CN1456743A - 龙须草书画纸的制造方法 - Google Patents

龙须草书画纸的制造方法 Download PDF

Info

Publication number
CN1456743A
CN1456743A CN 02113715 CN02113715A CN1456743A CN 1456743 A CN1456743 A CN 1456743A CN 02113715 CN02113715 CN 02113715 CN 02113715 A CN02113715 A CN 02113715A CN 1456743 A CN1456743 A CN 1456743A
Authority
CN
China
Prior art keywords
calligraphy
alpine rush
chinese alpine
manufacture method
painting paper
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Pending
Application number
CN 02113715
Other languages
English (en)
Inventor
李平
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Individual
Original Assignee
Individual
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Individual filed Critical Individual
Priority to CN 02113715 priority Critical patent/CN1456743A/zh
Publication of CN1456743A publication Critical patent/CN1456743A/zh
Pending legal-status Critical Current

Abstract

发明公开了一种以龙须草或竹子为主要原材料制成的用于手抄书画的纸的制造方法,经过备料、送料、蒸煮、漂白、打浆、配料、抄制、干燥、成品、包装等工序而制成,蒸煮工序中按蒸煮锅容量装锅2立方米(200千克)计时,蒸煮8-12小时,且最高压力为5千克/平方米,抄制工序中打浆疏解,叩解度20-40℃,龙须草的长度为5-20厘米,桑皮的长度为1-10厘米,麻的长度为1-10厘米,本发明强度和浸润性能能够满足书画艺术的要求,特别适用于重笔和反复渲染,纸质韧而润,折而无损,润墨性强,原料丰富且价格低。

Description

龙须草书画纸的制造方法
所属技术领域:
本发明涉及一种以龙须草为主要原材料制成的用于手抄书画的纸的制造方法。
背景技术:
随着物质文明的提高,精神文明也随之发展。棋琴书画是我国自古的传统。造纸术是我国的四大发明之一。目前有名的纸包括以皮纤维为主要原料的宣纸、以桑皮为主要原料的迁安皮纸。现有的纸种均存在强度和浸润性差的缺点,对于书画中的重笔和反复润墨的要求,一般不能达到其要求,拉力不够,润墨效果差,其效果影响书画艺术的发展,且宣纸和皮纸的原料资源不丰富,生产量受限,价格高。
发明内容:
本发明提供了一种以龙须草或竹子为主要原材料制成的用于手抄书画的纸的制造方法。这种制造方法是针对本申请人的另一专利申请“龙须草书画纸”而提出的,该纸的强度和浸润性能能够满足书画艺术的要求,特别适用于重笔和反复渲染,纸质韧而润,折而无损,润墨性强,原料丰富,价格低,本发明所述的制造方法简单、易于操作控制,生产成本低。
本发明的具体技术方案如下:
本发明包括备料、送料、蒸煮、漂白、打浆、配料、抄制、干燥、成品、包装等工序,其特征在于:
A、蒸煮工序中按蒸煮锅容量装锅2立方米(200千克)计时,蒸煮8-12小时,且最高压力为5千克/平方米;
B、抄制工序中打浆疏解,叩解度20-40℃。
本发明所述的龙须草的长度为5-20厘米。
本发明所述的桑皮的长度为1-10厘米。
本发明所述的麻的长度为1-10厘米。
本发明所述的成品的硫化度为8-20%。
本发明所述的成品的填率3-10%。
本发明所述的成品的漂率3-15%。
本发明的技术指标如下:
强度(纵向)2.00kg/15mm以上,强度(横向)1.20kg/15mm以上,吸收性40.00-60.00mm/100秒,撕裂度30.00-40.00g,湿强度(浸湿后)0.10-0.20kg/15mm,伸缩率(在水浸泡15-20分钟浸湿的湿纸和干纸的对比)小于1.00。
本发明成品强度和浸润性能能够满足书画艺术的要求,特别适用于重笔和反复渲染,纸质韧而润,折而无损,润墨性强,原料丰富,生产过程简单易于控制,生产成本低。
具体实施方式:
实施例1
选取竹子40克、龙须草20克、桑皮20克、麻20克、烧矸19克,硫化矸和漂液若干克,经过备料、送料、蒸煮、漂白、打浆、配料、抄制、干燥、成品、包装等工序而制成,蒸煮工序中按蒸煮锅容量装锅2立方米(200千克)计时,蒸煮10小时,压力为4千克/平方米;抄制工序中打浆疏解,叩解度30℃。成品硫化度为11%,填率5%,漂率5%。
实施例2
选取龙须草40克、桑皮30克、麻10克、烧矸20克,硫化矸和漂液若干克,经过备料、送料、蒸煮、漂白、打浆、配料、抄制、干燥、成品、包装等工序而制成蒸煮工序中按蒸煮锅容量装锅2立方米(200千克)计时,蒸煮9小时,且压力为4千克/平方米;抄制工序中打浆疏解,叩解度40℃。成品硫化度为11%,填率6%,漂率8%。
本发明强度和浸润性能能够满足书画艺术的要求,特别适用于重笔和反复渲染,纸质韧而润,折而无损,润墨性强,原料丰富且价格低。

Claims (7)

1、龙须草书画纸的制造方法,包括备料、送料、蒸煮、漂白、打浆、配料、抄制、干燥、成品、包装等工序,其特征在于:
A、蒸煮工序中按蒸煮锅容量装锅2立方米(200千克)计时,蒸煮8-12小时,且最高压力为5千克/平方米;
B、抄制工序中打浆疏解,叩解度20-40℃。
2、根据权利要求1所述的所述的龙须草书画纸的制造方法,其特征在于:龙须草的长度为5-20厘米。
3、根据权利要求1所述的所述的龙须草书画纸的制造方法,其特征在于:所述的桑皮的长度为1-10厘米。
4、根据权利要求1所述的所述的龙须草书画纸的制造方法,其特征在于:所述的麻的长度为1-10厘米。
5、根据权利要求1所述的所述的龙须草书画纸的制造方法,其特征在于:所述的成品的硫化度为8-20%。
6、根据权利要求1所述的所述的龙须草书画纸的制造方法,其特征在于:所述的成品的填率3-10%。
7、根据权利要求1所述的所述的龙须草书画纸的制造方法,其特征在于:所述的成品的漂率3-15%。
CN 02113715 2002-05-10 2002-05-10 龙须草书画纸的制造方法 Pending CN1456743A (zh)