CN109750758A - 预制夹心保温剪力墙外墙横向缝和竖向缝的施工方法 - Google Patents

预制夹心保温剪力墙外墙横向缝和竖向缝的施工方法 Download PDF

Info

Publication number
CN109750758A
CN109750758A CN201711092770.3A CN201711092770A CN109750758A CN 109750758 A CN109750758 A CN 109750758A CN 201711092770 A CN201711092770 A CN 201711092770A CN 109750758 A CN109750758 A CN 109750758A
Authority
CN
China
Prior art keywords
seam
stitched
laterally
exterior wall
heat preservation
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Pending
Application number
CN201711092770.3A
Other languages
English (en)
Inventor
范振江
姚树国
丁楠
刘尊强
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Shanghai Baoye Group Corp Ltd
Original Assignee
Shanghai Baoye Group Corp Ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Shanghai Baoye Group Corp Ltd filed Critical Shanghai Baoye Group Corp Ltd
Priority to CN201711092770.3A priority Critical patent/CN109750758A/zh
Publication of CN109750758A publication Critical patent/CN109750758A/zh
Pending legal-status Critical Current

Abstract

本发明公开了一种预制夹心保温剪力墙外墙横向缝和竖向缝的施工方法,本方法首先校正吊装到位的构件水平和垂直度达到设计及规范要求;相邻构件竖向缝内侧黏贴自粘性橡胶皮并延伸至竖向缝两侧,橡胶皮外侧进行防水密封胶施工;相邻构件横向缝的胶条至构件内侧边缘的横向缝空间进行灌浆腔封堵作业,然后填塞PE棒,横向缝表面进行防水密封胶施工;对构件外墙立面进行涂料施工,采用聚合物水泥砂浆对横竖向缝的凹陷处进行填塞,待干燥后涂刷素水泥浆一道,横竖向缝表面覆盖耐碱玻纤网格布并延伸至缝的两侧,整个外墙立面刮防水外墙腻子,最后喷真石漆饰面层。本方法有效解决外墙渗漏及涂料开裂脱落问题,提高了外墙施工质量,达到美观耐用的目的。

Description

预制夹心保温剪力墙外墙横向缝和竖向缝的施工方法
技术领域
本发明涉及一种预制夹心保温剪力墙外墙横向缝和竖向缝的施工方法。
背景技术
随着装配式建筑的大力推广,混凝土预制件的装配率逐渐提升,然而预制夹心保温剪力墙外墙横向缝和竖向缝的处理已成为施工现场的一大难题,采用传统施工方式对横向缝和竖向缝处理易导致外墙渗漏及外墙涂料开裂脱落,使得外墙的施工存在严重的质量问题,且影响外墙整体的美观性能。传统外墙横向缝和竖向缝施工时,防水密封胶外侧无砂浆封堵,当夏、冬季温度骤变,防水密封胶会发生一定的膨胀和收缩,从而导致外侧腻子及网格布开裂或空鼓脱落,直接影响外墙立面质量。
发明内容
本发明所要解决的技术问题是提供一种预制夹心保温剪力墙外墙横向缝和竖向缝的施工方法,本方法克服传统外墙横向缝和竖向缝施工方式的缺陷,有效解决外墙渗漏及外墙涂料开裂脱落问题,提高了外墙施工质量,达到美观耐用的目的。
为解决上述技术问题,本发明预制夹心保温剪力墙外墙横向缝和竖向缝的施工方法包括如下步骤:
步骤一、将混凝土预制构件吊装到位,校正构件的水平和垂直度达到设计及规范要求;
步骤二、在相邻构件竖向缝内侧黏贴自粘性橡胶皮并延伸至竖向缝两侧,用于防止浇筑相邻构件之间的暗柱时混凝土浮浆及混凝土进入竖向缝内,橡胶皮外侧进行防水密封胶施工,使相邻构件可靠连接,防止渗漏;
步骤三、构件安装后,对相邻构件横向缝的胶条至构件内侧边缘的横向缝空间进行灌浆腔封堵作业,灌浆腔封闭前清理待封闭区域,然后用水湿润,采用座浆料对该横向缝空间进行封闭;
步骤四、相邻构件横向缝胶条外侧填塞PE棒,填塞前对横向缝进行打磨清理,清除油渍、浮浆及混凝土块,PE棒规格根据横向缝宽度选用、填塞深度根据防水密封胶厚度确定,横向缝表面进行防水密封胶施工并保证防水密封胶的厚度及密实度;
步骤五、对构件外墙立面进行涂料施工,要求外墙立面平整度不大于2mm,采用聚合物水泥砂浆对竖向缝和横向缝的凹陷处进行填塞,起到更好的与防水密封胶粘结的作用,待聚合物水泥砂浆干燥后涂刷素水泥浆一道,然后在竖向缝和横向缝表面覆盖耐碱玻纤网格布并延伸至缝的两侧,整个外墙立面刮防水外墙腻子,最后喷真石漆饰面层。
进一步,所述竖向缝内侧黏贴的自粘性橡胶皮宽度为100mm,并延伸至竖向缝两侧各40mm。
进一步,所述横向缝灌浆腔待封闭区域清除油渍、浮浆及混凝土渣块。
进一步,所述聚合物水泥砂浆和素水泥浆内掺入5%重量份的聚乙烯醇缩甲醛胶。
进一步,所述耐碱玻纤网格布的宽度为220mm并延伸至缝两侧各100mm。
由于本发明预制夹心保温剪力墙外墙横向缝和竖向缝的施工方法采用了上述技术方案,即本方法首先校正吊装到位的构件水平和垂直度达到设计及规范要求;相邻构件竖向缝内侧黏贴自粘性橡胶皮并延伸至竖向缝两侧,橡胶皮外侧进行防水密封胶施工;相邻构件横向缝的胶条至构件内侧边缘的横向缝空间进行灌浆腔封堵作业,然后填塞PE棒,横向缝表面进行防水密封胶施工;对构件外墙立面进行涂料施工,采用聚合物水泥砂浆对竖向缝和横向缝的凹陷处进行填塞,待聚合物水泥砂浆干燥后涂刷素水泥浆一道,然后在竖向缝和横向缝表面覆盖耐碱玻纤网格布并延伸至缝的两侧,整个外墙立面刮防水外墙腻子,最后喷真石漆饰面层。本方法克服传统外墙横向缝和竖向缝施工方式的缺陷,有效解决外墙渗漏及外墙涂料开裂脱落问题,提高了外墙施工质量,达到美观耐用的目的。
附图说明
下面结合附图和实施方式对本发明作进一步的详细说明:
图1为本方法横向缝施工示意图;
图2为本方法竖向缝施工示意图。
具体实施方式
实施例如图1和图2所示,本发明预制夹心保温剪力墙外墙横向缝和竖向缝的施工方法包括如下步骤:
步骤一、将混凝土预制构件1吊装到位,校正构件的水平和垂直度达到设计及规范要求;
步骤二、在相邻构件竖向缝11内侧黏贴自粘性橡胶皮2并延伸至竖向缝11两侧,用于防止浇筑相邻构件之间的暗柱时混凝土浮浆及混凝土进入竖向缝11内,橡胶皮2外侧进行防水密封胶3施工,使相邻构件可靠连接,防止渗漏;
步骤三、构件安装后,对相邻构件横向缝12的胶条至构件内侧边缘的横向缝12空间进行灌浆腔封堵作业,灌浆腔封闭前清理待封闭区域,然后用水湿润,采用座浆料4对该横向缝12空间进行封闭;
步骤四、相邻构件横向缝12胶条外侧填塞PE棒5,填塞前对横向缝12进行打磨清理,清除油渍、浮浆及混凝土块,PE棒5规格根据横向缝12宽度选用、填塞深度根据防水密封胶6厚度确定,横向缝12表面进行防水密封胶6施工并保证防水密封胶6的厚度及密实度;
步骤五、对构件外墙立面进行涂料施工,要求外墙立面平整度不大于2mm,采用聚合物水泥砂浆7对竖向缝11和横向缝12的凹陷处进行填塞,起到更好的与防水密封胶3、6粘结的作用,待聚合物水泥砂浆7干燥后涂刷素水泥浆一道,然后在竖向缝11和横向缝12表面覆盖耐碱玻纤网格布8并延伸至缝的两侧,整个外墙立面刮防水外墙腻子,最后喷真石漆饰面层。
优选的,所述竖向缝11内侧黏贴的自粘性橡胶皮2宽度为100mm,并延伸至竖向缝11两侧各40mm。
优选的,所述横向缝12灌浆腔待封闭区域清除油渍、浮浆及混凝土渣块。
优选的,所述聚合物水泥砂浆7和素水泥浆内掺入5%重量份的聚乙烯醇缩甲醛胶。
优选的,所述耐碱玻纤网格布8的宽度为220mm并延伸至缝两侧各100mm。
针对混凝土预制构件的横向缝和竖向缝,传统施工方式在防水密封胶的外侧直接刮外墙腻子,导致了板缝处涂料开裂脱落,同时对板缝凹陷处未作进一步的处理,导致了板缝渗漏。经过多次实验,采用本施工方法后可有效缓解防水密封胶膨胀和收缩对外墙腻子的影响,有效解决外墙渗漏及外墙涂料开裂脱落问题,提高了外墙施工质量,达到美观耐用的目的。

Claims (5)

1.一种预制夹心保温剪力墙外墙横向缝和竖向缝的施工方法,其特征在于本方法包括如下步骤:
步骤一、将混凝土预制构件吊装到位,校正构件的水平和垂直度达到设计及规范要求;
步骤二、在相邻构件竖向缝内侧黏贴自粘性橡胶皮并延伸至竖向缝两侧,用于防止浇筑相邻构件之间的暗柱时混凝土浮浆及混凝土进入竖向缝内,橡胶皮外侧进行防水密封胶施工,使相邻构件可靠连接,防止渗漏;
步骤三、构件安装后,对相邻构件横向缝的胶条至构件内侧边缘的横向缝空间进行灌浆腔封堵作业,灌浆腔封闭前清理待封闭区域,然后用水湿润,采用座浆料对该横向缝空间进行封闭;
步骤四、相邻构件横向缝胶条外侧填塞PE棒,填塞前对横向缝进行打磨清理,清除油渍、浮浆及混凝土块,PE棒规格根据横向缝宽度选用、填塞深度根据防水密封胶厚度确定,横向缝表面进行防水密封胶施工并保证防水密封胶的厚度及密实度;
步骤五、对构件外墙立面进行涂料施工,要求外墙立面平整度不大于2mm,采用聚合物水泥砂浆对竖向缝和横向缝的凹陷处进行填塞,起到更好的与防水密封胶粘结的作用,待聚合物水泥砂浆干燥后涂刷素水泥浆一道,然后在竖向缝和横向缝表面覆盖耐碱玻纤网格布并延伸至缝的两侧,整个外墙立面刮防水外墙腻子,最后喷真石漆饰面层。
2.根据权利要求1所述的预制夹心保温剪力墙外墙横向缝和竖向缝的施工方法,其特征在于:所述竖向缝内侧黏贴的自粘性橡胶皮宽度为100mm,并延伸至竖向缝两侧各40mm。
3.根据权利要求1所述的预制夹心保温剪力墙外墙横向缝和竖向缝的施工方法,其特征在于:所述横向缝灌浆腔待封闭区域清除油渍、浮浆及混凝土渣块。
4.根据权利要求1所述的预制夹心保温剪力墙外墙横向缝和竖向缝的施工方法,其特征在于:所述聚合物水泥砂浆和素水泥浆内掺入5%重量份的聚乙烯醇缩甲醛胶。
5.根据权利要求1所述的预制夹心保温剪力墙外墙横向缝和竖向缝的施工方法,其特征在于:所述耐碱玻纤网格布的宽度为220mm并延伸至缝两侧各100mm。
CN201711092770.3A 2017-11-08 2017-11-08 预制夹心保温剪力墙外墙横向缝和竖向缝的施工方法 Pending CN109750758A (zh)