CN108297239A - A kind of perpendicular timber floor manufacturing method - Google Patents
A kind of perpendicular timber floor manufacturing method Download PDFInfo
- Publication number
- CN108297239A CN108297239A CN201710024684.2A CN201710024684A CN108297239A CN 108297239 A CN108297239 A CN 108297239A CN 201710024684 A CN201710024684 A CN 201710024684A CN 108297239 A CN108297239 A CN 108297239A
- Authority
- CN
- China
- Prior art keywords
- saw
- timber
- cross cut
- thickness
- timber floor
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Pending
Abstract
The invention discloses a kind of perpendicular timber floor manufacturing methods, belong to floor manufacturing technology field, cross cut saw material material head, small dimension wood, integrated timber are processed into perpendicular timber floor, wherein, the method that material head is processed into perpendicular timber floor includes that thickness, part cross cut saw, mortise, paint and packaging process are determined in sorting, fitting, sanding, wherein:The cross cut saw material material head and integrated timber that meet thickness and width error requirements are classified as one kind by sorting process, and a plane of selected cross cut saw material material head and integrated timber does gluing reference plane;Bonding process is cold-pressed glue laminating using two-component, the health 48h after 100KG pressure pushes 40min;The fixed thick process of sanding is with sander by blank thickness sanding to predetermined thickness;The method that small dimension wood is processed into perpendicular timber floor include change saw, scrape, dry, finishing, buck saw, pressing, mortise, paint and packaging process.The advantages of with improving timber utilization rate, promoting ornament materials diversification, increase the performance of enterprises.
Description
Technical field
The present invention relates to method for making floor, more particularly to it is a kind of small dimension wood, plank material head sum aggregate are become a useful person be processed into it is perpendicular
The manufacturing method of timber floor belongs to floor manufacturing technology field.
Background technology
With the continuous development of wood industry, the improvement of people's living standards, to the feature of environmental protection of house ornamentation, comfort and sense organ
It is required that being also higher and higher, it is raw material, big, central diameter timber that floor currently on the market, which is mostly used greatly the high-quality hardwood of big or middle diameter grade,
Production process is slow, in addition both at home and abroad to the protection of forest, improve timber go out material and utilization rate have become it is current
The task of top priority.
To improve the utilization rate of timber, using the small dimension wood, plank material head and integrated timber generated in production process, again
It is adhered on base material, carries out the index Designs such as unified width, pattern, mortise is fabricated to the perpendicular wood ground with artistic effect again
Plate will increase the style of flooring product on the basis of improving timber utilization rate.Investigation by early period to market is found
This floor with beautiful individual character is favored by consumer deeply, has the prodigious market space.
Invention content
In view of the defects existing in the prior art, the purpose of the present invention is to provide a kind of perpendicular timber floor manufacturing methods, will cut
Saw material material head, small dimension wood, integrated timber are processed into perpendicular timber floor, include the following steps:
The step of cross cut saw material material head is processed into perpendicular timber floor include, sorting, fitting, sanding determine thickness, part cross cut saw, mortise, paint,
Packaging process, wherein:
Sorting process is to sort cross cut saw material material head with integrated timber, and by thickness within 2mm, width error is in ± 0.02mm
Within cross cut saw material material head and integrated timber be classified as one kind, and a plane of selected cross cut saw material material head and integrated timber does gluing benchmark
Face;
Bonding process is cold-pressed glue laminating using two-component, material head is bonded on the glued board of 11mm thickness, one face gluing of glued board,
The gluing reference plane of material head applies curing agent, by hand bonds the gluing reference plane of the coated face of glued board and material head, is pressed in 100KG
Power pushes health 48h after 40min;
The fixed thick process of sanding is fixed thick to 15.2mm by blank thickness sanding at twice with three roller sanders, wherein fixed thickness for the first time
First roller sand paper is No. 20, the second roller sand paper is No. 20, third roller sand paper is No. 40, and second of fixed thick first roller sand paper is 60
Number, the second roller sand paper be No. 80, third roller sand paper is No. 120;
Part cross cut saw process be by semi-finished product cross cut saw at specification be 1228*188*15mm;
Mortise specification is 1200*160*15mm, and chase mortise latches 25 ° of chamfering * 0.3mm;
Paint process makes the color that suitable market needs with common process;
Packaging process is packed with common process.
Small dimension wood be processed into the step of perpendicular timber floor include change saw, scrape, dry, finishing, buck saw, pressing, mortise,
Paint, packaging process, wherein:
Log or the branch for changing any seeds of the saw process using the smaller diameter of diameter collection in 50-120mm, in order to adapt to back tender
Logs of small diameter cut-off should be cut into certain length, while rejecting defect by the requirement of skill, and equipment may be used along saw, cross cut saw;
Process of scraping, which scrapes sawed juggle, is processed into non-uniform thickness convenient for following process, equipment choosing band saw;
Drying process, which dries juggle in dry kiln to moisture content, reaches 6-9%;
Finishing step carries out essence after kiln discharge and cuts convenient for follow-up assembly, and integrated timber is made using four side moulder;
Integrated timber is made the dash board of 4mm by buck saw process;
The good dash board of frame is pressed into floor by pressing working procedure using hot press;
Mortise, paint, packaging process need to process with common process according to market.
The beneficial effects of the present invention are:A kind of perpendicular timber floor manufacturing method is provided, has and improves timber utilization rate, is promoted
Into ornament materials diversification, the advantages of increasing the performance of enterprises.
Specific implementation mode
In order to more clearly explain the embodiment of the invention or the technical proposal in the existing technology, the present invention will be with reference to embodiment
It is described more fully hereinafter.However, the present invention can be embodied and be should not be construed as being limited to many different forms
Specific embodiment set forth herein.On the contrary, these embodiments are supplied to the technical side those skilled in the art understand that the present invention
Case.
Embodiment 1
By taking cross cut saw material material head is processed into the method for perpendicular timber floor as an example, step includes that sorting, fitting, the fixed thick, part of sanding are cut
Saw, mortise, paint, packaging process, wherein:
Sorting process is to sort cross cut saw material material head with integrated timber, and by thickness within 2mm, width error is in ± 0.02mm
Within cross cut saw material material head and integrated timber be classified as one kind, and a plane of selected cross cut saw material material head and integrated timber does gluing benchmark
Face;Bonding process is cold-pressed glue laminating using two-component, material head is bonded on the glued board of 11mm thickness, one face gluing of glued board,
The gluing reference plane of material head applies curing agent, by hand bonds the gluing reference plane of the coated face of glued board and material head, is pressed in 100KG
Power pushes health 48h after 40min;Blank thickness sanding is determined thickness at twice with three roller sanders and arrived by the fixed thick process of sanding
15.2mm, wherein fixed thick first roller sand paper is No. 20 for the first time, the second roller sand paper is No. 20, third roller sand paper is No. 40, second
Secondary fixed thick first roller sand paper is No. 60, the second roller sand paper is No. 80, third roller sand paper is No. 120;Part cross cut saw process is by half
Finished product cross cut saw is 1228*188*15mm at specification;Mortise specification is 1200*160*15mm, and chase mortise latches 25 ° of chamfering * 0.3mm;
Paint process makes the color that suitable market needs with common process;Packaging process is normally packed with common process.
Embodiment 2
By taking small dimension wood is processed into the method for perpendicular timber floor as an example, step includes changing saw, scraping, dry, finishing, buck saw, pressure
Conjunction, mortise, paint, packaging process, wherein:
Log or the branch for changing any seeds of the saw process using the smaller diameter of diameter collection in 50-120mm, in order to adapt to back tender
Logs of small diameter cut-off should be cut into certain length, while rejecting defect by the requirement of skill, and equipment may be used along saw, cross cut saw;
Process of scraping, which scrapes sawed juggle, is processed into non-uniform thickness convenient for following process, equipment choosing band saw;Drying process will be wooden
Section, which is dried in dry kiln to moisture content, reaches 6-9%;Finishing step carries out essence after kiln discharge and cuts convenient for follow-up assembly, uses
Four side moulder makes integrated timber;Integrated timber is made the dash board of 4mm by buck saw process;Pressing working procedure uses hot press by the good dash board of frame
It is pressed into floor;Mortise, paint, packaging process need to process with common process according to market.
Unless otherwise defined, term used herein above(Including scientific and technical terminology)It should be construed as having as belonging to the present invention
The identical meaning that those skilled in the art are commonly understood by.It will also be understood that term used herein above should be explained
For with the meaning consistent with their meanings in the content of this specification and the relevant technologies, and should not be with idealization
Or excessive form is explained, unless expressly so limiting here.
Although the present invention has been described with reference to specific aspect, feature and the exemplary embodiment of the present invention herein, answer
When understanding, therefore processing method of the invention is not restricted, but is extended and covered numerous other variations, becomes
Type and alternate embodiment, as will be given those skilled in the art in the invention are implied based on disclosure herein.Accordingly
Ground, all within the spirits and principles of the present invention, any modification, equivalent substitution, improvement and etc. done should be included in the present invention
Protection domain within.
Claims (7)
1. cross cut saw material material head, small dimension wood, integrated timber are processed into perpendicular timber floor by a kind of perpendicular timber floor manufacturing method, feature exists
In,
The method that cross cut saw material material head is processed into perpendicular timber floor include sorting, fitting, sanding determine thickness, part cross cut saw, mortise, paint and
Packaging process, wherein:
Sorting process is to sort cross cut saw material material head with integrated timber, will meet the cross cut saw material material of thickness and width error requirements
Head and integrated timber are classified as one kind, and a plane of selected cross cut saw material material head and integrated timber does gluing reference plane;
Bonding process is cold-pressed glue laminating using two-component, material head is bonded on glued board, one face gluing of glued board, the painting of material head
Glue reference plane applies curing agent, by hand bonds the gluing reference plane of the coated face of glued board and material head, is pushed in 100KG pressure
Health 48h after 40min;
The fixed thick process of sanding is with sander by blank thickness sanding to predetermined thickness;
Part cross cut saw process be by semi-finished product cross cut saw at specification be 1228*188*15mm;
Mortise specification is 1200*160*15mm, and chase mortise latches 25 ° of chamfering * 0.3mm;
Paint process makes the color that suitable market needs with common process;
Packaging process is packed with common process;
Small dimension wood be processed into perpendicular timber floor method include change saw, scrape, dry, finishing, buck saw, pressing, mortise, paint and
Packaging process, wherein:
Change log or branch of the saw process using the smaller any seeds of diameter collection, and Logs of small diameter cut-off is blocked, rejects simultaneously
Defect;
Process of scraping, which scrapes sawed juggle, is processed into non-uniform thickness;
It is 6-9% that drying process, which dries juggle in dry kiln to moisture content,;
Finishing step carries out essence after kiln discharge and cuts convenient for follow-up assembly, and integrated timber is made using four side moulder;
Integrated timber is made the dash board of fixed thickness by buck saw process;
The good dash board of frame is pressed into floor by pressing working procedure using hot press;
Mortise, paint, packaging process need to process with common process according to market.
2. perpendicular timber floor manufacturing method according to claim 1, it is characterised in that:Thickness control is in 2mm in sorting process
Within, width error controls within ± 0.02mm.
3. perpendicular timber floor manufacturing method according to claim 1, it is characterised in that:Sander selects three roller sanders to be divided to two
It is secondary that blank thickness sanding is fixed thick to 15.2mm, wherein thick first roller sand paper fixed for the first time is No. 20, the second roller sand paper is 20
Number, third roller sand paper be No. 40, second fixed thick first roller sand paper is No. 60, the second roller sand paper is No. 80, third roller sand paper is
No. 120.
4. perpendicular timber floor manufacturing method according to claim 1, it is characterised in that:Change the straight of log or branch in saw process
Diameter takes 50-120mm.
5. perpendicular timber floor manufacturing method according to claim 1, it is characterised in that:Change saw process to select along saw, cross cut saw.
6. perpendicular timber floor manufacturing method according to claim 1, it is characterised in that:Process of scraping selects band saw.
7. perpendicular timber floor manufacturing method according to claim 1, it is characterised in that:Integrated timber is made into thickness in buck saw process
Degree is 4mm.