CN106905785A - A kind of glass transparent insulating nano paint and preparation method thereof - Google Patents

A kind of glass transparent insulating nano paint and preparation method thereof Download PDF

Info

Publication number
CN106905785A
CN106905785A CN201710243083.0A CN201710243083A CN106905785A CN 106905785 A CN106905785 A CN 106905785A CN 201710243083 A CN201710243083 A CN 201710243083A CN 106905785 A CN106905785 A CN 106905785A
Authority
CN
China
Prior art keywords
solid content
ato
transparent insulating
slurries
nano paint
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Pending
Application number
CN201710243083.0A
Other languages
Chinese (zh)
Inventor
龚伟
黄雪丽
邹建
刘华
刘光明
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Individual
Original Assignee
Individual
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Individual filed Critical Individual
Priority to CN201710243083.0A priority Critical patent/CN106905785A/en
Publication of CN106905785A publication Critical patent/CN106905785A/en
Pending legal-status Critical Current

Abstract

Invention is related to paint field.It is related to a kind of glass transparent insulating nano paint and preparation method thereof.The coating its raw material is calculated as by weight:55~65 parts of film-forming resin, solid content are 30 ± 2% 25~35 parts of nanoscale ATO-rare earths-polysilicon mixed slurries, 7~9 parts of deionized water, 0.8~1.2 part of defoamer, 0.4~0.6 part of coalescents, 0.4~0.6 part of auxiliary rheological agents.Product safety is nontoxic, with low cost and superior performance, there is good transmitance in visible region (380 ~ 780 nm), transmitance is up to 80 ~ 85%, light transmittance is 90% to clear glass in itself, so viewing from inside and daylighting are had no substantial effect on, and the rejection rate near infrared region (780 ~ 2500 nm) is significantly larger than automobile heat insulation film, and winter has same reflex to the infrared band of indoor generation, reach energy-saving heat preserving effect, energy-conservation is up to 25 ~ 30%.

Description

A kind of glass transparent insulating nano paint and preparation method thereof
Technical field
The present invention relates to paint field.It is related to a kind of glass transparent insulating nano paint and preparation method thereof.
Background technology
The summer high temperature time sustainable growth all over the world in view of the increasingly thin global climate of earth's ozone layer warms year by year.From National policy aspect is also fabulous guiding, the promulgation of National Renewable law of resources and Ministry of Construction's building energy conservation regulations, building section The implementation of energy regulations.Government advocates building energy conservation from each aspect Implementation of Recycling Economy, and the key of the weight of architectural energy consumption weight is just It is glass, reaches the standard of the energy-conservation 60% of national Tenth-Five Year Plan, it is to stand in the breach to solve glass power consumption.With the modern times The development of science and technology, energy-conservation and environmental protection receive the concern of more and more national.Building door glass pane, ceiling glass, vapour Car glass and ships glass have higher requirements to the permeability of visible ray, but make the same of visible light-transmissive daylighting needs are met When, the heat of sunshine is also transmitted therewith.Therefore, indoor temperature and air conditioner refrigerating energy consumption are produced a very large impact.Particularly exist Summer, the principal element of air conditioner load is constituted through the solar heat that windowpane gets in.The design temperature of usual air-conditioning with Load has following relation:The cryogenic temperature of setting improves 2 °C, and refrigeration electric load will reduce about 20%;What is set heats temperature Degree turns down 2 °C, and heating electric load will reduce about 30%.For energy saving, people employ metal coating heat-reflecting glass With various heat reflection pad pastings, to the energy in the sunshine of reflecting part, so as to reach the purpose of heat insulation and heat control.But, these There is visible region opacity and high reflectance in product, limit their range of application.And, some products are heat-insulated Effect on driving birds is not good, some light transmittances are relatively low, and the equipment for then needing costliness having, the control of process conditions is also very complicated.So product It is expensive, can only be used on vehicle glass, it is impossible on a large scale for Decoration Industry.
Make glass not only transparent but also heat-insulated, be always the key subjects that annoying technical specialist.Tradition solve glass every Heat problem mainly has three approach, and one is to use Heat insulation type adhering film, but the just valency of many units of every square metre of 300-600 of import thermal isolation film of factory Lattice make ordinary people be difficult to bear, and are only used on car at present;Two is to use thermal reflecting coating, but this product opacity, is made It cannot extensive use;Three is LOW-E double glazings, and there are production line, equipment and investment in You Ge famous brands producer of the current country Huge, operation cost is surging to cause every square metre of glass price in 280 or so units, many businessmans is not reluctant use comprehensively.
The appearance of brand-new material, for the solution of transparent heat-insulated problem provides new approach.With the painting that these materials are made Material, there is infrared shielding effect and good visible light transmissivity very high, meanwhile, also with certain intelligent.It is transparent heat-insulated What coating was that latest developments are got up a kind of has the transparency, both saturating to reach to the high reflectivity of infrared light district in visible region Bright and heat-insulated double effectses, and noise 20-30 decibels can be reduced.With very broad mass market prospect.
Tokyo Univ Japan scientific research personnel just have developed a kind of cost glass cheaper than vehicle explosion-proof film early in 2005 Insulating moulding coating.It is used primarily on door and window, curtain wall, glass roof, thus fashionable Japanese architecture industry., masschusetts, U.S.A reason in 2009 After engineering college adds a kind of nanometer glass microballon new material in the glass heat-insulating coating of Japan, propose product quality progress one High, cost is further reduced, and glass does not burst more at a high temperature of being spent 100!Contain mostly in existing glass nano coating There is wetting agent, but nano-glass microballon is expensive with wetting agent, causes coating with high costs.And existing glass heat-proof is applied Expect that resistance to rain brush is poor.
The content of the invention
It is an object of the invention to be directed to China's national situation, it is proposed that a kind of glass transparent insulating nano paint, can be effective Reduce the cost of glass transparent insulating nano paint.
To achieve these goals, the technical solution adopted in the present invention is, a kind of glass transparent insulating nano paint, its Raw material is calculated as by weight:55~65 parts of film-forming resin, solid content mix for 30 ± 2% nanoscale ATO-rare earths-polysilicons 25~35 parts of slurry, 7~9 parts of deionized water, 0.8~1.2 part of defoamer, 0.4~0.6 part of coalescents, auxiliary rheological agents 0.4~ 0.6 part.
Further, a kind of glass transparent insulating nano paint, its raw material is calculated as by weight:60 parts of film-forming resin, contain admittedly Measure is 30 ± 2% 30 parts of nanoscale ATO-rare earths-polysilicon mixed slurries, 8 parts of deionized water, 1 part of defoamer, coalescents 0.5 part, 0.5 part of auxiliary rheological agents.
Preferably, described film-forming resin is water-based fluorocarbon resin.
Further, described nanoscale ATO-rare earths-polysilicon mixed slurry use solid content for 65 ± 3% nanometer Level ATO slurries and solid content for 35 ± 2% rare earth-polysilicon mixed slurry mix after addition ethanol stir grind after institute .
Further, the preparation process of described rare earth-polysilicon mixed slurry is:By 30 ± 2% rare earth chloride finished products with 70 ± 4% polysilicon finished product is put into grinder, adds 2.8~3.2 times of dispersant, and 12h is ground in grinder, obtains 50- 60 nanoscale solid contents are 35 ± 2% rare earths-polycrystalline silica hybrid material.
The method for preparing glass transparent insulating nano paint as described above, comprises the following steps:
A. 30 ± 2% rare earth chloride finished products and 70 ± 4% polysilicon finished product are put into grinder, add 2.8~3.2 times Dispersant, grinds 12h in grinder, obtains solid content for 35 ± 2% rare earths-polycrystalline silica hybrid material;
B. by antimony tin powder, ethanol, dispersant and zirconium oxide mass ratio 1: 1.9~2.1:2.85~3.15:0.45~ 0.55 is placed in sand mill, and 36 h are ground under 2800~3200 r/min rotating speeds, is obtained the ATO that solid content is 65 ± 3% and is starched Material;
C. after ground ATO slurries are mixed with ground rare earth-polycrystalline silicon material again, mixed slurry in mass ratio:Second Alcohol=1: 1.9~2.1 add ethanol, are stirred on the high speed dispersor of 1100~1300 r/min, it is 30 to obtain solid content ± 2% will synthesize ATO slurries;
D. after film-forming resin, synthesis ATO slurries, deionized water, defoamer, coalescents, auxiliary rheological agents being mixed in proportion, Stirred on the high speed dispersor of 1100~1400 r/min, obtain product.
The solid content control of products obtained therefrom is coated 30% or so with 80# bars, is dried at room temperature, and thickness is at 15 μm Left and right.
Further, the step b is by antimony tin powder, ethanol, dispersant and zirconium oxide mass ratio 1: 2:3:0.5 puts In sand mill, 36 h are ground under 3000 r/min rotating speeds.
Further, the step c is again to mix ground ATO slurries with ground rare earth-polycrystalline silicon material Afterwards, mixed slurry in mass ratio:Ethanol=1: 2 add ethanol, are stirred on the high speed dispersor of 1200 r/min, obtain Solid content be 30% will synthesize ATO slurries.
Further, in the step d, mixing speed is 1200r/min.
Dynamic laser scattering method (DLS) granularmetric analysis is using N4 Plus nanometers of U.S. Beckman Coulter Grain Particle Size Analyzer, scattered slurry with water is diluted, using subsidiary particle size distribution prototype software calculate particle diameter and Particle diameter distribution.Visible and near infrared spectrum (Vis-NIR) analyzes the VarianCary in Varian Australia Pty Ltd Run on 500 ultraviolet-visible-near infrared spectrometers, wavelength is prepared on slide coating from 400~2500nm, And slide is placed on homemade In Situ Heating device, temperature-controlled precision is ± 0.1 DEG C.
The present invention possesses advantages below:
1. nanometer glass microballon instead of using nanoscale ATO-rare earth-polysilicon mixed slurries, effectively reduce product Cost, and each material proportioning is adapted to have fine infrared barrier effect;
2. expensive wetting agent is instead of with cheap deionized water, cost is further reduced;
3. nano-scale oxide is overcome in water instead of the polyurethane resin used by conventional nano coating using water-based fluorocarbon resin Property polyamide in be difficult decompose, easily reunite and sedimentation problem, while improve the water resistance of product, resistance to ag(e)ing and Finish;
4. product safety is nontoxic and has good transmitance in visible region (380~780nm), transmitance up to 80 ~ 85%, thoroughly Light transmittance is 90% to bright glass in itself, so have no substantial effect on viewing from inside and daylighting, and near infrared region (780~ Rejection rate 2500nm) is significantly larger than automobile heat insulation film, and winter, there is same reflection to make to the infrared band of indoor generation With, reaching energy-saving heat preserving effect, energy-conservation is up to 25~30%;
5. product has good construction quality, 20 minutes dry tack frees of constructing(Normal temperature), harden within 24 hours(Normal temperature), 7 days can It is fully cured;
6. preparation method advantages of simple, can be effectively obtained nano level mixed slurry, ensure product quality, and be easy to behaviour Work, device input are relatively low.
Specific embodiment
The present invention is described in further detail below by specific embodiment.
Embodiment 1:A kind of glass transparent insulating nano paint, its raw material is calculated as by weight:Water-based fluorocarbon resin 60 Part, solid content be 30 ± 2% 30 parts of nanoscale ATO-rare earths-polysilicon mixed slurries, 8 parts of deionized water, 1 part of defoamer, 0.5 part of coalescents, 0.5 part of auxiliary rheological agents.
The method for preparing glass transparent insulating nano paint as described above, comprises the following steps:
A. 30 ± 2% rare earth chloride finished products and 70 ± 4% polysilicon finished product are put into grinder, add 3 times of dispersant, 12h is ground in grinder, solid content is obtained for 35 ± 2% rare earths-polycrystalline silica hybrid material;
B. by antimony tin powder, ethanol, dispersant and zirconium oxide mass ratio 1: 2:3:0.5 is placed in sand mill, in 3000r/ 36 h are ground under min rotating speeds, the ATO slurries that solid content is 65 ± 3% are obtained;
C. after ground ATO slurries are mixed with ground rare earth-polycrystalline silicon material again, mixed slurry in mass ratio:Second Alcohol=1: 2 add ethanol, are stirred on the high speed dispersor of 1200 r/min, obtains solid content for 30 ± 2% will synthesize ATO slurries;
D. water-based fluorocarbon resin, synthesis ATO slurries, deionized water, defoamer, coalescents, auxiliary rheological agents are mixed in proportion Afterwards, stirred on the high speed dispersor of 1200 r/min, obtain product.
Solid content is obtained for 35 ± 2% rare earths-polycrystalline silica hybrid material particle diameter is 50 in can obtaining the step a by inspection ~60nm;It is 45~60nm that the ATO slurries particle diameter that solid content is 65 ± 3% is obtained in the step b, and the solid content of product is 30% Left and right, product other performances see the table below:
Infrared ray rejection rate More than 86% Cooling extent 4~8 DEG C
Ultraviolet isolating rate 99% Light transmittance ≥80%
Visible light transmissivity 84% Coating hardness 4H
Surface drying time 0.4h Adhesive force 1 grade
PH value 8-9 Brushing resistance >=2000 times
High temperature resistant 600℃ Peel strength 6N/mm
Embodiment 2:A kind of glass transparent insulating nano paint, its raw material is calculated as by weight:It is 65 parts of water-based fluorocarbon resin, solid Content is 30 ± 2% 35 parts of nanoscale ATO-rare earths-polysilicon mixed slurries, 9 parts of deionized water, 1.2 parts of defoamer, film forming 0.6 part of auxiliary agent, 0.6 part of auxiliary rheological agents.
The method for preparing glass transparent insulating nano paint as described above, comprises the following steps:
A. 30 ± 2% rare earth chloride finished products and 70 ± 4% polysilicon finished product are put into grinder, add 2.8 times of dispersion Agent, grinds 12h in grinder, obtains solid content for 35 ± 2% rare earths-polycrystalline silica hybrid material;
B. by antimony tin powder, ethanol, dispersant and zirconium oxide mass ratio 1: 1.9:2.85:0.45 is placed in sand mill, 36 h are ground under 3200r/min rotating speeds, the ATO slurries that solid content is 65 ± 3% are obtained;
C. after ground ATO slurries are mixed with ground rare earth-polycrystalline silicon material again, mixed slurry in mass ratio:Second Alcohol=1: 2.1 add ethanol, are stirred on the high speed dispersor of 1100 r/min, obtains solid content for 30 ± 2% will close Into ATO slurries;
D. after film-forming resin, synthesis ATO slurries, deionized water, defoamer, coalescents, auxiliary rheological agents being mixed in proportion, Stirred on the high speed dispersor of 1400 r/min, obtain product.
Embodiment 3:A kind of glass transparent insulating nano paint, its raw material is calculated as by weight:Water-based fluorocarbon resin 55 Part, solid content are 30 ± 2% 25 parts of nanoscale ATO-rare earths-polysilicon mixed slurries, 7 parts of deionized water, defoamer 0.8 Part, 0.4 part of coalescents, 0.4 part of auxiliary rheological agents.
The method for preparing glass transparent insulating nano paint as described above, comprises the following steps:
A. 30 ± 2% rare earth chloride finished products and 70 ± 4% polysilicon finished product are put into grinder, add 3.2 times of dispersion Agent, grinds 12h in grinder, obtains solid content for 35 ± 2% rare earths-polycrystalline silica hybrid material;
B. by antimony tin powder, ethanol, dispersant and zirconium oxide mass ratio 1: 2.1:2.85:0.55 is placed in sand mill, 36 h are ground under 2800r/min rotating speeds, the ATO slurries that solid content is 65 ± 3% are obtained;
C. after ground ATO slurries are mixed with ground rare earth-polycrystalline silicon material again, mixed slurry in mass ratio:Second Alcohol=1: 1.9 add ethanol, are stirred on the high speed dispersor of 1300 r/min, obtains solid content for 30 ± 2% will close Into ATO slurries;
D. after film-forming resin, synthesis ATO slurries, deionized water, defoamer, coalescents, auxiliary rheological agents being mixed in proportion, Stirred on the high speed dispersor of 1100 r/min, obtain product.
Embodiment 4:A kind of glass transparent insulating nano paint, its raw material is calculated as by weight:Water-based fluorocarbon resin 60 Part, solid content are 30 ± 2% 35 parts of nanoscale ATO-rare earths-polysilicon mixed slurries, 8 parts of deionized water, defoamer 1.2 Part, 0.55 part of coalescents, 0.45 part of auxiliary rheological agents.
The method for preparing glass transparent insulating nano paint as described above, comprises the following steps:
A. 30 ± 2% rare earth chloride finished products and 70 ± 4% polysilicon finished product are put into grinder, add 3 times of dispersant, 12h is ground in grinder, solid content is obtained for 35 ± 2% rare earths-polycrystalline silica hybrid material;
B. by antimony tin powder, ethanol, dispersant and zirconium oxide mass ratio 1: 2:3.15:0.55 is placed in sand mill, 36 h are ground under 3000r/min rotating speeds, the ATO slurries that solid content is 65 ± 3% are obtained;
C. after ground ATO slurries are mixed with ground rare earth-polycrystalline silicon material again, mixed slurry in mass ratio:Second Alcohol=1: 1.9 add ethanol, are stirred on the high speed dispersor of 1200 r/min, obtains solid content for 30 ± 2% will close Into ATO slurries;
D. after film-forming resin, synthesis ATO slurries, deionized water, defoamer, coalescents, auxiliary rheological agents being mixed in proportion, Stirred on the high speed dispersor of 1200r/min, obtain product.
Embodiment 5:A kind of glass transparent insulating nano paint, its raw material is calculated as by weight:Waterborne polyurethane resin 60 Part, solid content be 30 ± 2% 30 parts of nanoscale ATO-rare earths-polysilicon mixed slurries, 8 parts of deionized water, 1 part of defoamer, 0.5 part of coalescents, 0.5 part of auxiliary rheological agents.
The method for preparing glass transparent insulating nano paint as described above, comprises the following steps:
A. 30 ± 2% rare earth chloride finished products and 70 ± 4% polysilicon finished product are put into grinder, add 3 times of dispersant, 12h is ground in grinder, solid content is obtained for 35 ± 2% rare earths-polycrystalline silica hybrid material;
B. by antimony tin powder, ethanol, dispersant and zirconium oxide mass ratio 1: 2:3:0.5 is placed in sand mill, in 3000r/ 36 h are ground under min rotating speeds, the ATO slurries that solid content is 65 ± 3% are obtained;
C. after ground ATO slurries are mixed with ground rare earth-polycrystalline silicon material again, mixed slurry in mass ratio:Second Alcohol=1: 2 add ethanol, are stirred on the high speed dispersor of 1200 r/min, obtains solid content for 30 ± 2% will synthesize ATO slurries;
D. waterborne polyurethane resin, synthesis ATO slurries, deionized water, defoamer, coalescents, auxiliary rheological agents are mixed in proportion After conjunction, stirred on the high speed dispersor of 1200 r/min, obtain product.
Embodiment 6:Substantially similar to embodiment 1, its difference is that film-forming resin is using inorganic nano ceramics tree Fat.
Embodiment 7:Substantially similar to embodiment 2, its difference is that film-forming resin uses organic siliconresin.
The preferred embodiments of the present invention are the foregoing is only, is not intended to limit the invention, for the skill of this area For art personnel, there can be various modifications and variations in the spirit and principles in the present invention, these equivalent modifications or replacement etc., It is all contained within protection scope of the present invention.

Claims (8)

1. a kind of glass transparent insulating nano paint, it is characterised in that its raw material is calculated as by weight:Film-forming resin 55~65 Part, solid content are 30 ± 2% 25~35 parts of nanoscale ATO-rare earths-polysilicon mixed slurries, 7~9 parts of deionized water, froth breaking 0.8~1.2 part of agent, 0.4~0.6 part of coalescents, 0.4~0.6 part of auxiliary rheological agents.
2. a kind of glass transparent insulating nano paint according to claim 1, it is characterised in that its raw material is by weight For:60 parts of film-forming resin, solid content are 30 ± 2% 30 parts of nanoscale ATO-rare earths-polysilicon mixed slurries, deionized water 8 Part, 1 part of defoamer, 0.5 part of coalescents, 0.5 part of auxiliary rheological agents.
3. a kind of glass transparent insulating nano paint according to claim 1 and 2, it is characterised in that:Described film forming tree Fat is water-based fluorocarbon resin.
4. a kind of glass transparent insulating nano paint according to claim 1 and 2, it is characterised in that:Described nanoscale It is 35 ± 2% for 65 ± 3% nanoscale ATO slurries and solid content that ATO-rare earth-polysilicon mixed slurry uses solid content Gained after addition ethanol stirs and grinds after rare earth-polysilicon mixed slurry mixing.
5. a kind of glass transparent insulating nano paint according to claim 4, it is characterised in that:Described rare earth-polycrystalline The preparation process of silicon mixed slurry is:30 ± 2% rare earth chloride finished products and 70 ± 4% polysilicon finished product are put into grinder, 2.8~3.2 times of dispersant is added, 12h is ground in grinder, obtain 50-60 nanoscales solid content for 35 ± 2% rare earths-many Crystal silicon mixing material.
6. the method for preparing glass transparent insulating nano paint as described in claim 1-5 is any, it is characterised in that including with Lower step:
A. 30 ± 2% rare earth chloride finished products and 70 ± 4% polysilicon finished product are put into grinder, add 2.8~3.2 times Dispersant, grinds 12h in grinder, obtains solid content for 35 ± 2% rare earths-polycrystalline silica hybrid material;
B. by antimony tin powder, ethanol, dispersant and zirconium oxide mass ratio 1: 1.9~2.1:2.85~3.15:0.45~ 0.55 is placed in sand mill, and 36 h are ground under 2800~3200 r/min rotating speeds, is obtained the ATO that solid content is 65 ± 3% and is starched Material;
C. after ground ATO slurries are mixed with ground rare earth-polycrystalline silicon material again, mixed slurry in mass ratio:Second Alcohol=1: 1.9~2.1 add ethanol, are stirred on the high speed dispersor of 1100~1300 r/min, it is 30 to obtain solid content ± 2% will synthesize ATO slurries;
D. after film-forming resin, synthesis ATO slurries, deionized water, defoamer, coalescents, auxiliary rheological agents being mixed in proportion, Stirred on the high speed dispersor of 1100~1400 r/min, obtain product.
7. the preparation method of a kind of glass transparent insulating nano paint according to claim 6, it is characterised in that:The step Rapid b is by antimony tin powder, ethanol, dispersant and zirconium oxide mass ratio 1: 2:3:0.5 is placed in sand mill, in 3000 r/ 36 h are ground under min rotating speeds.
8. the preparation method of a kind of glass transparent insulating nano paint according to claim 6, it is characterised in that:The step Rapid c is after ground ATO slurries are mixed with ground rare earth-polycrystalline silicon material again, in mass ratio mixed slurry:Second Alcohol=1: 2 add ethanol, are stirred on the high speed dispersor of 1200 r/min, it is that 30% will synthesize ATO to obtain solid content Slurry.
CN201710243083.0A 2017-04-14 2017-04-14 A kind of glass transparent insulating nano paint and preparation method thereof Pending CN106905785A (en)