CN107434906A - A kind of lightweight carbon fiber epoxy composite environmental-friendly plate - Google Patents
A kind of lightweight carbon fiber epoxy composite environmental-friendly plate Download PDFInfo
- Publication number
- CN107434906A CN107434906A CN201710843698.7A CN201710843698A CN107434906A CN 107434906 A CN107434906 A CN 107434906A CN 201710843698 A CN201710843698 A CN 201710843698A CN 107434906 A CN107434906 A CN 107434906A
- Authority
- CN
- China
- Prior art keywords
- parts
- carbon fiber
- friendly plate
- composite environmental
- epoxy composite
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Pending
Abstract
The present invention provides a kind of lightweight carbon fiber epoxy composite environmental-friendly plate, it is characterised in that includes the component of following parts by weight:Carbon fiber:10 ~ 18 parts;Epoxy resin:35 ~ 50 parts;PTT:5 ~ 15 parts;Hollow powder:3 ~ 8 parts;Starch:10 ~ 25 parts;Expanded perlite:2 ~ 5 parts;Tissuemat E:3 ~ 8 parts;Environment-friendlyadhesive adhesive:15 ~ 30 parts;Antioxidant:0.5 ~ 2.5 part.The lightweight carbon fiber epoxy composite environmental-friendly plate, using epoxy resin-base, and it with the addition of carbon fiber and PTT, so that the composite materials property and good manufacturability, meanwhile, the composite density is low, loss of weight amplitude is big, raw material is green, has a wide range of application, and market potential is huge.
Description
Technical field
The present invention relates to building material field, is related specifically to a kind of lightweight carbon fiber epoxy composite environmental-friendly plate.
Background technology
With the innovation of China's materials for wall and the implementation of Building Energy Conservation Policy, the development and application of energy-saving building material by
Pay attention to extensive.Existing residential building wall uses reinforced concrete structure more, build up do after framework water-proofing treatment,
Decoration of exterior wall is laid and interior decoration.
However, current reality is, presence low intensity, the density of outer wall material are big, heat insulation effect is poor, and cost is high, is difficult to
The shortcomings that energy-conservation.Therefore, it is imperative that the high exterior wall environment-friendly materials of a kind of light weight, intensity are researched and developed.
The content of the invention
To solve above-mentioned problem, it is an object of the invention to provide a kind of lightweight carbon fiber epoxy complex loop
Protect plate.The lightweight carbon fiber epoxy composite environmental-friendly plate, using epoxy resin-base, and it with the addition of carbon fiber and gather to benzene
Naphthalate so that the composite materials property and good manufacturability, meanwhile, the composite density is low, subtracts
Weight amplitude is big, and raw material is green, has a wide range of application, and market potential is huge.
To reach above-mentioned purpose, the technical scheme is that:
A kind of lightweight carbon fiber epoxy composite environmental-friendly plate, include the component of following parts by weight:Carbon fiber:10 ~ 18 parts;Ring
Oxygen tree fat:35 ~ 50 parts;PTT:5 ~ 15 parts;Hollow powder:3 ~ 8 parts;Starch:10 ~ 25 parts;Expansion is precious
Zhu Yan:2 ~ 5 parts;Tissuemat E:3 ~ 8 parts;Environment-friendlyadhesive adhesive:15 ~ 30 parts;Antioxidant:0.5 ~ 2.5 part.Using epoxy resin-base,
And carbon fiber and PTT are with the addition of, improve bending and the tensile strength of composite so that described
Composite materials property and good manufacturability, meanwhile, density is low, and loss of weight amplitude is big, reaches the purpose for reducing composite weight.
Further, the component of following parts by weight is included:Carbon fiber:10 ~ 15 parts;Epoxy resin:35 ~ 42 parts;Poly- pair
Benzene dicarboxylic acid trimethylene glycol ester:5 ~ 12 parts;Hollow powder:3 ~ 5 parts;Starch:15 ~ 25 parts;Expanded perlite:2 ~ 4 parts;Polyethylene
Wax:4 ~ 8 parts;Environment-friendlyadhesive adhesive:15 ~ 23 parts;Antioxidant:0.5 ~ 1.5 part.
Further, the component of following parts by weight is included:Carbon fiber:12 parts;Epoxy resin:37 parts;Poly- terephthaldehyde
Acid propylene glycol ester:8 parts;Hollow powder:4 parts;Starch:20 parts;Expanded perlite:3 parts;Tissuemat E:5 parts;Environment-friendlyadhesive adhesive:22
Part;Antioxidant:1 part.
Further, the length of the carbon fiber is≤1mm, carbon content >=90%, ash content≤15%
Further, the starch is any of cornstarch, farina, starch from sweet potato.
Further, the environment-friendlyadhesive adhesive is formed by 100 parts of water and 16 ~ 28 parts of polyvinyl alcohol.
Further, the antioxidant is one or more of compositions in zinc oxide, titanium oxide, ceria.
The beneficial effects of the present invention are:
A kind of lightweight carbon fiber epoxy composite environmental-friendly plate of the present invention, using epoxy resin-base, and with the addition of carbon
Fiber and PTT so that the composite materials property and good manufacturability, meanwhile, the composite wood
Expect that density is low, loss of weight amplitude is big, and raw material is green, has a wide range of application, market potential is huge.
Embodiment
In order to make the purpose , technical scheme and advantage of the present invention be clearer, it is further detailed with reference to embodiments
Describe in detail bright.
Embodiment 1
A kind of lightweight carbon fiber epoxy composite environmental-friendly plate, include the component of following parts by weight:Carbon fiber:13 parts;Epoxy
Resin:48 parts;PTT:12 parts;Hollow powder:5 parts;Starch:10 parts;Expanded perlite:3 parts;It is poly-
Ethylene waxes:3 parts;Environment-friendlyadhesive adhesive:19 parts;Antioxidant:0.5 part.
Embodiment 2
A kind of lightweight carbon fiber epoxy composite environmental-friendly plate, include the component of following parts by weight:Carbon fiber:10 parts;Epoxy
Resin:35 parts;PTT:5 parts;Hollow powder:3 parts;Starch:15 parts;Expanded perlite:5 parts;Poly- second
Alkene wax:6 parts;Environment-friendlyadhesive adhesive:15 parts;Antioxidant:1 part.
Embodiment 3
A kind of lightweight carbon fiber epoxy composite environmental-friendly plate, include the component of following parts by weight:Carbon fiber:12 parts;Epoxy
Resin:37 parts;PTT:8 parts;Hollow powder:4 parts;Starch:20 parts;Expanded perlite:3 parts;Poly- second
Alkene wax:5 parts;Environment-friendlyadhesive adhesive:22 parts;Antioxidant:1 part.
Embodiment 4
A kind of lightweight carbon fiber epoxy composite environmental-friendly plate, include the component of following parts by weight:Carbon fiber:15 parts;Epoxy
Resin:50 parts;PTT:15 parts;Hollow powder:8 parts;Starch:18 parts;Expanded perlite:2 parts;It is poly-
Ethylene waxes:7 parts;Environment-friendlyadhesive adhesive:30 parts;Antioxidant:1.5 part.
Embodiment 5
A kind of lightweight carbon fiber epoxy composite environmental-friendly plate, include the component of following parts by weight:Carbon fiber:18 parts;Epoxy
Resin:45 parts;PTT:10 parts;Hollow powder:6 parts;Starch:13 parts;Expanded perlite:4 parts;It is poly-
Ethylene waxes:8 parts;Environment-friendlyadhesive adhesive:26 parts;Antioxidant:2.5 part.
The lightweight carbon fiber epoxy composite environmental-friendly plate, using epoxy resin-base, and it with the addition of carbon fiber and gather
Propylene glycol ester terephthalate so that the composite materials property and good manufacturability, meanwhile, the composite density
Low, only the 1/4 of Steel material, loss of weight amplitude is big, and raw material is green, has a wide range of application, market potential is huge.
It should be noted that the above embodiments are merely illustrative of the technical solutions of the present invention and it is unrestricted.Although with reference to compared with
The present invention is described in detail good embodiment, it will be understood by those within the art that, can be to the technology of invention
Scheme is modified or equivalent substitution, and without departing from the scope of technical solution of the present invention, it all should cover the power in the present invention
In sharp claimed range.
Claims (7)
1. a kind of lightweight carbon fiber epoxy composite environmental-friendly plate, it is characterised in that include the component of following parts by weight:Carbon is fine
Dimension:10 ~ 18 parts;Epoxy resin:35 ~ 50 parts;PTT:5 ~ 15 parts;Hollow powder:3 ~ 8 parts;Starch:
10 ~ 25 parts;Expanded perlite:2 ~ 5 parts;Tissuemat E:3 ~ 8 parts;Environment-friendlyadhesive adhesive:15 ~ 30 parts;Antioxidant:0.5 ~ 2.5 part.
2. a kind of lightweight carbon fiber epoxy composite environmental-friendly plate according to claim 1, it is characterised in that including as follows
The component of parts by weight:Carbon fiber:10 ~ 15 parts;Epoxy resin:35 ~ 42 parts;PTT:5 ~ 12 parts;It is empty
Heart micro mist:3 ~ 5 parts;Starch:15 ~ 25 parts;Expanded perlite:2 ~ 4 parts;Tissuemat E:4 ~ 8 parts;Environment-friendlyadhesive adhesive:15 ~ 23 parts;Antioxygen
Agent:0.5 ~ 1.5 part.
3. a kind of lightweight carbon fiber epoxy composite environmental-friendly plate according to claim 1, it is characterised in that including as follows
The component of parts by weight:Carbon fiber:12 parts;Epoxy resin:37 parts;PTT:8 parts;Hollow powder:4
Part;Starch:20 parts;Expanded perlite:3 parts;Tissuemat E:5 parts;Environment-friendlyadhesive adhesive:22 parts;Antioxidant:1 part.
4. a kind of lightweight carbon fiber epoxy composite environmental-friendly plate according to claim 1, it is characterised in that the carbon is fine
The length of dimension is≤1mm, carbon content >=90%, ash content≤15%.
A kind of 5. lightweight carbon fiber epoxy composite environmental-friendly plate according to claim 1, it is characterised in that the starch
For any of cornstarch, farina, starch from sweet potato.
A kind of 6. lightweight carbon fiber epoxy composite environmental-friendly plate according to claim 1, it is characterised in that the environmental protection
Glue is formed by 100 parts of water and 16 ~ 28 parts of polyvinyl alcohol.
A kind of 7. lightweight carbon fiber epoxy composite environmental-friendly plate according to claim 1, it is characterised in that the antioxygen
Agent is one or more of compositions in zinc oxide, titanium oxide, ceria.