CN118181001A - A process for precision grinding high-precision spring chuck - Google Patents

A process for precision grinding high-precision spring chuck Download PDF

Info

Publication number
CN118181001A
CN118181001A CN202410488700.3A CN202410488700A CN118181001A CN 118181001 A CN118181001 A CN 118181001A CN 202410488700 A CN202410488700 A CN 202410488700A CN 118181001 A CN118181001 A CN 118181001A
Authority
CN
China
Prior art keywords
paraffin
mandrel
grinding
collet
workpiece
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Pending
Application number
CN202410488700.3A
Other languages
Chinese (zh)
Inventor
杨凯
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Jinan Kaiter Machinery Co ltd
Original Assignee
Jinan Kaiter Machinery Co ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Jinan Kaiter Machinery Co ltd filed Critical Jinan Kaiter Machinery Co ltd
Priority to CN202410488700.3A priority Critical patent/CN118181001A/en
Publication of CN118181001A publication Critical patent/CN118181001A/en
Pending legal-status Critical Current

Abstract

The application discloses a process for precisely grinding a high-precision spring chuck, which comprises a step of filling paraffin between a mandrel and the spring chuck and a grinding step; according to the application, the mandrel is designed to be completely consistent with the inner hole size of the collet chuck, so that the mandrel and the inner hole wall of the workpiece are free from any extrusion and deformation, and the collet chuck workpiece is free from deformation and distortion; in the precise grinding process, the paraffin can play a role of a binder, and can temporarily bond the mandrel and the workpiece into a whole; in addition, the support and the stabilization can be realized; meanwhile, paraffin wax has good cooling and lubricating effects; the mandrel is used for matching paraffin to realize a stress-free and damage-free mode for connecting the mandrel and a workpiece together.

Description

Process for precisely grinding high-precision spring chuck
Technical Field
The invention relates to the technical field of grinding of multi-metal high-precision collet chucks, in particular to a process for precisely grinding a high-precision collet chuck.
Background
Spring chucks (also known as collets) are a part commonly used in machining (e.g., milling, drilling, engraving) to hold tools and are also a wearing part. A typical collet will gradually lose accuracy after hundreds or thousands of uses, requiring replacement.
At present, the competition is becoming more and more intense, many collet manufacturers feel unprecedented pressure, the price is becoming more and more transparent, and the quality requirements are gradually rising. The enterprise is urgently required to have a new process method capable of solving the defects, and the new process method is improved in yield, better in quality, higher in efficiency, lower in labor cost and lower in dependence on technical workers.
With the development of the tool industry, the collet has developed in various types: such as ER collet, SK collet, ST collet, TG collet, and various rubber compound collet, etc. (the basic profile is shown in fig. 4). Among them, the metal collet chuck has the greatest yield and the most widely used. The invention will be described with respect to the novel process and principles of the invention with respect to ER collets. The grinding process of other collets is similar to this. Common models of ER collets are: ER11, ER16, ER20, ER25, ER32, ER40, and the like. Whichever collet, the basic structural features are as shown in fig. 5.
The production and demand for various types of collets is enormous, with hundreds of millions of production being available only in the domestic market. The performance and accuracy of the collet is directly affected by the manufacturing process. Conventional manufacturing processes generally comprise fourteen key steps: 1. blanking; 2. turning the appearance and punching an inner hole; 3. heat treatment; 4. milling a groove after surface sand blasting; 5. deburring and rough grinding an outer circle and a conical surface; 6. grinding the inner hole; 7. milling through six-petal slit grooves; 8. the tool shaft is sleeved on the accurate grinding excircle, and the outer conical surface is accurately ground; 9. detecting accuracy such as jumping; 10. secondary refining of the outer conical surface (this is the secondary refining for a high precision collet); 11. detecting final precision; 12. polishing the surface; 13. marking the model by laser coding; 14. and (5) smearing rust-preventive oil and packaging.
And in the sixth step, after the inner hole is ground, the six-piece gap (the elastic expansion groove) of the collet needs to be completely disconnected, and the structural rigidity of the collet is greatly weakened by one-step operation, and the central hole of the collet is damaged at the moment and cannot be used as a positioning reference when the outer circle is ground. In the subsequent finish grinding of the outer cone, a special mandrel is generally used for positioning. The mandrel is penetrated in the inner hole of the collet chuck, two ends of the mandrel are exposed out of the collet chuck, and two ends of the mandrel are provided with center holes. Taking the ER collet mandrel as an example, the mandrel used is typically 0.15-0.3 mm thicker than the bore in order to generate sufficient friction. This results in the six-piece inner bore of the collet being stretched and elastically deformed after the mandrel is installed. The traditional process utilizes the friction force generated by the deformation to realize the accurate grinding of the outer circle of the collet chuck. However, this deformation will result in a very difficult control of the runout error of the collet after the outer cone has been refined (i.e. process step 8 above). In other words, it is difficult to control the final clamping accuracy of the product under the process conditions of deformation of the workpiece. In actual production, collet manufacturers often need to select collets meeting the high-precision requirement by piece-by-piece detection, which not only takes time and labor, but also has the probability of meeting the high-precision standard of less than 10%. Under the influence of this, the price of a high-precision collet (generally referred to as a collet holding measuring stick jumping less than 3 microns at five diameters and repeatedly loosening a rotating measuring stick to measure a plurality of different positions) circulated in the domestic market is often five to eight times that of the ordinary precision. The price of imported high precision is more striking, as much as 20 times.
Disclosure of Invention
The invention aims to provide a process for precisely grinding a high-precision spring chuck, which is used for greatly improving the grinding efficiency and the precision grade of the spring chuck, and combining an automatic detection and clamping system, a stable unmanned production line can be realized, and the process is an advanced process method for efficiently and stably producing the high-precision chuck in the future. The precision loss caused by the fact that the collet chuck is opened by the thicker mandrel in the prior art is avoided. Several times improvement in reliability and yield is obtained.
In order to solve the technical problems, the invention adopts the following technical scheme:
The invention provides a process for precisely grinding a high-precision spring chuck, which comprises the following steps of:
1. Blanking; 2. turning the appearance and punching an inner hole; 3. heat treatment; 4. milling a groove after surface sand blasting; 5. deburring and rough grinding an outer circle and a conical surface; 6. grinding the inner hole; 7. milling through six-petal slit grooves; 8. sleeving the outer conical surface on a special mandrel for finely grinding the outer circle; 9. detecting accuracy such as jumping; 10. secondary refining of the outer conical surface (this is the secondary refining for a high precision collet); 11. detecting final precision; 12. polishing the surface; 13. marking the model by laser coding; 14. smearing rust-preventive oil and packaging;
in particular, the invention improves the step 8 innovatively, improves the precision and the yield, and can save the steps 9 and 10 for most collet chucks;
and 8, sleeving the tool shaft for accurately grinding the outer circle, accurately grinding the outer conical surface, and specifically comprising the following steps of:
The method comprises the following steps:
S1, selecting a special mandrel;
When the outer edge of the collet chuck is finely ground, the difference between the outer diameter of the mandrel and the diameter of the detection measuring rod is close to zero, so that the size of an inner hole of the collet chuck is completely consistent with that of a grinding mandrel, and the condition that the inner hole wall of the workpiece of the collet chuck and the mandrel do not have any extrusion and deformation is met;
s2, selecting a connecting material;
Wherein the workpiece and the mandrel are temporarily connected by the low-temperature paraffin; wherein deformation grooves uniformly distributed on the surface of the collet chuck base body are utilized, so that enough paraffin is just contained in the grooves;
The paraffin with low melting point is selected to be softened at about 50 ℃ and is in a liquid state at about 55 ℃; the paraffin temperature at the temperature cannot cause energy loss due to too high melting point, is easy to construct, and has good safety;
s3, pouring paraffin;
firstly, placing a collet workpiece and a positioning mandrel on a die disc, pressing a pressing disc on the upper part of the collet workpiece and pressing a mesh on the lower part of the pressing disc, wherein the pressing disc is provided with low-melting-point paraffin;
When the temperature of the operating room environment or the special heating box reaches 55-60 ℃, paraffin on the pressure plate is gradually melted into liquid and flows onto the lower die plate, so that the collet and the mandrel are soaked in the paraffin liquid; after a period of time, the batch of workpieces can be cooled, so that paraffin in the die is completely solidified;
S4, precisely grinding;
When fine grinding is carried out, batch processing is adopted, and the grinding mode is basically the same as the traditional process; the grinding quantity is generally controlled to be between 0.01 and 0.03mm, and the grinding time is generally only a short number of seconds;
Preferably, in the step S1, surface knurling or other rolling modes can be adopted on the design of the mandrel, so that the surface roughness of the mandrel is increased, and the connection strength of a workpiece and the mandrel is greatly improved; the mandrel surface is also provided with hundreds of grooves for receiving paraffin.
Preferably, the central holes at two ends of the mandrel in the step S1 are centered and coaxial, the roundness is less than 1 micron, the cylindricity of the mandrel is less than 3 microns, and the consistency of the whole batch is less than 3 microns.
Preferably, in S3, when paraffin is poured, the inner surface and the outer surface of the workpiece are subjected to cleaning treatment, so that the influence of greasy dirt and dirty matters on the positioning of the mandrel and the reduction of the connection strength are avoided.
Preferably, in S3, paraffin liquid is vibrated by a small amplitude to promote paraffin flow into each gap between the collet workpiece and the positioning mandrel.
Preferably, in S3, the mold disc used is provided with a hole adapted to the shape of the collet workpiece, so as to save the amount of paraffin, avoid the excessive thick paraffin wrapping the surface of the workpiece, cause unnecessary waste and slow down the grinding process, and enable the collet and the mandrel to be tightly combined in a proper pressure state, so that the paraffin adapts to the shape of the workpiece through expansion and contraction of the paraffin in the whole cooling process.
Preferably, in S3, the paraffin pouring structure includes a heating tank, a mold disc disposed on the heating tank and stacked layer by layer, a spring chuck to be injected disposed on the mold disc, a pressing plate disposed on the top of the spring chuck to be injected, and a paraffin tank disposed at the uppermost layer;
Wherein reserved slots which are matched with the outer wall of the spring chuck to be injected with wax are uniformly formed on the die plate;
wherein, a reserved slotted hole which is convenient for facing the spring chuck to be injected with wax is arranged on the pressure plate.
Preferably, in S4, when fast dewaxing is desired, paraffin melting is accelerated by using hot water or hot oil to which rust inhibiting additives are added.
Compared with the prior art, the invention has the beneficial technical effects that:
According to the application, the mandrel is designed to be completely consistent with the inner hole size of the collet chuck, so that the mandrel and the inner hole wall of the workpiece are free from any extrusion and deformation, the knurling or densely distributed pits on the surface of the mandrel are utilized, and paraffin is poured into gaps of the collet chuck, so that the mandrel can drive the workpiece to rotate, the finish grinding of only a few wires is realized, and the mandrel and the workpiece are connected together in a stress-free and damage-free manner by adopting the paraffin in the process;
In the precise grinding process, the paraffin can play a role of a binder, and can temporarily bond the mandrel and the workpiece into a whole; in addition, the support and the stabilization can be realized; because the broken collet is less rigid, the finely ground grinding wheel is not corrected very sharply, and the grinding force is larger at the moment, so that the grinding deformation is increased. The paraffin is well filled and adhered between the gaps of the collet, so that the rigidity of the collet is obviously increased, and the grinding deformation is reduced greatly;
At the same time, paraffin wax has good cooling and lubricating effects. In the precise grinding process, the load of grinding can be reduced, the service life of the grinding wheel is prolonged, and the grinding heat can be compensated and cooled in the grinding area with insufficient cooling liquid, so that the influence of thermal stress on the workpiece structure is alleviated. During the grinding process, about 30% to 60% of the paraffin wax is melted by the grinding heat after grinding; the residual paraffin can be melted by heating, and in short, the paraffin in the application can be recycled in a reasonable way.
Drawings
The invention is further described with reference to the following description of the drawings.
FIG. 1 is a schematic diagram of equipment used in the process of precisely grinding a high-precision spring chuck according to the invention;
FIG. 2 is a schematic diagram of a mandrel used in the process of precisely grinding a high-precision spring chuck according to the present invention;
FIG. 3 is a schematic diagram of the operation of a conventional grinding high precision collet;
FIG. 4 is a basic outline schematic of a prior art spring clip;
FIG. 5 is a basic external schematic view of a prior ER collet.
Reference numerals illustrate:
1. A mandrel; 11. a first mandrel end; 12. surface knurling; 13. a second mandrel end; 2. an existing mandrel; 3. a spring chuck; 4. grinding wheel; 5. a heating tank; 51. a tank body; 6. a mold plate; 7. a pressure plate; 8. a paraffin tank.
Detailed Description
The embodiment discloses a process for precisely grinding a high-precision spring chuck, which is characterized in that in the specific step 8, the process is sleeved on a tool shaft for precisely grinding an outer circle and a precisely grinding an outer conical surface for improvement;
The precision loss caused by the fact that the collet chuck is opened by a thicker mandrel in the prior art is avoided; several times improvement in reliability and yield is obtained.
The process principle is as follows:
First, the fifth step (deburring and rough grinding of the outer circle and conical surface) is to be controlled strictly to ensure that the rear positioning surface and the front locking surface of the collet (the front 60 ° taper portion of the ER collet) are to be kept coaxial within 0.003 and the roundness of each part is less than 0.002. This step ensures that good accuracy is critical to the accurate grinding of the inner bore. The cylindricity of the accurate grinding inner hole is less than 0.004, and the roundness is less than 0.002; the good inner hole shape is the basis for the subsequent fine grinding of the outer circle.
Of course, heat treatment and material selection are critical, wherein the heat treatment is performed at least three times, including one sub-zero treatment. The internal stress of the heat-treated material is completely released, the structure is uniform, and the hardness is moderate. The collet can basically maintain the original shape precision after the milling groove is broken. With these assurance requirements, it is particularly important how to refine the outer cone (i.e., the locating cone). If the thicker mandrel is adopted to be spread, new stress can be generated, and the deformed workpiece can generate random deformation and errors under the influence of grinding force and grinding heat. The qualified rate is seriously affected, and the previous efforts of each process step are lost, so that huge waste is caused, and the previous work is abandoned.
Therefore, the largest difference in the size of the special mandrel when the outer cone is refined is that the outer diameter differs little from the diameter of the measuring stick (or from the tool shank that is actually to be clamped). For example: the inner hole is a collet chuck with the diameter of 6+/-0.001, and when the conical surface is finely ground, a process mandrel with the diameter of 6+/-0.001 is used for clamping and positioning, at the moment, the size of the inner hole of the collet chuck is almost completely consistent with that of a grinding mandrel, that is, the mandrel and the inner hole wall of the workpiece are not extruded and deformed, and the workpiece cannot be deformed and distorted certainly under the state. In addition, the center holes at the two ends of the mandrel are centered and coaxial, the roundness is less than 1 micron, the cylindricity of the mandrel is less than 2 microns, and the consistency of the whole batch is less than 3 microns. The roundness and coaxiality of the center hole directly affect the final runout of the workpiece.
In order to achieve the purpose that the mandrel drives the workpiece to rotate and achieve accurate grinding of only a few wires, the workpiece needs to be prevented from slipping on the mandrel, and certain measures need to be taken, namely, the mandrel and the workpiece are connected in a stress-free and damage-free mode. So that the grinding can be smoothly performed and the mandrel can be reused.
Through repeated experiments and screening comparison, the pen applicant creatively finds that the workpiece and the mandrel can be well and temporarily connected by using low-temperature paraffin. And the surface knurling mode can be adopted in the design of the mandrel, so that the surface roughness is increased, and the connection strength of the workpiece and the mandrel is greatly improved. The mandrel of fig. 4 is surface rolled so that the surface is covered with hundreds of grooves which can hold paraffin, and whatever elastic collet has uniformly distributed deformation grooves on the surface of the collet base, and enough paraffin is just held in the grooves.
Paraffin plays two key roles in the precision grinding process. Firstly, can play the effect of binder, can temporarily bond dabber and work piece into an organic whole, and secondly, play support and firm effect. Because the broken collet is less rigid, the finely ground grinding wheel is not corrected very sharply, and the grinding force is larger at the moment, so that the grinding deformation is increased. The paraffin is well filled and adhered in the gaps of the collet, so that the rigidity of the collet is obviously increased, and the grinding deformation is reduced greatly. Thirdly, paraffin also has a very good cooling and lubricating effect. In the precise grinding process, the load of grinding can be reduced, the service life of the grinding wheel is prolonged, and the grinding heat can be compensated and cooled in the grinding area with insufficient cooling liquid, so that the influence of thermal stress on the workpiece structure is alleviated. In practice, about 30% to 60% of the paraffin will melt after grinding due to the grinding heat, as the cutting fluid enters the water tank. Thus, a paraffin separation device is arranged in the water tank.
Generally, the melting point of paraffin waxes is between 40-80 ℃, the specific values depending on the type, purity and manufacturing process. The process particularly selects low-melting-point paraffin, and the paraffin begins to soften at about 50 ℃ and is completely in a liquid state at a temperature of more than 52-55 ℃. The paraffin temperature at the temperature can not cause energy loss due to too high melting point, is easy to construct, and has good safety (operators can not be scalded). The paraffin melted at about 40 ℃ is not selected because the paraffin with a melting point of 40 ℃ is easily changed into a liquid state due to the influence of the ambient temperature and the grinding heat, and the construction is not easy, especially when the air temperature is high in summer, the material is easy to deteriorate.
The method comprises the steps of firstly cleaning and cleaning a workpiece, removing dirt and greasy dirt in an inner hole and a gap of the workpiece, then placing the workpiece and the positioning mandrel on a die disc, (particularly, a paraffin groove for placing the workpiece is specially made according to the appearance of the workpiece, a paraffin groove of an ER collet is shaped), a pressure plate is pressed above the workpiece, meshes are arranged below the pressure plate, low-melting-point paraffin (such as No. 52 paraffin) is arranged on the pressure plate, after the ambient temperature of an operation room reaches 55-60 ℃, the paraffin on the pressure plate is gradually melted into liquid and flows onto the die disc below, so that the collet and the mandrel are soaked in paraffin liquid. The paraffin flow into each slit can be promoted by small vibrations. Then the batch of workpieces is cooled to about 18-20 degrees, (the process can be accelerated by placing the workpieces in a groove pool with dry ice for 1-2 minutes) until the liquid paraffin is completely solidified. The purpose-made mould disk not only can save the dosage of paraffin, avoid the too thick paraffin of work piece surface parcel, cause unnecessary waste and the slowing down of grinding beat, but also in order to closely combine collet chuck and dabber with certain pressure state for paraffin adapts to the appearance of work piece through self expansion and shrink in whole cooling process. Therefore, the pressure plates of different collets have different weights, the weight is not required to be too heavy, the pressure of the inner wall of the hole is 3-5 kg/cm 2, and the accuracy is slightly influenced by the too light pressure.
Finally, batch processing is adopted when finish grinding is carried out, and the grinding mode is basically the same as the traditional process. The grinding amount is controlled to be between 0.01 and 0.03, and the grinding time is only a few seconds. During this time, the grinding heat melts the paraffin on the surface of the workpiece and is carried away by the cutting fluid. The paraffin wax inside the workpiece and around the mandrel remains firmly present after grinding. For this purpose, the remaining paraffin can be melted by slow heating. Generally, when the temperature is about 52 ℃, paraffin gradually melts into liquid and flows down. The paraffin which flows down can be reused after being filtered. If rapid dewaxing is desired, hot water or hot oil thawing may be used, with the addition of rust inhibiting additives to the water.
In the process, the workpiece is heated and cooled at a low temperature, so that the thermal deformation influence is not generated on the workpiece, and the dimensional stability of the workpiece is increased. Because the temperature variation range is basically consistent with the technological process of the paraffin fixing method in the actual use process of the chuck. In practice, during high-speed heavy cutting, the friction heat generated by the cutter and the heat generated by the high-speed rotation of the main shaft bearing are conducted to the chuck, so that the working temperature of the chuck is as high as five sixty degrees, and the paraffin process measure at the temperature is adopted, so that the process has a great advantage.
The collet chuck ground by the process overcomes the unavoidable defects of a plurality of traditional methods, increases the rigidity of a workpiece, reduces deformation and reduces the influence caused by grinding heat. Thereby greatly improving the grinding precision and powerfully ensuring the workpiece precision. So that the grinding efficiency is not reduced and the grinding efficiency is not reversely increased, and the economic benefit is considerable.
The technological method and the principle are applicable to all metal elastic collet chucks, and the difference is only in the size of the waxing disc, the pressing disc and the mandrel. The method needs to ensure that the dimensional consistency of the mandrel is good, the cylindricity tolerance is small, the mandrel after heat treatment can be processed in batches by a high-precision cylindrical grinding machine, and in practice, the mandrel is controlled to have cylindricity of 2 microns and roundness of less than 1 micron is not difficult.
The actual effect of the process method is that the grinding yield is improved by 3-5 times, and when each process step is strictly controlled, the yield of more than 90% can be basically achieved. Namely, 9 of 10 collets can be processed into a high-precision collet, and the economic benefit is quite considerable.
The foregoing embodiments are merely illustrative of the preferred embodiments of the present invention, and are not intended to limit the scope of the present invention, and various modifications and improvements made by those skilled in the art to which the present invention pertains should fall within the scope of the invention as defined in the appended claims without departing from the spirit of the invention.

Claims (8)

1. A process for precisely grinding a high-precision spring chuck is characterized by comprising the following steps of: the method comprises the following steps:
S1, selecting a special mandrel;
When the outer edge of the collet chuck is finely ground, the difference between the outer diameter of the mandrel and the diameter of the detection measuring rod is close to zero, so that the size of an inner hole of the collet chuck is completely consistent with that of a grinding mandrel, and the condition that the inner hole wall of the workpiece of the collet chuck and the mandrel do not have any extrusion and deformation is met;
s2, selecting a connecting material;
Wherein the workpiece and the mandrel are temporarily connected by the low-temperature paraffin; wherein deformation grooves uniformly distributed on the surface of the collet chuck base body are utilized, so that enough paraffin is just contained in the grooves;
The paraffin with low melting point is selected, so that the paraffin begins to soften at 50 ℃ and is in a liquid state at about 55 ℃; the paraffin temperature at the temperature cannot cause energy loss due to too high melting point, is easy to construct, and has good safety;
s3, pouring paraffin;
firstly, placing a collet workpiece and a positioning mandrel on a die disc, pressing a pressing disc on the upper part of the collet workpiece and pressing a mesh on the lower part of the pressing disc, wherein the pressing disc is provided with low-melting-point paraffin;
When the temperature of the operating room environment or the special heating box reaches 55-60 ℃, paraffin on the pressure plate is gradually melted into liquid and flows onto the lower die plate, so that the collet and the mandrel are soaked in the paraffin liquid; after a period of time, the batch of workpieces can be cooled, so that paraffin in the die is completely solidified;
S4, precisely grinding;
When fine grinding is carried out, batch processing is adopted, and the grinding mode is basically the same as the traditional process; the grinding quantity is generally controlled to be between 0.01 and 0.03mm, and the grinding time is generally only a short number of seconds;
during grinding, the grinding heat can melt paraffin on the surface of the workpiece; after grinding, paraffin inside the workpiece and around the mandrel still exists firmly; for this purpose, the remaining paraffin can be melted by slow heating; when the temperature is generally heated to above 52 ℃, paraffin naturally flows down; the paraffin which flows down can be recycled after being recovered and filtered.
2. The process for precisely grinding the high-precision collet as defined in claim 1, wherein: and S3, when paraffin is poured, cleaning treatment is carried out on the inner and outer surfaces of the workpiece, so that the influence of greasy dirt and dirty matters on the positioning of the mandrel and the reduction of the connection strength are avoided.
3. The process for precisely grinding the high-precision collet as defined in claim 1, wherein:
In the S1, the surface knurling mode can be adopted in the design of the mandrel, so that the surface roughness is increased, and the connection strength of a workpiece and the mandrel is greatly improved;
Or/and, the surface of the mandrel is covered with pits for containing paraffin, so that the connection strength with the workpiece is improved.
4. The process for precisely grinding the high-precision collet as defined in claim 1, wherein: the central holes at the two ends of the mandrel in the S1 are required to be strictly centered and coaxial, the roundness is less than 1 micron, the cylindricity of the mandrel is not more than 2 microns, and the consistency of the whole batch is required to be less than 3 microns.
5. The process for precisely grinding the high-precision collet as defined in claim 1, wherein: in S3, the paraffin liquid is vibrated by a small margin to promote paraffin to flow into each gap between the collet workpiece and the positioning mandrel.
6. The process for precisely grinding the high-precision collet as defined in claim 1, wherein: in S3, the die plate is provided with a die plate which is matched with the shape of the collet chuck workpiece, so that the dosage of paraffin is saved, the phenomenon that the surface of the workpiece is coated with too thick paraffin to cause unnecessary waste and slowing down of grinding beats is avoided, and in addition, the collet chuck and the mandrel are tightly combined in a proper pressure state, so that the paraffin adapts to the shape of the workpiece through expansion and contraction of the paraffin in the whole cooling process.
7. The process for precisely grinding the high-precision collet as defined in claim 1, wherein: in S4, when fast dewaxing is required, paraffin melting is accelerated by using hot water or hot oil, to which an anti-rust additive is added.
8. The process for precisely grinding the high-precision collet as defined in claim 1, wherein: in S3, the paraffin pouring structure comprises a heating groove (5), a die disc (6) which is arranged on the heating groove (5) and stacked layer by layer, a spring chuck to be injected which is arranged on the die disc (6), a pressure disc (7) which is arranged at the top of the spring chuck to be injected, and a paraffin groove (8) which is positioned at the uppermost layer;
wherein reserved slots which are matched with the outer wall of the spring chuck to be injected with wax are uniformly formed on the die plate (6);
wherein, a reserved slotted hole which is convenient to be right opposite to the spring chuck to be injected is arranged on the pressure plate (7).
CN202410488700.3A 2024-04-23 2024-04-23 A process for precision grinding high-precision spring chuck Pending CN118181001A (en)