CN201366446Y - 多边形钢丝拉拔模具 - Google Patents
多边形钢丝拉拔模具 Download PDFInfo
- Publication number
- CN201366446Y CN201366446Y CNU2009200892573U CN200920089257U CN201366446Y CN 201366446 Y CN201366446 Y CN 201366446Y CN U2009200892573 U CNU2009200892573 U CN U2009200892573U CN 200920089257 U CN200920089257 U CN 200920089257U CN 201366446 Y CN201366446 Y CN 201366446Y
- Authority
- CN
- China
- Prior art keywords
- steel wire
- die
- polygonal
- polygon
- wire drawing
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Expired - Fee Related
Abstract
一种多边形钢丝拉拔模具,其特征在于:所述模具包括模套(1)、以过盈配合方式嵌装在模套中空腔内的模芯(2);所述模芯的模孔定型区(3)的横截面呈弧边多边形结构。本实用新型将现有技术的多边形模孔的直线边改为弧线,使原料由圆形截面先变形为弧边多边形,再逐步过渡到直边多边形,从而解决了棱角部位的拉拔润滑问题,避免了多边形钢丝拉拔时产生裂纹。
Description
多边形钢丝拉拔模具
技术领域
本实用新型涉及一种金属拉丝模具,具体说是涉及一种特别适用于拉拔多边 形截面钢丝半成品工序的多边形钢丝拉拔模具。
背景技术
现有技术的多边形截面钢丝普遍采用直边结构的多边孔型的模具经若干道 次拉拔成型。用这种模具进行半成品(前几道次)拉拔时,钢丝的棱角部位难 以得到足够的润滑,很容易在拉拔时产生裂纹。
发明内容
本实用新型的目的正是针对上述现有技术中所存在的不足之处而提供一种 多边形钢丝拉拔模具。
本实用新型的目的可通过下述技术措施来实现-
本实用新型的多边形钢丝拉拔模具包括模套、以过盈配合方式嵌装在模套
中空腔内的模芯;所述模芯的模孔定型区的横截面呈弧边多边形结构。 本实用新型的有益效果如下:
由于本实用新型将现有技术中的半成品拉丝模的模孔定型区由直边多边形 结构改为弧边多边形结构,使被拉拔的原料由圆形截面先变形为弧边多边形, 再经由后道工序逐步过渡到直边多边形,从而解决了棱角部位的拉拔润滑问题, 避免了多边形钢丝拉拔时产生裂纹。
附图说明
图1为本实用新型的结构主视图。
图2为图1的俯视图。
图l、图2中序号:1模套,2模芯,3模孔定型区。 具体实施方式本实用新型以下将结合实施例(附图)作进一步描述:
如图1所示,本实用新型的本实用新型的多边形钢丝拉拔模具包括模套1、 以过盈配合方式嵌装在模套中空腔内的模芯2;所述模芯的模孔定型区3的横截 面呈弧边多边形结构。
Claims (1)
1、一种多边形钢丝拉拔模具,其特征在于:所述模具包括模套(1)、以过盈配合方式嵌装在模套中空腔内的模芯(2);所述模芯的模孔定型区(3)的横截面呈弧边多边形结构。