CN112077278B - Pouring assembly suitable for side pouring of multiple lift tubes - Google Patents

Pouring assembly suitable for side pouring of multiple lift tubes Download PDF

Info

Publication number
CN112077278B
CN112077278B CN202010842275.5A CN202010842275A CN112077278B CN 112077278 B CN112077278 B CN 112077278B CN 202010842275 A CN202010842275 A CN 202010842275A CN 112077278 B CN112077278 B CN 112077278B
Authority
CN
China
Prior art keywords
shaped
wheel
pouring
special
casting
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Active
Application number
CN202010842275.5A
Other languages
Chinese (zh)
Other versions
CN112077278A (en
Inventor
张虎
张花蕊
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Beihang University
Original Assignee
Beihang University
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Beihang University filed Critical Beihang University
Priority to CN202010842275.5A priority Critical patent/CN112077278B/en
Publication of CN112077278A publication Critical patent/CN112077278A/en
Application granted granted Critical
Publication of CN112077278B publication Critical patent/CN112077278B/en
Active legal-status Critical Current
Anticipated expiration legal-status Critical

Abstract

本发明公开了一种适用于多升液管边注的异形浇口套,所述异形浇注组件在车轮模具轮辋正下方的位置与模具的型腔入口相连通,包括浇口杯和异形浇口套,所述异形浇口套的上口为异形口,并且内表面构成与模具型腔连通的进液通道,所述进液通道大致与铸型在此充型处的型腔入口形状随形,所述浇口杯的下口与升液管连通。本发明的异形浇口套可以应用于浇口设置在车轮的轮辋正下方的多升液管边注方式,在凝固结束从车轮的轮辋正下方位置对金属熔体进行补缩加压,可使金属熔体的充型距离相比现有阶段显著缩短,解决了大尺寸车轮的长距离补缩难题,显著提高了冷却强度和车轮的机械性能。

The present invention discloses a special-shaped sprue sleeve suitable for multi-liter liquid pipe side injection, wherein the special-shaped pouring component is connected to the mold cavity entrance at a position directly below the wheel mold rim, and comprises a pouring cup and a special-shaped sprue sleeve, wherein the upper opening of the special-shaped sprue sleeve is a special-shaped opening, and the inner surface forms a liquid inlet channel connected to the mold cavity, wherein the liquid inlet channel is roughly in the shape of the mold cavity entrance at this filling position of the casting, and the lower opening of the pouring cup is connected to the liquid riser. The special-shaped sprue sleeve of the present invention can be applied to the multi-liter liquid pipe side injection method in which the gate is set directly below the wheel rim, and the metal melt is fed and pressurized from the position directly below the wheel rim at the end of solidification, which can significantly shorten the filling distance of the metal melt compared to the existing stage, solve the problem of long-distance feeding of large-sized wheels, and significantly improve the cooling intensity and mechanical properties of the wheel.

Description

一种适用于多升液管边注的浇注组件A pouring assembly suitable for side pouring of multi-liter liquid pipes

技术领域Technical Field

本发明涉及铸造技术领域,尤其是涉及一种适用于多升液管边注的异形浇注组件。The invention relates to the technical field of casting, in particular to a special-shaped casting component suitable for edge pouring of a multi-liter liquid pipe.

背景技术Background Art

轻量化是燃油汽车节能减排、新能源汽车降耗增程的最重要途径之一,以铝合金等轻量化材料代替传统的钢铁材料,已成为汽车设计更新换代的必然选择。用于汽车上的铝合金可分为铸造铝合金和变形铝合金,铸造铝合金主要用于制造发动机、离合器壳体、车轮、底盘件等零部件。随着对铸件质量提升的需求和铸造技术的发展,更多的零部件采用低压铸造、差压铸造及调压铸造的方式来生产,均属于反重力铸造方法。该种铸造基本原理是用低压气体驱动坩埚或保温炉内的金属熔体,使其通过升液管上升并进入模具型腔,充型结束后铸型内金属熔体完成在压力作用下的凝固和补缩。Lightweighting is one of the most important ways to save energy and reduce emissions for fuel vehicles and to reduce consumption and increase range for new energy vehicles. Replacing traditional steel materials with lightweight materials such as aluminum alloys has become an inevitable choice for the renewal of automobile design. Aluminum alloys used in automobiles can be divided into cast aluminum alloys and deformed aluminum alloys. Cast aluminum alloys are mainly used to manufacture components such as engines, clutch housings, wheels, and chassis parts. With the demand for improved casting quality and the development of casting technology, more parts are produced by low-pressure casting, differential pressure casting, and pressure-regulated casting, all of which belong to anti-gravity casting methods. The basic principle of this type of casting is to use low-pressure gas to drive the molten metal in the crucible or holding furnace, so that it rises through the riser and enters the mold cavity. After the filling is completed, the molten metal in the mold completes solidification and shrinkage compensation under pressure.

传统的铝合金低压、差压及调压车轮铸造技术通常采用单浇口的单升液管充型技术。以铝合金车轮为例,在车轮的中央位置即车轮的轮心位置设置升液管,使金属熔体进入型腔并完成充型与凝固,该方法设计简单,易于实现,但缺点在于充型距离长,成型困难,为避免产生冷隔,车轮金属型模具温度一般高达400℃以上,导致车轮冷却速度低,组织粗大,并容易在热节部位形成缩孔缩松等铸造缺陷。为了细化组织、消除缩孔缩松等铸造缺陷,现有技术中一般采用水冷、水雾冷等方式加强车轮模具的冷却,然而,加强冷却使车轮凝固时间大为缩短,如加强冷却后的大尺寸车轮的凝固时间可以缩短到100s以内,但同时又引起生产过程中对车轮冷却和凝固过程的温度场难以控制的问题,导致难以实现顺序凝固,产品性能不稳定,合格率低。Traditional aluminum alloy low-pressure, differential pressure and pressure-regulated wheel casting technology usually adopts a single-gate single-riser tube filling technology. Taking aluminum alloy wheels as an example, a riser tube is set at the center of the wheel, that is, the wheel center position of the wheel, so that the metal melt enters the mold cavity and completes the filling and solidification. This method is simple in design and easy to implement, but the disadvantages are that the filling distance is long and the molding is difficult. In order to avoid cold shut, the temperature of the wheel metal mold is generally as high as 400°C or above, resulting in a low cooling rate of the wheel, coarse structure, and easy formation of shrinkage cavities and shrinkage in the hot joints. Casting defects such as shrinkage cavities and shrinkage are easy to form. In order to refine the structure and eliminate casting defects such as shrinkage cavities and shrinkage, water cooling, water mist cooling and other methods are generally used in the prior art to strengthen the cooling of the wheel mold. However, strengthening the cooling greatly shortens the solidification time of the wheel. For example, the solidification time of a large-size wheel after strengthening cooling can be shortened to less than 100s, but at the same time, it causes the problem of difficulty in controlling the temperature field of the wheel cooling and solidification process during the production process, resulting in difficulty in achieving sequential solidification, unstable product performance, and low pass rate.

车轮现有技术中已有其它充型方式的尝试。专利CN201010107026.8公开了一种铝合金车轮低压铸造双边浇工艺及装置,在车轮两侧设置浇口,使铝液从轮辋处进入,通过对冷却控制使铝液在急冷的模具温度下由轮心向轮辋进行结晶,缩短了铝液流动的距离,配合冷却,减少了R角或轮辋部位的缩松缺陷。专利CN201310557627.2、CN201410825962.0等文献公开了采用中心浇口和两侧浇口结合的方式,以期望能减轻轮毂的重量,提高机械强度。 CN201610390494.8采用一机双模轮毂模具,浇口同样设置在轮辋位置上,实现一次浇注两个轮毂。There have been attempts at other filling methods in the prior art of wheels. Patent CN201010107026.8 discloses a low-pressure casting double-sided pouring process and device for aluminum alloy wheels. Gates are set on both sides of the wheel to allow molten aluminum to enter from the rim. By controlling the cooling, the molten aluminum crystallizes from the wheel center to the rim at the rapidly cooled mold temperature, shortening the distance the molten aluminum flows. Combined with cooling, shrinkage defects at the R angle or rim area are reduced. Patents CN201310557627.2, CN201410825962.0 and other documents disclose the use of a combination of a central gate and a gate on both sides in the hope of reducing the weight of the hub and improving the mechanical strength. CN201610390494.8 uses a one-machine dual-mold hub mold, and the gate is also set at the rim position to achieve one-time casting of two hubs.

但上述装置和方法同样存在明显的缺陷,对于铝液仅从轮辋处进入的方式,入口设在轮辋中部,进入后会导致分流,即同时向轮心处和轮缘处充型,造成各处的充型时间不可控,进而造成凝固顺序不可控,容易形成缩孔缩松缺陷。而对于采用中心浇口和两侧浇口结合的方式,由于铝液从两个入口进入,在中间位置会形成汇流,容易因气体排出不顺等原因造成冷隔等。However, the above-mentioned device and method also have obvious defects. For the method in which the aluminum liquid enters only from the rim, the inlet is set in the middle of the rim, which will cause diversion after entering, that is, filling the wheel center and the wheel rim at the same time, resulting in uncontrollable filling time at each location, and then uncontrollable solidification sequence, which is easy to form shrinkage defects. For the method of combining the central gate and the gate on both sides, since the aluminum liquid enters from two inlets, it will form a convergence in the middle position, which is easy to cause cold shut due to reasons such as poor gas discharge.

本申请人设计了一种基于多升液管的快速顺序凝固车轮成型装置与方法,模具的浇口设置在车轮的轮辋正下方或下轮缘的上方R角外侧。通过在多个升液管升液充型,解决了此处充型后长距离补缩问题。但由于浇口的位置和形状发生了变化,因而,无法再采用传统的圆形浇注组件进行充型,如何实现在该方式下的稳定充型,成为一个亟待解决的问题。The applicant has designed a rapid sequential solidification wheel molding device and method based on multiple riser tubes, in which the gate of the mold is set just below the wheel rim or outside the R angle above the lower rim. By filling the mold with liquid in multiple riser tubes, the problem of long-distance shrinkage compensation after filling is solved. However, due to the change in the position and shape of the gate, it is no longer possible to use the traditional circular casting assembly for filling. How to achieve stable filling in this way has become a problem to be solved urgently.

发明内容Summary of the invention

为解决上述技术问题,本发明提供了一种适用于多升液管边注的异形浇注组件。In order to solve the above technical problems, the present invention provides a special-shaped casting component suitable for edge casting of multi-liter liquid pipes.

本发明完整的技术方案包括:The complete technical solution of the present invention includes:

一种适用于多升液管边注的异形浇注组件,其特征在于,所述异形浇注组件在车轮模具轮辋正下方的位置与模具的型腔入口相连通,包括浇口杯和异形浇口套,所述异形浇口套的上口为异形口,并且内表面构成与模具型腔连通的进液通道,所述进液通道大致与铸型在此充型处的型腔入口形状随形,所述浇口杯的下口与升液管连通。A special-shaped casting component suitable for side casting with multiple riser tubes, characterized in that the special-shaped casting component is connected to the cavity entrance of the mold at a position directly below the rim of the wheel mold, and includes a pouring cup and a special-shaped pouring sleeve. The upper opening of the special-shaped pouring sleeve is a special-shaped opening, and the inner surface constitutes a liquid inlet channel connected to the mold cavity. The liquid inlet channel is roughly the same shape as the cavity entrance of the casting at this filling point, and the lower opening of the pouring cup is connected to the riser tube.

所述进液通道的截面形状为:包括第一弧形段和第二弧形段,第一弧形段和第二弧形段同心,且第一弧形段的半径和尺寸均小于第二弧形段,第一弧形段和第二弧形段两侧通过连接段连接。The cross-sectional shape of the liquid inlet channel is: including a first arc segment and a second arc segment, the first arc segment and the second arc segment are concentric, and the radius and size of the first arc segment are smaller than the second arc segment, and the first arc segment and the second arc segment are connected on both sides by a connecting segment.

所述浇口套的上口内设有用于放网槽,用以放置过滤网。A net placing groove is provided in the upper opening of the sprue sleeve for placing the filter net.

所述异形浇口套和浇口杯通过台阶部实现定位安装。异形浇注组件数量为两个,在相对车轮轴线的两侧对称设置。The special-shaped pouring sleeve and pouring cup are positioned and installed through the step portion. There are two special-shaped pouring components, which are symmetrically arranged on both sides relative to the wheel axis.

异形浇注组件数量大于两个,环绕车轮轴线设置。The number of the special-shaped casting components is greater than two and they are arranged around the wheel axis.

本发明相对于现有技术的优点在于:The advantages of the present invention over the prior art are:

本申请人提出的基于多升液管的快速顺序凝固车轮成型装置与方法,模具的浇口设置在车轮的轮辋正下方。通过在多个升液管升液充型,使金属熔体的充型距离相比现有单升液管模式缩短一半以上,金属型模具温度可以由现有的420℃降低到320℃以下,自然地加快了车轮冷却速度与冷却效果,实现了快速顺序凝固。由于浇口的位置和形状发生了变化,因而,无法再采用传统的圆形浇注组件进行充型。本发明设计的异形浇注组件,适应于浇口设置在车轮的轮辋正下方的多升液管边注方式,所设计的放网槽,可以放置随形的过滤网,同时内表面的进液通道大于浇口,使过滤网可以被压实在浇口下方。配合多升液管边注方式使用,可使金属熔体的充型距离相比现有阶段缩短一半以上,打破了现有的大尺寸车轮长距离补缩困难的难题。同时进一步缩短了凝固时间,显著提高了生产效率和车轮的力学性能。通过优化后的两段式充型加压工艺设计,使初期充型的金属熔体流动平稳,随后快速充满型腔,发挥了多升液管充型迅速的优势,提高了生产效率。The present applicant proposes a rapid sequential solidification wheel forming device and method based on a multi-lift liquid tube, in which the gate of the mold is set directly below the rim of the wheel. By filling the mold with liquid in multiple lift liquid tubes, the filling distance of the metal melt is shortened by more than half compared with the existing single lift liquid tube mode, and the temperature of the metal mold can be reduced from the existing 420°C to below 320°C, which naturally accelerates the cooling speed and cooling effect of the wheel and achieves rapid sequential solidification. Since the position and shape of the gate have changed, the traditional circular casting component can no longer be used for filling. The special-shaped casting component designed by the present invention is suitable for the multi-lift liquid tube side injection method in which the gate is set directly below the rim of the wheel. The designed net placing groove can place a conforming filter net, and the liquid inlet channel on the inner surface is larger than the gate, so that the filter net can be compacted under the gate. Used in conjunction with the multi-lift liquid tube side injection method, the filling distance of the metal melt can be shortened by more than half compared with the existing stage, breaking the problem of the difficulty of long-distance shrinkage compensation of existing large-sized wheels. At the same time, the solidification time is further shortened, and the production efficiency and the mechanical properties of the wheel are significantly improved. Through the optimized two-stage filling and pressurizing process design, the metal melt flows smoothly in the initial filling and then quickly fills the cavity, giving full play to the advantage of rapid filling of multi-liter liquid tubes and improving production efficiency.

附图说明BRIEF DESCRIPTION OF THE DRAWINGS

图1为异形浇注组件的结构示意图。FIG. 1 is a schematic diagram of the structure of a special-shaped casting component.

图2为浇注组件浇口套的进液通道横截面图。FIG. 2 is a cross-sectional view of the liquid inlet channel of the pouring assembly sprue sleeve.

图3为现有技术中的车轮结构示意图。FIG. 3 is a schematic diagram of a wheel structure in the prior art.

图4为与本发明异形浇注组件相配套的车轮成型装置结构示意图。FIG. 4 is a schematic diagram of the structure of a wheel forming device matched with the special-shaped casting assembly of the present invention.

图5a为图4装置充型过程中的易发生卷气部位。FIG. 5 a shows a portion of the device of FIG. 4 that is prone to air entrainment during the filling process.

图5b为图5a的局部放大图。FIG. 5 b is a partial enlarged view of FIG. 5 a .

图5c为图5a处在慢速充型时的充型顺序示意图。FIG. 5c is a schematic diagram of the filling sequence of FIG. 5a during slow filling.

具体实施方式DETAILED DESCRIPTION

下面结合附图和具体实施方式对本发明做进一步说明。The present invention will be further described below in conjunction with the accompanying drawings and specific embodiments.

如图1所示,本发明的该浇注组件包括浇口杯1和异形浇口套2,异形浇口套和浇口杯通过台阶部3实现定位安装,浇口套的外壁4和浇口杯内壁之间留有一定的安装余量,浇口套的下口与浇口杯的上口连通,浇口套的上口5为异形口,并且与模具型腔连通,浇口套的上口开设有放网槽6,用以放置过滤网7,所述浇口杯的下口8与升液管相连通。As shown in Figure 1, the casting assembly of the present invention includes a pouring cup 1 and a special-shaped pouring sleeve 2. The special-shaped pouring sleeve and the pouring cup are positioned and installed through a step portion 3. A certain installation margin is left between the outer wall 4 of the pouring sleeve and the inner wall of the pouring cup. The lower opening of the pouring sleeve is connected with the upper opening of the pouring cup. The upper opening 5 of the pouring sleeve is a special-shaped opening and is connected with the mold cavity. The upper opening of the pouring sleeve is provided with a net placing groove 6 for placing a filter net 7. The lower opening 8 of the pouring cup is connected with the liquid riser.

所述浇口套内表面构成的进液通道,大致是与铸型在此充型处的型腔浇口形状随形,具体的,其截面形状包括第一弧形段9和第二弧形段10,第一弧形段和第二弧形段同心,且第一弧形段的半径和尺寸均小于第二弧形段。第一弧形段和第二弧形段两侧通过连接段11连接。The liquid inlet channel formed by the inner surface of the gate sleeve is roughly in the shape of the cavity gate of the casting mold at this filling position. Specifically, its cross-sectional shape includes a first arc segment 9 and a second arc segment 10. The first arc segment and the second arc segment are concentric, and the radius and size of the first arc segment are smaller than the second arc segment. The first arc segment and the second arc segment are connected on both sides by a connecting segment 11.

在一种优选的实施方式中,该过滤网的截面形状与进液通道相同。In a preferred embodiment, the cross-sectional shape of the filter screen is the same as that of the liquid inlet channel.

在一种优选的实施方式中,第一弧形段的长度为76mm,第二弧形段的长度为80mm,两侧连接段的长度为10mm。In a preferred embodiment, the length of the first arc segment is 76 mm, the length of the second arc segment is 80 mm, and the length of the connecting segments on both sides is 10 mm.

下面对与本发明异形浇注组件相配套使用的车轮成型装置,以及配套工艺进行说明。The following is a description of the wheel forming device used in conjunction with the special-shaped casting assembly of the present invention, and the supporting process.

图3为一个典型的车轮构造图,其中在现有技术中,通常将车轮的中央位置称为轮心,在车轮外侧,与轮胎装配配合,支撑轮胎的部分称为轮辋,与车轴轮心实施安装连接,并支撑轮辋的车轮部分称为轮辐,多个轮辐中间留有窗口。保持并支撑轮胎方向的轮辋部分称为轮缘。Figure 3 is a typical wheel structure diagram, in which in the prior art, the center of the wheel is usually called the wheel center, the part on the outside of the wheel that is assembled with the tire and supports the tire is called the rim, the wheel part that is installed and connected to the axle wheel center and supports the rim is called the spoke, and windows are left in the middle of the multiple spokes. The rim part that maintains and supports the direction of the tire is called the flange.

现有的低压或差压铸造铝合金车轮生产中,几乎全部采用在在车轮的中央轮心位置设置升液管,并使熔体通过连接在升液管上的保温杯和浇注组件,由轮心处的浇口进入型腔,在分流锥的作用下进行分流,并沿着轮心-轮辐-轮辋-轮缘的顺序依次充型,充满型腔后实现凝固,这是由于在实际生产中,在此处设置浇口和升液管最为容易实现,且浇口的截面形状为规则的圆形,加工简单。同时浇口的面积大,可以使充型速度快。但是上述浇注充型方式带来的一些问题始终无法很好解决,如浇口距离远,充型距离过长,在轮辋与轮辐连接等热节部位非常难以补缩,容易形成缩孔缩松,成为困扰车轮行业生产的一大难题。虽然采用对该处采用水冷、水雾冷等方式加强冷却,以期望实现顺序凝固,但是由于车轮充型和凝固时间短,难以对温度场进行精确控制,仍然不可避免的会产生相当比例的废品。In the existing production of low-pressure or differential-pressure cast aluminum alloy wheels, almost all of them use a riser pipe set at the central wheel center position of the wheel, and allow the melt to pass through the insulation cup and pouring assembly connected to the riser pipe, enter the mold cavity from the gate at the wheel center, and be diverted under the action of the diverter cone, and fill the mold in the order of wheel center-spoke-rim-rim, and solidify after filling the mold cavity. This is because in actual production, it is easiest to set the gate and riser pipe here, and the cross-sectional shape of the gate is a regular circle, which is simple to process. At the same time, the area of the gate is large, which can make the filling speed fast. However, some problems caused by the above-mentioned pouring and filling method have never been well solved, such as the long gate distance, the long filling distance, and it is very difficult to compensate for shrinkage at the hot joints such as the connection between the rim and the spoke, which is easy to form shrinkage cavities and shrinkage, becoming a major problem that plagues the production of the wheel industry. Although water cooling, water mist cooling and other methods are used to enhance cooling in order to achieve sequential solidification, the short filling and solidification time of the wheel makes it difficult to accurately control the temperature field, and a considerable proportion of scrap is still inevitable.

而现有技术中采用在轮辋侧面中部位置进行双边浇注的方式,同样由于充型分流导致的充型和凝固顺序不可控也非常容易形成缩孔缩松缺陷。In the prior art, bilateral pouring is performed at the middle of the rim side. However, the filling and solidification sequence is uncontrollable due to the filling diversion, which also easily leads to shrinkage defects.

基于此问题,本发明提出了一种与前述异形浇注组件配套所适用的,基于多升液通道的车轮成型装置,如图4所示,包括盛有铝液的保温炉12,保温炉内连接有高压气源,保温炉内设有多个升液管13,该多个升液管的下部浸入铝液14中。在采用高压气源对炉内的铝液进行加压时,铝液可以沿着多个升液管上升。升液管上方通过保温杯和本发明公开的异形浇注组件15与模具的浇口连接,并进入模具的型腔16。Based on this problem, the present invention proposes a wheel forming device based on multiple liquid riser channels, which is suitable for matching with the above-mentioned special-shaped casting component, as shown in FIG4 , including a heat preservation furnace 12 containing aluminum liquid, a high-pressure gas source is connected to the heat preservation furnace, and multiple liquid risers 13 are arranged in the heat preservation furnace, and the lower parts of the multiple liquid risers are immersed in the aluminum liquid 14. When the aluminum liquid in the furnace is pressurized by the high-pressure gas source, the aluminum liquid can rise along the multiple liquid risers. The upper part of the liquid riser is connected to the gate of the mold through a thermos cup and the special-shaped casting component 15 disclosed in the present invention, and enters the mold cavity 16 of the mold.

模具的浇口,设置在车轮的轮辋正下方的圆环面上,特别说明的,本发明中所述“轮辋正下方的圆环面”是指轮辋上与轮缘相对的一侧,环绕车轮中心轴线所形成的圆环面。构成该圆环的外圆是该面上车轮最外圈轮廓线所构成的圆,内圆是车轮的窗口区外侧轮廓线围绕车轮中心轴线所构成的圆。如图3所示。对应的,浇注组件与模具相连通的位置同样设置在该处。The gate of the mold is set on the annular surface directly below the rim of the wheel. It is particularly noted that the "annular surface directly below the rim" in the present invention refers to the annular surface formed on the side of the rim opposite to the wheel flange, surrounding the center axis of the wheel. The outer circle of the annular ring is the circle formed by the outermost contour line of the wheel on the surface, and the inner circle is the circle formed by the outer contour line of the window area of the wheel around the center axis of the wheel. As shown in Figure 3. Correspondingly, the position where the casting assembly is connected to the mold is also set at this place.

尤其优选的是,该浇口和浇注组件可以设置在该圆环面上对应窗口区外侧的位置,也可以设置于该圆环面上对应轮辋与轮辐连接的位置。Particularly preferably, the gate and the casting assembly can be arranged at a position on the annular surface corresponding to the outer side of the window area, or at a position on the annular surface corresponding to the connection between the rim and the spoke.

在一种优选的实施方式中,该浇口可以设置为两个,可在车轮两侧对称设置,也可以为环绕车轮轴线设置多个浇口。与该浇口相对应的,升液管可以设置为两个,可在车轮两侧对称设置,也可以为环绕车轮轴线设置多个升液管。In a preferred embodiment, the gate can be provided with two, which can be symmetrically arranged on both sides of the wheel, or multiple gates can be arranged around the wheel axis. Corresponding to the gate, the riser can be provided with two, which can be symmetrically arranged on both sides of the wheel, or multiple riser can be arranged around the wheel axis.

还包括在模具上对应车轮的轮心位置下方,设置的局部加压装置,以促进轮心位置处的补缩,该局部加压装置包括压力驱动机构17、压力传递机构和压力施加机构18,压力施加机构19与金属熔体接触,并在充型结束后对金属熔体施加压力。It also includes a local pressurizing device arranged below the wheel center position corresponding to the wheel on the mold to promote shrinkage compensation at the wheel center position. The local pressurizing device includes a pressure driving mechanism 17, a pressure transmission mechanism and a pressure applying mechanism 18. The pressure applying mechanism 19 contacts the metal melt and applies pressure to the metal melt after filling is completed.

尤其是,该压力驱动机构可以为液压油缸,压力传递机构可以为液压杆,压力施加机构可以为压力块。具体的加压工艺为在充型结束后施加1000KPa~12000KPa的机械压力。使此处的铝液在极高压下进行凝固,防止由于边缘补缩压力不够而在此处形成缩孔缩松缺陷。In particular, the pressure driving mechanism may be a hydraulic cylinder, the pressure transmission mechanism may be a hydraulic rod, and the pressure applying mechanism may be a pressure block. The specific pressurization process is to apply a mechanical pressure of 1000KPa to 12000KPa after the filling is completed. The aluminum liquid here is solidified under extremely high pressure to prevent shrinkage cavities and shrinkage defects from forming here due to insufficient edge shrinkage pressure.

还可以在车轮模具,对应车轮轮心的位置上方,即对应于传统中心底注充型方式的分流锥处,设置的一个细化装置,该细化机构可以为超声细化机构或振动细化机构。如包括振动发生器20和振动杆21,振动杆21探入铝液中,在凝固过程中对铝液进行振动,使铝液结晶形成的枝晶被打破,增强形核,以细化晶粒,提高车轮的机械性能。A refinement device may also be provided above the wheel mold corresponding to the position of the wheel center, that is, corresponding to the diverter cone of the traditional center bottom injection molding method. The refinement mechanism may be an ultrasonic refinement mechanism or a vibration refinement mechanism. For example, the refinement device may include a vibration generator 20 and a vibration rod 21. The vibration rod 21 is inserted into the aluminum liquid to vibrate the aluminum liquid during the solidification process, so that the dendrites formed by the aluminum liquid crystallization are broken, the nucleation is enhanced, the grains are refined, and the mechanical properties of the wheel are improved.

本发明同时公开了一种适应于该充型方式下的低压/差压铸造工艺,由于本发明的浇注充型方式相对于现有技术做了巨大的变化,原有的充型方式和凝固工艺无法适用于本发明,基于此,本发明同时设计了一种适合该充型位置的工艺。The present invention also discloses a low-pressure/differential pressure casting process suitable for the filling mode. Since the pouring and filling method of the present invention has undergone tremendous changes compared with the prior art, the original filling method and solidification process cannot be applied to the present invention. Based on this, the present invention also designs a process suitable for the filling position.

具体包括如下步骤:The specific steps include:

(1)升液:通过高压气源对保温炉内的铝液进行加压,使铝液在压力下沿着升液管上升到浇口位置,该阶段升压速度为2.8~4.0KPa/s,将压力增加到20KPa;(1) Liquor lifting: The aluminum liquid in the holding furnace is pressurized by a high-pressure gas source, so that the aluminum liquid rises to the pouring gate position along the liquid riser under pressure. The pressure raising speed in this stage is 2.8-4.0 KPa/s, and the pressure is increased to 20 KPa;

(2)充型:继续升压,使铝液通过浇口进入型腔,该充型阶段为两段式加压,第一阶段升压速度为0.1~0.2KPa/s,时间为2~4s,随后进入第二阶段快速升压,直至将型腔充满,此时压力达到35KPa;(2) Filling: Continue to increase the pressure to allow the aluminum liquid to enter the mold cavity through the gate. This filling stage is a two-stage pressurization. The pressure increase rate in the first stage is 0.1-0.2 KPa/s for 2-4 seconds. Then enter the second stage to increase the pressure rapidly until the mold cavity is filled. At this time, the pressure reaches 35 KPa.

该第二阶段的升压速度P′由如下方式确定:The pressure increase speed P' of the second stage is determined as follows:

式中:Where:

P′为升压速度,单位为kPa/s;H为型腔总高度,单位为mm;ρ为金属熔体密度,单位为g/cm3;K为阻力系数,其取值范围为1~1.5;t为预设充型时间,单位为s,优选取10s;102为单位换算系数;N为升液管数量,其取值范围为2~6,可根据不同型号车轮的窗口数量进行选择,优选取2~4;x为其升液指数,取值范围为0.2~0.8,在本实施方式所采用轮型的方案中,取值选0.5。P' is the pressure increase rate, in kPa/s; H is the total height of the cavity, in mm; ρ is the metal melt density, in g/ cm3 ; K is the resistance coefficient, in the range of 1 to 1.5; t is the preset filling time, in seconds, preferably 10 seconds; 102 is the unit conversion coefficient; N is the number of liquid riser tubes, in the range of 2 to 6, which can be selected according to the number of windows of different types of wheels, preferably 2 to 4; x is the liquid rise index, in the range of 0.2 to 0.8, and in the wheel type scheme adopted in this embodiment, the value is 0.5.

(3)结晶增压保压:充型结束后,以8~10KPa/的升压速度将压力快速增加到150KPa,并保压60~150s,此时车轮凝固完成。(3) Crystallization pressurization and pressure holding: After filling is completed, the pressure is rapidly increased to 150 KPa at a pressure increase rate of 8 to 10 KPa/, and the pressure is maintained for 60 to 150 seconds. At this time, the wheel solidification is completed.

(4)卸压放气:铝合金车轮凝固完毕,解除保温炉内的气体压力,使升液管和浇道口未凝固的铝液流回到保温炉中。(4) Depressurization and venting: After the aluminum alloy wheel has solidified, the gas pressure in the holding furnace is released, allowing the unsolidified aluminum liquid in the riser and pouring nozzle to flow back into the holding furnace.

对于升液阶段和充型阶段的升压速度选择,由于在升液时,升液管的内径固定,基本不会产生紊流,所以采用快速的升压速度,使金属熔体能快速升液达到浇口位置,缩短升液时间。而在充型阶段,则要考虑到型腔和浇口的复杂形状,在传统的充型方式中,由于采用从轮心位置进行浇注的方式,升液管和浇口的截面积相差不大,且轮心处的型腔截面积大,不易产生紊流,因此可以采用经验或者试验得到充型升压速度。而对于本发明的充型方式,采用在轮辋圆环面上进行充型,为不规则随形浇口,升液管和浇口的形状面积差距很大,同时轮辋处的空间较小,如充型压力不合理极易产生紊流卷气,造成气孔缺陷。而现有技术中的充型压力设计均采用理想状态下的计算方式,结合阻力系数等进行修正。没有考虑到升液管和浇口的截面积变化造成的流动状态变化。因此无法采用现有技术中的经验式得到理想的充型升压速度。As for the selection of the pressure increasing speed in the liquid raising stage and the mold filling stage, since the inner diameter of the liquid raising pipe is fixed during the liquid raising, turbulence will basically not be generated, so a fast pressure increasing speed is adopted so that the metal melt can be quickly raised to the gate position and the liquid raising time is shortened. In the mold filling stage, the complex shapes of the mold cavity and the gate must be taken into consideration. In the traditional mold filling method, since the method of pouring from the wheel center position is adopted, the cross-sectional area of the liquid raising pipe and the gate is not much different, and the cross-sectional area of the mold cavity at the wheel center is large, and turbulence is not easy to be generated. Therefore, the filling pressure increasing speed can be obtained by experience or experiment. For the mold filling method of the present invention, the mold filling is carried out on the annular surface of the rim, which is an irregular conformal gate. The shape area of the liquid raising pipe and the gate is very different. At the same time, the space at the rim is small. If the filling pressure is unreasonable, turbulent air is easily generated, resulting in pore defects. The filling pressure design in the prior art adopts the calculation method under the ideal state, combined with the resistance coefficient, etc. for correction. The flow state change caused by the change of the cross-sectional area of the liquid raising pipe and the gate is not considered. Therefore, it is impossible to obtain the ideal filling and pressurizing speed by using the empirical formula in the prior art.

因此,本发明对上述问题进行了研究,结合升液管、浇口、浇口上方型腔形状与截面积,以及金属熔体的流动特性。发现对于车轮轮辋位置,如图5a中箭头所示的圆框处,在充型的最初阶段存在两个面积发生明显变化的部位,如图5b中箭头所示的圆框处,如果产生紊流,该位置处极易形成卷气,经过设计和计算,本发明采用两段式加压,第一阶段明显地降低升压速度,使金属熔体在充型最初阶段实现平稳流动,充满上述区域以避免卷气,如图5c所示 (此处箭头为熔体充型方向),随后进入第二阶段快速升压以缩短充型时间。在本发明第二阶段的充型过程中,研究发现充型稳定性与升液管数量与明显关系,因为传统的从轮心位置进行浇注的方式仅有一个升液管和浇口,因此通过试验即可得到规律并做定量处理。而本发明的充型方式,升液管和浇口数量可以为2个或更多。同样升压条件下,在浇口处流速、在浇口上方型腔内的流速均会发生明显变化,从而导致充型流动方式不可控。因此本发明通过研究,得到第二阶段的升压方式,从公式(1)中可以看出,在相同的预设充型时间内,随着升液管数量增加,其可采用的升压速度可以逐步增大,并且不会造成紊流卷气等问题。阻力系数取值与金属液粘度、铸型型腔复杂度等有关,阻力小时取下限,阻力大时取上限。Therefore, the present invention has studied the above-mentioned problems, combining the riser, gate, the shape and cross-sectional area of the cavity above the gate, and the flow characteristics of the metal melt. It is found that for the wheel rim position, such as the circular frame shown by the arrow in Figure 5a, there are two locations where the area changes significantly in the initial stage of filling, such as the circular frame shown by the arrow in Figure 5b. If turbulence occurs, air entrainment is very likely to form at this location. After design and calculation, the present invention adopts a two-stage pressurization. The first stage significantly reduces the pressurization speed, so that the metal melt can achieve a smooth flow in the initial stage of filling, fill the above area to avoid air entrainment, as shown in Figure 5c (the arrow here is the melt filling direction), and then enters the second stage of rapid pressurization to shorten the filling time. In the second stage of the filling process of the present invention, it is found that the filling stability is significantly related to the number of riser tubes, because the traditional method of pouring from the wheel center position has only one riser and gate, so the law can be obtained through experiments and quantitative processing can be performed. In the filling method of the present invention, the number of riser tubes and gates can be 2 or more. Under the same boosting condition, the flow rate at the gate and the flow rate in the cavity above the gate will change significantly, resulting in uncontrollable filling flow mode. Therefore, the present invention obtains the boosting mode of the second stage through research. It can be seen from formula (1) that within the same preset filling time, as the number of riser pipes increases, the boosting speed that can be adopted can be gradually increased, and will not cause turbulent air entrainment and other problems. The value of the resistance coefficient is related to the viscosity of the molten metal, the complexity of the casting cavity, etc. When the resistance is small, the lower limit is taken, and when the resistance is large, the upper limit is taken.

实施例1:Embodiment 1:

采用2个升液管和浇口,所用金属熔体质量百分比组成如下:Si:7~9%,Mg:0.6~0.9%, Zr:0.01~0.02%,B:0.005~0.007%,RE:0.002~0.005%,Nd:0.002~0.005%,Fe:0~0.15%, Mn:0.05~0.1%,Ti:0.12~0.14%,其余为Al和不可避免的杂质。Two riser tubes and pouring gates are used, and the mass percentage composition of the metal melt used is as follows: Si: 7-9%, Mg: 0.6-0.9%, Zr: 0.01-0.02%, B: 0.005-0.007%, RE: 0.002-0.005%, Nd: 0.002-0.005%, Fe: 0-0.15%, Mn: 0.05-0.1%, Ti: 0.12-0.14%, and the rest is Al and unavoidable impurities.

(1)升液:通过高压气源对保温炉内的铝液进行加压,使铝液在压力下沿着升液管上升到浇口位置,该阶段升压速度为3.5kPa/s,将压力增加到20KPa;(1) Liquor lifting: The aluminum liquid in the holding furnace is pressurized by a high-pressure gas source, so that the aluminum liquid rises to the pouring gate position along the liquid riser under pressure. The pressure raising speed in this stage is 3.5 kPa/s, and the pressure is increased to 20 kPa;

(2)充型:继续升压,使铝液通过浇口进入型腔,第一阶段升压速度为0.2KPa/s,时间为1.8s,使金属熔体平稳充满图5b箭头所示区域,随后进入第二阶段随后以 0.66KPa/s的升压速度快速充型,直至将型腔充满。(2) Filling: Continue to increase the pressure to allow the aluminum liquid to enter the mold cavity through the gate. The pressure increase rate in the first stage is 0.2 KPa/s, and the time is 1.8 s, so that the metal melt can smoothly fill the area indicated by the arrow in Figure 5b. Then enter the second stage and quickly fill the mold at a pressure increase rate of 0.66 KPa/s until the mold cavity is filled.

(3)结晶增压保压:充型结束后,以8KPa/s的升压速度将压力快速增加到150KPa,并保压,液压油缸带动液压杆驱动压力块对轮心位置处施加2000KPa的机械压力,振动发生器带动振动杆对铝液进行振动细化,直到车轮凝固完成。在保压过程中,在浇口处对一直保持轮辋热节的高压力补缩,在高压铝液的补缩下,完全消除了该处的缩孔缩松产生的可能性。同时压力块对轮心处金属液进行局部加压,消除了该处产生缩孔缩松的可能性。(3) Crystallization pressurization and pressure holding: After the filling is completed, the pressure is quickly increased to 150KPa at a pressure increase rate of 8KPa/s, and the pressure is maintained. The hydraulic cylinder drives the hydraulic rod to drive the pressure block to apply 2000KPa mechanical pressure to the wheel center position, and the vibration generator drives the vibration rod to vibrate and refine the aluminum liquid until the wheel solidifies. During the pressure holding process, the high pressure shrinkage of the rim hot section is maintained at the gate. Under the high-pressure aluminum liquid shrinkage, the possibility of shrinkage cavities and shrinkage at this location is completely eliminated. At the same time, the pressure block locally pressurizes the metal liquid at the wheel center, eliminating the possibility of shrinkage cavities and shrinkage at this location.

(4)卸压放气:铝合金车轮凝固完毕,解除保温炉内的气体压力,使升液管和浇道口未凝固的铝液流回到保温炉中。(4) Depressurization and venting: After the aluminum alloy wheel has solidified, the gas pressure in the holding furnace is released, allowing the unsolidified aluminum liquid in the riser and pouring nozzle to flow back into the holding furnace.

以上所述,仅是本发明的较佳实施例,并非对本发明作任何限制,凡是根据本发明技术实质对以上实施例所作的任何简单修改、变更以及等效结构变化,均仍属于本发明技术方案的保护范围内。The above description is only a preferred embodiment of the present invention and does not limit the present invention in any way. Any simple modification, change and equivalent structural change made to the above embodiment based on the technical essence of the present invention still falls within the protection scope of the technical solution of the present invention.

Claims (7)

1. The special-shaped pouring assembly suitable for side pouring of the multi-lift tube is characterized by comprising a pouring cup and a special-shaped pouring sleeve, wherein the upper opening of the special-shaped pouring sleeve is a special-shaped opening, the inner surface of the special-shaped pouring sleeve forms a liquid inlet channel communicated with a die cavity, the liquid inlet channel is conformal with the shape of a cavity inlet of a casting mold at the filling position, and the lower opening of the pouring cup is communicated with the lift tube;
The section shape of the liquid inlet channel is as follows: the device comprises a first arc-shaped section and a second arc-shaped section, wherein the first arc-shaped section and the second arc-shaped section are concentric, the radius and the size of the first arc-shaped section are smaller than those of the second arc-shaped section, and two sides of the first arc-shaped section and two sides of the second arc-shaped section are connected through a connecting section;
The special-shaped pouring assembly is communicated with a cavity inlet of the mold at a position right below a rim of the wheel mold, a pouring gate of the mold is arranged on a circular surface right below the rim of the wheel, and the circular surface right below the rim is a circular surface formed by encircling a central axis of the wheel on one side, opposite to the rim, of the rim; the outer circle forming the circular ring is a circle formed by the outline of the outermost ring of the wheel on the surface, and the inner circle is a circle formed by the outline of the outer side of the window area of the wheel around the central axis of the wheel;
The multi-lift tube side note includes:
(1) Lifting liquid: pressurizing the aluminum liquid in the heat preservation furnace by a high-pressure air source to enable the aluminum liquid to rise to a gate position along the liquid lifting pipe under pressure;
(2) Filling: continuously boosting, namely enabling the aluminum liquid to enter a cavity through a gate, wherein the mold filling stage is two-stage pressurization, the boosting speed in the first stage is 0.1-0.2 kPa/s, the time is 2-4 s, and then the second stage is performed to quickly boost until the cavity is full;
boost speed of the second stage Is determined by the following way:
(1)
wherein: The unit is kPa/s for the boosting speed; h is the total height of the cavity, and the unit is mm; The density of the metal melt is expressed as g/cm 3; Is a resistance coefficient, and the value range is 1-1.5; the unit is s for presetting the filling time; 102 is a unit conversion coefficient; n is the number of liquid lifting pipes, and the value range is 2-6; The value range of the liquid lifting index is 0.2-0.8;
(3) Crystallization pressurizing and pressure maintaining: after the filling is finished, the pressure is quickly increased to 150 kPa at the step-up speed of 8-10 kPa/s, and the pressure is maintained for 60-150 s, so that the solidification of the wheels is finished;
(4) Pressure relief and deflation: after the solidification of the aluminum alloy wheel is finished, the gas pressure in the heat preservation furnace is relieved, so that the aluminum liquid which is not solidified at the riser tube and the pouring gate flows back to the heat preservation furnace.
2. The special-shaped casting assembly suitable for side injection of a plurality of lift tubes according to claim 1, wherein a net discharging groove is arranged in an upper opening of the sprue bush for placing a filter net.
3. The profiled casting assembly of claim 2 wherein the cross-sectional shape of the drain and filter screen is the same as the inlet channel.
4. A shaped casting assembly for side casting of multiple lift tubes according to claim 1 or 2, wherein the shaped sprue bush and the sprue cup are positioned and mounted by a step.
5. A shaped casting assembly for use in a multi-riser edge casting according to claim 1 or 2, wherein the number of shaped casting assemblies is two and symmetrically disposed on opposite sides of the wheel axis.
6. A shaped casting assembly for use in a multi-riser edge casting as claimed in claim 1 wherein the number of shaped casting assemblies is greater than two and is disposed about the wheel axis.
7. The shaped casting assembly for side casting of multiple lift tubes according to claim 1, wherein the longitudinal section of the shaped sprue bush is semi-trapezoidal.
CN202010842275.5A 2020-08-20 2020-08-20 Pouring assembly suitable for side pouring of multiple lift tubes Active CN112077278B (en)