CN113698872A - Water-based environment-friendly automobile paint repair wax and preparation method thereof - Google Patents
Water-based environment-friendly automobile paint repair wax and preparation method thereof Download PDFInfo
- Publication number
- CN113698872A CN113698872A CN202110996158.9A CN202110996158A CN113698872A CN 113698872 A CN113698872 A CN 113698872A CN 202110996158 A CN202110996158 A CN 202110996158A CN 113698872 A CN113698872 A CN 113698872A
- Authority
- CN
- China
- Prior art keywords
- parts
- wax
- automobile paint
- friendly
- minutes
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Pending
Abstract
The invention belongs to the technical field of automobile repair wax, and particularly relates to aqueous environment-friendly automobile paint repair wax and a preparation method thereof.
Description
Technical Field
The invention belongs to the technical field of automobile repair wax, and particularly relates to water-based environment-friendly automobile paint repair wax and a preparation method thereof.
Background
With the increasing economic prosperity of the country, the holding capacity of the automobile is increased, and the automobile paint is stained in the long-time driving process, so that the automobile paint is dull.
Most car owners protect the car paint method is to wash and wax the car paint, and the waxing can bring the effects of decontamination, polishing and protection to the car paint surface, thereby avoiding that stains are difficult to remove after the car paint exists for a long time and the flatness of the car paint is finally influenced.
The existing car wax mainly comprises wax, silicone oil and a solvent, and the solvent of the car wax with the formula is volatile in the construction process, so that the environment of the ambient air is easily polluted, and the problems of discomfort caused by the fact that the volatile gas of the car wax is inhaled for a long time and the like are easily caused.
Disclosure of Invention
In order to make up for the defects of the prior art and solve the problems that the solvent of the vehicle wax is easy to volatilize in the construction process, the surrounding air environment is easy to be polluted, and the body is easy to be uncomfortable due to the fact that the volatilized gas of the vehicle wax is inhaled for a long time.
The technical scheme adopted by the invention for solving the technical problems is as follows: the water-based environment-friendly automobile paint repair wax comprises the following raw materials in parts by weight:
5-20 parts of an environment-friendly aliphatic hydrocarbon solvent;
1-10 parts of acid montan wax;
1-10 parts of dimethyl silicone oil;
1-5 parts of a surfactant;
1-5 parts of polyhydric alcohol;
5-20 parts of polishing powder;
1-5 parts of a thickening agent;
0.1-1 part of preservative;
0.01-0.1 part of pigment;
30-70 parts of deionized water.
Preferably, the environment-friendly aliphatic hydrocarbon solvent is at least one of odorless kerosene D40, odorless kerosene D60 and isoparaffin solvent L.
Preferably, the acid montan wax is one or a mixture of two of a craine S wax, an LP wax, and an OP wax; the dimethyl silicone oil is one or a mixture of 100cs, 350cs, 1000cs and 12500cs of Dow Corning PMX-200 silicone oil.
Preferably, the surfactant is one of GP200, A165, a Tween/span composite emulsification system and an oleic acid/morpholine composite emulsification system.
Preferably, the polyalcohol is one of ethylene glycol, propylene glycol and glycerol; the polishing powder is one of kaolin, diatomite and quartz sand.
Preferably, the thickener is one of inorganic or organic thickener; the preservative is one of sodium benzoate, potassium sorbate and KF-88; the pigment is at least one of water-soluble yellow powder and water-soluble red powder.
A preparation method of water-based environment-friendly automobile paint repair wax comprises the following steps:
s1: preparing a preparation raw material of the repair wax according to the mass part;
s2: putting an aliphatic hydrocarbon solvent, acid montan wax and dimethyl silicone oil into an oil pan according to the mass parts, heating to 80-95 ℃ under the condition of continuous stirring, and keeping the temperature for 5-30 minutes when the materials are completely dissolved to be transparent liquid;
s3: adding deionized water, a surfactant, polyhydric alcohol and polishing powder into an emulsifying pot according to the mass parts, heating to 70-90 ℃ while stirring, and keeping the temperature for 5-30 minutes;
s4: starting high-speed stirring equipment of the emulsifying pot, pumping the materials in the oil pot into the emulsifying pot for 2-10 minutes, reacting for 10-60 minutes at 60-90 ℃, and then cooling to 60-80 ℃;
s5: adding materials such as thickening agent, preservative, pigment and the like, continuously stirring at high speed for 2-10 minutes, and obtaining a finished product after the inspection is qualified.
Preferably, in S1, the preparation raw materials for preparing the repair wax include, by mass, an environmentally friendly aliphatic hydrocarbon solvent, an acidic montan wax, dimethyl silicone oil, a surfactant, a polyol, a polishing powder, a thickener, an antiseptic, a pigment, and deionized water.
The invention has the technical effects and advantages that:
1. the invention provides an aqueous environment-friendly automobile paint repair wax and a preparation method thereof, the aqueous environment-friendly automobile paint repair wax with low solvent content is prepared by utilizing an environment-friendly aliphatic hydrocarbon solvent, acid montan wax, dimethyl silicone oil, a surfactant, polyhydric alcohol, polishing powder, a thickening agent, a preservative, a pigment and deionized water, the wax not only has the effects of decontamination, polishing and protection of the traditional automobile wax, but also has the effects of removing scratches and filling the paint, the comprehensive performance of the automobile wax is further expanded, and the low-solvent content automobile wax reduces the volatilization of the solvent during use, is beneficial to reducing the pollution to the air and has the effect of environmental protection.
Drawings
The invention will be further explained with reference to the drawings.
FIG. 1 is a flow chart of the preparation method of the present invention.
Detailed Description
In order to make the technical means, the creation characteristics, the achievement purposes and the effects of the invention easy to understand, the invention is further described with the specific embodiments.
The invention relates to a water-based environment-friendly automobile paint repair wax, which comprises the following raw materials in parts by weight:
5-20 parts of an environment-friendly aliphatic hydrocarbon solvent;
1-10 parts of acid montan wax;
1-10 parts of dimethyl silicone oil;
1-5 parts of a surfactant;
1-5 parts of polyhydric alcohol;
5-20 parts of polishing powder;
1-5 parts of a thickening agent;
0.1-1 part of preservative;
0.01-0.1 part of pigment;
30-70 parts of deionized water.
In one embodiment of the present invention, the environmentally friendly aliphatic hydrocarbon solvent is at least one of odorless kerosene D40, odorless kerosene D60, and isoparaffin solvent L.
As an embodiment of the invention, the acid montan wax is one of a Craine S wax, an LP wax, an OP wax, or a mixture of the two; the dimethyl silicone oil is one or a mixture of 100cs, 350cs, 1000cs and 12500cs of Dow Corning PMX-200 silicone oil.
As an embodiment of the present invention, the surfactant is one of GP200, a165, tween/span complex emulsion system, and oleic acid/morpholine complex emulsion system.
In one embodiment of the present invention, the polyhydric alcohol is one of ethylene glycol, propylene glycol and glycerol; the polishing powder is one of kaolin, diatomite and quartz sand.
As an embodiment of the present invention, the thickener is one of an inorganic or organic thickener; the preservative is one of sodium benzoate, potassium sorbate and KF-88; the pigment is at least one of water-soluble yellow powder and water-soluble red powder.
The first embodiment is as follows:
as shown in fig. 1, a preparation method of an aqueous environment-friendly automobile paint repair wax comprises the following steps:
s1: preparing a preparation raw material of the repair wax according to the mass part;
s2: putting 20 parts of aliphatic hydrocarbon solvent, 5 parts of acid montan wax and 5 parts of dimethyl silicone oil into an oil pan, heating to 85 ℃ under the condition of continuous stirring, and keeping the temperature for 10 minutes when the materials are completely dissolved to be transparent liquid;
s3: adding 49.9 parts of deionized water, 2 parts of surfactant, 5 parts of polyol and 10 parts of polishing powder into an emulsifying pot in parts by mass, heating to 75 ℃ while stirring, and keeping the temperature for 5 minutes;
s4: starting high-speed stirring equipment of the emulsifying pot, pumping the materials in the oil pot into the emulsifying pot within 5 minutes, reacting for 30 minutes at 80 ℃, and then cooling to 70 ℃;
s5: adding materials such as 2 parts of thickening agent, 1 part of preservative, 0.1 part of pigment and the like, continuously stirring at a high speed for 5 minutes, and obtaining a finished product after the inspection is qualified.
In an embodiment of the present invention, in S1, raw materials for preparing the repair wax include, in parts by mass, an environmentally friendly aliphatic hydrocarbon solvent, an acidic montan wax, dimethicone, a surfactant, a polyol, a polishing powder, a thickener, an antiseptic, a pigment, and deionized water.
Example two:
as shown in fig. 1, a preparation method of an aqueous environment-friendly automobile paint repair wax comprises the following steps:
s1: preparing a preparation raw material of the repair wax according to the mass part;
s2: putting 15 parts of aliphatic hydrocarbon solvent, 6 parts of acid montan wax and 4 parts of dimethyl silicone oil into an oil pan, heating to 90 ℃ under the condition of continuous stirring, and keeping the temperature for 10 minutes when the materials are completely dissolved to be transparent liquid;
s3: adding 47.9 parts of deionized water, 2 parts of surfactant, 5 parts of polyol and 15 parts of polishing powder into an emulsifying pot in parts by mass, heating to 80 ℃ while stirring, and keeping the temperature for 5 minutes;
s4: starting high-speed stirring equipment of the emulsifying pot, pumping the materials in the oil pot into the emulsifying pot for 3 minutes, reacting for 40 minutes at 80 ℃, and then cooling to 65 ℃;
s5: adding 4 parts of thickening agent, 1 part of preservative, 0.1 part of pigment and other materials, continuously stirring at a high speed for 5 minutes, and obtaining a finished product after the inspection is qualified.
In an embodiment of the present invention, in S1, raw materials for preparing the repair wax include, in parts by mass, an environmentally friendly aliphatic hydrocarbon solvent, an acidic montan wax, dimethicone, a surfactant, a polyol, a polishing powder, a thickener, an antiseptic, a pigment, and deionized water.
Example three:
as shown in fig. 1, a preparation method of an aqueous environment-friendly automobile paint repair wax comprises the following steps:
s1: preparing a preparation raw material of the repair wax according to the mass part;
s2: putting 12 parts of aliphatic hydrocarbon solvent, 7 parts of acid montan wax and 6 parts of dimethyl silicone oil into an oil pan, heating to 80 ℃ under the condition of continuous stirring, and keeping the temperature for 15 minutes when the materials are completely dissolved to be transparent liquid;
s3: adding 54.9 parts of deionized water, 2 parts of surfactant, 5 parts of polyol and 10 parts of polishing powder into an emulsifying pot in parts by mass, heating to 80 ℃ while stirring, and keeping the temperature for 5 minutes;
s4: starting high-speed stirring equipment of the emulsifying pot, pumping the materials in the oil pot into the emulsifying pot within 5 minutes, reacting for 30 minutes at 80 ℃, and then cooling to 70 ℃;
s5: adding materials such as 2 parts of thickening agent, 1 part of preservative, 0.1 part of pigment and the like, continuously stirring at a high speed for 5 minutes, and obtaining a finished product after the inspection is qualified.
In an embodiment of the present invention, in S1, raw materials for preparing the repair wax include, in parts by mass, an environmentally friendly aliphatic hydrocarbon solvent, an acidic montan wax, dimethicone, a surfactant, a polyol, a polishing powder, a thickener, an antiseptic, a pigment, and deionized water.
Example four:
as shown in fig. 1, a preparation method of an aqueous environment-friendly automobile paint repair wax comprises the following steps:
s1: preparing a preparation raw material of the repair wax according to the mass part;
s2: putting 10 parts of aliphatic hydrocarbon solvent, 8 parts of acid montan wax and 7 parts of dimethyl silicone oil into an oil pan, heating to 90 ℃ under the condition of continuous stirring, and keeping the temperature for 10 minutes when the materials are completely dissolved to be transparent liquid;
s3: adding 49.9 parts of deionized water, 2 parts of surfactant, 3 parts of polyol and 15 parts of polishing powder into an emulsifying pot in parts by mass, heating to 80 ℃ while stirring, and keeping the temperature for 5 minutes;
s4: starting high-speed stirring equipment of the emulsifying pot, pumping the materials in the oil pot into the emulsifying pot for 5 minutes, reacting for 25 minutes at 85 ℃, and then cooling to 65 ℃;
s5: adding 4 parts of thickening agent, 1 part of preservative, 0.1 part of pigment and other materials, continuously stirring at a high speed for 5 minutes, and obtaining a finished product after the inspection is qualified.
In an embodiment of the present invention, in S1, raw materials for preparing the repair wax include, in parts by mass, an environmentally friendly aliphatic hydrocarbon solvent, an acidic montan wax, dimethicone, a surfactant, a polyol, a polishing powder, a thickener, an antiseptic, a pigment, and deionized water.
Example five:
as shown in fig. 1, a preparation method of an aqueous environment-friendly automobile paint repair wax comprises the following steps:
s1: preparing a preparation raw material of the repair wax according to the mass part;
s2: putting 18 parts of aliphatic hydrocarbon solvent, 6 parts of acid montan wax and 8 parts of dimethyl silicone oil into an oil pan, heating to 85 ℃ under the condition of continuous stirring, and keeping the temperature for 15 minutes when the materials are completely dissolved to be transparent liquid;
s3: adding 60 parts of deionized water, 3 parts of surfactant, 2 parts of polyol and 18 parts of polishing powder into an emulsifying pot in parts by mass, stirring and heating to 85 ℃, and keeping the temperature for 20 minutes;
s4: starting high-speed stirring equipment of the emulsifying pot, pumping the materials in the oil pot into the emulsifying pot for 8 minutes, reacting for 30 minutes at 80 ℃, and then cooling to 60 ℃;
s5: adding 3 parts of thickening agent, 0.8 part of preservative, 0.06 part of pigment and other materials, continuously stirring at a high speed for 6 minutes, and obtaining a finished product after the inspection is qualified.
In an embodiment of the present invention, in S1, raw materials for preparing the repair wax include, in parts by mass, an environmentally friendly aliphatic hydrocarbon solvent, an acidic montan wax, dimethicone, a surfactant, a polyol, a polishing powder, a thickener, an antiseptic, a pigment, and deionized water.
The functional indexes of the water-based environment-friendly automobile paint repair wax prepared by the invention are shown in the following table:
inspection item | Index (I) |
Appearance of the product | Are all fine paste bodies |
Smell(s) | Virgin waxTaste of Chinese herbs |
Colour(s) | Golden yellow colour |
Degree of gloss | Increase by more than 12 |
Hydrophobicity (contact Angle) | Greater than 100 ° |
Detergency | High strength |
Scratch repairability | Repairable fine scratch |
Filling property of painted surface | Can be filled with fine voids |
Influence on automobile paint film | Is free of |
The foregoing illustrates and describes the principles, general features, and advantages of the present invention. It will be understood by those skilled in the art that the present invention is not limited to the embodiments described above, which are described in the specification and illustrated only to illustrate the principle of the present invention, but that various changes and modifications may be made therein without departing from the spirit and scope of the present invention, which fall within the scope of the invention as claimed. The scope of the invention is defined by the appended claims and equivalents thereof.
Claims (8)
1. The water-based environment-friendly automobile paint repair wax is characterized by comprising the following components in parts by weight: the repair wax comprises the following raw materials in parts by weight:
5-20 parts of an environment-friendly aliphatic hydrocarbon solvent;
1-10 parts of acid montan wax;
1-10 parts of dimethyl silicone oil;
1-5 parts of a surfactant;
1-5 parts of polyhydric alcohol;
5-20 parts of polishing powder;
1-5 parts of a thickening agent;
0.1-1 part of preservative;
0.01-0.1 part of pigment;
30-70 parts of deionized water.
2. The aqueous environment-friendly automobile paint repair wax as claimed in claim 1, wherein: the environment-friendly aliphatic hydrocarbon solvent is at least one of odorless kerosene D40, odorless kerosene D60 and isoparaffin solvent L.
3. The aqueous environment-friendly automobile paint repair wax as claimed in claim 2, wherein: the acid montan wax is one or a mixture of two of Kelain S wax, LP wax and OP wax; the dimethyl silicone oil is one or a mixture of 100cs, 350cs, 1000cs and 12500cs of Dow Corning PMX-200 silicone oil.
4. The aqueous environment-friendly automobile paint repair wax as claimed in claim 3, wherein: the surfactant is one of GP200, A165, a Tween/span composite emulsification system and an oleic acid/morpholine composite emulsification system.
5. The aqueous environment-friendly automobile paint repair wax as claimed in claim 4, wherein: the polyalcohol is one of ethylene glycol, propylene glycol and glycerol; the polishing powder is one of kaolin, diatomite and quartz sand.
6. The aqueous environment-friendly automobile paint repair wax as claimed in claim 5, wherein: the thickening agent is one of inorganic or organic thickening agents; the preservative is one of sodium benzoate, potassium sorbate and KF-88; the pigment is at least one of water-soluble yellow powder and water-soluble red powder.
7. A preparation method of water-based environment-friendly automobile paint repair wax is characterized by comprising the following steps: the preparation method comprises the following steps:
s1: preparing a preparation raw material of the repair wax according to the mass part;
s2: putting an aliphatic hydrocarbon solvent, acid montan wax and dimethyl silicone oil into an oil pan according to the mass parts, heating to 80-95 ℃ under the condition of continuous stirring, and keeping the temperature for 5-30 minutes when the materials are completely dissolved to be transparent liquid;
s3: adding deionized water, a surfactant, polyhydric alcohol and polishing powder into an emulsifying pot according to the mass parts, heating to 70-90 ℃ while stirring, and keeping the temperature for 5-30 minutes;
s4: starting high-speed stirring equipment of the emulsifying pot, pumping the materials in the oil pot into the emulsifying pot for 2-10 minutes, reacting for 10-60 minutes at 60-90 ℃, and then cooling to 60-80 ℃;
s5: adding materials such as thickening agent, preservative, pigment and the like, continuously stirring at high speed for 2-10 minutes, and obtaining a finished product after the inspection is qualified.
8. The preparation method of the water-based environment-friendly automobile paint repair wax as claimed in claim 7, wherein the preparation method comprises the following steps: in the S1, preparing raw materials of the repair wax according to the mass parts, wherein the raw materials comprise an environment-friendly aliphatic hydrocarbon solvent, acid montan wax, dimethyl silicone oil, a surfactant, polyhydric alcohol, polishing powder, a thickening agent, a preservative, a pigment and deionized water.