CN106833185A - A kind of preparation method of extinguishing waterborn coating - Google Patents

A kind of preparation method of extinguishing waterborn coating Download PDF

Info

Publication number
CN106833185A
CN106833185A CN201611245011.1A CN201611245011A CN106833185A CN 106833185 A CN106833185 A CN 106833185A CN 201611245011 A CN201611245011 A CN 201611245011A CN 106833185 A CN106833185 A CN 106833185A
Authority
CN
China
Prior art keywords
parts
preparation
extinguishing waterborn
bastose
modified
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Pending
Application number
CN201611245011.1A
Other languages
Chinese (zh)
Inventor
邓金玲
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Dalian Bi Cheng Environmental Protection Science And Technology Co Ltd
Original Assignee
Dalian Bi Cheng Environmental Protection Science And Technology Co Ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Dalian Bi Cheng Environmental Protection Science And Technology Co Ltd filed Critical Dalian Bi Cheng Environmental Protection Science And Technology Co Ltd
Priority to CN201611245011.1A priority Critical patent/CN106833185A/en
Publication of CN106833185A publication Critical patent/CN106833185A/en
Pending legal-status Critical Current

Abstract

The invention belongs to water paint field, and in particular to a kind of preparation method of extinguishing waterborn coating, the water paint is prepared from the following raw materials in parts by weight:60 65 parts of water, 16 18 parts of polyvinyl alcohol, 20 23 parts of acrylic resins, 58 parts of nano silicons, 34 parts of diatomite, 10 15 parts of modified bastoses, 26 parts of dioctyl phthalates, 15 parts of organic silicon defoamers, 10 12 parts of triethanolamines, 0.2 0.5 parts of silane coupler KH570,0.1 0.5 parts of dodecyl sodium sulfates.The present invention in hydrotropism's coating system by adding modified fire retardant, improve the anti-flammability of water paint, and the halogen-free flame retardants, flame retarding efficiency is high, anti-flammability is lasting, environmentally safe, the water paint only with extremely low toxicity alcohol ethers solvent, improve process environment conditions, what is more important, the water paint has good weatherability and adhesive force, and preparation method is simple, have a wide range of application, be adapted to promote and mass produce.

Description

A kind of preparation method of extinguishing waterborn coating
Technical field
The invention belongs to water paint field, and in particular to a kind of preparation method of extinguishing waterborn coating.
Background technology
Extinguishing waterborn coating can be reduced by the combustibility of painting material surface, effectively prevent fire from spreading rapidly, improve knot The material of structure fire endurance, the extinguishing waterborn coating of prior art is generally by adding expansion resistance in polyurethane-based paints, matrix Combustion system obtains anti-flaming dope.At present, more conventional Intumescent Retardant System is melamine-polyphosphoric acid amine composite, The composite can produce substantial amounts of cigarette in preparation and burning, and the system weatherability, heatproof oxidation performance aspect are poor.Separately A kind of outer anti-flaming dope is to adding PVC in matrix, although has good flame retardant effect after adding PVC, but contains in PVC Chlorine element, can resolve into toxic gas in combustion, therefore, such anti-flaming dope hardly consistent with fire-fighting, building requirement, It is difficult to promote the use of.In sum, this area needs a kind of extinguishing waterborn coating of environmental protection badly.
The content of the invention
To solve, extinguishing waterborn coating flame retarding efficiency in the prior art is low, anti-flammability is not lasting, be also easy to produce pollution air A kind of problem of noxious material, there is provided preparation method of the extinguishing waterborn coating of environmental protection.
The present invention is adopted the following technical scheme that:A kind of extinguishing waterborn coating is prepared from the following raw materials in parts by weight:60-65 Part water, 16-18 parts of polyvinyl alcohol, 20-23 parts of acrylic resin, 5-8 parts of nano silicon, 3-4 parts of diatomite, 10-15 parts Modified bastose, 2-6 parts of dioctyl phthalate, 1-5 parts of organic silicon defoamer, 10-12 parts of triethanolamine, 0.2-0.5 Part KH570,0.1-0.5 part of dodecyl sodium sulfate of silane coupler;
The preparation method of described modified bastose is:By bastose cut-out, powder is broken into, it is dry in 60-70 DEG C After dry 5 hours, swelling 10 minutes in alkali lye, by swelling bastose, Polyphenyl phosphate, TBAB according to matter Amount compares 1:1:0.05 is placed in stirring container, in being reacted 3-6 hours at 70-80 DEG C, after reaction terminates, is washed with acetone, will wash Product after washing is dried in drying box, and modified bastose is obtained;
The preparation method of described extinguishing waterborn coating is:First acrylic resin is heated and is melted, be slowly added into polyethylene Alcohol, is stirred 20-35 minutes, and 85-90 DEG C is heated in stirred tank is added water to after polyvinyl alcohol all dissolving, and mixing speed is 500r/min, after stirring 0.5-1 hours, adds organic silicon defoamer, stirs 0.5-1 hours, is cooled to 35 DEG C, adds dodecane Base sodium sulfonate, dioctyl phthalate, after being further continued for stirring 1 hour, stop stirring, to adding nanometer titanium dioxide in reactor Silicon, modified bastose, after ultrasonic vibration 1-1.5 hours, 75 DEG C of constant temperature are warming up to 2 hours by reactor, and diatom is added again Soil, triethanolamine, silane coupler KH570, constant temperature 5 hours close reactor, obtain final product extinguishing waterborn coating.
Used as a preferred embodiment, extinguishing waterborn coating is prepared from the following raw materials in parts by weight:65 parts of water, 17 parts Polyvinyl alcohol, 22 parts of acrylic resins, 6 parts of nano silicons, 4 parts of diatomite, 12 parts of modified bastoses, 5 parts of adjacent benzene two Formic acid dioctyl ester, 2 parts of organic silicon defoamers, 11 parts of triethanolamines, 0.4 part of silane coupler KH570,0.5 part of dodecyl sulphur Sour sodium.
Further, described polyvinyl alcohol is PVA 1788.
The present invention improves the anti-flammability of water paint by adding modified fire retardant in hydrotropism's coating system, and The fire retardant by bastose chemical modification, the halogen-free flame retardants that Polyphenyl phosphate is obtained being grafted on its strand, Flame retarding efficiency is high, anti-flammability is lasting, environmentally safe, and the water paint improves only with the alcohol ethers solvent of extremely low toxicity Process environment conditions, it is even more important that the water paint has good weatherability and adhesive force, preparation method is simple, should It is wide with scope, it is adapted to promote and mass produces.
Specific embodiment
With reference to specific embodiment to technical scheme further instruction, but the present invention is not in any form It is limited to embodiment content.Experimental technique described in embodiment unless otherwise specified, is conventional method, unless otherwise specified, The chemical reagent and material, commercially obtain.The degree of polymerization of the PVA 1788 is 1700, and alcoholysis degree is 88%.
Embodiment 1
By the cut-out of 15 weight portion bastoses, powder is broken into, in after 65 DEG C of dryings 5 hours, swelling 10 points in alkali lye Clock, by swelling bastose, Polyphenyl phosphate, TBAB according to mass ratio 1:1:0.05 is placed in stirring container In, in being reacted 5 hours at 75 DEG C, after reaction terminates, washed with acetone, the product after washing is dried in drying box, it is obtained Modified bastose.
Embodiment 2
A kind of extinguishing waterborn coating is prepared from the following raw materials in parts by weight:60g water, 16g polyvinyl alcohol 1788,20g third Olefin(e) acid resin, 6g nano silicons, 4g diatomite, 10g are modified bastose, 2g dioctyl phthalates, 4g organosilicons Defoamer, 12g triethanolamines, 0.5g silane coupler KH570,0.2g dodecyl sodium sulfates.
The preparation method of described extinguishing waterborn coating is:First acrylic resin is heated and is melted, be slowly added into polyethylene Alcohol, is stirred 35 minutes, and 90 DEG C are heated in stirred tank is added water to after polyvinyl alcohol all dissolving, and mixing speed is 500r/ Min, after stirring 40 minutes, adds organic silicon defoamer, stirs 1 hour, is cooled to 35 DEG C, adds dodecyl sodium sulfate, neighbour Dioctyl phthalate, after being further continued for stirring 1 hour, stops stirring, to addition nano silicon, modified bluish dogbane in reactor Fiber, ultrasonic vibration is after 1 hour, and reactor is warming up into 75 DEG C of constant temperature 2 hours, and diatomite, triethanolamine, silane are added again Coupling agent KH570, constant temperature 5 hours closes reactor, obtains final product extinguishing waterborn coating.
Embodiment 3
A kind of extinguishing waterborn coating is prepared from the following raw materials in parts by weight:65g water, 18g polyvinyl alcohol, 23g acrylic acid Resin, 8g nano silicons, 3g diatomite, 15g are modified bastose, 5g dioctyl phthalates, 1g organosilicon froth breakings Agent, 10g triethanolamines, 0.2g silane coupler KH570,0.1g dodecyl sodium sulfates.
The preparation method of described extinguishing waterborn coating is:First acrylic resin is heated and is melted, be slowly added into polyethylene Alcohol, is stirred 35 minutes, and 85 DEG C are heated in stirred tank is added water to after polyvinyl alcohol all dissolving, and mixing speed is 500r/ After min, stirring 0.5 hour, add organic silicon defoamer, stir 0.5 hour, be cooled to 35 DEG C, add dodecyl sodium sulfate, Dioctyl phthalate, after being further continued for stirring 1 hour, stops stirring, to adding nano silicon, modified red in reactor Flaxen fiber, ultrasonic vibration is after 1.5 hours, and reactor is warming up into 75 DEG C of constant temperature 2 hours, add again diatomite, triethanolamine, Silane coupler KH570, constant temperature 5 hours closes reactor, obtains final product extinguishing waterborn coating.
Embodiment 4
A kind of extinguishing waterborn coating is prepared from the following raw materials in parts by weight:65g water, 17g polyvinyl alcohol, 22g acrylic acid Resin, 5g nano silicons, 4g diatomite, 12g are modified bastose, 5g dioctyl phthalates, 2g organosilicon froth breakings Agent, 11g triethanolamines, 0.4g silane coupler KH570,0.5g dodecyl sodium sulfates;
The preparation method of described extinguishing waterborn coating is:First acrylic resin is heated and is melted, be slowly added into polyethylene Alcohol, is stirred 35 minutes, and 90 DEG C are heated in stirred tank is added water to after polyvinyl alcohol all dissolving, and mixing speed is 500r/ Min, after stirring 1 hour, adds organic silicon defoamer, stirs 1 hour, is cooled to 35 DEG C, adds dodecyl sodium sulfate, adjacent benzene Diformazan dioctyl phthalate, after being further continued for stirring 1 hour, stops stirring, and to being added in reactor, nano silicon, modified bluish dogbane are fine Dimension, ultrasonic vibration is after 1 hour, and reactor is warming up into 75 DEG C of constant temperature 2 hours, and diatomite, triethanolamine, silane idol are added again Connection agent KH570, constant temperature 5 hours closes reactor, obtains final product extinguishing waterborn coating.
Comparative example
A kind of extinguishing waterborn coating is prepared from the following raw materials in parts by weight:65g water, 18g polyvinyl alcohol, 23g acrylic acid Resin, 8g nano silicons, 5g dioctyl phthalates, 1g organic silicon defoamers, 10g triethanolamines, 0.2g silane idols Connection agent KH570,0.1g dodecyl sodium sulfate.
The preparation method of described extinguishing waterborn coating is:First acrylic resin is heated and is melted, be slowly added into polyethylene Alcohol, is stirred 35 minutes, and 90 DEG C are heated in stirred tank is added water to after polyvinyl alcohol all dissolving, and mixing speed is 500r/ Min, after stirring 1 hour, adds organic silicon defoamer, stirs 1 hour, is cooled to 35 DEG C, adds dodecyl sodium sulfate, adjacent benzene Diformazan dioctyl phthalate, after being further continued for stirring 1 hour, stops stirring, to adding nano silicon, ultrasonic vibration 1 in reactor After hour, reactor is warming up to 75 DEG C of constant temperature 2 hours, triethanolamine, silane coupler KH570 are added again, constant temperature 5 is small When, reactor is closed, obtain final product extinguishing waterborn coating.
Test example:
The embodiment of the present invention and comparative example are carried out into experimental test according to GBT/T 9756-2009 national standards, is measured Experimental data is as shown in table 1.
Table 1:
Flame retardant rating Alkali resistance (48h) Coating appearance Water Resistance Test (160h)
Embodiment 2 V-0 It is without exception Normally It is without exception
Embodiment 3 V-0 It is without exception Normally It is without exception
Embodiment 4 V-0 It is without exception Normally It is without exception
Comparative example HB It is without exception Normally It is without exception
, without precipitation, without caking, water resistance experiment is without exception, and alkaline resistance test is as good as the coating appearance of the embodiment of the present invention Often, abrasion resistance experiment:Pass through for 10000 times, film can reach V-0 without breakage, flame retardant rating, there are cigarette burning < 10s, smokelessly Burning < 30s, only micro or a small amount of white cigarette occurs, and flame retarding efficiency is high, and fire-retardant persistence is good.

Claims (3)

1. a kind of preparation method of extinguishing waterborn coating, it is characterised in that the extinguishing waterborn coating is by following parts by weight Raw material is made:60-65 parts of water, 16-18 parts of polyvinyl alcohol, 20-23 parts of acrylic resin, 5-8 parts of nano silicon, 3-4 parts Diatomite, 10-15 part of modified bastose, 2-6 parts of dioctyl phthalate, 1-5 parts of organic silicon defoamer, 10-12 parts three Monoethanolamine, 0.2-0.5 part of silane coupler KH570,0.1-0.5 part dodecyl sodium sulfate;
The preparation method of described modified bastose is:By bastose cut-out, powder is broken into, it is small in 60-70 DEG C of drying 5 Shi Hou, swelling 10 minutes in alkali lye, by swelling bastose, Polyphenyl phosphate, TBAB according to mass ratio 1:1:0.05 is placed in stirring container, in being reacted 3-6 hours at 70-80 DEG C, after reaction terminates, is washed with acetone, after washing Product dried in drying box, modified bastose is obtained;
The preparation method of described extinguishing waterborn coating is:First acrylic resin is heated and is melted, be slowly added into polyvinyl alcohol, stirred Mix 20-35 minutes, 85-90 DEG C is heated in stirred tank is added water to after polyvinyl alcohol all dissolving, mixing speed is 500r/ Min, after stirring 0.5-1 hours, adds organic silicon defoamer, stirs 0.5-1 hours, is cooled to 35 DEG C, adds dodecyl sulphur Sour sodium, dioctyl phthalate, be further continued for stirring 1 hour after, stop stirring, in reactor add nano silicon, Modified bastose, after ultrasonic vibration 1-1.5 hour, 75 DEG C of constant temperature is warming up to 2 hours by reactor, again addition diatomite, Triethanolamine, silane coupler KH570, constant temperature 5 hours close reactor, obtain final product extinguishing waterborn coating.
2. the preparation method of extinguishing waterborn coating according to claim 1, it is characterised in that extinguishing waterborn coating is by following The raw material of parts by weight is made:65 portions of water, 17 portions of polyvinyl alcohol, 22 portions of acrylic resins, 6 portions of nano silicons, 4 portions of diatoms Soil, 12 parts of modified bastoses, 5 parts of dioctyl phthalates, 2 parts of organic silicon defoamers, 11 parts of triethanolamines, 0.4 part of silicon Alkane coupling agent KH570,0.5 part of dodecyl sodium sulfate.
3. the preparation method of extinguishing waterborn coating according to claim 1, it is characterised in that described polyvinyl alcohol is PVA 1788。
CN201611245011.1A 2016-12-29 2016-12-29 A kind of preparation method of extinguishing waterborn coating Pending CN106833185A (en)