CN1626297A - 铁型覆砂无芯制造曲轴的方法 - Google Patents
铁型覆砂无芯制造曲轴的方法 Download PDFInfo
- Publication number
- CN1626297A CN1626297A CN 200310119018 CN200310119018A CN1626297A CN 1626297 A CN1626297 A CN 1626297A CN 200310119018 CN200310119018 CN 200310119018 CN 200310119018 A CN200310119018 A CN 200310119018A CN 1626297 A CN1626297 A CN 1626297A
- Authority
- CN
- China
- Prior art keywords
- sand
- core
- chill
- iron mold
- sand covered
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Pending
Abstract
铁型覆砂无芯制造曲轴的方法,涉及一种铁型覆砂制造曲轴工艺。主要是为解决现有的用铁型覆砂工艺制造曲轴时需要下芯铸造,产品合格率低、工序复杂的问题而设计的。本发明是首先制造随型冷铁,用螺丝将其固定在铁型上,在型板上做出芯盒部分,通过射砂直接将砂层覆着在冷铁上。优点是不需下芯,一次成型,有冷铁,曲轴各部位同时冷却凝固,产品合格率高,而且工序少,成本低。
Description
技术领域:本发明涉及一种铁型覆砂制造曲轴工艺。
背景技术:目前用铁型覆砂工艺制造曲轴时分型面为平面,曲轴有的拐不在分型面上,需要下芯铸造,下芯时芯上砂层较厚,不能与曲轴其它部位达到同时冷却、凝固,容易出现缺陷,降低产品合格率,还需要有制芯和下芯工序。
发明内容:本发明的目的是提供一种铁型覆砂无芯制造曲轴的方法。
本发明的目的是这样实现的:首先制作随型冷铁(芯骨),将其固定在铁型上,通过射砂直接将砂层覆着在冷铁上,直接带出原来所需下芯部分。
本发明的优点是:不需下芯,一次成型,有冷铁,曲轴各部位同时冷却凝固,产品合格率大大提高,而且工序少,成本低。
具体实施方式:首先制造随型冷铁,用螺丝将其固定在铁型上,在型板上做出芯盒部分,通过射砂直接将砂层覆着在冷铁上。
Claims (1)
1.铁型覆砂无芯制造曲轴的方法,其特征是首先制作随型冷铁,将其固定在铁型上,通过射砂直接将砂层覆着在冷铁上。