CN107061736A - 一种用于中高压蒸汽系统密封面受损快速修复方法 - Google Patents
一种用于中高压蒸汽系统密封面受损快速修复方法 Download PDFInfo
- Publication number
- CN107061736A CN107061736A CN201611001856.6A CN201611001856A CN107061736A CN 107061736 A CN107061736 A CN 107061736A CN 201611001856 A CN201611001856 A CN 201611001856A CN 107061736 A CN107061736 A CN 107061736A
- Authority
- CN
- China
- Prior art keywords
- sealing surface
- impaired
- mesohigh
- sealing
- equipment
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Pending
Abstract
本发明涉及一种用于中高压蒸汽系统密封面受损快速修复方法,属于以中高压蒸汽为介质的管道及设备相关领域,本分明提供的专项技术解决了中高压蒸汽管道法兰、阀门、汽机缸盖及其他蒸汽连接设备密封面被蒸汽冲刷冲蚀产生沟槽,密封面损坏漏汽修复困难的问题;与在线堵漏高昂的维修费用及需要专门设备进行维修相比,本发明无需专门的设备进行修复,手工修复便可,维修费用极低,同时本发明密封修复方法还具有修复时间短、见效快的特点;无需更换设备(法兰、阀门等)直接修复,省去了设备购置及安装费用;无需返厂进行受损密封面焊接切削处理,可现场进行维修,避免发生返厂维修费用,同时也大大缩短了维修时间。
Description
技术领域
本发明属于以中高压蒸汽为介质的管道及设备相关领域,具体地说,涉及一种用于中高压蒸汽系统密封面受损快速修复方法。
背景技术
由于蒸汽工况波动管道收缩膨胀等原因,蒸汽管道法兰阀门,汽机缸盖等设备密封面容易出现泄漏,有时因泄漏不能得到及时处理,蒸汽长时间冲刷导致密封面出现沟槽,一旦密封面出现沟槽,更换垫片便不能解决蒸汽泄漏问题,目前国内处理蒸汽密封面受损方法有以下几种:
1、在线堵漏。方法是在泄漏部位装设专用设备,利用密封部位和专用设备之间形成的腔室,采用专用的高压注胶工具将密封胶注入腔室,并充满整个腔室空间,使密封胶的挤压力与泄漏介质的压力相平衡,建立一个新的密封结构来堵塞泄漏孔隙各通道,阻塞介质的外泄。此密封面修复方法比较成熟,但维修成本高,一般一个尺寸大小为DN300阀门修复费用约2万元,如果工厂处于偏远地区,维修成本会更高。
2、石墨、石墨纸堵漏。该方法简单,耗材便宜,但效果不理想,用于低压蒸汽管线已频繁发生二次泄漏,不能用于中高压蒸汽系统。
3、密封面重新加工,将密封面损坏设备返厂焊接车削加工密封面。该方法对于工厂而言基本不适用,原因是多数设备均是焊接于管道上(如法兰),而大型设备(如汽机缸体)则不利于返厂,再者返厂维修耗时长,加工成本高,对工厂而言经济损失太大。
4、直接更换受损设备。目前企业多采用此方法,因此需库存各种规格备件以备随时更换,备件积压量大,企业运营成本高。
以上各种方法均存在很大不足之处。
发明内容
为了克服背景技术中存在的问题,本发明提供了一种用于中高压蒸汽系统密封面受损快速修复方法,解决了蒸汽管道及设备连接面泄漏造成密封面受损修复困难的问题。
为实现上述目的,本发明是通过如下技术方案实现的:
一种用于中高压蒸汽系统密封面受损快速修复方法,具体步骤为:
1)受损密封面的清洁
将受损密封面进行清洁,根据受损密封面的受损程度及设备精密性,采用粗砂纸、细砂纸或塑料砂纸将受损密封面打磨,打磨要求为受损密封面现金属光泽,然后用干净的抹布将受损密封面清洁干净;
2)涂抹密封胶覆盖受损点
将密封胶涂抹于受损密封面受损处,或涂抹整个密封面,密封胶涂抹厚度要求为高于设备密封平面2mm左右;
3)布置密封绳
将密封绳沿受损密封面内外各布置一圈。
进一步地,步骤2)中所述的密封胶为耐高温、防水密封胶。
进一步地,步骤3)中所述的密封绳采用具有粘稠性、能耐高温、防水、具有可压缩性的石棉或石墨制成。
本发明的有益效果:
1、与在线堵漏高昂的维修费用及需要专门设备进行维修相比,本发明无需专门的设备进行修复,手工修复便可,维修费用极低,耗材为密封垫、少量密封胶及密封绳,同时本发明密封修复方法还具有修复时间短、见效快的特点;
2、无需更换设备(法兰、阀门等)直接修复,省去了设备购置及安装费用;
3、无需返厂进行受损密封面焊接切削处理,可现场进行维修,避免发生返厂维修费用,同时也大大缩短了维修时间。
附图说明
图1为步骤1)的示意图;
图2为步骤2)的示意图;
图3为步骤3)的示意图。
图中,1-受损密封面、2-密封胶、3-密封绳。
具体实施方式
一种用于中高压蒸汽系统密封面受损快速修复方法,具体步骤为:
1)受损密封面的清洁
将受损密封面1进行清洁,根据受损密封面1的受损程度及设备精密性,采用粗砂纸、细砂纸或塑料砂纸将受损密封面1打磨,打磨要求为受损密封面1现金属光泽,然后用干净的抹布将受损密封面1清洁干净;
2)涂抹密封胶覆盖受损点
将密封胶涂抹于受损密封面1受损处,或涂抹整个密封面,密封胶涂抹厚度要求为高于设备密封平面2mm左右;
3)布置密封绳
将密封绳3沿受损密封面1内外各布置一圈。
步骤2)中所述的密封胶2为耐高温、防水密封胶。
步骤3)中所述的密封绳3采用具有粘稠性、能耐高温、防水、具有可压缩性的石棉或石墨制成。
与在线堵漏高昂的维修费用及需要专门设备进行维修相比,本发明无需专门的设备进行修复,手工修复便可,维修费用极低,耗材为密封垫、少量密封胶及密封绳,同时本发明密封修复方法还具有修复时间短、见效快的特点;无需更换设备(法兰、阀门等)直接修复,省去了设备购置及安装费用;无需返厂进行受损密封面焊接切削处理,可现场进行维修,避免发生返厂维修费用,同时也大大缩短了维修时间。
最后说明的是,以上优选实施例及附图仅用以说明本发明的技术方案而非限制,尽管通过上述优选实施例已经对本发明进行了详细的描述,但本领域技术人员应当理解,可以在形式上和细节上对其作出各种各样的改变,而不偏离本发明权利要求书所限定的范围。
Claims (3)
1.一种用于中高压蒸汽系统密封面受损快速修复方法,其特征在于:具体步骤为:
1)受损密封面的清洁
将受损密封面进行清洁,根据受损密封面的受损程度及设备精密性,采用粗砂纸、细砂纸或塑料砂纸将受损密封面打磨,打磨要求为受损密封面现金属光泽,然后用干净的抹布将受损密封面清洁干净;
2)涂抹密封胶覆盖受损点
将密封胶涂抹于受损密封面受损处,或涂抹整个密封面,密封胶涂抹厚度要求为高于设备密封平面2mm左右;
3)布置密封绳
将密封绳沿受损密封面内外各布置一圈。
2.根据权利要1所述的一种用于中高压蒸汽系统密封面受损快速修复方法,其特征在于:步骤2)中所述的密封胶为耐高温、防水密封胶。
3.根据权利要1所述的一种用于中高压蒸汽系统密封面受损快速修复方法,其特征在于:步骤3)中所述的密封绳采用具有粘稠性、能耐高温、防水、具有可压缩性的石棉或石墨制成。