CN107901571B - A kind of method for adhering film of camber display screen - Google Patents
A kind of method for adhering film of camber display screen Download PDFInfo
- Publication number
- CN107901571B CN107901571B CN201711268798.8A CN201711268798A CN107901571B CN 107901571 B CN107901571 B CN 107901571B CN 201711268798 A CN201711268798 A CN 201711268798A CN 107901571 B CN107901571 B CN 107901571B
- Authority
- CN
- China
- Prior art keywords
- adhesive film
- display screen
- curved edge
- pressing
- camber display
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Active
Abstract
The invention discloses a kind of method for adhering film of camber display screen, comprising steps of S1, rotation adhesive film, tilt the second side of adhesive film upwards relative to first side;S2, the adhesive film is pushed using pressing device, adhesive film is made to be in contact first with the first tangent line;S3, pressing device persistently compress the adhesive film and to close to the movements of the direction of the second curved edge, adhesive film are pressed together in mid-plane, until reaching at the second tangent line;The tangent line is the phase tangent line of curved edge and mid-plane on camber display screen;S4, pressing device continue to compress the adhesive film and move along the outer surface of the second curved edge, and the second side of adhesive film is pressed together on the second curved edge;S5, the pressing device is lifted, and return to pressing device on the position of the first tangent line, pressing device compresses the adhesive film again and moves along the outer surface of the first curved edge, and the first side of adhesive film is pressed together on the first curved edge, to complete pad pasting process.
Description
Technical field
The present invention relates to display screen Filming Technology field more particularly to a kind of method for adhering film of camber display screen.
Background technique
With the development of electronic technology, camber display screen is used more and more, and camber display screen is in the fabrication process
It needs to attach various film layers on camber display screen.Camber display screen includes mid-plane and is connected to mid-plane two sides
The method for adhering film of curved edge, previous planar display screen can not well adapt to the pad pasting of camber display screen, especially
Fitting effect at the curved edge of its two sides is poor, and human assistance is needed to complete, and cannot achieve full-automatic production.
Summary of the invention
The technical problems to be solved by the present invention are: a kind of method for adhering film of camber display screen is provided, it can be automatically
The pad pasting process of camber display screen is completed, guarantees the pad pasting quality of camber display screen entirety.
In order to solve the above-mentioned technical problem, the technical solution adopted by the present invention are as follows:
A kind of method for adhering film of camber display screen, comprising steps of
S1, rotation adhesive film, tilt the second side of adhesive film upwards relative to first side, the first side,
Second side is corresponding with the first curved edge of camber display screen, the second curved edge respectively;
S2, the adhesive film is pushed using pressing device, adhesive film is made to be in contact first with the first tangent line, described first cuts
Line is the phase tangent line of the first curved edge and mid-plane on camber display screen;
S3, pressing device persistently compress the adhesive film and the direction movement to close second curved edge, by adhesive film
It is pressed together in mid-plane, until reaching at the second tangent line;Second tangent line be camber display screen on the second curved edge with
The phase tangent line of mid-plane;
S4, pressing device continue to compress the adhesive film and move along the outer surface of the second curved edge, by adhesive film
Second side is pressed together on the second curved edge;
S5, the pressing device is lifted, and returns to pressing device on the position of the first tangent line, pressing device compresses again
The adhesive film is simultaneously moved along the outer surface of the first curved edge, and the first side of adhesive film is pressed together on the first curved edge
On.
The beneficial effects of the present invention are: the present invention first rotates adhesive film before fitting, makes adhesive film and song to be fit
Face display screen is a certain included angle, and using the phase tangent line of the first side as the initial position of pressing, at this time the first side of adhesive film
Side is in vacant state, will not encounter camber display screen, and middle section and second side are in tilting state, will not touch
The bad phenomenons such as bubble will not be generated to camber display screen, therefore in fitting;It is moved in one direction since initial position
Pressing device realizes the fitting of mid-plane and the second curved edge, then returns initial position and move in the opposite direction
The fitting of the first curved edge can be completed in pressing device, and entire fitting process can not only guarantee that camber display screen is whole especially
It is the good fitting quality at the curved edge of two sides, and the method for adhering film can be completed by machine full-automation, no
It needs manually to participate in, is greatly improved efficiency, save human cost.
Detailed description of the invention
Fig. 1 is status diagram of the method for adhering film in pad pasting initial position of the embodiment of the present invention;
Fig. 2 is status diagram of the method for adhering film of the embodiment of the present invention when being bonded mid-plane;
Fig. 3 is status diagram of the method for adhering film of the embodiment of the present invention on the left of fitting when curved edge;
Fig. 4 is status diagram of the method for adhering film of the embodiment of the present invention on the right side of fitting when curved edge;
Label declaration:
1, pressing device;2, vacuum absorption device;3, camber display screen.
Specific embodiment
To explain the technical content, the achieved purpose and the effect of the present invention in detail, below in conjunction with embodiment and cooperate attached
Figure is explained.
The most critical design of the present invention is: rotating adhesive film before fitting, make adhesive film and curved-surface display to be fit
Screen 3 is a certain included angle, and using the phase tangent line on right side as the initial position of pressing, court moves left pressing since initial position
Device 1 realizes the fitting of mid-plane and left side curved edge, then returns initial position court and moves right pressing device 1
Complete the fitting of right side curved edge.
Please refer to Fig. 1 to Fig. 4, a kind of method for adhering film of camber display screen, comprising steps of
S1, rotation adhesive film, tilt the second side of adhesive film upwards relative to first side, the first side,
Second side is corresponding with the first curved edge of camber display screen 3, the second curved edge respectively;
S2, the adhesive film is pushed using pressing device 1, adhesive film is made to be in contact first with the first tangent line, described first
Tangent line is the phase tangent line of the first curved edge and mid-plane on camber display screen 3;
S3, pressing device 1 persistently compress the adhesive film and the direction movement to close second curved edge, by adhesive film
It is pressed together in mid-plane, until reaching at the second tangent line;Second tangent line be camber display screen 3 on the second curved edge with
The phase tangent line of mid-plane;
S4, pressing device 1 continue to compress the adhesive film and move along the outer surface of the second curved edge, by adhesive film
Second side is pressed together on the second curved edge;
S5, the pressing device 1 is lifted, and returns to pressing device 1 on the position of first tangent line, pressing device 1 is again
It compresses the adhesive film and is moved along the outer surface of the first curved edge, the first side of adhesive film is pressed together on the first arc-shaped side
On edge.
As can be seen from the above description, the beneficial effects of the present invention are: the present invention first rotates adhesive film before fitting, makes to paste
Film is a certain included angle with camber display screen to be fit, and using the phase tangent line of the first side as the initial position of pressing, at this time
The first side of adhesive film is in vacant state, will not encounter camber display screen, and middle section and second side are in and stick up
The state of rising will not encounter camber display screen, therefore will not generate the bad phenomenons such as bubble in fitting;Since initial position
Pressing device is moved in one direction, is realized the fitting of mid-plane and the second curved edge, is then returned initial position
Moving pressing device in the opposite direction can be completed the fitting of the first curved edge, and entire fitting process can not only guarantee curved surface
Good fitting quality of the display screen especially at the curved edge of two sides, and the method for adhering film can pass through machine full-automation
It completes, does not need manually to participate in, be greatly improved efficiency, save human cost.
Further, further include step S0 before step S1: drawing the adhesive film with vacuum absorption device 2, and make
Expose outside vacuum absorption device 2 first side of adhesive film.
Seen from the above description, adhesive film is drawn with vacuum absorption device, not only adhesive film will not be caused to damage, but also
Adhesive film is easy to be detached to bond with display screen from adsorbent equipment during pressing;Expose the first side of adhesive film
Outside vacuum absorption device, starting positioning pressing is carried out at the first tangent line convenient for pressing device.
Further, the step S0 further include: the position of adjustment vacuum absorption device 2 makes on vacuum absorption device 2
Adhesive film is aligned with camber display screen 3 to be pasted.
Seen from the above description, vacuum absorption device can be mounted on an XYZT motion platform, step S1 it
Before, the position of vacuum absorption device is adjusted, guarantees the fitting regularity of film.
Further, the pressing device 1 is idler wheel mechanism, and the idler wheel mechanism includes cylinder and the pressure for being connected to cylinder
Idler wheel is closed, in the bonding processes described in step S2-S5, the pressing roller compression is on the adhesive film.
Seen from the above description, pressing idler wheel rolls on adhesive film, adhesive film can be pressed together on camber display screen, presses
Closing idler wheel can not only avoid scratching adhesive film, and pressing idler wheel can preferably complete the pressing at curved edge.
Further, the idler wheel mechanism further includes back-up roller wheel, and the back-up roller wheel connects with pressing idler wheel rolling
Touching, pressing idler wheel are located at the lower section of back-up roller wheel, and the diameter of back-up roller wheel is greater than the diameter of the pressing idler wheel.
Seen from the above description, because existing camber display screen is chiefly used in handheld device, and the curved surface in handheld device
The curved edge curvature of display screen is smaller, and what the diameter for pressing idler wheel had to do smaller can preferably complete arc-shaped side
Pressing at edge, the smaller idler wheel rigidity of diameter are easy to happen bending deformation with regard to smaller, are unfavorable for the pressing of adhesive film, and our
Method is arranged a back-up roller wheel being relatively large in diameter in the top of pressing idler wheel and is in rolling contact therewith, can play support to pressing idler wheel
Effect avoids pressing idler wheel stress deformation during the pressing process.
Further, the radius of the pressing idler wheel is 3-4mm.
Further, further include step S40 between the step S4 and S5: after the pressing for completing the second curved edge,
Make pressing device 1 that original moving direction be kept persistently to move forward, so that pressing device 1 is mutually separated with adhesive film.
Seen from the above description, the adhesive film that above-mentioned steps can avoid having been pressed on the second curved edge is by band again
Get up.
Further, in the step S1, the second side of the adhesive film is acclivitous relative to first side
Angle is 10-20 °.
Seen from the above description, the tilt angle of the range is optimum tilt angle, has not only facilitated the pressing of pressing device, but also
It can guarantee during pad pasting, the adhesive film not pressed will not encounter camber display screen.
Further, in the step S3, the movement speed of the pressing device 1 is 80-120mm/s;In step S4
In step S5, the movement speed of the pressing device 1 is 15-20mm/s.
Seen from the above description, step S3 is the pressing of mid-plane, and the pressing in plane is easier to, and can properly increase pressure
Speed is closed, pressing efficiency is improved;Step S4 and S5 are the pressing of curved edge, and it is undesirable that the pressing in cambered surface is easy to appear fitting
Phenomenon, can appropriate slow-down, guarantee fitting quality.
Embodiment one
The embodiment of the present invention one are as follows: a kind of method for adhering film of camber display screen, including following rapid:
S1, the camber display screen 3 to pad pasting is lain in a horizontal plane in X/Y plane, the length of the curved edge of camber display screen 3
It is parallel with X-axis to spend direction;The adhesive film is drawn with vacuum absorption device 2, and makes the right edge and and right tangent of adhesive film
Corresponding position is completely exposed outside vacuum absorption device 2;The right edge is the right side arc of adhesive film and camber display screen 3
The corresponding part in edge;The right tangent is the phase tangent line of right side curved edge and mid-plane on camber display screen 3.
S2, the position for adjusting vacuum absorption device 2 keep the adhesive film on vacuum absorption device 2 and the curved surface to pad pasting aobvious
Display screen 3 is aligned, specifically, vacuum absorption device 2 can be mounted on XYZT mobile platform, is carried out to vacuum absorption device 2 flat
Shifting and rotation about the z axis, are aligned adhesive film on X/Y plane with camber display screen 3, but between adhesive film and camber display screen 3
There are certain differences in height.
S3, as shown in Figure 1, rotation adhesive film, tilt the left side of adhesive film upwards relative to right edge, inclined angle
Degree can be 15 °, and the left side is adhesive film part corresponding with the left side curved edge of camber display screen 3.
S4, the adhesive film for exposing the right tangent corresponding position outside vacuum absorption device 2 is pushed down using pressing device 1, make to paste
Film is in contact with the right tangent of camber display screen 3 first.
Pressing device 1 is idler wheel mechanism, and the idler wheel mechanism includes cylinder and the pressing idler wheel and branch for being connected to cylinder
Idler wheel is supportted, the stretching or contraction of cylinder piston rod can drive pressing idler wheel and back-up roller wheel to rise or fall.The back-up roller wheel
It is in rolling contact with the pressing idler wheel, pressing idler wheel is located at the lower section of back-up roller wheel, and the diameter of back-up roller wheel is greater than the pressing
The diameter of idler wheel.During entire pad pasting, what is be in contact with adhesive film is pressing idler wheel.To guarantee the pressing at curved edge
Quality, the radius of the pressing idler wheel can be 3-4mm, and in the present embodiment, the radius of the pressing idler wheel is preferably
3.2mm.The diameter of the back-up roller wheel can be substantially larger than pressing idler wheel, to provide preferable support for pressing idler wheel, avoid pressing
Close idler wheel stress deformation during pressing.
S5, pressing device 1 persistently compress the adhesive film, while pressing device 1 is synchronous with vacuum absorption device 2 even to the left
Speed is mobile, adhesive film is pressed together in the mid-plane of camber display screen 3, as shown in Fig. 2, until reaching at left cut line;It is described
Left cut line is the phase tangent line of camber display screen 3 upper left side curved edge and mid-plane.In this step, the pressing device 1
Movement speed can be 80-120mm/s, in the present embodiment, the movement speed of pressing device 1 is 100mm/s.
S6, pressing device 1 continue to compress the adhesive film, and vacuum absorption device 2 and pressing device 1 are persistently moved to the left,
Cylinder gradually drives pressing idler wheel decline simultaneously, as shown in figure 3, making pressing idler wheel can just be along the appearance of left side curved edge
Face is mobile, so that the left side of adhesive film is pressed together on the left side curved edge of camber display screen 3.In this step, described
The movement speed of pressing device 1 can be 15-25mm/s, and in the present embodiment, the movement speed of the pressing device 1 is preferably
20mm/s。
S7, after completing the pressing of left side curved edge, it is moved to the left pressing device 1 persistently, so that pressing device 1 and viscous
Pad pasting mutually separates, and then lifts the pressing device 1, and return to pressing device 1 on the position of the right tangent.
S8, as shown in figure 4, pressing device 1 compresses the adhesive film again and moves along the outer surface of right side curved edge,
The right edge of adhesive film is pressed together on the right side curved edge of camber display screen 3, to complete the patch of entire camber display screen 3
Membrane process.In this step, the movement speed of the pressing device 1 can be 15-25mm/s, in the present embodiment, the pressure
Attaching together and setting 1 movement speed is preferably 20mm/s.
In conclusion the method for adhering film of camber display screen provided by the invention can not only guarantee camber display screen 3 two
Good fitting quality at the curved edge of side, and the method for adhering film can be completed by machine full-automation, be not required to very important person
Work participates in, and is greatly improved efficiency, saves human cost.
The above description is only an embodiment of the present invention, is not intended to limit the scope of the invention, all to utilize this hair
Equivalents made by bright specification and accompanying drawing content are applied directly or indirectly in relevant technical field, similarly include
In scope of patent protection of the invention.
Claims (9)
1. a kind of method for adhering film of camber display screen, which is characterized in that comprising steps of
S1, rotation adhesive film, tilt the second side of adhesive film upwards relative to first side, the first side, second
Side is corresponding with the first curved edge of camber display screen, the second curved edge respectively;
S2, the adhesive film is pushed using pressing device, adhesive film is made to be in contact first with the first tangent line, first tangent line is
The phase tangent line of first curved edge and mid-plane on camber display screen;
S3, pressing device persistently compress the adhesive film and to close to the movements of the direction of the second curved edge, and adhesive film is pressed
In mid-plane, until reaching at the second tangent line;Second tangent line is the second curved edge and centre on camber display screen
The phase tangent line of plane;
S4, pressing device continue to compress the adhesive film and move along the outer surface of the second curved edge, by the second of adhesive film
Side is pressed together on the second curved edge;
S5, the pressing device is lifted, and returns to pressing device on the position of the first tangent line, described in pressing device compresses again
Adhesive film is simultaneously moved along the outer surface of the first curved edge, and the first side of adhesive film is pressed together on the first curved edge.
2. the method for adhering film of camber display screen as described in claim 1, which is characterized in that before step S1 further include step
S0: drawing the adhesive film with vacuum absorption device, and exposes the first side of adhesive film outside vacuum absorption device.
3. the method for adhering film of camber display screen as claimed in claim 2, which is characterized in that the step S0 further include: adjustment
The position of vacuum absorption device is aligned the adhesive film on vacuum absorption device with camber display screen to be pasted.
4. the method for adhering film of camber display screen as described in claim 1, which is characterized in that the pressing device is roller machine
Structure, the idler wheel mechanism include cylinder and the pressing idler wheel for being connected to cylinder, in the bonding processes described in step S2-S5, institute
Pressing roller compression is stated on the adhesive film.
5. the method for adhering film of camber display screen as claimed in claim 4, which is characterized in that the idler wheel mechanism further includes support
Idler wheel, the back-up roller wheel are in rolling contact with the pressing idler wheel, and pressing idler wheel is located at the lower section of back-up roller wheel, back-up roller wheel
Diameter is greater than the diameter of the pressing idler wheel.
6. the method for adhering film of camber display screen as claimed in claim 5, which is characterized in that the radius of the pressing idler wheel is 3-
4mm。
7. the method for adhering film of camber display screen as described in claim 1, which is characterized in that between the step S4 and S5 also
Including step S40: after the pressing for completing the second curved edge, making pressing device that original moving direction be kept to continue to Forward
It is dynamic, so that pressing device is mutually separated with adhesive film.
8. the method for adhering film of camber display screen as described in claim 1, which is characterized in that in the step S1, described viscous
The second side of pad pasting is 10-20 ° relative to the acclivitous angle in first side.
9. the method for adhering film of camber display screen as described in claim 1, which is characterized in that in the step S3, the pressure
Attaching together the movement speed set is 80-120mm/s;In step S4 and step S5, the movement speed of the pressing device is 15-
20mm/s。