CN114346116A - 钢筋的矫正方法 - Google Patents
钢筋的矫正方法 Download PDFInfo
- Publication number
- CN114346116A CN114346116A CN202011090244.5A CN202011090244A CN114346116A CN 114346116 A CN114346116 A CN 114346116A CN 202011090244 A CN202011090244 A CN 202011090244A CN 114346116 A CN114346116 A CN 114346116A
- Authority
- CN
- China
- Prior art keywords
- steel bar
- steel
- hammer
- straightening
- workbench
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Withdrawn
Abstract
本发明公开一种钢筋的矫正方法,直径在12毫米以上的粗钢筋,采用人工调直。其操作程序是:先将钢筋弯折处放到扳柱铁板的扳柱间,用平头横口扳子将弯折处基本扳直,然后放到工作台上,用大锤将钢筋小弯处锤平,操作时需要两人配合好,一人掌握钢筋,站在工作台一端,将钢筋反复转动和来回移动,另一人掌握大锤,站在工作台的侧面,见弯就锤,掌锤者应根据钢筋粗细和弯度大小来掌握落锤轻重,握钢筋者应视钢筋在工作台上可以滚动时则认为调直合格。与相关技术相比,本发明的钢筋的矫正方法矫正效果更好。
Description
技术领域
本发明涉及钢筋加工技术领域,尤其涉及一种钢筋的矫正方法。
背景技术
在大量的建筑施工中,会使用大量的钢筋,钢筋在投入使用之前,通常会在长度方向存在弯曲变形,因此,钢筋使用之前需要对弯曲变形的钢筋进行矫正,调整其直线度。
目前对钢筋进行矫正有人工矫正和机器矫正两种方式,人工矫正成本低,但效率不高;机器矫正效率高,但成本较高。
因此,实有必要提供一种新的钢筋的矫正方法解决上述技术问题。
发明内容
本发明的目的是克服上述技术问题,提供一种矫正效果好的钢筋的矫正方法。
本发明提供一种钢筋的矫正方法,所述矫正方法包括:
直径在12毫米以上的粗钢筋,采用人工调直。其操作程序是:先将钢筋弯折处放到扳柱铁板的扳柱间,用平头横口扳子将弯折处基本扳直,然后放到工作台上,用大锤将钢筋小弯处锤平,操作时需要两人配合好,一人掌握钢筋,站在工作台一端,将钢筋反复转动和来回移动,另一人掌握大锤,站在工作台的侧面,见弯就锤,掌锤者应根据钢筋粗细和弯度大小来掌握落锤轻重,握钢筋者应视钢筋在工作台上可以滚动时则认为调直合格。
优选的,所述方法还包括:
直径在12毫米以下的盘圆钢筋为细钢筋,细钢筋主要采用机械调直,但在工程量小或无冷拉设备的情况下,也可采用人工调直,人工调直又分小锤敲直和绞磨拉直两种,不管哪一种都需要先放盘,前者是按需要长度截成小段在工作台上用小锤平直,后者是按一定长度截断,分别将两端夹在地锚和绞磨的夹具上,然后人工推动绞磨将钢筋拉直,这种方法简单可行,但只宜拉直I级钢筋中的Φ6盘圆,且劳动强度较大,目前已不常使用。
优选的,所述方法还包括:
冷拔低碳钢丝一般采用机械调直。但在设备困难的情况下,也可以采用蛇形管人工调直。
优选的,蛇形管是用长一米左右的厚壁钢管弯成蛇形,钢管内径稍大于钢丝,管两端连接喇叭状进出口,固定在支架上,需要调直的钢丝穿过固定的蛇形管,用人力牵引,即可将钢丝基本拉直,钢丝若有局部小弯再用小锤敲直。
与现有技术相比,本发明提供的钢筋的矫正方法矫正效果更好。
具体实施方式
下面将对本发明实施例中的技术方案进行清楚、完整地描述,显然,所描述的实施例仅是本发明的一部分实施例,而不是全部的实施例。基于本发明中的实施例,本领域普通技术人员在没有做出创造性劳动前提下所获得的所有其它实施例,都属于本发明保护的范围。
筑用热轧钢筋分盘圆和直条两类。直径在12毫米以下的钢筋一般制成盘圆,以便于运输。盘圆钢筋在下料前,一般要经过放盘、冷拉工序,以达到调直的目的。直径在12毫米以上的钢筋,一般轧制成6—12米长的直条。由于在运输过程中,几经装卸,会使直条钢筋造成局部弯折。
本发明提供一种钢筋的矫正方法,所述矫正方法包括:
直径在12毫米以上的粗钢筋,采用人工调直。其操作程序是:先将钢筋弯折处放到扳柱铁板的扳柱间,用平头横口扳子将弯折处基本扳直,然后放到工作台上,用大锤将钢筋小弯处锤平,操作时需要两人配合好,一人掌握钢筋,站在工作台一端,将钢筋反复转动和来回移动,另一人掌握大锤,站在工作台的侧面,见弯就锤,掌锤者应根据钢筋粗细和弯度大小来掌握落锤轻重,握钢筋者应视钢筋在工作台上可以滚动时则认为调直合格。
优选的,所述方法还包括:
直径在12毫米以下的盘圆钢筋为细钢筋,细钢筋主要采用机械调直,但在工程量小或无冷拉设备的情况下,也可采用人工调直,人工调直又分小锤敲直和绞磨拉直两种,不管哪一种都需要先放盘,前者是按需要长度截成小段在工作台上用小锤平直,后者是按一定长度截断,分别将两端夹在地锚和绞磨的夹具上,然后人工推动绞磨将钢筋拉直,这种方法简单可行,但只宜拉直I级钢筋中的Φ6盘圆,且劳动强度较大,目前已不常使用。
优选的,所述方法还包括:
冷拔低碳钢丝一般采用机械调直。但在设备困难的情况下,也可以采用蛇形管人工调直。
优选的,蛇形管是用长一米左右的厚壁钢管弯成蛇形,钢管内径稍大于钢丝,管两端连接喇叭状进出口,固定在支架上,需要调直的钢丝穿过固定的蛇形管,用人力牵引,即可将钢丝基本拉直,钢丝若有局部小弯再用小锤敲直。
与现有技术相比,本发明提供的钢筋的矫正方法矫正效果更好。
以上所述仅为本发明的实施例,并非因此限制本发明的专利范围,凡是利用本发明说明书内容所作的等效结构或等效流程变换,或直接或间接运用在其它相关的技术领域,均同理包括在本发明的专利保护范围内。
Claims (4)
1.一种钢筋的矫正方法,其特征在于,所述矫正方法包括:
直径在12毫米以上的粗钢筋,采用人工调直。其操作程序是:先将钢筋弯折处放到扳柱铁板的扳柱间,用平头横口扳子将弯折处基本扳直,然后放到工作台上,用大锤将钢筋小弯处锤平,操作时需要两人配合好,一人掌握钢筋,站在工作台一端,将钢筋反复转动和来回移动,另一人掌握大锤,站在工作台的侧面,见弯就锤,掌锤者应根据钢筋粗细和弯度大小来掌握落锤轻重,握钢筋者应视钢筋在工作台上可以滚动时则认为调直合格。
2.根据权利要求1所述的钢筋的矫正方法,其特征在于,所述方法还包括:
直径在12毫米以下的盘圆钢筋为细钢筋,细钢筋主要采用机械调直,但在工程量小或无冷拉设备的情况下,也可采用人工调直,人工调直又分小锤敲直和绞磨拉直两种,不管哪一种都需要先放盘,前者是按需要长度截成小段在工作台上用小锤平直,后者是按一定长度截断,分别将两端夹在地锚和绞磨的夹具上,然后人工推动绞磨将钢筋拉直,这种方法简单可行,但只宜拉直I级钢筋中的Φ6盘圆,且劳动强度较大,目前已不常使用。
3.根据权利要求1所述的钢筋的矫正方法,其特征在于,所述方法还包括:
冷拔低碳钢丝一般采用机械调直。但在设备困难的情况下,也可以采用蛇形管人工调直。
4.根据权利要求3所述的钢筋的矫正方法,其特征在于,蛇形管是用长一米左右的厚壁钢管弯成蛇形,钢管内径稍大于钢丝,管两端连接喇叭状进出口,固定在支架上,需要调直的钢丝穿过固定的蛇形管,用人力牵引,即可将钢丝基本拉直,钢丝若有局部小弯再用小锤敲直。