CN106113209A - A kind of New planing plank floor - Google Patents
A kind of New planing plank floor Download PDFInfo
- Publication number
- CN106113209A CN106113209A CN201610483410.5A CN201610483410A CN106113209A CN 106113209 A CN106113209 A CN 106113209A CN 201610483410 A CN201610483410 A CN 201610483410A CN 106113209 A CN106113209 A CN 106113209A
- Authority
- CN
- China
- Prior art keywords
- wood
- plank
- wood shavings
- glue
- floor
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Pending
Abstract
The invention discloses the production method on a kind of new floor of planing the plank: (1) wood shavings fiber pretreatment: pretreatment fluid of being sprayed water by wood shavings fiber, regulation is to water content 10%, glue mixing wood shavings are arranged by two top layers up and down of oriented wood chipboard by its machine direction stringer, and sandwich layer wood shavings are transversely arranged, composition three-decker plate embryo, and then hot pressing makes oriented wood chipboard, the orienting spreading of oriented wood chipboard makes it have the feature of higher-strength in a direction, plywood can be replaced to do structural wood and use;(2) high temperature high pressure process;(3) balance;(4) PVC board is overlayed;(5) smooth must put more than 72 hours after hot pressing, then cut;(6) finished product floor must seal paint, tongue and groove sealing wax overleaf.
Description
Technical field
The present invention relates to a kind of New planing plank floor and preparation method thereof, belong to timber floor and make field.
Background technology
Chinese forest resource is hidden weary, and timber supply and demand is uneven, since country implements wildwood protected project, and domestic wood
Material insufficiency of supply-demand increases year by year.At present, annual timber breach is huge.
Particieboard (Particle board) be again particle board, particle board, bagasse board, by timber or other lignocellulose
The particle that material is made, the wood-based plate composed under heating power and pressure effect after applying adhesive, also known as flakeboard.Main use
In Furniture manufacture and building industry and train, automobile bodies manufacture.
Because particieboard structure comparison is uniform, good processability can be processed into the sheet material of large format as required, is system
Make the preferable raw material of furniture of different size, pattern.Manufactured goods particieboard need not after drying, can directly use, and inhales
Sound and sound insulation value are the most fine.But it also has the shortcoming that it is intrinsic, because edge roughness, easy moisture absorption, so the particieboard system of using
The edge sealing of furniture technique made just seems particular importance.Relatively big additionally, due to particieboard volume, use its Hepplewhite, relative to it
For his sheet material, the most heavier.
Glue-free particieboard production process can be without any adhesive and chemical agent, it is possible to rely on therein
The change studied point and reaction are produced from glued effect, the not harmful gas such as Diazolidinyl Urea during producing and using, no
Production environment and environment for human survival can be produced any impact.Carry out the research of glue-free particieboard, be possible not only to reduce wood shavings
Plate production cost, and particieboard product specification can be promoted, expand product purpose, alleviate problem of environmental pollution.Therefore,
Glue-free particieboard development prospect is wide.But, the glue-free particieboard physical and mechanical property that common heat pressing process manufactures is poor, especially
Being that thickness swelling rate is big, the production cycle is long, and production efficiency is low.During particieboard steam injection pressing, slab bears water and heat
Synergism, can produce more from glued composition, improve sheet material mechanical property, be greatly shortened pressing cycle.
It is desirable to provide a kind of new floor of planing the plank, in the material being commonly used in wall of planing the plank, the present invention
Plane the plank and may be used in floor, this material is economic and environment-friendly, and quality is softer, good heat insulating, particularly with the addition of
Layer of PVC, advantage is that anti-deformation nature is good, top layer is PVC board, wear-resisting, glossy.
Summary of the invention
The technical problem existed based on background technology, the present invention provides a kind of new floor of planing the plank, general using of planing the plank
In the material of wall, the present invention plane the plank and may be used in floor, this material is economic and environment-friendly, and quality is relatively
Soft, good heat insulating, particularly with the addition of layer of PVC, advantage is that anti-deformation nature is good, and top layer is PVC board, wear-resisting, glossy.
Technical scheme is as follows:
A kind of production method on new floor of planing the plank, its step is as follows:
(1) wood shavings fiber pretreatment:
By wood shavings fiber water spray pretreatment fluid, regulation is to water content 10%, and two top layers up and down of oriented wood chipboard are by glue mixing wood shavings
Arrange by its machine direction stringer, and sandwich layer wood shavings are transversely arranged, form three-decker plate embryo, and then oriented shaving is made in hot pressing
Plate, the orienting spreading of oriented wood chipboard makes it have the feature of higher-strength in a direction, and plywood can be replaced to do structure
Material uses;
The formula of described pretreatment is: according to mass fraction, 0.5-1.1% lactic acid, 1.2% sodium citrate, remaining is water;
(2) high temperature high pressure process:
Solid wood is used to laminate technology and " zero formaldehyde " technique to wood deep processing, press pressure > 60MPa, operating temperature 170-190
Degree Celsius, 700 seconds press times;
(3) balance:
Plane the plank and overlay factory from dispatching from the factory to, the most all more than some months, balance kiln must be introduced into for this and be balanced, treat
The whole Zhang Pingjun of moisture content can overlay in 8% right and left;
(4) PVC board is overlayed:
Overlaying the non-aldehyde low-temperature glue using Tai Er company to produce with glue, glue-spread is 250g/m2, temperature 70 degrees Celsius, pressure
8kg/cm2,500 seconds time;
(5) smooth must put more than 72 hours after hot pressing, then cut;
(6) finished product floor must seal paint, tongue and groove sealing wax overleaf.
The invention have benefit that:
1. the preparation technology of the present invention belongs to glue-free particieboard, natural environmental-protective, and class is high;
2. the preparation technology of the present invention is through high temperature high pressure process, uses solid wood to laminate technology and " zero formaldehyde " technique to timber
Deep processing, the advantage brought has: bending strength is high, and moisture resistance performance is strong, and linear expansion coefficient is little, is difficult to deformation, nail-holding ability, shock resistance
Power is strong.
Detailed description of the invention
Embodiment 1:
A kind of production method on new floor of planing the plank, its step is as follows:
(1) wood shavings fiber pretreatment:
By wood shavings fiber water spray pretreatment fluid, regulation is to water content 10%, and two top layers up and down of oriented wood chipboard are by glue mixing wood shavings
Arrange by its machine direction stringer, and sandwich layer wood shavings are transversely arranged, form three-decker plate embryo, and then oriented shaving is made in hot pressing
Plate, the orienting spreading of oriented wood chipboard makes it have the feature of higher-strength in a direction, and plywood can be replaced to do structure
Material uses;
The formula of described pretreatment is: according to mass fraction, 0.5% lactic acid, 1.2% sodium citrate, and remaining is water;
(2) high temperature high pressure process:
Solid wood is used to laminate technology and " zero formaldehyde " technique to wood deep processing, press pressure > 60MPa, operating temperature 190 is Celsius
Degree, 700 seconds press times;
(3) balance:
Plane the plank and overlay factory from dispatching from the factory to, the most all more than some months, balance kiln must be introduced into for this and be balanced, treat
The whole Zhang Pingjun of moisture content can overlay in 8% right and left;
(4) PVC board is overlayed:
Overlaying the non-aldehyde low-temperature glue using Tai Er company to produce with glue, glue-spread is 250g/m2, temperature 70 degrees Celsius, pressure
8kg/cm2,500 seconds time;
(5) smooth must put more than 72 hours after hot pressing, then cut;
(6) finished product floor must seal paint, tongue and groove sealing wax overleaf.
Embodiment 2:
A kind of production method on new floor of planing the plank, its step is as follows:
(1) wood shavings fiber pretreatment:
By wood shavings fiber water spray pretreatment fluid, regulation is to water content 10%, and two top layers up and down of oriented wood chipboard are by glue mixing wood shavings
Arrange by its machine direction stringer, and sandwich layer wood shavings are transversely arranged, form three-decker plate embryo, and then oriented shaving is made in hot pressing
Plate, the orienting spreading of oriented wood chipboard makes it have the feature of higher-strength in a direction, and plywood can be replaced to do structure
Material uses;
The formula of described pretreatment is: according to mass fraction, 1.1% lactic acid, 1.2% sodium citrate, and remaining is water;
(2) high temperature high pressure process:
Solid wood is used to laminate technology and " zero formaldehyde " technique to wood deep processing, press pressure > 60MPa, operating temperature 170 is Celsius
Degree, 700 seconds press times;
(3) balance:
Plane the plank and overlay factory from dispatching from the factory to, the most all more than some months, balance kiln must be introduced into for this and be balanced, treat
The whole Zhang Pingjun of moisture content can overlay in 8% right and left;
(4) PVC board is overlayed:
Overlaying the non-aldehyde low-temperature glue using Tai Er company to produce with glue, glue-spread is 250g/m2, temperature 70 degrees Celsius, pressure
8kg/cm2,500 seconds time;
(5) smooth must put more than 72 hours after hot pressing, then cut;
(6) finished product floor must seal paint, tongue and groove sealing wax overleaf.
Embodiment 3:
A kind of production method on new floor of planing the plank, its step is as follows:
(1) wood shavings fiber pretreatment:
By wood shavings fiber water spray pretreatment fluid, regulation is to water content 10%, and two top layers up and down of oriented wood chipboard are by glue mixing wood shavings
Arrange by its machine direction stringer, and sandwich layer wood shavings are transversely arranged, form three-decker plate embryo, and then oriented shaving is made in hot pressing
Plate, the orienting spreading of oriented wood chipboard makes it have the feature of higher-strength in a direction, and plywood can be replaced to do structure
Material uses;
The formula of described pretreatment is: according to mass fraction, 0.6% lactic acid, 1.2% sodium citrate, and remaining is water;
(2) high temperature high pressure process:
Solid wood is used to laminate technology and " zero formaldehyde " technique to wood deep processing, press pressure > 60MPa, operating temperature 180 is Celsius
Degree, 700 seconds press times;
(3) balance:
Plane the plank and overlay factory from dispatching from the factory to, the most all more than some months, balance kiln must be introduced into for this and be balanced, treat
The whole Zhang Pingjun of moisture content can overlay in 8% right and left;
(4) PVC board is overlayed:
Overlaying the non-aldehyde low-temperature glue using Tai Er company to produce with glue, glue-spread is 250g/m2, temperature 70 degrees Celsius, pressure
8kg/cm2,500 seconds time;
(5) smooth must put more than 72 hours after hot pressing, then cut;
(6) finished product floor must seal paint, tongue and groove sealing wax overleaf.
Embodiment 4:
A kind of production method on new floor of planing the plank, its step is as follows:
(1) wood shavings fiber pretreatment:
By wood shavings fiber water spray pretreatment fluid, regulation is to water content 10%, and two top layers up and down of oriented wood chipboard are by glue mixing wood shavings
Arrange by its machine direction stringer, and sandwich layer wood shavings are transversely arranged, form three-decker plate embryo, and then oriented shaving is made in hot pressing
Plate, the orienting spreading of oriented wood chipboard makes it have the feature of higher-strength in a direction, and plywood can be replaced to do structure
Material uses;
The formula of described pretreatment is: according to mass fraction, 1.0% lactic acid, 1.2% sodium citrate, and remaining is water;
(2) high temperature high pressure process:
Solid wood is used to laminate technology and " zero formaldehyde " technique to wood deep processing, press pressure > 60MPa, operating temperature 175 is Celsius
Degree, 700 seconds press times;
(3) balance:
Plane the plank and overlay factory from dispatching from the factory to, the most all more than some months, balance kiln must be introduced into for this and be balanced, treat
The whole Zhang Pingjun of moisture content can overlay in 8% right and left;
(4) PVC board is overlayed:
Overlaying the non-aldehyde low-temperature glue using Tai Er company to produce with glue, glue-spread is 250g/m2, temperature 70 degrees Celsius, pressure
8kg/cm2,500 seconds time;
(5) smooth must put more than 72 hours after hot pressing, then cut;
(6) finished product floor must seal paint, tongue and groove sealing wax overleaf.
Embodiment 5:
A kind of production method on new floor of planing the plank, its step is as follows:
(1) wood shavings fiber pretreatment:
By wood shavings fiber water spray pretreatment fluid, regulation is to water content 10%, and two top layers up and down of oriented wood chipboard are by glue mixing wood shavings
Arrange by its machine direction stringer, and sandwich layer wood shavings are transversely arranged, form three-decker plate embryo, and then oriented shaving is made in hot pressing
Plate, the orienting spreading of oriented wood chipboard makes it have the feature of higher-strength in a direction, and plywood can be replaced to do structure
Material uses;
The formula of described pretreatment is: according to mass fraction, 0.7% lactic acid, 1.2% sodium citrate, and remaining is water;
(2) high temperature high pressure process:
Solid wood is used to laminate technology and " zero formaldehyde " technique to wood deep processing, press pressure > 60MPa, operating temperature 185 is Celsius
Degree, 700 seconds press times;
(3) balance:
Plane the plank and overlay factory from dispatching from the factory to, the most all more than some months, balance kiln must be introduced into for this and be balanced, treat
The whole Zhang Pingjun of moisture content can overlay in 8% right and left;
(4) PVC board is overlayed:
Overlaying the non-aldehyde low-temperature glue using Tai Er company to produce with glue, glue-spread is 250g/m2, temperature 70 degrees Celsius, pressure
8kg/cm2,500 seconds time;
(5) smooth must put more than 72 hours after hot pressing, then cut;
(6) finished product floor must seal paint, tongue and groove sealing wax overleaf.
Embodiment 6:
Detecting planing the plank before overlaying PVC board, its testing result is as follows:
As can be seen here, the invention provides a kind of new floor of planing the plank, in the material being commonly used in wall of planing the plank, this
Invention plane the plank and may be used in floor, this material is economic and environment-friendly, and quality is softer, good heat insulating, especially
Adding layer of PVC, advantage is that anti-deformation nature is good, and top layer is PVC board, wear-resisting, glossy.
The above, the only present invention preferably detailed description of the invention, but protection scope of the present invention is not limited thereto,
Any those familiar with the art in the technical scope that the invention discloses, according to technical scheme and
Inventive concept equivalent or change in addition, all should contain within protection scope of the present invention.
Claims (3)
1. the production method on new floor of planing the plank, its step is as follows:
(1) wood shavings fiber pretreatment:
By wood shavings fiber water spray pretreatment fluid, regulation is to water content 10%, and two top layers up and down of oriented wood chipboard are by glue mixing wood shavings
Arrange by its machine direction stringer, and sandwich layer wood shavings are transversely arranged, form three-decker plate embryo, and then oriented shaving is made in hot pressing
Plate, the orienting spreading of oriented wood chipboard makes it have the feature of higher-strength in a direction, and plywood can be replaced to do structure
Material uses;
(2) high temperature high pressure process:
Solid wood is used to laminate technology and " zero formaldehyde " technique to wood deep processing, press pressure > 60MPa, operating temperature 170-190
Degree Celsius, 700 seconds press times;
(3) balance:
Plane the plank and overlay factory from dispatching from the factory to, the most all more than some months, balance kiln must be introduced into for this and be balanced, treat
The whole Zhang Pingjun of moisture content can overlay in 8% right and left;
(4) PVC board is overlayed:
Overlaying the non-aldehyde low-temperature glue using Tai Er company to produce with glue, glue-spread is 250g/m2, temperature 70 degrees Celsius, pressure
8kg/cm2,500 seconds time;
(5) smooth must put more than 72 hours after hot pressing, then cut;
(6) finished product floor must seal paint, tongue and groove sealing wax overleaf.
2. the production method on the floor of planing the plank described in claim 1, it is characterised in that:
The formula of described pretreatment is: according to mass fraction, 0.5-1.1% lactic acid, 1.2% sodium citrate, remaining is water.
3. the method described in any one of claim 1-2 produces the floor of planing the plank obtained.