CN201218383Y - 一种内衬穿插法修复的旧管道 - Google Patents

一种内衬穿插法修复的旧管道 Download PDF

Info

Publication number
CN201218383Y
CN201218383Y CNU2008200710320U CN200820071032U CN201218383Y CN 201218383 Y CN201218383 Y CN 201218383Y CN U2008200710320 U CNU2008200710320 U CN U2008200710320U CN 200820071032 U CN200820071032 U CN 200820071032U CN 201218383 Y CN201218383 Y CN 201218383Y
Authority
CN
China
Prior art keywords
pipeline
old pipeline
old
density polyethylene
polyethylene pipe
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Expired - Lifetime
Application number
CNU2008200710320U
Other languages
English (en)
Inventor
张严甫
曹世东
葛延超
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Henan Zhongtuo Petroleum Engineering Technology Co., Ltd.
Original Assignee
Zhongtuo Pipeline Cheaning And Repairing Engineering Co Ltd Puyang City
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Zhongtuo Pipeline Cheaning And Repairing Engineering Co Ltd Puyang City filed Critical Zhongtuo Pipeline Cheaning And Repairing Engineering Co Ltd Puyang City
Priority to CNU2008200710320U priority Critical patent/CN201218383Y/zh
Application granted granted Critical
Publication of CN201218383Y publication Critical patent/CN201218383Y/zh
Anticipated expiration legal-status Critical
Expired - Lifetime legal-status Critical Current

Abstract

本实用新型提供一种内衬穿插法修复的旧管道,包括旧管道和内衬于旧管道内的高密度聚乙烯管,所述旧管道的两端分别设置有连接法兰,所述高密度聚乙烯管的两端分别沿对应的所述连接法兰外翻形成PE翻边;所述旧管道一端的连接法兰设置有镶嵌PE翻边的槽和水纹线,所述旧管道另一端的连接法兰设置有夹固PE翻边用的防脱台;该内衬穿插法修复的旧管道结构设计科学,耐磨性强,实用性强,其能够有效避免管道在输送介质的过程中所存在的沙石及其它固体颗粒进入高密度聚乙烯管与管道的夹层中,避免了内衬管道被输送介质中的沙石及其它固体颗粒破坏的危险,保证了内衬穿插法修复旧管道的施工质量。

Description

一种内衬穿插法修复的旧管道
技术领域
本实用新型涉及一种旧管道修复技术,具体的说,涉及一种内衬穿插法修复的旧管道。
背景技术
对于铺设于地表下的运输管道,当管道内层磨损一定程度后,就产生了影响生产的安全隐患,此时,通常需要对管道进行修复;
现有的管道修复技术是采用卷扬机强制牵引高密度聚乙烯(HDPE)管进入旧管道,并将高密度聚乙烯(HDPE)管内衬于旧管道内;
但是,当内衬的高密度聚乙烯管与旧管道内壁贴合不严时,在旧管道内输送介质的过程中,其夹杂的沙石或固体颗粒会进入高密度聚乙烯管内衬层与旧管道内壁的缝隙中,进而,使该内衬旧管道逐渐被破坏,若发生这种情况,不仅达不到修复旧管道的目的,而且又给旧管道的正常运行带来更大的安全隐患。
为了克服以上存在的问题,人们一直在寻找一种适于实用的技术解决方案。
发明内容
本实用新型的目的在于克服现有技术的不足,从而提供一种结构设计科学、耐磨实用的内衬穿插法修复的旧管道。
本实用新型的目的是通过下面的技术方案来实现的:
一种内衬穿插法修复的旧管道,包括旧管道和内衬于旧管道内的高密度聚乙烯管,所述旧管道的两端分别设置有连接法兰,所述高密度聚乙烯管的两端分别沿对应的所述连接法兰端部外翻形成PE翻边;
所述旧管道一端的连接法兰设置有镶嵌PE翻边的槽和水纹线,所述旧管道另一端的连接法兰设置有夹固PE翻边用的防脱台。
本实用新型相对于现有技术具有实质性特点和进步性,具体的说,该内衬穿插法修复的旧管道结构设计科学,耐磨性强,实用性强,其能够有效避免管道在输送介质的过程中所存在的沙石及其它固体颗粒进入高密度聚乙烯管与管道的夹层中,避免了内衬管道被输送介质中的沙石及其它固体颗粒破坏的危险,保证了内衬穿插法修复旧管道的施工质量。
附图说明
图1是本实用新型的结构示意图。
具体实施方式
为了更进一步的说明本实用新型的优点和技术特征,下面结合附图给出本实用新型的具体实施方式:
如图1所示,一种内衬穿插法修复的旧管道,包括旧管道1和内衬于旧管道1内的高密度聚乙烯管3,所述旧管道1的两端分别设置有连接法兰2和连接法兰4;所述旧管道1与所述连接法兰(2,4)焊接连接,二者内径相同;
所述高密度聚乙烯管3的两端分别沿对应的所述连接法兰(2,4)端部外翻形成PE翻边;
所述PE翻边与对应的所述连接法兰(2,4)紧密配合;
所述旧管道1一端的连接法兰设置有槽和水纹线,所述槽和水纹线可起到镶嵌PE翻边的目的;
所述旧管道1另一端的连接法兰设置有防脱台,两根旧管道通过螺栓连接到一起时,所述防脱台可起到夹固PE翻边的目的。
所述高密度聚乙烯管3的两端的所述PE翻边与所述连接法兰(2,4)结合,使旧管道1两端形成了径向的保护,进而使通过所述高密度聚乙烯管3的运输介质无法进入所述高密度聚乙烯管3与所述旧管道1之间的夹层内。
翻边制作方法:将特制模具固定在穿入后的高密度聚乙烯管端头,然后,通过加热处理一次形成与内衬管一体的PE翻边,使PE翻边紧贴在铸铁或钢的连接法兰前面,从而形成复合法兰;
这种技术处理后的端口特点为连接法兰和内衬高密度聚乙烯管为一整体,且施工方便,质量可靠,已在多个工程中试验成功。
最后应当说明的是:以上实施例仅用以说明本实用新型的技术方案而非对其限制;尽管参照较佳实施例对本实用新型进行了详细的说明,所属领域的普通技术人员应当理解:依然可以对本实用新型的具体实施方式进行修改或者对部分技术特征进行等同替换;而不脱离本实用新型技术方案的精神,其均应涵盖在本实用新型请求保护的技术方案范围当中。

Claims (2)

1、一种内衬穿插法修复的旧管道,包括旧管道和内衬于旧管道内的高密度聚乙烯管,其特征在于:所述旧管道的两端分别设置有连接法兰,所述高密度聚乙烯管的两端分别沿对应的所述连接法兰端部外翻形成PE翻边。
2、根据权利要求1所述的一种内衬穿插法修复的旧管道,其特征在于:所述旧管道一端的连接法兰设置有镶嵌PE翻边用的槽和水纹线,所述旧管道另一端的连接法兰设置有夹固PE翻边用的防脱台。
CNU2008200710320U 2008-06-16 2008-06-16 一种内衬穿插法修复的旧管道 Expired - Lifetime CN201218383Y (zh)