CN113654980A - A test device for early crack resistance of concrete - Google Patents

A test device for early crack resistance of concrete Download PDF

Info

Publication number
CN113654980A
CN113654980A CN202111047398.0A CN202111047398A CN113654980A CN 113654980 A CN113654980 A CN 113654980A CN 202111047398 A CN202111047398 A CN 202111047398A CN 113654980 A CN113654980 A CN 113654980A
Authority
CN
China
Prior art keywords
plate
concrete
connecting plate
groups
sets
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Withdrawn
Application number
CN202111047398.0A
Other languages
Chinese (zh)
Inventor
杨蓓蕊
李会州
王疆豫
丁远
宋忠祥
张丁丁
马艳会
常东阳
李慧超
王志敏
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Individual
Original Assignee
Individual
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Individual filed Critical Individual
Priority to CN202111047398.0A priority Critical patent/CN113654980A/en
Publication of CN113654980A publication Critical patent/CN113654980A/en
Withdrawn legal-status Critical Current

Abstract

The invention provides a concrete early anti-cracking performance test device, which comprises a bottom plate; the front end and the rear end of the bottom plate are respectively fixedly connected with a bracket with an L-shaped structure, the left end and the right end of the bottom plate are respectively fixedly connected with a fixed baffle, and the surface direct blowing mechanism of the test piece is connected to a group of fixed baffles; the surface vibrator is arranged on the upper support frame. Utilize electric block to drive upper junction plate and the downward motion of the board that vibrates, make the board that vibrates arrange the concrete in on the surface in, vibrate the concrete through vibrating motor drive vibrating plate activity, through driving motor, drive the scraping plate and move to the other end, strike off the surface of concrete, through two sets of fans, and utilize out the tuber pipe and send wind to concrete surface department, parallel vertical blowing concrete surface, through pulling down the deep bead, and wear the pole to take out, thereby take movable baffle off, so that can discharge out the concrete in the mould.

Description

Concrete early crack resistance test device
Technical Field
The invention belongs to the technical field of concrete tests, and particularly relates to a concrete early-stage crack resistance test device.
Background
Concrete crack resistance refers to the ability of concrete to resist cracking. The crack resistance of concrete is a comprehensive performance, has a certain relation with tensile strength, ultimate tensile deformation capacity, tensile elastic modulus, autogenous volume deformation, creep and thermal performance, and is usually detected by a concrete crack resistance testing device.
If the application number is: CN201810963192.4 discloses a concrete early anti-cracking performance test device, which structurally comprises an adjusting controller top plate, a hydraulic telescopic cylinder, an anti-cracking stress rod, a support column, a fixed support seat, a compression dust removal multi-aspect test device and an operation table, wherein the hydraulic telescopic cylinder is arranged below the adjusting controller top plate and connected in a nesting mode. The device can test and detect the crack resistance of the concrete in multiple aspects, not only can perform basic detection on the crack resistance of the concrete through external stress, but also can further perform test on the crack resistance of the concrete through temperature stress generated by changing temperature, so that the crack resistance of the concrete is improved, the integrity, the durability, even the safety and the stability of a building are enhanced, and the device can collect and compress dust generated in the test process, prevent the dust from scattering around to enter equipment gaps and increase the abrasion of equipment.
Based on the above, when testing the anti-crack performance of concrete, need the manual work to carry out the tamping vibration to the concrete in the mould to after tamping manually strickle off the surface of concrete, still need blow through the surface of equipment to the concrete, whole operation is more troublesome moreover.
Disclosure of Invention
In order to solve the technical problems, the invention provides a concrete early-stage crack resistance testing device, which aims to solve the problems that the concrete in a mould needs to be manually tamped, the surface of the concrete needs to be manually scraped after tamping, the surface of the concrete needs to be blown by equipment, and the whole operation is troublesome.
The invention relates to a concrete early crack resistance test device, which is realized by the following specific technical means:
a concrete early crack resistance test device comprises a bottom plate;
the front end and the rear end of the bottom plate are respectively fixedly connected with a bracket with an L-shaped structure, the left end and the right end of the bottom plate are respectively fixedly connected with a fixed baffle plate, and the fixed baffle plate is provided with a pin hole;
the device comprises an upper support frame, wherein one end of the bottom of the upper support frame is provided with a strip-shaped lower connecting plate, the lower connecting plate is fixedly connected to a group of fixed baffles, the other end of the bottom of the upper support frame is respectively provided with two groups of lower connecting blocks, the two groups of lower connecting blocks are respectively and fixedly connected to the other group of fixed baffles, the four bottom ends of the inner side of the upper support frame are respectively connected with an L-shaped limiting plate, and a guide column is connected between the L-shaped limiting plate and the top of the upper support frame;
the bottom end of the stress induction generator is welded and fixed with the bottom plate, the upper end of the stress induction generator is 10cm lower than the top end of the fixed baffle, and the stress induction generator is formed by welding angle steel and a steel plate;
the test piece surface direct blowing mechanism is connected to the group of fixed baffles;
the surface vibrator is arranged on the upper support frame.
Furthermore, the front end and the rear end of the bottom plate are respectively and movably provided with eight groups of movable baffles, the eight groups of movable baffles are arranged on the bracket and positioned between the two groups of fixed baffles, and the eight groups of movable baffles and the fixed baffles are fixed through penetrating rods.
Furthermore, bayonets are respectively arranged on the lower connecting plate and the two groups of lower connecting blocks, two ends of the wind shield are respectively clamped into the bayonets and attached to the movable baffle, and the height of the wind shield is the same as that of the lower connecting plate.
Further, the test piece surface direct blowing mechanism comprises:
the air collecting box is of a square structure, the bottom and two sides of the air collecting box are of closed structures, and two groups of square mounting openings are formed in the outer end of the air collecting box;
two groups of fans are arranged and are embedded in the square mounting port in a sealing manner;
and the air outlet pipes are provided with twelve groups, the bottom ends of the air outlet pipes are inserted into the air collecting box, and the upper ends of the air outlet pipes are obliquely inserted into the lower connecting plate.
Further, the surface vibrator includes:
the electric hoist is fixedly arranged in the middle of the top end of the upper support frame through a bolt;
the four ends of the upper connecting plate are respectively and slidably arranged on the guide columns, and the upper connecting plate is also hung on the hook of the electric hoist through two groups of hanging rings;
eight groups of vibrating plates are arranged and are connected with the lower side of the upper connecting plate through two groups of movable connecting rods;
one end of the movable connecting rod is rotatably connected with the upper connecting plate, and the other end of the movable connecting rod is rotatably connected with the vibrating plate;
the vibrating motor is fixedly arranged in the middle of the vibrating plate.
Furthermore, the outer end angles of the two outer groups of the vibrating plates are respectively provided with a notch, the size of the notch is matched with that of the L-shaped limiting plate, and when the four end angles of the upper connecting plate are arranged on the L-shaped limiting plate, the two outer groups of the vibrating plates downwards pass through the L-shaped limiting plate.
Further, rotate respectively between the lower extreme of upper bracket and install two sets of screw rods, and still install on two sets of screw rods and scrape the flat board, the upside both ends angle department of scraping the flat board is equipped with the internal thread hole respectively, and scrapes the flat board and pass through internal thread hole and screw rod threaded connection, the outer end of screw rod is connected through the V belt transmission, and wherein a set of screw rod still with be connected through the V belt transmission between driving motor's the motor shaft, driving motor installs on the triangle-shaped support on a set of fixed stop, and scrape the flat board, the flat portion is scraped with the driving motor constitution jointly to the screw rod.
Furthermore, the lower end of the scraping plate is of a wedge-shaped structure and is flush with the upper end of the fixed baffle, and the thickness of the scraping plate is the same as that of the lower connecting plate and is 1/2 the thickness of the fixed baffle.
The invention at least comprises the following beneficial effects:
1. the invention is provided with the surface vibrator, after concrete is poured into a mould which is composed of the bottom plate, the fixed baffle and the movable baffle, the upper connecting plate and the vibrating plate are driven by the electric hoist to move downwards, the upper connecting plate is arranged on the L-shaped limiting plate, the vibrating plate is arranged on the surface of the concrete, and the vibrating plate is driven by the vibrating motor to vibrate the concrete.
2. According to the invention, the scraping part is arranged, after vibration is finished, the upper connecting plate and the vibrating plate are driven to return upwards through the electric hoist, the driving motor is started to drive the two groups of screw rods to rotate, and the scraping plate is driven to move towards the other end under the threaded connection of the screw rods and the inner threaded holes in the scraping plate, so that the surface of concrete is scraped, and meanwhile, the scraping plate is attached to the air outlet of the air outlet pipe, so that the concrete is prevented from flowing into the air outlet pipe and blocking the air outlet pipe.
3. According to the invention, the test piece surface direct blowing mechanism is arranged, after concrete is formed for 30 minutes, air is sent to the concrete surface by the two groups of fans and the air outlet pipe, and the test piece surface direct blowing mechanism is parallel to the concrete surface under the action of the wind shield, so that the anti-cracking performance of the concrete can be tested.
3. According to the invention, through the movable baffle, after the measurement is finished, the wind shield is detached and the penetrating rod is pulled out, so that the movable baffle is detached, and the concrete in the mold can be discharged.
Drawings
Fig. 1 is a schematic structural view of the present invention.
Fig. 2 is an enlarged schematic view of the invention at a in fig. 1.
Fig. 3 is a schematic view of the structure of fig. 1 from another view angle according to the present invention.
Fig. 4 is a schematic view illustrating the structure of the invention in which the upper connecting plate moves downward to the L-shaped stopper plate in fig. 1.
Fig. 5 is an enlarged view of the structure of fig. 4 at B according to the present invention.
FIG. 6 is a schematic illustration of the invention shown in FIG. 1 with the flapper and the windshield removed.
Fig. 7 is a schematic structural view of the two-sided flapper and the windshield of fig. 6 with the flapper in motion and the screed plate in accordance with the present invention.
Fig. 8 is a schematic view of the connection structure of the upper connecting plate and the vibrating plate according to the present invention.
In the drawings, the corresponding relationship between the component names and the reference numbers is as follows:
1. a base plate; 101. a bracket; 103. fixing a baffle plate; 1021. a pin hole; 1022. a triangular bracket; 103. an upper support frame; 1031. a lower connecting plate; 1032. a lower connecting block; 1033. an L-shaped limiting plate; 1034. a guide post; 1035. a bayonet; 104. a movable baffle; 105. penetrating a rod; 106. a wind deflector;
2. a stress-inducing generator;
3. a test piece surface direct blowing mechanism; 301. an air collecting box; 3011. a square mounting port; 302. a fan; 303. an air outlet pipe;
4. a surface vibrator; 401. an electric hoist; 402. an upper connecting plate; 4021. a hoisting ring; 403. a vibrating plate; 404. a movable connecting rod; 405. a vibration motor;
5. a scraping part; 501. scraping the plate; 502. a screw; 503. the motor is driven.
Detailed Description
The embodiments of the present invention will be described in further detail with reference to the drawings and examples. The following examples are intended to illustrate the invention but are not intended to limit the scope of the invention.
In the description of the present invention, "a plurality" means two or more unless otherwise specified; the terms "coaxial," "bottom," "one end," "top," "middle," "other end," "upper," "side," "top," "inner," "front," "center," "two ends," and the like are used in an orientation or positional relationship indicated in the drawings for convenience in describing and simplifying the description, and are not intended to indicate or imply that the device or element being referred to must have a particular orientation, be constructed and operated in a particular orientation, and thus should not be construed as limiting the invention. Furthermore, the terms "first," "second," "third," and the like are used for descriptive purposes only and are not to be construed as indicating or implying relative importance.
In the description of the present invention, it should be noted that, unless explicitly stated or limited otherwise, the terms "mounted," "disposed," "connected," "fixed," "screwed" and the like are to be understood broadly, and for example, they may be fixedly connected, detachably connected, or integrated; can be mechanically or electrically connected; the terms may be directly connected or indirectly connected through an intermediate, and may be communication between two elements or interaction relationship between two elements, unless otherwise specifically limited, and the specific meaning of the terms in the present invention will be understood by those skilled in the art according to specific situations.
Example (b):
as shown in figures 1 to 8:
the invention provides a concrete early anti-cracking performance test device, which comprises a bottom plate 1;
the front end and the rear end of the bottom plate 1 are respectively fixedly connected with a bracket 101 with an L-shaped structure, the left end and the right end of the bottom plate 1 are respectively fixedly connected with a fixed baffle plate 102, and the fixed baffle plate 102 is provided with a pin hole 1021;
an upper support frame 103, wherein one end of the bottom of the upper support frame 103 is provided with a strip-shaped lower connecting plate 1031, the lower connecting plate 1031 is fixedly connected to one group of fixed baffles 102, the other end of the bottom of the upper support frame 103 is respectively provided with two groups of lower connecting blocks 1032, the two groups of lower connecting blocks 1032 are respectively fixedly connected to the other group of fixed baffles 102, the four bottom ends of the inner side of the upper support frame 103 are respectively connected with an L-shaped limiting plate 1033, and a guide post 1034 is connected between the L-shaped limiting plate 1033 and the top of the upper support frame 103;
referring to fig. 7, the bottom end of the stress inducing generator 2 is welded and fixed to the bottom plate 1, the upper end of the stress inducing generator 2 is 10cm lower than the top end of the fixed baffle 102, and the stress inducing generator 2 is formed by welding angle steel and a steel plate;
referring to fig. 3, the specimen surface direct blowing mechanism 3 is connected to a set of fixed baffles 102; the test piece surface direct blowing mechanism 3 includes: the air collecting box 301 is of a square structure, the bottom and two sides of the air collecting box 301 are of closed structures, and two groups of square mounting holes 3011 are formed in the outer ends of the air collecting box 301; two groups of fans 302 are arranged, and the fans 302 are hermetically embedded in the square mounting port 3011; the air outlet pipes 303 are provided with twelve groups, the bottom ends of the air outlet pipes 303 are inserted into the air collecting box 301, the upper ends of the air outlet pipes are obliquely inserted into the lower connecting plate 1031, after the concrete is formed for 30 minutes, the two groups of fans 302 are started, air is sent to the surface of the concrete through the air outlet pipes 303, and the air is blown to the surface of the concrete in parallel under the action of the wind shield 106;
referring to fig. 7 and 8, the surface vibrator 4 is mounted on the upper frame 103, and the surface vibrator 4 includes: the electric hoist 401 is fixedly arranged in the middle of the top end of the upper support frame 103 through bolts; the four ends of the upper connecting plate 402 are slidably mounted on the guide posts 1034 respectively, and the upper connecting plate 402 is also hung on the hook of the electric hoist 401 through the two lifting rings 4021; eight groups of vibrating plates 403 are arranged on the vibrating plates 403 and are connected to the lower side of the upper connecting plate 402 through two groups of movable connecting rods 404; one end of the movable connecting rod 404 is rotatably connected with the upper connecting plate 402, and the other end of the movable connecting rod 404 is rotatably connected with the vibrating plate 403; the vibrating motor 405 is fixedly arranged in the middle of the vibrating plate 403, the electric hoist 401 is started to drive the upper connecting plate 402 and the vibrating plate 403 to move downwards, firstly, the two groups of vibrating plates 403 on the outer side downwards pass through the L-shaped limiting plate 1033 under the action of gaps of the vibrating plates, then, the upper connecting plate 402 is placed on the L-shaped limiting plate 1033, meanwhile, the vibrating plates 403 are placed on the surface of concrete, the electric hoist 401 is closed, the vibrating motor is started, and the vibrating plates 403 are driven to vibrate the concrete under the action of the movable connecting rod 404; after the vibration is finished, the electric hoist 401 drives the upper connecting plate 402 and the vibrating plate 403 to return upwards.
Referring to fig. 1 and 6, eight groups of movable baffles 104 are movably mounted at the front end and the rear end of the bottom plate 1 respectively, the eight groups of movable baffles 104 are arranged on the bracket 101 and are positioned between the two groups of fixed baffles 102, the eight groups of movable baffles 104 and the fixed baffles 102 are fixed through the penetrating rods 105, and after the measurement is completed, the penetrating rods 105 are pulled out, so that the movable baffles 104 are taken down, and the concrete in the mold can be discharged.
Referring to fig. 5, the lower connecting plate 1031 and the two sets of lower connecting blocks 1032 are respectively provided with a bayonet 1035, two ends of the wind deflector 106 are respectively clamped into the bayonet 1035 and attached to the movable baffle 104, and the wind deflector 106 and the lower connecting plate 1031 have the same height.
Referring to fig. 8, two sets of outer end angles of the outer side of the vibrating plate 403 are respectively provided with a notch, the size of the notch is adapted to the size of the L-shaped limiting plate 1033, and when the four end angles of the upper connecting plate 402 are placed on the L-shaped limiting plate 1033, the two sets of vibrating plates 403 on the outer side pass through the L-shaped limiting plate 1033, and when the upper connecting plate 402 and the vibrating plates 403 move downward, the two sets of vibrating plates 403 on the outer side can pass through the L-shaped limiting plate 1033 and be placed on the surface of concrete, so as to vibrate the concrete.
Referring to fig. 5 and 7, two sets of screws 502 are respectively rotatably mounted between the lower ends of the upper support frame 103, and a scraping plate 501 is further mounted on the two sets of screws 502, two end corners of the upper side of the scraping plate 501 are respectively provided with an internal thread hole, and the scraping plate 501 is in threaded connection with the screws 502 through the internal thread hole, the outer ends of the screws 502 are in transmission connection through a triangular belt, and one set of screws 502 is also in transmission connection with the motor shaft of a driving motor 503 through the triangular belt, the driving motor 503 is mounted on a triangular bracket 1022 on a set of fixed baffle 102, and the scraping plate 501, the screws 502 and the driving motor 503 form a scraping portion 5, and by starting the driving motor 503, the two sets of screws 502 are driven to rotate, and under the threaded connection of the internal thread hole and the screws 502 on the scraping plate 501, the scraping plate 501 is driven to move towards the other end, so as to scrape the surface of the concrete.
In another embodiment, referring to fig. 7, the lower end of the scraping plate 501 is of a wedge-shaped structure and is flush with the upper end of the fixed baffle 102, the thickness of the scraping plate 501 is the same as that of the lower connecting plate 1031, and is 1/2 equal to that of the fixed baffle 102, when the scraping plate 501 scrapes the surface of the concrete, the smoothness of the scraping plate 501 during scraping is increased, and the scraping plate 501 can be attached to the lower connecting plate 1031, and the scraping plate 504 is attached to the air outlet of the air outlet pipe 303, so that the concrete is prevented from flowing into the air outlet pipe 303 and blocking the air outlet pipe 303.
The specific use mode and function of the embodiment are as follows:
in the invention, concrete is poured into a mould which is composed of a bottom plate 1, a fixed baffle plate 102 and a movable baffle plate 104, the surface of the concrete is slightly higher than the top end of the fixed baffle plate 102, an electric hoist 401 is started to drive an upper connecting plate 402 and vibrating plates 403 to move downwards, firstly, two groups of vibrating plates 403 on the outer side downwards pass through an L-shaped limiting plate 1033 under the action of gaps of the vibrating plates, then the upper connecting plate 402 is placed on the L-shaped limiting plate 1033, meanwhile, the vibrating plates 403 are placed on the surface of the concrete, the electric hoist 401 is closed, a vibrating motor is started, and the vibrating plates 403 are driven to vibrate the concrete under the action of a movable connecting rod 404; after vibrating, the electric hoist 401 drives the upper connecting plate 402 and the vibrating plate 403 to return upwards, the driving motor 503 is started to drive the two groups of screws 502 to rotate, and the scraping plate 501 is driven to move towards the other end under the threaded connection of the internal threaded hole on the scraping plate 501 and the screws 502, so that the surface of the concrete is scraped; after the concrete is formed for 30 minutes, two groups of fans 302 are started, wind is sent to the surface of the concrete through a wind outlet pipe 303, and the wind is blown to the surface of the concrete in parallel and directly under the action of a wind shield 106;
measuring the crack from the time when the concrete is stirred and water is added to the concrete to 24 hours, wherein the length of the crack is based on the crack visible by naked eyes, measuring the length of the crack by using a straight steel ruler, taking the linear distance between two ends of the crack as the length of the crack, adding the lengths of the two cracks when two cracks exist on a knife edge, converting the lengths into one crack, measuring the width of the crack by using a reading microscope (the division value is 0.01mm) with the magnification of 40 times, and measuring the width of each crack; measuring to obtain crack data after concrete pouring for 24 hours, and calculating the average crack area, the number of cracks in unit area and the total crack area in unit area;
after the measurement is completed, wind deflector 106 is removed and rod 105 is withdrawn, removing flapper 104 so that the concrete in the mold can be discharged.
The invention is not described in detail, but is well known to those skilled in the art.
The embodiments of the present invention have been presented for purposes of illustration and description, and are not intended to be exhaustive or limited to the invention in the form disclosed. Many modifications and variations will be apparent to those of ordinary skill in the art. The embodiment was chosen and described in order to best explain the principles of the invention and the practical application, and to enable others of ordinary skill in the art to understand the invention for various embodiments with various modifications as are suited to the particular use contemplated.

Claims (8)

1.一种混凝土早期抗裂性能试验装置,其特征在于:包括底板(1);1. a concrete early crack resistance test device, is characterized in that: comprise bottom plate (1); 所述底板(1)的前后两端分别固定连接有L型结构的托架(101),且底板(1)的左右两端分别固定连接有固定挡板(102),固定挡板(102)上设有销孔(1021);The front and rear ends of the bottom plate (1) are respectively fixedly connected with brackets (101) of L-shaped structure, and the left and right ends of the bottom plate (1) are respectively fixedly connected with a fixed baffle plate (102), and the fixed baffle plate (102) There is a pin hole (1021) on it; 上撑架(103),上撑架(103)的底部一端设有长条状的下连接板(1031),下连接板(1031)固定连接在一组固定挡板(102)上,上撑架(103)的底部另一端分别设有两组下连接块(1032),两组下连接块(1032)分别固定连接在另一组固定挡板(102)上,上撑架(103)的内侧四底端分别连接有L型限位板(1033),且L型限位板(1033)与上撑架(103)的顶部之间连接有导向柱(1034);The upper support frame (103), the bottom end of the upper support frame (103) is provided with an elongated lower connecting plate (1031), and the lower connecting plate (1031) is fixedly connected to a set of fixed baffles (102), and the upper support The other end of the bottom of the frame (103) is respectively provided with two sets of lower connecting blocks (1032), and the two sets of lower connecting blocks (1032) are respectively fixedly connected to another set of fixed baffles (102), and the upper support frame (103) The inner four bottom ends are respectively connected with L-shaped limit plates (1033), and guide columns (1034) are connected between the L-shaped limit plates (1033) and the top of the upper support frame (103); 应力诱导发生器(2),应力诱导发生器(2)的底端与底板(1)焊接固定,其上端比固定挡板(102)顶端低10cm,且应力诱导发生器(2)由角钢与钢板焊接而成;The stress inducing generator (2), the bottom end of the stress inducing generator (2) is welded and fixed with the bottom plate (1), the upper end of which is 10 cm lower than the top of the fixed baffle plate (102), and the stress inducing generator (2) is made of angle steel and Welded steel plate; 试件表面直吹机构(3),试件表面直吹机构(3)连接在一组固定挡板(102)上;a direct blowing mechanism (3) on the surface of the test piece, and the direct blowing mechanism (3) on the surface of the test piece is connected to a set of fixed baffles (102); 表面式振捣器(4),表面式振捣器(4)安装在上撑架(103)上。The surface vibrator (4) is mounted on the upper support frame (103). 2.如权利要求1所述混凝土早期抗裂性能试验装置,其特征在于,所述底板(1)的前后两端还分别活动安装有八组活动挡板(104),八组活动挡板(104)置于托架(101)上,并位于两组固定挡板(102)之间,且八组活动挡板(104)与固定挡板(102)之间通过穿杆(105)固定。2. The concrete early crack resistance test device as claimed in claim 1, wherein the front and rear ends of the bottom plate (1) are also movably installed with eight groups of movable baffles (104) respectively, and the eight groups of movable baffles (104). 104) is placed on the bracket (101) and located between the two sets of fixed baffles (102), and the eight groups of movable baffles (104) and the fixed baffles (102) are fixed by through rods (105). 3.如权利要求2所述混凝土早期抗裂性能试验装置,其特征在于,所述下连接板(1031)与两组下连接块(1032)上分别设有卡口(1035),挡风板(106)的两端分别卡入到卡口(1035)中,并贴在活动挡板(104)上,且挡风板(106)与下连接板(1031)的高度相同。3. The concrete early crack resistance test device according to claim 2, characterized in that, said lower connecting plate (1031) and two sets of lower connecting blocks (1032) are respectively provided with bayonet (1035), and the windshield The two ends of the (106) are respectively snapped into the bayonet (1035) and attached to the movable baffle (104), and the height of the wind baffle (106) and the lower connecting plate (1031) is the same. 4.如权利要求1所述混凝土早期抗裂性能试验装置,其特征在于,所述试件表面直吹机构(3)包括:4. The concrete early crack resistance test device according to claim 1, wherein the direct blowing mechanism (3) on the surface of the test piece comprises: 集风箱(301),集风箱(301)为方形结构,其底部与两侧均为封闭结构,其外端设有两组方形安装口(3011);The bellows box (301), the bellows box (301) has a square structure, the bottom and both sides of which are closed structures, and two sets of square installation openings (3011) are arranged at the outer ends thereof; 风扇(302),风扇(302)设有两组,并密封嵌装在方形安装口(3011)内;A fan (302), the fan (302) is provided with two groups, and is sealed and embedded in the square installation opening (3011); 出风管(303),出风管(303)设有十二组,其底端插入到集风箱(301)中,上端斜插在下连接板(1031)中。The air outlet pipe (303) is provided with twelve groups, the bottom end of which is inserted into the air collecting box (301), and the upper end is obliquely inserted into the lower connecting plate (1031). 5.如权利要求1所述混凝土早期抗裂性能试验装置,其特征在于,所述表面式振捣器(4)包括:5. The concrete early crack resistance test device according to claim 1, wherein the surface vibrator (4) comprises: 电动葫芦(401),电动葫芦(401)通过螺栓固定安装在上撑架(103)的顶端中间;An electric hoist (401), the electric hoist (401) is fixedly installed in the middle of the top end of the upper support frame (103) by means of bolts; 上连接板(402),上连接板(402)的四端滑动分别安装在导向柱(1034)上,且上连接板(402)还通过两组吊环(4021)吊装在电动葫芦(401)的挂钩上;The upper connecting plate (402), the four ends of the upper connecting plate (402) are slidably installed on the guide columns (1034), and the upper connecting plate (402) is also hoisted on the lower part of the electric hoist (401) through two sets of lifting rings (4021). on the hook; 捣振板(403),捣振板(403)设有八组,并通过两组活动连杆(404)连接在上连接板(402)的下侧;The pounding plate (403), the pounding plate (403) is provided with eight groups, and is connected to the lower side of the upper connecting plate (402) through two groups of movable connecting rods (404); 活动连杆(404),活动连杆(404)的一端与上连接板(402)转动连接,另一端与捣振板(403)转动连接;A movable connecting rod (404), one end of the movable connecting rod (404) is rotatably connected with the upper connecting plate (402), and the other end is rotatably connected with the pounding plate (403); 振动电机(405),振动电机(405)固定安装在捣振板(403)的中间位置。The vibration motor (405) is fixedly installed at the middle position of the pounding plate (403). 6.如权利要求5所述混凝土早期抗裂性能试验装置,其特征在于,所述捣振板(403)中外侧两组的外端角处分别设有缺口,且缺口的大小与L型限位板(1033)的大小相适应,且上连接板(402)的四端角置于L型限位板(1033)上时,外侧的两组捣振板(403)已向下通过L型限位板(1033)。6. The concrete early crack resistance test device according to claim 5, characterized in that, the outer end corners of the two groups of the middle and outer sides of the tamping plate (403) are respectively provided with notches, and the size of the notches is the same as the L-shaped limit. When the size of the position plate (1033) is suitable, and the four end corners of the upper connecting plate (402) are placed on the L-shaped limit plate (1033), the two sets of vibration plates (403) on the outside have passed down through the L-shaped limiter plate (403). Limiting Plate (1033). 7.如权利要求1所述混凝土早期抗裂性能试验装置,其特征在于,所述上撑架(103)的下端之间分别转动安装有两组螺杆(502),且两组螺杆(502)上还安装有刮平板(501),刮平板(501)的上侧两端角处分别设有内螺纹孔,且刮平板(501)通过内螺纹孔与螺杆(502)螺纹连接,螺杆(502)的外端通过三角带传动连接,且其中一组螺杆(502)还与驱动电机(503)的电机轴之间通过三角带传动连接,驱动电机(503)安装在一组固定挡板(102)上的三角形支架(1022)上,且刮平板(501)、螺杆(502)与驱动电机(503)共同组成刮平部(5)。7. The concrete early crack resistance test device according to claim 1, characterized in that, two sets of screws (502) are respectively rotatably installed between the lower ends of the upper brackets (103), and the two sets of screws (502) A scraper plate (501) is also installed on the scraper plate (501), and the two end corners of the upper side of the scraper plate (501) are respectively provided with internal thread holes, and the scraper plate (501) is threadedly connected with the screw rod (502) through the internal screw hole, and the screw rod (502) ) are connected by a V-belt drive, and a group of screws (502) are also connected with the motor shaft of a drive motor (503) by a V-belt drive, and the drive motor (503) is installed on a set of fixed baffles (102). ) on the triangular bracket (1022), and the scraping plate (501), the screw (502) and the driving motor (503) together form the scraping part (5). 8.如权利要求7所述混凝土早期抗裂性能试验装置,其特征在于,所述刮平板(501)的下端为楔状结构,并与固定挡板(102)的上端持平,刮平板(501)的厚度与下连接板(1031)的厚度相同,并均为固定挡板(102)厚度的1/2。8. The concrete early crack resistance test device according to claim 7, characterized in that, the lower end of the scraper plate (501) is a wedge-shaped structure, and is flush with the upper end of the fixed baffle plate (102), and the scraper plate (501) The thickness of the lower connecting plate (1031) is the same as that of the lower connecting plate (1031), and both are 1/2 of the thickness of the fixed baffle plate (102).
CN202111047398.0A 2021-09-08 2021-09-08 A test device for early crack resistance of concrete Withdrawn CN113654980A (en)