CN107740219A - A kind of preparation method of first silk and corn fiber blending satin fabric - Google Patents

A kind of preparation method of first silk and corn fiber blending satin fabric Download PDF

Info

Publication number
CN107740219A
CN107740219A CN201711203893.XA CN201711203893A CN107740219A CN 107740219 A CN107740219 A CN 107740219A CN 201711203893 A CN201711203893 A CN 201711203893A CN 107740219 A CN107740219 A CN 107740219A
Authority
CN
China
Prior art keywords
silk
sizing
fabric
fiber
zein fiber
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Pending
Application number
CN201711203893.XA
Other languages
Chinese (zh)
Inventor
熊原
刘渊民
程小潭
余胜
蔡丽娟
许鹤
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Jihua 3509 Textile Co Ltd
Original Assignee
Jihua 3509 Textile Co Ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Jihua 3509 Textile Co Ltd filed Critical Jihua 3509 Textile Co Ltd
Priority to CN201711203893.XA priority Critical patent/CN107740219A/en
Publication of CN107740219A publication Critical patent/CN107740219A/en
Pending legal-status Critical Current

Abstract

The present invention relates to a kind of preparation method of first silk/corn fiber blending satin fabric, the blend fabric by first silk/zein fiber 9.8tex (70/30) and first silk/zein fiber 9.8tex (70/30) by the production of 4/1 satin weave.Specific method is that first silk/zein fiber 9.8tex warp thread is weaved through warping, sizing, denting together with weft yarn member silk/zein fiber 9.8tex, tension force, arrangement, winding are uniformly crucial in warping process, discrete method configures tension force before, during and after, and edge adds 4 grams of tension piece increase tension force than proparea;Sizing using " double-clip-double-nip tandem sizing box, middle pressure, in it is dense, low viscous " sizing technique, slurry solid content 13.5 ± 1%;Weaving is using the Process configuration of " small tension receiving coil, big opening, the high back rest, early opening ", the rubber temple of three row's prickers of loom.First silk/corn fiber blending satin fabric produced by the invention is a kind of feature novel fabric as snug as a bug in a rug.

Description

A kind of preparation method of first silk and corn fiber blending satin fabric
Technical field
The present invention relates to a kind of preparation method of fabric, more particularly to a kind of first silk and corn fiber blending satin fabric Preparation method.
Background technology
First silk fiber is a kind of brand-new fiber produced using wood pulp as raw material through solvent spinning process.It has the comfortable of cotton Property, terylene toughness.Zein fiber is using starch such as corn, wheats as raw material, and the fermented lactic acid that changes into is aggregated again, spinning and Manufactured synthetic fibers.This fiber has zein fiber softly smooth, and intensity is big, and moisture absorption is breathed freely, and the product of processing has as silk Gloss and comfortable skin sense of touch and feel, drapability is good, good heat resistance and anti-ultraviolet function, and wearability is good.
The content of the invention
The purpose of the present invention is to be directed to above-mentioned present situation, there is provided a kind of preparation side of first silk and corn fiber blending satin fabric Method.
The technical solution adopted by the present invention:A kind of preparation method of first silk and corn fiber blending satin fabric, step is such as Under:
S1 materials prepare:Warp thread:First silk/zein fiber 9.8tex (70/30), yarn strength are more than 180CN;Weft yarn:Member Silk/zein fiber 9.8tex (70/30), yarn strength are more than 180CN;
S2 warping process:Discrete method configures tension force before, during and after, and edge adds 4 grams of tension piece increases than proparea Power, both sides alignment, warp beam edge are smooth;
S3 sizing operations:Sizing is using few PVA sizing techniques, slurry solid content 13.5 ± 1%;
S4 denting:Make warp thread in order, damaged with avoiding misdrawing, wearing strand and warp thread is produced because action is excessive, cause to break Head;
S5 weaving processes:Warp thread member silk/zein fiber 9.8tex and weft yarn member silk/zein fiber 9.8tex are interleaved Formed fabric, loom speed 480r/min, 2000 ± 200N of warp tension, 310 degree of heald level time, back rest position it is front and rear/ Highly be № .4~(40), menopause rack position it is front and rear/be highly № .2-5-30, the heald frame height of page 1~7 be 110mm, 110mm, 108mm, 105mm, 105mm, 112mm, 112mm, opening value are:70mm、55mm、60mm、45mm、100mm、 80mm, 70mm, easing amount be 310 degree-under;
S6 arranging processes:220 yards of croppings, obtain first silk and corn fiber blending satin fabric.
The present invention interweaves warp thread member silk/zein fiber 9.8tex and weft yarn member silk/zein fiber 9.8tex by 4/1 satin weave The satin fabric of production.First silk/corn fiber blending satin fabric of production is a kind of feature novel fabric as snug as a bug in a rug.
Embodiment
The principles and features of the present invention are described below, and the given examples are served only to explain the present invention, is not intended to limit Determine the scope of the present invention.
The present invention is by first silk/zein fiber yarn member silk/zein fiber 9.8tex and first silk/zein fiber yarn member silk/corn Fiber 9.8tex interweaves by 4/1 satin weave produces first silk/corn fiber blending satin fabric.Step is as follows:
S1 materials prepare:Warp thread:First silk/zein fiber 9.8tex (70/30), yarn strength are more than 180CN;Weft yarn:Member Silk/zein fiber 9.8tex (70/30), yarn strength are more than 180CN;
S2 warping process:Discrete method configures tension force before, during and after, and edge adds 4 grams of tension piece increases than proparea Power, warp beam edge are smooth;
Therefore warping process takes following measures and requirement:
1st, tension force:Tension force uses configuration less than normal to be segmented to reduce the strength loss of yarn stress before, during and after Method configures tension force, and edge warp tension ratio proparea is more 4 grams;
2nd, speed control is relatively low, controls 500 ms/min, and speed must accomplish stabilization, to reduce elongation and broken end;
3rd, equipment requirement:1. it is consistent with the position correspondence of tension bracket at spool rack guide, it is same with row between tension bracket Column alignment being aligned;2. yarn path is required without corrupted, burr, regeneration filoplume and extension occurs in warping path to prevent yarn It is disconnected;3. bobbin support height upper-lower position requires straight alignment;
4th, operation requires:1. requiring that all passages of yarn and head thoroughly clean before driving, done in time in startup procedure Cleaning makes to spend without product everywhere, prevents flyings to be enclosed in;Expansion reed product flower is cleared up at any time, product flower under yarn face in expansion reed, is cleared up per axle Once;2. touring in time in startup procedure, whether flexible, whether come off if observing the revolution of each tension pulley;3. 5 meters before driving, strictly Alignment both sides, occur without dilute or folding situation, to reach tension force arrangement, winding, uniform, the generation of reduction flyings regeneration filoplume; 4. to accomplish " repiece is uniform, change is accurate, it is suitable to manage head, and joint is firm " in operation, mosquito section is beaten, to eliminate strand head and break Head, improve warp beam quality.
S3 sizing operations:Sizing is using few PVA sizing techniques, and slurry solid content 13.5 ± 1%, formula of size is by following heavy Amount proportioning composition:
PVA-1799 10Kg/ bucket TH-100 50Kg/ bucket GR-796 50Kg/ bucket bleeding agent 1Kg/ buckets;
Size mixing:Slurry bucket, stock line cleaning are clean;Strictly performed by above wet end furnish, high pressure bucket is sized mixing, vexed slurry 20 Minute, it is ensured that grind slurries quality.
Stock tank viscosity, temperature stabilization, tension force is appropriate, plays sizing enhancing and protects the effect stretched.
Operation:Warp thread must arrange parallel uniform when sizing arranges reed, avoid the occurrence of broken end and twist head, influence loom efficiency.
S4 denting processes:
1. denting process must make warp thread in order, prevent to misdraw, wear strand;
2. comprehensive, reed, piece etc. must accomplish smooth no corrupted, impulse- free robustness;
3. operation requires:Warp thread is ramuscule cotton yarn, it is desirable to which operative employee acts when wearing button steadily to be avoided due to acting Damage is produced to warp thread greatly, causes to break end.
S5 weaving processes, warp thread member silk/zein fiber 9.8tex and weft yarn member silk/zein fiber 9.8tex are interleaved Form fabric, it is desirable to:
1. rubber rollers temple of the loom with three row's coronules, prevent edge broken end and needle path
2. stopping gap between latitude pin and drum barrel is less than 0.5 millimeter, double weft and looped weft are prevented.
3. relative humidity is 78--82%,
4. disconnected through beating mosquito knot, 0.3--0.4 centimetres of tieing yarn tail length during joint, anti-root yarn here is caused instead due to de- head Multiple disconnected warp
5. 220 yards of croppings, prevent narrow.
6. loom knitting technology and weaving situation are as follows:Loom type Tianjin field coltfoal ZA9100, loom speed 480r/min, 2000 ± 200N of warp tension, 310 degree of heald level time, back rest position it is front and rear/be highly № .4~(40), menopause rack position It is front and rear/be highly № .2-5-30, the heald frame height of page 1~7 be 110mm, 110mm, 108mm, 105mm, 105mm, 112mm, 112mm, opening value be 70mm, 55mm, 60mm, 45mm, 100mm, 80mm, 70mm, easing amount for 310 degree-under;Produce member Silk/zein fiber 9.8tex/ members silk/zein fiber 9.8tex 793.5 × 386 270.5 yuan silk/corn fiber blending crowfoot satin Thing.
S6 arranging processes, after 220 yards of croppings, knit requirement by repairing and produce first silk/zein fiber 9.8tex/ members silk/corn Fiber 9.8tex 793.5 × 386 270.5 yuan silk/corn fiber blending satin fabric.
The foregoing is only presently preferred embodiments of the present invention, be not intended to limit the invention, it is all the present invention spirit and Within principle, any modification, equivalent substitution and improvements made etc., it should be included in the scope of the protection.

Claims (3)

1. the preparation method of a kind of yuan of silk and corn fiber blending satin fabric, it is characterised in that step is as follows:
S1 materials prepare:Warp thread:First silk/zein fiber 9.8tex (70/30), yarn strength are more than 180CN;Weft yarn:First silk/jade Rice fiber 9.8tex (70/30), yarn strength are more than 180CN;
S2 warping process:Discrete method configures tension force before, during and after, and edge adds 4 grams of tension pieces increase tension force than proparea, and two Side is alignd, and warp beam edge is smooth;
S3 sizing operations:Sizing is using few PVA sizing techniques, slurry solid content 13.5 ± 1%;
S4 denting:Make warp thread in order, damaged with avoiding misdrawing, wearing strand and warp thread is produced because action is excessive, cause to break end;
S5 weaving processes:Warp thread member silk/zein fiber 9.8tex and weft yarn member silk/zein fiber 9.8tex are interleaved and formed Fabric, loom speed 480r/min, 2000 ± 200N of warp tension, 310 degree of heald level time, front and rear/height of back rest position For № .4~(40), menopause rack position it is front and rear/be highly № .2-5-30, the heald frame height of page 1~7 be 110mm, 110mm, 108mm, 105mm, 105mm, 112mm, 112mm, opening value are:70mm, 55mm, 60mm, 45mm, 100mm, 80mm, 70mm, Easing amount be 310 degree-under;
S6 arranging processes:220 yards of croppings, obtain first silk and corn fiber blending satin fabric.
2. the preparation method of a kind of first silk according to claim 1 and corn fiber blending satin fabric, it is characterised in that Formula of size is made up of following weight proportion:
PVA-1799 10Kg/ buckets, TH-100 50Kg/ buckets,
GR-796 50Kg/ buckets, bleeding agent 1Kg/ buckets.
3. the preparation method of a kind of first silk according to claim 2 and corn fiber blending satin fabric, it is characterised in that In step S5, rubber rollers temple of the weaving process loom with three row's coronules, stop gap between latitude pin and drum barrel and be less than 0.5 milli Rice, relative humidity are 78%~82%.
CN201711203893.XA 2017-11-27 2017-11-27 A kind of preparation method of first silk and corn fiber blending satin fabric Pending CN107740219A (en)