontal keels through tenons; vertical wood texture of the veneer laminated material is parallel to the length direction of the border of the door frame and the keels of the door leaf skeleton, and a plastic surface is vertical to the surface of a door leaf; the border of the door frame is 90-110mm wide and 40-50mm thick; and side keels of the door leaf skeleton are 50-60mm wide, the middle keels of the door leaf skeleton are 40-50mm wide,, and the door leaf skeleton is 35-40mm thick. The wooden fire-proof door made of flame-retardant veneer laminated material which is manufactured with the low-quality fast-growing wood improves the use value of low-quality wood, and protects natural forest resources.

Description

Flame-retardant veneer laminated fire-proof wooden door

Technical field

The utility model belongs to the labeled door field, is specifically related to a kind of fire-proof wooden door that utilizes the flame-retardant veneer laminated making of fast growing wood.

Background technology

The doorframe of fire-proof wooden door and door leaf skeleton are the key components of fire-proof wooden door, directly have influence on the fire resistance of fire-proof wooden door.The doorframe of fire-proof wooden door and door leaf skeleton all adopt the high-quality solid wood through flame treatment to be made all the time, but because the thickness of solid wood is big, cause the flame treatment difficulty big, the length of penetration of fire retardant is shallow, usually less than 10mm, make that the flame retardant effect of fire-retardant solid wood is poor, fire-retardant cost height.Also can produce distortion through flame treatment and dried solid wood, in use subsequently, need cut shaping processing to fire-retardant solid wood, so just fire-retardant solid wood top layer is absorbed the maximum part of fire retardant and machined away, both weaken the flame retardant effect of solid wood, caused waste simultaneously again.Along with the minimizing day by day of wildwood resource, the high-quality timber resources is also fewer and feweri, and price rises steadily, and makes the cost of manufacture of fire-proof wooden door increase gradually.And the cultivated area of China's fast growing wood constantly enlarges, and the accumulation of fast growing wood and cutting increase year by year.But because there are some natural defects in fast growing wood, material is lower, and is little as the footpath level, density is low, easy deformation etc., makes fast growing wood be difficult to directly to satisfy the requirement of the doorframe and the door leaf skeleton of fire-proof wooden door.

Summary of the invention

Problems such as present high-quality natural timber resource is fewer and feweri in order to solve, solid wood flame treatment difficulty big, flame retardant effect is poor, cost height, and the use value that improves the low-quality fast growing wood, the utility model provides a kind of fire-proof wooden door that utilizes the flame-retardant veneer laminated making of fast growing wood.

The utility model is achieved through the following technical solutions:

A kind of flame-retardant veneer laminated fire-proof wooden door comprises doorframe, and described doorframe is made by fast growing wood is flame-retardant veneer laminated; The fiery face that is subjected at doorframe is pasted with PLASTIC LAMINATED, decorative plywood successively, has groove at doorframe inner surface and door leaf periphery contact position, is provided with the fire prevention expanding sealing strips in groove.

The further improvement project of the utility model is, the vertical texture of laminated veneer lumber wood grain is parallel to the vertical frame of doorframe and the length direction of horizontal frame up and down, and the glue layer of laminated veneer lumber that constitutes doorframe is perpendicular to door leaf surface.

The further improvement project of the utility model is that the border width of doorframe is that 90~110mm, thickness are 40~50mm.

A kind of flame-retardant veneer laminated fire-proof wooden door comprises door leaf skeleton, door leaf, and described door leaf skeleton is made by fast growing wood is flame-retardant veneer laminated; Described door leaf skeleton constitutes frame by two horizontal keel with two vertical keel, at least be provided with vertical keel and horizontal keel in the frame, be pasted with labeled door liner plate, decorative plywood successively in described door leaf skeleton both sides, in labeled door liner plate folder chamber, be filled with inorganic fireproof material.

The further improvement project of the utility model is, the vertical texture of laminated veneer lumber wood grain is parallel to the length direction of door leaf skeleton keel, and the glue layer of laminated veneer lumber that constitutes door leaf skeleton is perpendicular to door leaf surface.

The further improvement project of the utility model is, the limit portion keel siding of door leaf skeleton is that 50~60mm, middle keel siding are 40~50mm, and the thickness of door leaf skeleton is 35~40mm.

A kind of preparation method of aforesaid flame-retardant veneer laminated fire-proof wooden door comprises the following steps:

A) the low-quality fast growing wood being peeled into thickness is that 1.75~2.5mm, book size are the veneer of 1300mm * 830mm, and dries the veneers to 10~12% moisture content;

B) two ends with dried single board process the identical inclined-plane of direction opposite slope respectively, and bevel angle is 6~8 °;

C) two ends are processed bevelled veneer and carry out normal pressure dipping flame treatment, veneer is vertically placed in fire-retardant pond, and immerses fully in the fire resistant fluid, and the liquid level of fire resistant fluid exceeds veneer upper end 400mm; Before veneer began to soak, the fire resistant fluid initial concentration was 25%, and initial temperature is 80~90 ℃, no longer heats in the dipping process;

D) veneer soaks to take out after 5~8 hours to drench in fire resistant fluid and does; Veneer makes moisture content drop to 8~10% through air dry and artificial seasoning after drenching and doing again;

E) will carry out gluing through fire-retardant and dry veneer, bonding adhesive is formed by the melamine resin adehsive modulation of 70% urea-formaldehyde resin adhesive and 30%, and the double spread amount is 320~380g/m 2

F) with blanket glued veneer along the parallel assembly of rift grain direction, slab is with the end chamfer overlap joint of layer veneer, adjacent layer veneer inclined-plane lap-joint staggers mutually; The flame-retardant veneer laminated slab that is used for doorframe and door leaf skeleton carries out assembly respectively, the number of plies of slab is decided according to the thickness of veneer thickness, door jamb or the width and the veneer decrement of door leaf skeleton keel, and the length of slab is decided according to the frame length of doorframe and the length of door leaf skeleton keel respectively;

G) slab was carried out precompressed 2~4 hours, pressure is 1.2MPa;

H) slab after the precompressed make through hot pressing flame-retardant veneer laminated, 110~120 ℃ of hot pressing temperatures, hot pressing pressure 1.8~2.0MPa, hot pressing time 80~90s/mm;

I) flame-retardant veneer laminated after the hot pressing through cooling and health, carry out thick surely sanding, make flame-retardant veneer laminated thickness equal the thickness of door jamb thickness or door leaf skeleton keel, require sawing along its length to become door jamb or door leaf skeleton keel square-section section bar according to door jamb width or door leaf skeleton keel siding again;

J) select the inner surface of a surface of door jamb square-section section bar width as framework, process the groove that the fire prevention expanding sealing strips is installed along its length on this surface, the sectional dimension of groove is identical with the cross section of fire prevention expanding sealing strips; Length according to vertical frame of doorframe and horizontal frame is blocked the square-section section bar, and processes tenon at two ends, is assembled into framework; Framework be subjected to overlay PLASTIC LAMINATED on the fiery face, overlay decorative plywood again in PLASTIC LAMINATED outside; In groove, paste the fire prevention expanding sealing strips, make fireproof door frame;

K) according to the length of each keel of door leaf skeleton the square-section section bar is blocked, and process tenon and tongue-and-groove, be assembled into whole door leaf skeleton at corresponding site; Overlay labeled door liner plate and decorative plywood in the both sides of door leaf skeleton, in labeled door liner plate folder chamber, fill the inorganic fire heat-barrier material, finally make fireproof door leaf.

The both sides that overlay PLASTIC LAMINATED, decorative plywood, fire prevention expanding sealing strips and door leaf skeleton on doorframe described in the utility model overlay the labeled door liner plate and the used bonding adhesive of decorative plywood is fire prevention glue.

In preparation method of the present utility model, the used fire retardant prescription of described veneer normal pressure dipping flame treatment is an ammonium sulfate: ammonium dihydrogen phosphate (ADP): boric acid=1: 8: 1.

Described PLASTIC LAMINATED, labeled door liner plate, decorative plywood, fire prevention expanding sealing strips are market and buy.

The beneficial effects of the utility model are:

A) adopt the rotary cut venner of low-quality timber to make flame-retardant veneer laminated fireproof door frame and door leaf skeleton, improved the use value of low-quality timber, reduced the dependence of fire-proof wooden door, protected the wildwood resource high-quality timber;

B) through hot pressing, flame-retardant veneer laminated density is greater than 600kg/m 3, being higher than solid wood, physical and mechanical property also improves thereupon;

C) veneer is carried out normal pressure dipping flame treatment, method is simple, and veneer can reach 14~17% to the uptake height of fire retardant, and flame-retardant veneer laminated flame retardant agent content is inside and outside consistent, and fire resistance is good, and cost is low;

D) buckling deformation does not take place in the laminated veneer lumber of making after the veneer process high temperature flame-proof impregnation process, and dimensional stability is good;

E) flame-retardant veneer laminated length can require compacting according to vertical keel length with gauge and door leaf skeleton of the length of door jamb and width requirement with thickness, and the post-production loss is little, the timber utilization rate height;

F) the vertical texture of laminated veneer lumber wood grain is parallel to door jamb or door leaf skeleton keel length direction, and glue layer is perpendicular to door leaf surface simultaneously, and when fire-proof wooden door was subjected to fiery face to be subjected to flame and high temperature action, doorframe and door leaf were difficult for occuring bending and deformation.

Description of drawings

Fig. 1 is flame-retardant veneer laminated fire-proof wooden door floor map.Among the figure, 13-fire prevention hinge, 14-door closer, 15-Fire-proof lock.

Fig. 2 is the A-A generalized section of Fig. 1.Among the figure, the horizontal frame of 10-doorframe, 11-door leaf skeleton by-level keel, the horizontal keel of 12-door leaf skeleton limit portion.

Fig. 3 is the B-B generalized section of Fig. 1.Among the figure, inorganic filling material, 7-door leaf skeleton intermediate vertical keel, 8-labeled door liner plate, 9-door leaf decorative plywood in the vertical frame of 1-doorframe, 2-fire prevention expanding sealing strips, 3-PLASTIC LAMINATED, 4-doorframe decorative plywood, the vertical keel of 5-door leaf skeleton limit portion, the 6-door leaf.

The specific embodiment

Below in conjunction with diagram the specific embodiment of the present utility model is described.As Fig. 1, Fig. 2 and shown in Figure 3, the flame-retardant veneer laminated fire-proof wooden door that the utility model provides is made up of doorframe, door leaf skeleton, door skin, door leaf inner stuffing and fire prevention Hardware fitting etc.

Still as Fig. 1, Fig. 2 and shown in Figure 3, doorframe by about vertical frame 1 and horizontal up and down frame 10 by tenon in conjunction with constituting, be pasted with PLASTIC LAMINATED 3 at the fiery face that is subjected to of doorframe, be pasted with decorative plywood 4 outside the PLASTIC LAMINATED; On the doorframe inner surface, have groove, in groove, be pasted with fire prevention expanding sealing strips 2 with door leaf periphery contact position.Door leaf skeleton by vertical keel of horizontal keel of two limit portions 11, two limit portions 12, intermediate vertical keel 5 and three by-level keel 7 by tenon in conjunction with constituting.The both sides of door leaf skeleton overlay labeled door liner plate 8 and door leaf decorative plywood 9, and (in the labeled door liner plate folder chamber) filled fire-proof heat-insulating material 6 and made door leaf in door leaf inside.Described doorframe, door leaf skeleton are made by fast growing wood is flame-retardant veneer laminated, the vertical texture of laminated veneer lumber wood grain is parallel to the vertical frame of doorframe and the length direction of horizontal frame up and down, and the length direction of door leaf skeleton keel, simultaneously the glue layer of the used laminated veneer lumber of doorframe, door leaf skeleton is perpendicular to door leaf surface.The border width of doorframe is that 90~110mm, thickness are 40~50mm; The limit portion keel siding of door leaf skeleton is that 50~60mm, middle keel siding are 40~50mm, and the thickness of door leaf skeleton is 35~40mm.

The preparation method of the flame-retardant veneer laminated fire-proof wooden door that the utility model provides is that it is flame-retardant veneer laminated at first to utilize fast growing wood to make, and utilizes flame-retardant veneer laminated making doorframe and door leaf skeleton again.Then doorframe be subjected to overlay PLASTIC LAMINATED and decorative plywood on the fiery face, the fire prevention expanding sealing strips is installed in the inboard groove of framework, make fireproof door frame.Overlay PLASTIC LAMINATED and decorative plywood in the both sides of door leaf skeleton,, make fireproof door leaf at the inner fire-proof heat-insulating material of filling of door leaf.Specific embodiment is as follows:

It is that 1.75~2.5mm, book size are the veneer of 1300mm * 830mm that fast growing wood is peeled into thickness, and dries the veneers to 10~12% moisture content; The two ends of dried single board are processed the identical inclined-plane of direction opposite slope respectively, and bevel angle is 6~8 °; Two ends are processed bevelled veneer carry out normal pressure dipping flame treatment, veneer is vertically placed in fire-retardant pond, and immerses fully in the fire resistant fluid, and the liquid level of fire resistant fluid exceeds veneer upper end 400mm; Before veneer began to soak, the fire resistant fluid initial concentration was 25%, and initial temperature is 80~90 ℃, no longer heats in the dipping process; Veneer soaks to take out after 5~8 hours to drench in fire resistant fluid to be done; Veneer makes moisture content drop to 8~10% through air dry and artificial seasoning after drenching and doing again; To carry out gluing through fire-retardant and dry veneer, bonding adhesive is formed by the melamine resin adehsive modulation of 70% urea-formaldehyde resin adhesive and 30%, and the double spread amount is 320~380g/m 2Along the parallel assembly of rift grain direction, slab is with the end chamfer overlap joint of layer veneer with blanket glued veneer, and adjacent layer veneer inclined-plane lap-joint staggers mutually; The flame-retardant veneer laminated slab that is used for doorframe and door leaf skeleton carries out assembly respectively, the number of plies of slab is decided according to the thickness of veneer thickness, door jamb or the width and the veneer decrement of door leaf skeleton keel, and the length of slab is decided according to the frame length of doorframe and the length of door leaf skeleton keel respectively; Slab was carried out precompressed 2~4 hours, and pressure is 1.2MPa; Slab after the precompressed is made flame-retardant veneer laminated through hot pressing, 110~120 ℃ of hot pressing temperatures, hot pressing pressure 1.8~2.0MPa, hot pressing time 80~90s/mm; Flame-retardant veneer laminated after the hot pressing through cooling and health, carry out thick surely sanding, make flame-retardant veneer laminated thickness equal the width of door jamb thickness or door leaf skeleton keel, require sawing along its length to become door jamb or door leaf skeleton keel square-section section bar according to door jamb width or door leaf skeleton keel siding again; Select the inner surface of a surface of door jamb square-section section bar width as framework, process the groove that the fire prevention expanding sealing strips is installed along its length on this surface, the sectional dimension of groove is identical with the cross section of fire prevention expanding sealing strips; Length according to vertical frame of doorframe and horizontal frame is blocked the square-section section bar, and processes tenon at two ends, is assembled into framework; Framework be subjected to overlay PLASTIC LAMINATED on the fiery face, overlay decorative plywood again in PLASTIC LAMINATED outside; In groove, paste the fire prevention expanding sealing strips, make fireproof door frame; Length according to each keel of door leaf skeleton is blocked the square-section section bar, and processes tenon and tongue-and-groove at corresponding site, is assembled into whole door leaf skeleton; Both sides by skeleton overlay labeled door liner plate and decorative plywood, fill fire-proof heat-insulating material in door leaf inside, finally make fireproof door leaf.

Claims (7)

1. a flame-retardant veneer laminated fire-proof wooden door comprises doorframe, it is characterized in that: the vertical frame of described doorframe, horizontal frame are made by fast growing wood is flame-retardant veneer laminated; The fiery face that is subjected at doorframe is pasted with PLASTIC LAMINATED (3), decorative plywood (4) successively, has groove at doorframe inner surface and door leaf periphery contact position, is provided with fire prevention expanding sealing strips (2) in groove.
2. a kind of flame-retardant veneer laminated fire-proof wooden door as claimed in claim 1, it is characterized in that: the vertical texture of laminated veneer lumber wood grain is parallel to the vertical frame of doorframe and the length direction of horizontal frame up and down, and the glue layer of laminated veneer lumber is perpendicular to door leaf surface simultaneously.
3. a kind of flame-retardant veneer laminated fire-proof wooden door as claimed in claim 1 is characterized in that: the border width of doorframe is that 90~110mm, thickness are 40~50mm.
4. a flame-retardant veneer laminated fire-proof wooden door comprises door leaf skeleton, it is characterized in that: described door leaf skeleton is made by fast growing wood is flame-retardant veneer laminated; Described door leaf skeleton constitutes frame by two horizontal keel (11) with two vertical keel (12), is provided with vertical keel (5) and horizontal keel (7) in the frame at least.
5. a kind of flame-retardant veneer laminated fire-proof wooden door as claimed in claim 4 is characterized in that: the vertical texture of laminated veneer lumber wood grain is parallel to the length direction of door leaf skeleton keel, and the glue layer of laminated veneer lumber is perpendicular to door leaf surface simultaneously.
6. a kind of flame-retardant veneer laminated fire-proof wooden door as claimed in claim 4 is characterized in that: the limit portion keel siding of door leaf skeleton is that 50~60mm, middle keel siding are 40~50mm, and the thickness of door leaf skeleton is 35~40mm.
7. a kind of flame-retardant veneer laminated fire-proof wooden door as claimed in claim 4 is characterized in that: be pasted with labeled door liner plate, decorative plywood successively in described door leaf skeleton both sides, be filled with inorganic fireproof material in labeled door liner plate folder chamber.
CN2010205671391U 2010-10-19 2010-10-19 Wooden fire-proof door made of flame-retardant veneer laminated material CN201810170U (en)