CN1075985C - Non-toxic disposable heating transfer manufacturing technology on metal surface - Google Patents

Non-toxic disposable heating transfer manufacturing technology on metal surface Download PDF

Info

Publication number
CN1075985C
CN1075985C CN97125656A CN97125656A CN1075985C CN 1075985 C CN1075985 C CN 1075985C CN 97125656 A CN97125656 A CN 97125656A CN 97125656 A CN97125656 A CN 97125656A CN 1075985 C CN1075985 C CN 1075985C
Authority
CN
China
Prior art keywords
non
toxic
metal surface
text
ink pattern
Prior art date
Application number
CN97125656A
Other languages
Chinese (zh)
Other versions
CN1220212A (en
Inventor
谭哲豪
Original Assignee
谭哲豪
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Family has litigation
Application filed by 谭哲豪 filed Critical 谭哲豪
Priority to CN97125656A priority Critical patent/CN1075985C/en
Publication of CN1220212A publication Critical patent/CN1220212A/en
Priority claimed from US09/365,317 external-priority patent/US6579400B1/en
Application granted granted Critical
Publication of CN1075985C publication Critical patent/CN1075985C/en
First worldwide family litigation filed litigation Critical https://patents.darts-ip.com/?family=5177350&utm_source=google_patent&utm_medium=platform_link&utm_campaign=public_patent_search&patent=CN1075985(C) "Global patent litigation dataset” by Darts-ip is licensed under a Creative Commons Attribution 4.0 International License.

Abstract

本发明公开一种金属表面无毒一次性加热转印的制作工艺,采用国际公认的无毒油墨,喷、涂、刷或打印在转印媒介上,用特制的薄膜覆盖,使无毒油墨图案、文字暂时吸附在特制的薄膜上,贴在金属表面上,经过一段时间加热,使图案、文字牢固印制在金属表面上。 The present invention discloses a non-toxic metal surface disposable thermal transfer production technology, internationally recognized non-toxic ink, spraying, coating, brushing, or printing on a transfer medium, with a special film covering the non-toxic ink pattern , the text is temporarily adsorbed in a special film, attached to the metal surface, after a period of heating of the pattern, the text printed on the metal surfaces firmly.

Description

金属表面无毒一次性加热转印的制作工艺 Non-toxic metal surface was added in one production process of the thermal transfer

本发明涉及在金属表面印制彩色图案、文字制作工艺的改进,特别是选用无毒油墨采用一次性加热制作工艺的方法,实现金属表面彩色图案、文字印制。 The present invention relates to a pattern printed on the metal surface to improve the color, character of the production process, in particular the use non-toxic method disposable heating the ink production process, the metal surface to achieve color patterns, printed text.

目前,在金属表面印制图案、文字是采用丝网印刷方法或移印方法等完成的,其缺点是丝网印刷只能在金属平面上操作,移印的缺点是印刷面积小,变形度大,大面积印刷漏印点较多,而且操作复杂,设备投资大。 Currently, the metal surface of the printed patterns, characters or a printing method using a screen printing method or the like and has as its only drawback is that the screen printing operations on a metal plane, the disadvantage is a small pad printing area, a large degree of deformation large area printing more were missing the point, and complex operation, large equipment investment.

本发明的目的是针对上述的缺点,研究一种新的方法,采用无毒油墨一次性加热转印的工艺,把需要印刷的图案、文字首先用丝网印制的方法,印制在平面的转印媒介上,然后在无毒油墨图案、文字上复盖特制的薄膜,油墨图案、文字吸附在特制的薄膜上。 Object of the present invention is directed to the above-mentioned drawbacks, a new method for research, non-toxic inks disposable thermal transfer process, the pattern to be printed, first text screen printing method, the printed planar a transfer medium, and then covered with a special thin film on a non-toxic ink pattern, text, ink pattern, text adsorbed on special film. 把特制的薄膜转贴在金属表面上,经过一次性加热,油墨图案、文字可以牢固的印制在金属表面上,达到可在大面积、不规则表面印制各种油墨图案、文字的目的。 Posted to a special film on the metal surface, through the disposable heating, the ink pattern, the text can be securely printed on the metal surface, it can reach a large area, various irregular surface of the printed ink pattern, the purpose of the text. 同时操作简单、设备投入少,灵活性高。 At the same time simple, less equipment investment, high flexibility.

本发明的目的是按以下工艺实现的:选用国际公认的无毒油墨,按设计的图案、文字,喷、涂、刷或打印在转印媒介上,然后在无毒油墨图案、文字上复盖特制的薄膜,使无毒油墨暂时吸附在特制的薄膜上。 Object of the present invention is achieved by the following process: selection of internationally recognized non-toxic ink, according to the design patterns, text, sprayed, painted, brushed or printed on the transfer medium, and then covered in a non-toxic ink pattern, text special film, so that the ink is temporarily adsorbed non-toxic in a special film. 把特制的薄膜准确的贴在需要印制图案、文字的金属表面上,把贴好特制薄膜的金属工件加热40至200℃,保温到时间是1至60分钟,无毒油墨图案、文字牢固印制在金属表面上。 The special film need to be printed in the exact pattern of the paste on the metal surface of the text, the special stickers good film to a metal workpiece 200 is heated for 40 deg.] C, the holding time is 1 to 60 minutes, non-toxic ink pattern, a solid printed text system on a metal surface.

由于采用本发明,可以有效的解决丝网印刷只能在平面上施实,移印在大面积印制中漏印、图案变形以及操作复杂、设备投入大等缺点。 As a result of the present invention, can effectively solve the screen printing can be applied on a real plane, stencil printing, pattern modifications and complex operation, equipment investment and other shortcomings of large-area printing.

结合实施例,进一步描述本发明的制作工艺方法:采用国际公认的无毒油墨,按设计的图案、文字喷、涂、刷或打印在转印媒介上,然后,在无毒油墨图案、文字上复盖特制的薄膜,使无毒的油墨图案、文字暂时吸附在特制的薄膜上。 Connection with the embodiment is further described production process of the present invention: non-toxic ink internationally recognized, according to the design patterns, text sprayed, painted, brushed or printed on the transfer medium, and then, non-toxic ink pattern, text special film covering the non-toxic ink pattern, text is temporarily adsorbed in a special film. 把带有无毒油墨图案、文字的特制的薄膜准确的贴在金属工件表面上,加热到90℃,保温20分钟,无毒油墨图案、文字牢固的印制在金属表面上。 The special film with non-toxic ink pattern, characters accurately attached to the surface of a metal workpiece heated to 90 ℃, incubated for 20 minutes, non-toxic ink pattern, the text printed on the solid metal surface. 能达到国际安全标准,如欧洲的EN71或美国ASTM标准。 Meet international safety standards, such as EN71 in Europe or the United States ASTM standards.

本发明所指的金属表面,包括金属原表面和经过表面处理后的金属表面。 The present invention refers to a metal surface, comprising the metal surface and the original surface after treated metal surface.

Claims (1)

1.金属表面无毒一次性加热转印的制作工艺,其特征是采用国际公认的无毒油墨,按设计的图案、文字喷、涂、刷或打印在转印媒介上,然后,在无毒油墨图案、文字上复盖特制的薄膜,使无毒的油墨图案,文字暂时吸附在特制的薄膜上,把带有无毒的油墨图案、文字的特制薄膜准确的贴在金属工件表面上,加热40至200℃,保温1至60分钟,无毒油墨图案、文字牢固印制在金属表面上,本发明所指的金属表面,包括金属原表面和经过表面处理后的金属表面。 1. Non-toxic metal surface of the heat transfer was added in one production process, characterized in that the internationally recognized non-toxic ink, according to the design patterns, text sprayed, painted, brushed or printed on the transfer medium, and then, in a non-toxic ink pattern, a special film covering the text, so that a non-toxic ink pattern, a special character is temporarily adsorbed on the film, the ink pattern with non-toxic, a special character accurate film attached to the surface of a metal workpiece heated 40 to 200 ℃, incubated for 1 to 60 minutes, non-toxic ink pattern, the text printed on the solid metal surface, the metal surface of the present invention referred to, include a metal surface and the original surface treatment after the metal surface.
CN97125656A 1997-12-19 1997-12-19 Non-toxic disposable heating transfer manufacturing technology on metal surface CN1075985C (en)