CN115851149A - A kind of plate sealing film and PCR hot lid sealing film method - Google Patents
A kind of plate sealing film and PCR hot lid sealing film method Download PDFInfo
- Publication number
- CN115851149A CN115851149A CN202211651732.8A CN202211651732A CN115851149A CN 115851149 A CN115851149 A CN 115851149A CN 202211651732 A CN202211651732 A CN 202211651732A CN 115851149 A CN115851149 A CN 115851149A
- Authority
- CN
- China
- Prior art keywords
- film
- sealing
- pcr
- sealing film
- thermal
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Granted
Abstract
本发明提供一种封板膜及PCR热盖封膜方法。封板膜包括由上向下依次设置的热解失粘胶层、基材层和封板胶层,所述热解失粘胶层的热解失粘温度为80‑95℃,所述封板胶层在20‑105℃仍保持一定的粘合力。在应用在PCR仪上时,只需要先将封板膜贴于热盖上,热盖关闭或加压后即可完成对样本孔板的封膜;由于在PCR扩增过程中,热盖温度已达到热解失粘温度,在PCR完成后,热盖打开后即可与封板膜失粘分离;在PCR检测前,无需先专门对样本孔板进行封膜操作,在PCR仪上同步完成封膜和扩增检测,大大提升了PCR检测效率。
The invention provides a plate sealing film and a PCR hot cover sealing film method. The sealing film includes a pyrolysis adhesive loss layer, a substrate layer and a sealing adhesive layer which are sequentially arranged from top to bottom. The adhesive layer of the board still maintains a certain degree of adhesion at 20‑105 °C. When applied to a PCR instrument, it is only necessary to stick the sealing film on the hot cover first, and the sealing of the sample orifice plate can be completed after the hot cover is closed or pressurized; due to the temperature of the hot cover during the PCR amplification process, It has reached the thermal debonding temperature. After the PCR is completed, the thermal lid can be separated from the sealing film after opening; before the PCR detection, there is no need to specially seal the sample orifice plate, and it is completed synchronously on the PCR instrument. Sealing film and amplification detection greatly improve the efficiency of PCR detection.
Description
技术领域technical field
本发明涉及封膜技术领域,具体是一种封板膜及PCR热盖封膜方法。The invention relates to the technical field of sealing film, in particular to a plate sealing film and a method for sealing the film with a PCR hot lid.
背景技术Background technique
在对生物样本检测过程中,为了防止样本逸散,通常需要采用封板膜对装有样本的试剂管孔口进行密封。封膜仪即是用于封膜的仪器,目前的封膜步骤是先将封板膜虚放在样本孔板上,然后再放入封膜仪内进行封膜。但是在封膜前封板膜在样本孔板上位置不稳定,在移动过程容易与封膜仪发生刮碰或遇到气流影响时,会发生封板膜移位的情形,造成封膜不合格。将不合格封膜撕除重新封膜过程中,又容易造成样本的泼洒,影响实验效率。In the process of detecting biological samples, in order to prevent the samples from escaping, it is usually necessary to use a sealing film to seal the orifices of the reagent tubes containing the samples. The film sealing machine is an instrument used for sealing the film. The current film sealing step is to first place the sealing film on the sample orifice plate, and then put it into the film sealing machine for sealing. However, before sealing the film, the position of the sealing film on the sample orifice plate is not stable. During the moving process, it is easy to scratch against the sealing machine or encounter the influence of air flow, and the sealing film will shift, resulting in unqualified sealing film. . In the process of tearing off the unqualified sealing film and resealing the film, it is easy to cause the sample to be spilled, which affects the efficiency of the experiment.
另外,在常用的PCR(聚合酶链式反应)检测中,通常需要先对样本孔板进行封膜,然后再将封膜后的样本孔板放置到PCR仪内进行扩增检测。对于实验室来说,需要同步配置封膜仪和PCR仪,增加配置成本。先封膜再检测,步骤多,影响PCR检测效率。In addition, in the commonly used PCR (polymerase chain reaction) detection, it is usually necessary to seal the sample orifice first, and then place the sealed sample orifice in a PCR machine for amplification detection. For the laboratory, it is necessary to configure the sealing machine and the PCR machine simultaneously, which increases the configuration cost. First seal the film and then detect, there are many steps, which affects the efficiency of PCR detection.
发明内容Contents of the invention
为了克服上述现有技术的不足,本发明的目的是提供了一种封板膜及PCR热盖封膜方法。In order to overcome the deficiencies of the above-mentioned prior art, the object of the present invention is to provide a sealing film and a method for sealing the film of a PCR hot lid.
为达到上述目的,本发明解决其技术问题所采用的技术方案是:一种封板膜,包括由上向下依次设置的热解失粘胶层、基材层和封板胶层,所述热解失粘胶层的热解失粘温度为80-95℃,所述封板胶层在20-105℃仍保持一定的粘合力。In order to achieve the above-mentioned purpose, the technical solution adopted by the present invention to solve the technical problems is: a sealing film, comprising a thermally decomposed adhesive layer, a base material layer and a sealing adhesive layer arranged sequentially from top to bottom. The thermal detackification temperature of the thermal detackification loss adhesive layer is 80-95°C, and the sealing board adhesive layer still maintains a certain adhesive force at 20-105°C.
采用本发明技术方案,在应用在封膜仪上时,在封膜前,先将封板膜的热解失粘胶层与封膜仪具有加热功能的上盖板贴合;封膜时,上盖板连同封板膜下压在待封膜孔板上表面,封板胶层与待封膜孔板相粘合;在封膜的同时不断提升上盖板的温度,在达到失粘温度后,移开上盖板,上盖板与封板膜脱离,完成对样本孔板的封膜。由于上盖板与孔板放置座的位置定位比较精准,封板膜在上盖板上贴附位置也比较精准,这样封板膜与样本孔板不会发生错位,大大提升了封膜质量。在应用在PCR仪上时,只需要先将封板膜贴于热盖上,热盖关闭或加压后即可完成对样本孔板的封膜;由于在PCR扩增过程中,热盖温度已达到热解失粘温度,在PCR完成后,热盖打开后即可与封板膜失粘分离;在PCR检测前,无需先专门对样本孔板进行封膜操作,在PCR仪上同步完成封膜和扩增检测,大大提升了PCR检测效率。Adopting the technical solution of the present invention, when applied to a film sealing device, before sealing the film, the thermally decomposed viscose layer of the sealing film is first bonded to the upper cover plate of the film sealing device with heating function; when sealing the film, The upper cover plate and the sealing film are pressed down on the surface of the orifice plate to be sealed, and the adhesive layer of the sealing plate is bonded to the orifice plate to be sealed; while sealing the film, the temperature of the upper cover plate is continuously raised, and when it reaches the loss of viscosity temperature Finally, the upper cover is removed, and the upper cover is separated from the sealing film to complete the sealing of the sample orifice plate. Since the position of the upper cover plate and the orifice plate placement seat is relatively accurate, the position of the sealing film on the upper cover plate is also relatively accurate, so that the sealing film and the sample orifice plate will not be misaligned, which greatly improves the quality of the sealing film. When applied to a PCR instrument, it is only necessary to stick the sealing film on the hot cover first, and the sealing of the sample orifice plate can be completed after the hot cover is closed or pressurized; due to the temperature of the hot cover during the PCR amplification process, It has reached the thermal debonding temperature. After the PCR is completed, the thermal lid can be separated from the sealing film after opening the thermal cover; before the PCR detection, there is no need to specially seal the sample orifice plate, and it can be completed synchronously on the PCR instrument Sealing film and amplification detection greatly improve the efficiency of PCR detection.
进一步地,还包括覆盖于所述热解失粘胶层上表面的上离型膜,以及覆盖于所述封板胶层下表面的下离型膜。Further, it also includes an upper release film covering the upper surface of the thermally decomposed adhesive layer, and a lower release film covering the lower surface of the sealing plate adhesive layer.
采用上述优选的方案,通过上、下离型膜对热解失粘胶层和封板胶层进行保护,方便周转。By adopting the above-mentioned preferred scheme, the pyrolysis-lost adhesive layer and the sealing plate adhesive layer are protected by the upper and lower release films, which is convenient for turnover.
进一步地,所述上离型膜和下离型膜的颜色不同。Further, the colors of the upper release film and the lower release film are different.
进一步地,所述上离型膜和下离型膜上设有用于区分封板膜上表面和下表面的标记。Further, the upper release film and the lower release film are provided with marks for distinguishing the upper surface and the lower surface of the sealing film.
采用上述优选的方案,方便区分封板膜的上下表面,防止反向误用。By adopting the above-mentioned preferred scheme, it is convenient to distinguish the upper and lower surfaces of the sealing film and prevent reverse misuse.
进一步地,所述热解失粘胶层的热解失粘温度为90℃。Further, the thermal detackification loss temperature of the thermal detackification loss layer is 90°C.
采用上述优选的方案,更适用于PCR仪热盖封膜使用。Adopting the above-mentioned preferred scheme is more suitable for thermal lid sealing film of PCR instrument.
进一步地,所述热解失粘胶层由多个相互隔离的热解失粘胶小单元构成。Further, the pyrolysis viscose-losing layer is composed of a plurality of pyrolysis viscose-losing small units isolated from each other.
进一步地,所述热解失粘胶小单元成点状、圆形或方形。Further, the pyrolysis-losing viscose small units are in the shape of dots, circles or squares.
采用上述优选的方案,方便在贴膜时,进行排气,提高封板膜在热盖上贴附平整度。Adopting the above-mentioned preferred scheme is convenient for venting when the film is pasted, and improves the flatness of the sealing film on the heat cover.
一种PCR热盖封膜方法,基于PCR仪,PCR仪包括热盖组件以及位于热盖组件下方的孔板加热座组件,热盖组件包括热盖、制热元件和加压机构,包括如下步骤:A PCR hot lid sealing method, based on a PCR machine, the PCR machine includes a hot lid assembly and an orifice heating seat assembly located below the hot lid assembly, the hot lid assembly includes a hot lid, a heating element and a pressurization mechanism, including the following steps :
A1,将封板膜贴付到PCR仪热盖下表面,贴膜方向为:封板膜的热解失粘胶层上表面与热盖下表面贴靠;A1. Paste the sealing film on the lower surface of the hot cover of the PCR instrument. The film sticking direction is: the upper surface of the thermally decomposed adhesive layer of the sealing film is attached to the lower surface of the hot cover;
A2,将未封膜的样本孔板放置到PCR仪孔板加热座组件上进样;A2, place the unsealed sample well plate on the well plate heating seat assembly of the PCR instrument for sample injection;
A3,关闭PCR仪热盖组件,进行PCR扩增检测;A3, close the thermal lid assembly of the PCR instrument, and perform PCR amplification detection;
A4,PCR检测完成后,热盖组件打开,退出检测样本孔板。A4, after the PCR detection is completed, the heat cover assembly is opened, and the detection sample orifice plate is withdrawn.
采用上述方案,由于在PCR扩增过程中,热盖温度已达到热解失粘温度,在PCR完成后,热盖打开后即可与封板膜失粘分离;在PCR检测前,无需先专门对样本孔板进行封膜操作,在PCR仪上同步完成封膜和扩增检测,大大提升了PCR检测效率。Using the above scheme, since the temperature of the hot cover has reached the thermal detackification temperature during the PCR amplification process, after the PCR is completed, the hot cover can be separated from the sealing film after opening; before the PCR detection, there is no need to specialize The film sealing operation is performed on the sample well plate, and the film sealing and amplification detection are simultaneously completed on the PCR instrument, which greatly improves the efficiency of PCR detection.
一种PCR热盖封膜方法,基于PCR仪,PCR仪包括热盖组件以及位于热盖组件下方的孔板加热座组件,热盖组件包括热盖、制热元件和加压机构,热盖包括热盖主体和贴膜中继板,贴膜中继板可拆卸地安装于热盖主体,包括如下步骤:A PCR hot lid sealing method, based on a PCR machine, the PCR machine includes a hot lid assembly and an orifice heating seat assembly located below the hot lid assembly, the hot lid assembly includes a hot lid, a heating element and a pressurization mechanism, and the hot lid includes The heat cover main body and the film relay board, the film film relay board is detachably installed on the heat cover main body, including the following steps:
B1,将封板膜贴付到贴膜中继板下表面,贴膜方向为:封板膜的热解失粘胶层上表面与贴膜中继板下表面贴靠;B1. Paste the sealing film on the lower surface of the film-attached relay board. The direction of the film is: the upper surface of the thermally decomposed adhesive layer of the sealing film is attached to the lower surface of the film-attached relay board;
B2,将贴有封板膜的贴膜中继板安装到热盖主体上;B2, install the film relay board with the sealing film on the main body of the heat cover;
B3,将未封膜的样本孔板放置到PCR仪孔板加热座组件上进样;B3, place the unsealed sample orifice plate on the heating seat assembly of the PCR instrument orifice plate for sample injection;
B4,关闭或加压PCR仪热盖组件,进行PCR扩增检测;B4, close or pressurize the thermal lid assembly of the PCR instrument, and perform PCR amplification detection;
B5,PCR检测完成后,热盖组件打开或解压,退出检测样本孔板;B5, after the PCR test is completed, the hot cover assembly is opened or decompressed, and the test sample orifice plate is withdrawn;
B6,抽出贴膜中继板冷却待循环利用。B6, pull out the film relay board to cool down and wait for recycling.
采用上述优选的方案,通过与热盖主体分体设置的贴膜中继板来定位附着封板膜,提高了贴膜便利性,也方便循环周转。Using the above-mentioned preferred solution, the sealing film is positioned and attached through the film-attaching relay plate provided separately from the main body of the heat cover, which improves the convenience of film-attaching and facilitates the circulation.
进一步地,所述贴膜中继板的下表面设有用于贴附封板膜的基准。Further, the lower surface of the film sticking relay board is provided with a datum for pasting the sealing film.
采用上述优选的方案,方便贴膜对齐,提高封膜位置精度。Adopting the above preferred scheme facilitates the alignment of the film and improves the accuracy of the position of the film.
附图说明Description of drawings
为了更清楚地说明本发明实施例或现有技术中的技术方案,下面将对实施例或现有技术描述中所需要使用的附图作简单地介绍,显而易见地,下面描述中的附图仅仅是本发明的一些实施例,对于本领域普通技术人员来讲,在不付出创造性劳动的前提下,还可以根据这些附图获得其他的附图。In order to more clearly illustrate the technical solutions in the embodiments of the present invention or the prior art, the following will briefly introduce the drawings that need to be used in the description of the embodiments or the prior art. Obviously, the accompanying drawings in the following description are only These are some embodiments of the present invention. Those skilled in the art can also obtain other drawings based on these drawings without creative work.
图1是本发明封板膜一种实施方式的截面图;Fig. 1 is a cross-sectional view of an embodiment of the sealing film of the present invention;
图2是本发明封板膜另一种实施方式的截面图;Fig. 2 is a cross-sectional view of another embodiment of the sealing film of the present invention;
图3是本发明封板膜另一种实施方式的俯视图;Fig. 3 is a top view of another embodiment of the sealing film of the present invention;
图4是封板膜一种贴附方式在热盖底面的位置示意图;Fig. 4 is a schematic diagram of the position of the sealing film on the bottom surface of the heat cover in one way of attachment;
图5是封板膜一种贴附方式在PCR仪上的位置示意图;Fig. 5 is a schematic diagram of the position of an attachment method of the sealing film on the PCR instrument;
图6是封板膜另一种贴附方式在热盖贴膜中继板底面的位置示意图;Figure 6 is a schematic diagram of the position of another attachment method of the sealing film on the bottom surface of the heat cover film relay board;
图7是封板膜另一种贴附方式在PCR仪上的位置示意图。Fig. 7 is a schematic diagram of the position of another way of attaching the plate sealing film on the PCR instrument.
图中数字和字母所表示的相应部件的名称:Names of corresponding parts indicated by numbers and letters in the figure:
10-封板膜;11-热解失粘胶层;111-热解失粘胶小单元;12-基材层;13-封板胶层;14-上离型膜;15-下离型膜;21-热盖;211-热盖主体;212-贴膜中继板;2121-基准;22-制热元件;23-加压机构;24-孔板加热座组件;31-孔板。10-sealing film; 11-pyrolysis adhesive loss layer; 111-pyrolysis adhesive loss small unit; 12-substrate layer; 13-sealing adhesive layer; 14-upper release film; 15-lower release type Membrane; 21-heat cover; 211-heat cover body; 212-film relay plate; 2121-baseline; 22-heating element; 23-pressurizing mechanism;
具体实施方式Detailed ways
下面将结合本发明实施例中的附图,对本发明实施例中的技术方案进行清楚、完整地描述,显然,所描述的实施例仅仅是本发明一部分实施例,而不是全部的实施例。基于本发明中的实施例,本领域普通技术人员在没有作出创造性劳动前提下所获得的所有其他实施例,都属于本发明保护的范围。The following will clearly and completely describe the technical solutions in the embodiments of the present invention with reference to the accompanying drawings in the embodiments of the present invention. Obviously, the described embodiments are only some, not all, embodiments of the present invention. Based on the embodiments of the present invention, all other embodiments obtained by persons of ordinary skill in the art without creative efforts fall within the protection scope of the present invention.
如图1所示,一种封板膜,包括由上向下依次设置的热解失粘胶层11、基材层12和封板胶层13,热解失粘胶层11的热解失粘温度为80-95℃,13封板胶层至少在20-105℃温度区间仍保持一定的粘合力。As shown in Figure 1, a kind of board sealing film comprises the pyrolysis
采用上述技术方案的有益效果是:在应用在封膜仪上时,在封膜前,先将封板膜的热解失粘胶层与封膜仪具有加热功能的上盖板贴合;封膜时,上盖板连同封板膜下压在待封膜孔板上表面,封板胶层与待封膜孔板相粘合;在封膜的同时不断提升上盖板的温度,在达到失粘温度后,移开上盖板,上盖板与封板膜脱离,完成对样本孔板的封膜。由于上盖板与孔板放置座的位置定位比较精准,封板膜在上盖板上贴附位置也比较精准,这样封板膜与样本孔板不会发生错位,大大提升了封膜质量。在应用在PCR仪上时,如图5所示,只需要先将封板膜10贴于热盖21上,热盖关闭或加压后即可完成对样本孔板的封膜;由于在PCR扩增过程中,热盖温度已达到热解失粘温度,在PCR完成后,热盖打开后即可与封板膜失粘分离;在PCR检测前,无需先专门对样本孔板进行封膜操作,在PCR仪上同步完成封膜和扩增检测,大大提升了PCR检测效率。The beneficial effect of adopting the above-mentioned technical solution is: when applied to a film sealing device, before sealing the film, the thermally decomposed viscose layer of the sealing film is first bonded to the upper cover plate of the sealing device with heating function; When filming, the upper cover plate and the sealing plate film are pressed down on the surface of the orifice plate to be sealed, and the sealing plate adhesive layer is bonded to the orifice plate to be sealed; while sealing the film, the temperature of the upper cover plate is continuously raised, and when it reaches After the viscosity loss temperature, remove the upper cover plate, the upper cover plate is separated from the sealing film, and the sealing film of the sample orifice plate is completed. Since the position of the upper cover plate and the orifice plate placement seat is relatively accurate, the position of the sealing film on the upper cover plate is also relatively accurate, so that the sealing film and the sample orifice plate will not be misaligned, which greatly improves the quality of the sealing film. When applied to a PCR instrument, as shown in Figure 5, it is only necessary to stick the
在本发明中,热解失粘胶层11的具体材质可从现有技术中获取,如采用昆山权富莱电子有限公司销售的高温热解失粘膜。另外可供选择的,在申请公布号为CN 105131860A的专利文献中也公开了一种热解失粘胶带,其中记载了一种热解失粘胶层及其原理,热解失粘胶层内预埋有加热可膨胀发泡的可膨胀微球发泡剂,可膨胀微球发泡剂是一种核壳结构,外壳为热塑性丙烯酸树脂类聚合物,内核为烷烃类气体组成的微球颗粒,颗粒的直径为10-45微米,微球发泡的温度范围为75℃-260℃,可根据各种不同加工温度和工艺要求,选择最合适的微球型号。In the present invention, the specific material of the
在本发明中,基材层12具体材质不作限定,可从现有技术中选择,如PET或其他高强度基材。In the present invention, the specific material of the
在本发明中,封板胶层13在常温和高温下均保持一定的粘合力,其具体材质不作限定,可从现有技术中选择,如丙烯酸粘合胶或其他具有粘合力的胶层。In the present invention, the
如图2所示,在本发明的另一些实施方式中,还包括覆盖于热解失粘胶层11上表面的上离型膜14,以及覆盖于封板胶层13下表面的下离型膜15。采用上述技术方案的有益效果是:通过上、下离型膜对热解失粘胶层和封板胶层进行保护,方便周转。As shown in Figure 2, in other embodiments of the present invention, it also includes an
在本发明的另一些实施方式中,为了区分热解失粘胶层和封板胶层所在面,上离型膜14和下离型膜15的颜色不同。In some other embodiments of the present invention, in order to distinguish the surface where the thermally decomposed adhesive layer and the sealing adhesive layer are located, the colors of the
在本发明的另一些实施方式中,上离型膜14和下离型膜15上设有用于区分封板膜上表面和下表面的标记。In other embodiments of the present invention, the
在本发明的另一些实施方式中,热解失粘胶层11的热解失粘温度为90℃,更适用于PCR仪热盖封膜使用。In some other embodiments of the present invention, the thermal detackification temperature of the thermal detackification loss
如图3所示,在本发明的另一些实施方式中,热解失粘胶层11由多个相互隔离的热解失粘胶小单元111构成。热解失粘胶小单元111的形状可以成点状、圆形、方形等。采用上述技术方案的有益效果是:方便在贴膜时,进行排气,提高封板膜在热盖上贴附平整度。As shown in FIG. 3 , in other embodiments of the present invention, the pyrolysis
如图4、5所示,一种PCR热盖封膜方法,包括热盖21、制热元件22和封板膜10,制热元件22安装在热盖21上表面或嵌设于热盖21内,封板膜的热解失粘胶层11上表面贴设于热盖21的下表面。As shown in Figures 4 and 5, a PCR thermal cover sealing method includes a
如图5所示,本发明封板膜能够应用在现有的PCR仪上,PCR仪具体的结构不再赘述,可从现有技术中获取。一般地,PCR仪都包括热盖组件以及位于热盖组件下方的孔板加热座组件24,热盖组件包括热盖21、制热元件22和加压机构23。As shown in FIG. 5 , the plate sealing film of the present invention can be applied to an existing PCR instrument, and the specific structure of the PCR instrument will not be described in detail, and can be obtained from the prior art. Generally, a PCR instrument includes a heating cover assembly and an orifice
PCR热盖封膜方法,基于PCR仪,包括如下步骤:The PCR hot lid sealing method, based on a PCR instrument, comprises the following steps:
A1,将封板膜贴付到PCR仪热盖下表面,贴膜方向为:封板膜的热解失粘胶层上表面与热盖下表面贴靠;A1. Paste the sealing film on the lower surface of the hot cover of the PCR instrument. The film sticking direction is: the upper surface of the thermally decomposed adhesive layer of the sealing film is attached to the lower surface of the hot cover;
A2,将未封膜的样本孔板放置到PCR仪孔板加热座组件上进样;A2, place the unsealed sample well plate on the well plate heating seat assembly of the PCR instrument for sample injection;
A3,关闭PCR仪热盖组件,进行PCR扩增检测;A3, close the thermal lid assembly of the PCR instrument, and perform PCR amplification detection;
A4,PCR检测完成后,热盖组件打开,退出检测样本孔板。A4, after the PCR detection is completed, the heat cover assembly is opened, and the detection sample orifice plate is withdrawn.
由于在PCR扩增过程中,热盖21温度已达到热解失粘温度,在PCR完成后,热盖21打开后即可与封板膜10失粘分离;在PCR检测前,无需先专门对样本孔板进行封膜操作,在PCR仪上同步完成封膜和扩增检测,大大提升了PCR检测效率。Because in the PCR amplification process, the temperature of the
如图6、7所示,在本发明的另一些实施方式中,PCR仪都包括热盖组件以及位于热盖组件下方的孔板加热座组件24,热盖组件包括热盖21、制热元件22和加压机构23,热盖21包括热盖主体211和贴膜中继板212,贴膜中继板212可拆卸地安装于热盖主体211。As shown in Figures 6 and 7, in other embodiments of the present invention, the PCR instrument includes a thermal cover assembly and an orifice
PCR热盖封膜方法,基于上述PCR仪,包括如下步骤:The PCR hot lid sealing method, based on the above-mentioned PCR instrument, comprises the following steps:
B1,将封板膜贴付到贴膜中继板下表面,贴膜方向为:封板膜的热解失粘胶层上表面与贴膜中继板下表面贴靠;B1. Paste the sealing film on the lower surface of the film-attached relay board. The direction of the film is: the upper surface of the thermally decomposed adhesive layer of the sealing film is attached to the lower surface of the film-attached relay board;
B2,将贴有封板膜的贴膜中继板安装到热盖主体上;B2, install the film relay board with the sealing film on the main body of the heat cover;
B3,将未封膜的样本孔板放置到PCR仪孔板加热座组件上进样;B3, place the unsealed sample orifice plate on the heating seat assembly of the PCR instrument orifice plate for sample injection;
B4,关闭或加压PCR仪热盖组件,进行PCR扩增检测;B4, close or pressurize the thermal lid assembly of the PCR instrument, and perform PCR amplification detection;
B5,PCR检测完成后,热盖组件打开或解压,退出检测样本孔板;B5, after the PCR test is completed, the hot cover assembly is opened or decompressed, and the test sample orifice plate is withdrawn;
B6,抽出贴膜中继板冷却待循环利用。B6, pull out the film relay board to cool down and wait for recycling.
先将封板膜与贴膜中继板贴付,然后再一起插配到热盖主体上,提高了贴膜便利性,也方便循环周转。The sealing film and the film relay board are pasted first, and then they are mated together on the main body of the heat cover, which improves the convenience of film sticking and facilitates cycle turnover.
如图6所示,在本发明的另一些实施方式中,贴膜中继板212的下表面设有用于贴附封板膜10的基准2121。采用上述技术方案的有益效果是:方便贴膜对齐,提高封膜位置精度。As shown in FIG. 6 , in other embodiments of the present invention, the lower surface of the film-attaching
上述实施例只为说明本发明的技术构思及特点,其目的在于让本领域普通技术人员能够了解本发明的内容并加以实施,并不能以此限制本发明的保护范围,凡根据本发明精神实质所作的等效变化或修饰,都应涵盖在本发明的保护范围内。The above-described embodiments are only to illustrate the technical concept and characteristics of the present invention, and its purpose is to allow those of ordinary skill in the art to understand the content of the present invention and implement it, and cannot limit the protection scope of the present invention with this. All equivalent changes or modifications should fall within the protection scope of the present invention.
Claims (10)