CN107881513A - A kind of family expenses rust remover preparation method - Google Patents
A kind of family expenses rust remover preparation method Download PDFInfo
- Publication number
- CN107881513A CN107881513A CN201711449946.6A CN201711449946A CN107881513A CN 107881513 A CN107881513 A CN 107881513A CN 201711449946 A CN201711449946 A CN 201711449946A CN 107881513 A CN107881513 A CN 107881513A
- Authority
- CN
- China
- Prior art keywords
- parts
- rust remover
- family expenses
- acid
- preparation
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Withdrawn
Abstract
A kind of family expenses rust remover preparation method disclosed by the invention, meter includes following component in parts by weight, and 13 parts of hydrochloric acid, 39 parts of malic acid, 24 parts of hydroxy ethylidene triphosphoric acid, 39 parts of hydrogen chloride, 5 15 parts of polyethylene glycol, 26 parts of ammonium chloride, 13 parts of sodium metasilicate, 80 240 parts of deionized water, composition is simple, configuration is convenient, cost is relatively low, and derusting effect is good, non-hazardous, it is convenient to facilitate, derusting operation need not be carried out repeatedly, save substantial amounts of human and material resources, can more meet the needs of producer.
Description
Technical field
The invention belongs to rust remover field, and in particular to a kind of rust remover.
Background technology
Ferrous metal(Steel)It is placed under outdoor or open-air condition and gets rusty easily, not only influences presentation quality, can also influence
Being normally carried out for the techniques such as spray painting, bonding, such as handles, can more cause scrapping for material not in time, causes unnecessary economic damage
Lose.Rust remover is also referred to as pine rust agent, and main function is the fastener that gets rusty of loosening, and lubricates non-detachable fastener, easy to disassemble
The fastener to get rusty.It can form lasting anti-corrosion protection in exposed metal surface, prevent new corrosion from being formed.Rust remover
And preferable metalworking coolant, suitable for stainless steel, surface of aluminum plate tapping.Dry electronic equipment can also be effectively cleaned, is changed
Kind conductive performance.It can be widely applied to manufacturing industry, construction industry, repairing trades, traffic, the energy, electric power, oil and mining etc.
A variety of industries, suitable for removing for the steel such as plant equipment, vehicle, ship, ordnance, hardware & tools, building template, metal spare and accessory parts
Rust.Its superior performance can bring you unexpected convenience and material benefit.But existing rust remover derusts, effect is poor, past
Toward after needing repetitious use, the effect of derusting is can be only achieved, cost is higher, can not meet the demand of user.
The content of the invention
In view of the above-mentioned problems, the invention discloses a kind of family expenses rust remover preparation method.
Specific technical scheme is as follows:
A kind of family expenses rust remover preparation method, its preparation method are as follows:
(1)Following components, hydrochloric acid 1-3 parts, malic acid 3-9 parts, hydroxy ethylidene triphosphoric acid 2-4 parts, chlorination are weighed by weight
Hydrogen 3-9 parts, polyethylene glycol 5-15 parts, ammonium chloride 2-6 parts, sodium metasilicate 1-3 parts, deionized water 80-240 parts,;
(2)Hydrochloric acid, malic acid and deionized water are put into reactor, at 30 DEG C -40 DEG C, uniform stirring 5-15min;
(3)After temperature is promoted to 45 DEG C -55 DEG C, hydroxy ethylidene triphosphoric acid and polyethylene glycol are added, continues to stir 10-20
min;
(4)After temperature is promoted to 60 DEG C -70 DEG C, hydrogen chloride and ammonium chloride are added, continues to stir 5-15min;
(5)After temperature is promoted to 75 DEG C -85 DEG C, sodium metasilicate is added, continues to stir 5-15min;
(6)After temperature is promoted to 90 DEG C -100 DEG C, reactor is closed, reactant is taken out and is positioned over ventilation 3-5h, you can
Finished product.
A kind of above-mentioned family expenses rust remover preparation method, wherein, the ratio of the hydrochloric acid and malic acid is 1:3.
A kind of above-mentioned family expenses rust remover preparation method, wherein, the ratio of the hydroxy ethylidene triphosphoric acid and hydrogen chloride is
2:3.
A kind of above-mentioned family expenses rust remover preparation method, wherein, the ratio of the polyethylene glycol and ammonium chloride is 5:2.
A kind of above-mentioned family expenses rust remover preparation method, wherein, the ratio of the sodium metasilicate and deionized water is 1:80.
Beneficial effects of the present invention are:
A kind of family expenses rust remover preparation method disclosed by the invention, in parts by weight meter include following component, hydrochloric acid 1-3 parts, apple
Tartaric acid 3-9 parts, hydroxy ethylidene triphosphoric acid 2-4 parts, hydrogen chloride 3-9 parts, polyethylene glycol 5-15 parts, ammonium chloride 2-6 parts, sodium metasilicate 1-
3 parts, deionized water 80-240 parts, composition is simple, and configuration is convenient, and cost is relatively low, and derusting effect is good, and non-hazardous, it is convenient to facilitate, nothing
Derusting operation need to be carried out repeatedly, save substantial amounts of human and material resources, can more meet the needs of producer.
Embodiment
A kind of family expenses rust remover preparation method, its preparation method are as follows:
(1)Following components, hydrochloric acid 1-3 parts, malic acid 3-9 parts, hydroxy ethylidene triphosphoric acid 2-4 parts, chlorination are weighed by weight
Hydrogen 3-9 parts, polyethylene glycol 5-15 parts, ammonium chloride 2-6 parts, sodium metasilicate 1-3 parts, deionized water 80-240 parts,;
(2)Hydrochloric acid, malic acid and deionized water are put into reactor, at 30 DEG C -40 DEG C, uniform stirring 5-15min;
(3)After temperature is promoted to 45 DEG C -55 DEG C, hydroxy ethylidene triphosphoric acid and polyethylene glycol are added, continues to stir 10-20
min;
(4)After temperature is promoted to 60 DEG C -70 DEG C, hydrogen chloride and ammonium chloride are added, continues to stir 5-15min;
(5)After temperature is promoted to 75 DEG C -85 DEG C, sodium metasilicate is added, continues to stir 5-15min;
(6)After temperature is promoted to 90 DEG C -100 DEG C, reactor is closed, reactant is taken out and is positioned over ventilation 3-5h, you can
Finished product.
A kind of above-mentioned family expenses rust remover preparation method, wherein, the ratio of the hydrochloric acid and malic acid is 1:3.
A kind of above-mentioned family expenses rust remover preparation method, wherein, the ratio of the hydroxy ethylidene triphosphoric acid and hydrogen chloride is
2:3.
A kind of above-mentioned family expenses rust remover preparation method, wherein, the ratio of the polyethylene glycol and ammonium chloride is 5:2.
A kind of above-mentioned family expenses rust remover preparation method, wherein, the ratio of the sodium metasilicate and deionized water is 1:80.
A kind of family expenses rust remover preparation method disclosed by the invention, in parts by weight meter include following component, hydrochloric acid 1-3
Part, malic acid 3-9 parts, hydroxy ethylidene triphosphoric acid 2-4 parts, hydrogen chloride 3-9 parts, polyethylene glycol 5-15 parts, ammonium chloride 2-6 parts, silicon
Sour sodium 1-3 parts, deionized water 80-240 parts, composition is simple, and configuration is convenient, and cost is relatively low, and derusting effect is good, non-hazardous, convenient
It is convenient, without repeatedly carry out derusting operation, save substantial amounts of human and material resources, can more meet the needs of producer.
The foregoing is only a preferred embodiment of the present invention, but protection scope of the present invention be not limited thereto,
Any one skilled in the art the invention discloses technical scope in, the change or replacement that can readily occur in,
It should all cover within the scope of the present invention.Therefore, protection scope of the present invention should be with the protection domain of claims
It is defined.
Claims (5)
1. a kind of family expenses rust remover preparation method, it is characterized in that, its preparation method is as follows:
(1)Following components, hydrochloric acid 1-3 parts, malic acid 3-9 parts, hydroxy ethylidene triphosphoric acid 2-4 parts, chlorination are weighed by weight
Hydrogen 3-9 parts, polyethylene glycol 5-15 parts, ammonium chloride 2-6 parts, sodium metasilicate 1-3 parts, deionized water 80-240 parts,;
(2)Hydrochloric acid, malic acid and deionized water are put into reactor, at 30 DEG C -40 DEG C, uniform stirring 5-15min;
(3)After temperature is promoted to 45 DEG C -55 DEG C, hydroxy ethylidene triphosphoric acid and polyethylene glycol are added, continues to stir 10-20
min;
(4)After temperature is promoted to 60 DEG C -70 DEG C, hydrogen chloride and ammonium chloride are added, continues to stir 5-15min;
(5)After temperature is promoted to 75 DEG C -85 DEG C, sodium metasilicate is added, continues to stir 5-15min;
(6)After temperature is promoted to 90 DEG C -100 DEG C, reactor is closed, reactant is taken out and is positioned over ventilation 3-5h, you can
Finished product.
2. a kind of family expenses rust remover preparation method as claimed in claim 1, it is characterized in that, the ratio of the hydrochloric acid and malic acid
For 1:3.
3. a kind of family expenses rust remover preparation method as claimed in claim 1, it is characterized in that, the hydroxy ethylidene triphosphoric acid and chlorine
The ratio for changing hydrogen is 2:3.
4. a kind of family expenses rust remover preparation method as claimed in claim 1, it is characterized in that, the polyethylene glycol and ammonium chloride
Ratio is 5:2.
5. a kind of family expenses rust remover preparation method as claimed in claim 1, it is characterized in that, the sodium metasilicate and deionized water
Ratio is 1:80.