CN112643837A - Manufacturing method of green environment-friendly process box - Google Patents

Manufacturing method of green environment-friendly process box Download PDF

Info

Publication number
CN112643837A
CN112643837A CN202010881533.0A CN202010881533A CN112643837A CN 112643837 A CN112643837 A CN 112643837A CN 202010881533 A CN202010881533 A CN 202010881533A CN 112643837 A CN112643837 A CN 112643837A
Authority
CN
China
Prior art keywords
box
wood
friendly
log
environment
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Pending
Application number
CN202010881533.0A
Other languages
Chinese (zh)
Inventor
刘继东
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Chongqing Haoxiang Products Co ltd
Original Assignee
Chongqing Haoxiang Products Co ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Chongqing Haoxiang Products Co ltd filed Critical Chongqing Haoxiang Products Co ltd
Priority to CN202010881533.0A priority Critical patent/CN112643837A/en
Publication of CN112643837A publication Critical patent/CN112643837A/en
Pending legal-status Critical Current

Abstract

The invention relates to the technical field of environment-friendly process boxes and discloses a manufacturing method of a green environment-friendly process box, which comprises the following steps: s1, slicing the log or cutting the log into required box wood boards by a wood saw; s2, putting the log board into a vacuum dryer; s3, splicing and repairing the dried log boards; s4, attaching the steel wire mesh between the two original wood boards coated with the glue; s5, paving a waterproof and moistureproof layer on the outer wall of the wood board after the hot pressing; s6, nailing the wood boards into an integral rectangular shape by iron nails in sequence according to the customized size; and S7, nailing one copper corner protector at each periphery of the process box, thereby completing the manufacture of the green environment-friendly process box. The manufacturing method of the environment-friendly process box ensures that the manufacturing method of the process box can save wood resources, does not cause the problems of deformation, warping and cracking of the process box, prolongs the service life of the process box, and prolongs the period of the process box needing to be replaced, thereby saving wood consumption.

Description

Manufacturing method of green environment-friendly process box
Technical Field
The invention relates to the technical field of environment-friendly process boxes, in particular to a manufacturing method of an environment-friendly process box.
Background
People can store grains and save money for living in an peaceful place; enterprises can store funds and resources in order to smoothly develop production; human beings store "green capital" in order to maintain ecological safety. Because green is not only a symbol of life and health, but also a mark of civilization and environmental protection, the green is the primary color of the environment on which we rely for survival. Without green color, the survival and development of human beings are threatened, and the earth is also confronted with species extinction. Therefore, the coexistence of 'green capital' with hands has become a consensus and responsibility for dealing with ecological crisis in all countries of the world. Storing the 'green capital', namely, planting trees to protect green and expanding greening. To store more "green capital," the most efficient direct method is afforestation. The afforestation not only beautifies the living environment and prevents water and soil loss, but also can effectively reduce the carbon dioxide of the ozone layer of the earth, provide clean and fresh air for human beings, improve the ecological environment and regulate the climate. Humans have recognized the importance of storing "green capital". Tree planting sections are set in many countries in the world, environmental protection and greening awareness of people is enhanced through activities such as tree planting and green protection, and the enthusiasm of people for tree planting and green protection is promoted, so that the aims of storing green capital and keeping ecological balance are fulfilled.
The process box combined by the solid wood decorative plates in the market at present is made of raw wood plates and spliced plates as commonly used raw materials, so that a large amount of wood resources are wasted, a series of problems such as deformation, warping, cracking and the like can occur in the process box when the process box is used in the environment with variable humidity, the service life of the process box is shortened, the damaged process box needs to be replaced, the consumption of wood is increased, and the requirements of environmental protection are not met, so that the method for manufacturing the environment-friendly process box is provided.
Disclosure of Invention
Aiming at the defects of the prior art, the invention provides a method for manufacturing a green environment-friendly process box, which solves the problems that the process box is combined by solid wood decorative plates in the current market, the commonly used raw materials are made of original wood plates and spliced wood plates, so that a large amount of wood resources are wasted, the process box is deformed, warped, cracked and the like when being used in the environment with variable humidity, the service life of the process box is shortened, the damaged process box needs to be replaced, the consumption of wood is increased, and the green environment-friendly requirements are not met.
In order to ensure that the manufacturing method of the process box can save wood resources, and the process box cannot cause the problems of deformation, warping and cracking when being used in the environment with variable humidity, such as spring, summer, autumn and winter, the service life of the process box is prolonged, the period of the process box needing to be replaced is prolonged, the consumption of wood is saved, and the method accords with the idea of environmental protection, and the following technical scheme is provided: a manufacturing method of a green environment-friendly process box comprises the following steps:
s1, slicing the log or sawing the log into a required box wood board with the thickness of 0.5-1 cm, the length of 68 cm, the side width of 28 cm and the side height of 25 cm;
s2, putting the raw wood board into a vacuum dryer, and controlling the water content of the raw wood board to be 4-6% in the drying process;
s3, splicing and repairing the dried log boards, and uniformly coating glue on the log board surfaces on the upper surface and the lower surface;
s4, adhering the steel wire mesh between the two original wood boards coated with the glue, and performing hot-pressing treatment on the two original wood boards by using hot-pressing forming equipment;
s5, paving a waterproof and moistureproof layer on the outer wall of the board after hot pressing, shaping, and then adhering a decorative layer on one end of the waterproof and moistureproof layer;
s6, nailing the wood boards into an integral rectangular shape by iron nails in sequence according to the customized size, covering the wood boxes with the height of 68 multiplied by the width of 28 multiplied by the height of 40cm, nailing, and then screwing the wood boxes with self-tapping screws to finish the process to lean against side chains;
and S7, nailing one copper corner protector at each periphery of the process box, and nailing the corner protector by using copper nails matched with the copper corner protectors, thereby completing the manufacture of the environment-friendly process box.
Preferably, the step S1 is to cut a process case cover wood board with the thickness of 0.5-11 cm, the side width of 28 cm, the length of 68 cm and the side height of 15 cm.
Preferably, the standard of the glue in S3 is environment-friendly EO grade, the glue concentration is 70%, and the selection of the glue is as follows: melamine resins or phenol resin adhesives (PF).
Preferably, the hot pressing temperature in the S4 is 180-220 ℃, and the hot pressing pressure is 40kg/cm 2-75 kg/cm 2.
Preferably, the waterproof and moisture-proof layer is a waterproof coating material prepared by taking synthetic rubber or contract resin as a main film forming substance and adding other auxiliary materials.
Preferably, in S7, the process box is locked by copper nails up and down at the middle position of the joint between the upper edge cover and the box body of the process box, and then the copper lock is provided, so as to complete the locking treatment of the process box.
Compared with the prior art, the invention provides a manufacturing method of a green environment-friendly process box, which has the following beneficial effects:
the manufacturing method of the environment-friendly process box comprises the steps of slicing logs or cutting logs by using a wood saw, drying log boards, attaching a steel wire mesh between two original wood boards coated with glue, paving a waterproof and moistureproof layer on the outer walls of the wood boards after hot pressing, and nailing the wood boards into an integral rectangular shape by iron nails in sequence according to a customized size, so that the manufacturing of the environment-friendly process box is completed, the wood resources can be saved by the manufacturing method of the process box, the problems of deformation, warping and cracking of the process box can be avoided when the process box is used in the environment with humidity change, such as spring, summer, autumn, winter, the service life of the process box is prolonged, the period of the process box needing to be replaced is prolonged, wood consumption is saved, and the environment-friendly concept is met.
Detailed Description
The technical solutions in the embodiments of the present invention will be clearly and completely described below with reference to the contents of the present invention, and it is obvious that the described embodiments are only a part of the embodiments of the present invention, and not all of the embodiments. All other embodiments, which can be derived by a person skilled in the art from the embodiments given herein without making any creative effort, shall fall within the protection scope of the present invention.
A manufacturing method of a green environment-friendly process box comprises the following steps:
s1, slicing the log or sawing the log into a required box wood board with the thickness of 0.5-1 cm, the length of 68 cm, the side width of 28 cm and the side height of 25 cm;
s2, putting the raw wood board into a vacuum dryer, and controlling the water content of the raw wood board to be 4-6% in the drying process;
s3, splicing and repairing the dried log boards, and uniformly coating glue on the log board surfaces on the upper surface and the lower surface;
s4, adhering the steel wire mesh between the two original wood boards coated with the glue, and performing hot-pressing treatment on the two original wood boards by using hot-pressing forming equipment;
s5, paving a waterproof and moistureproof layer on the outer wall of the board after hot pressing, shaping, and then adhering a decorative layer on one end of the waterproof and moistureproof layer;
s6, nailing the wood boards into an integral rectangular shape by iron nails in sequence according to the customized size, covering the wood boxes with the height of 68 multiplied by the width of 28 multiplied by the height of 40cm, nailing, and then screwing the wood boxes with self-tapping screws to finish the process to lean against side chains;
and S7, nailing one copper corner protector at each periphery of the process box, and nailing the corner protector by using copper nails matched with the copper corner protectors, thereby completing the manufacture of the environment-friendly process box.
S1, cutting a process box cover wood plate with the thickness of 0.5-11 cm, the side width of 28 cm, the length of 68 cm and the side height of 15 cm; the standard of the glue in S3 is environment-friendly EO grade, the glue concentration is 70%, and the glue is selected as follows: melamine resins or phenol resin adhesives (PF); s4, the hot pressing temperature is 180-220 ℃, and the hot pressing pressure is 40kg/cm 2-75 kg/cm 2; the waterproof and moistureproof layer is a waterproof coating material prepared by taking synthetic rubber or contract resin as a main film forming substance and adding other auxiliary materials; and S7, the upper edge cover of the process box and the middle position of the box body combination part are locked by copper nails, and then the copper locks are matched to finish the locking treatment of the process box.
In conclusion, firstly, the logs are sliced or sawed into required box body wood boards with the thickness of 0.5-1 cm, the length of 68 cm, the side width of 28 cm and the side height of 25 cm, and then the required box body wood boards with the thickness of 0.5-11 cm, the side width of 28 cm, the length of 68 cm and the side height of 15 cm are cut into the process box cover wood boards, so that the process box can be conveniently adjusted to be a box cover; splicing and repairing the dried log boards, and uniformly coating glue on the log boards on the upper surface and the lower surface, wherein the glue standard is an environment-friendly EO grade, the glue concentration is 70%, and the glue is selected: melamine resin or phenolic resin glue (PF), the glue is selected from environment-friendly glue; attaching a steel wire mesh between the two original wood boards coated with the glue, and performing hot pressing treatment on the two original wood boards by using hot pressing forming equipment, wherein the hot pressing temperature is 180-220 ℃, and the hot pressing pressure is 40kg/cm 2-75 kg/cm2, so that the original wood boards are good in pressing effect; laying a waterproof and moistureproof layer on the outer wall of the board after hot pressing, carrying out shaping treatment, then adhering a decorative layer on one end of the waterproof and moistureproof layer, and ensuring the attractiveness of the process box by using the decorative layer, wherein the waterproof and moistureproof layer is a waterproof coating material prepared by taking synthetic rubber or contract resin as a main film forming substance and adding other auxiliary materials; the wood board is nailed into an integral rectangular shape by iron nails according to a customized size in sequence, the wood board comprises a wood box with the height of 68 multiplied by the width of 28 multiplied by the height of 40cm, the wood box is nailed and then a process wood box is nailed by a self-tapping screw to be used for installing a side chain, copper angle protectors are nailed respectively at the periphery of the process box, the angle protectors are nailed by copper nails matched with the copper angle protectors, the copper angle protectors are installed at the periphery of the process box, the use strength of the process box can be ensured to be higher, the manufacture of the environment-friendly process box is finished, wherein lock catches are nailed by the copper nails up and down at the middle position of the upper edge of the process box and the joint part of the box body, and then the copper locks are matched.
It is noted that, herein, relational terms such as first and second, and the like may be used solely to distinguish one entity or action from another entity or action without necessarily requiring or implying any actual such relationship or order between such entities or actions. Also, the terms "comprises," "comprising," or any other variation thereof, are intended to cover a non-exclusive inclusion, such that a process, method, article, or apparatus that comprises a list of elements does not include only those elements but may include other elements not expressly listed or inherent to such process, method, article, or apparatus.
Although embodiments of the present invention have been shown and described, it will be appreciated by those skilled in the art that changes, modifications, substitutions and alterations can be made in these embodiments without departing from the principles and spirit of the invention, the scope of which is defined in the appended claims and their equivalents.

Claims (6)

1. The manufacturing method of the green environment-friendly process box is characterized by comprising the following steps of:
s1, slicing the log or sawing the log into a required box wood board with the thickness of 0.5-1 cm, the length of 68 cm, the side width of 28 cm and the side height of 25 cm;
s2, putting the raw wood board into a vacuum dryer, and controlling the water content of the raw wood board to be 4-6% in the drying process;
s3, splicing and repairing the dried log boards, and uniformly coating glue on the log board surfaces on the upper surface and the lower surface;
s4, adhering the steel wire mesh between the two original wood boards coated with the glue, and performing hot-pressing treatment on the two original wood boards by using hot-pressing forming equipment;
s5, paving a waterproof and moistureproof layer on the outer wall of the board after hot pressing, shaping, and then adhering a decorative layer on one end of the waterproof and moistureproof layer;
s6, nailing the wood boards into an integral rectangular shape by iron nails in sequence according to the customized size, covering the wood boxes with the height of 68 multiplied by the width of 28 multiplied by the height of 40cm, nailing, and then screwing the wood boxes with self-tapping screws to finish the process to lean against side chains;
and S7, nailing one copper corner protector at each periphery of the process box, and nailing the corner protector by using copper nails matched with the copper corner protectors, thereby completing the manufacture of the environment-friendly process box.
2. The method for manufacturing the green environmental protection process box according to claim 1, wherein the method comprises the following steps: and in the step S1, cutting a board with the thickness of 0.5-11 cm, the side width of 28 cm, the length of 68 cm and the side height of 15 cm to obtain the process box cover.
3. The method for manufacturing the green environmental protection process box according to claim 1, wherein the method comprises the following steps: the standard of the S3 medium adhesive is environment-friendly EO grade, the adhesive concentration is 70%, and the selection of the adhesives is as follows: melamine resins or phenol resin adhesives (PF).
4. The method for manufacturing the green environmental protection process box according to claim 1, wherein the method comprises the following steps: the hot pressing temperature of S4 is 180-220 ℃, and the hot pressing pressure is 40kg/cm 2-75 kg/cm 2.
5. The method for manufacturing the green environmental protection process box according to claim 1, wherein the method comprises the following steps: the waterproof and moistureproof layer is a waterproof coating material prepared by taking synthetic rubber or contract resin as a main film forming substance and adding other auxiliary materials.
6. The method for manufacturing the green environmental protection process box according to claim 1, wherein the method comprises the following steps: and in the step S7, the upper edge cover of the process box and the middle position of the joint part of the box body are vertically nailed by copper nails to be locked, and then a copper lock is matched to finish the locking treatment of the process box.
CN202010881533.0A 2020-08-27 2020-08-27 Manufacturing method of green environment-friendly process box Pending CN112643837A (en)