CN105968481A - Rubber dehumidifying agent and preparation method thereof - Google Patents
Rubber dehumidifying agent and preparation method thereof Download PDFInfo
- Publication number
- CN105968481A CN105968481A CN201610498453.0A CN201610498453A CN105968481A CN 105968481 A CN105968481 A CN 105968481A CN 201610498453 A CN201610498453 A CN 201610498453A CN 105968481 A CN105968481 A CN 105968481A
- Authority
- CN
- China
- Prior art keywords
- parts
- rubber
- calcium carbonate
- dehumidizer
- kaolin
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Pending
Abstract
The invention discloses a rubber dehumidifying agent. The rubber dehumidifying agent comprises, by weight, 30-40 parts of calcium carbonate, 5-10 parts of kaolin, 4-8 parts of natural perfume and 2-6 parts of silicon carbide. The rubber dehumidifying agent is reasonable in material selection, easy in raw material obtaining, good in dehumidifying effect, long in storage time, wide in application range, and the like.
Description
Technical field
The present invention relates to dehumidizer, particularly relate to a kind of rubber dehumidizer and preparation method thereof.
Background technology
Calcium oxide is strong perception oxide, and white or band Lycoperdon polymorphum Vitt bulk or granule, to wet sensitive sense, easily react with water,
Being widely used in the every field of industry, and can do filler, construction material, desiccant etc., calcium oxide can be as one
Planting rubber dehumidizer, its good stability and effect on moisture extraction are widely praised, and the most common rubber dehumidifying
Agent preparation process is slow, and enterprise puts into relatively big, and production effect is unsatisfactory.
Summary of the invention
In order to overcome the defect of above-mentioned prior art, it is an object of the invention to provide a kind of rubber dehumidizer and preparation side thereof
Method.
The present invention takes techniques below scheme to realize: a kind of rubber dehumidizer formula, by following according to weight portion
Raw material composition: calcium carbonate 30 ~ 40 parts, Kaolin 5 ~ 10 parts, natural perfume material 4 ~ 8 parts, carborundum 2 ~ 6 parts.
Above-mentioned a kind of rubber dehumidizer formula, is made up of according to the raw material of weight portion following: calcium carbonate 30 ~ 38 parts, Kaolin 5
~ 8 parts, natural perfume material 4 ~ 6 parts, carborundum 2 ~ 4 parts.
Above-mentioned a kind of rubber dehumidizer formula, is made up of according to the raw material of weight portion following: calcium carbonate 35 parts, Kaolin
8 parts, natural perfume material 6 parts, carborundum 4 parts.
The preparation method of above-mentioned a kind of rubber dehumidizer, comprises the steps of:
(1) calcium carbonate is put into calcining furnace calcining, and calcium carbonate can generate calcium oxide and carbon dioxide through fully calcined;
(2) take out after calcium to be oxidized cooling, add Kaolin, carborundum and natural perfume material and be sufficiently mixed stirring;
(3) mixture is put into extruder extrude;
(4) after molding, vanning seals.
The method have the advantages that the present invention has material selection in sum reasonable, raw material is easy to get, dehumidifying effect
The best, the advantages such as the storage time is long, applied range.
Detailed description of the invention
A kind of rubber dehumidizer formula, is made up of according to the raw material of weight portion following: calcium carbonate 30 ~ 40 parts, and Kaolin 5 ~
10 parts, natural perfume material 4 ~ 8 parts, carborundum 2 ~ 6 parts.
Above-mentioned a kind of rubber dehumidizer formula, is made up of according to the raw material of weight portion following: calcium carbonate 30 ~ 38 parts, Kaolin 5
~ 8 parts, natural perfume material 4 ~ 6 parts, carborundum 2 ~ 4 parts.
Above-mentioned a kind of rubber dehumidizer formula, is made up of according to the raw material of weight portion following: calcium carbonate 35 parts, Kaolin
8 parts, natural perfume material 6 parts, carborundum 4 parts.
The preparation method of above-mentioned a kind of rubber dehumidizer, comprises the steps of:
(1) calcium carbonate is put into calcining furnace calcining, and calcium carbonate can generate calcium oxide and carbon dioxide through fully calcined;
(2) take out after calcium to be oxidized cooling, add Kaolin, carborundum and natural perfume material and be sufficiently mixed stirring;
(3) mixture is put into extruder extrude;
(4) after molding, vanning seals.
The present invention has that material selection is reasonable, and raw material is easy to get, and effect on moisture extraction is good, stores the time long, and applied range etc. is excellent
Point.
The above is embodiments of the invention, therefore all according to the structure described in the present patent application scope, feature and principle institute
The equivalence change done or modification, in the range of being all included in present patent application.
Claims (4)
1. a rubber dehumidizer formula, it is characterised in that be made up of according to the raw material of weight portion following: calcium carbonate 30 ~ 40 parts,
Kaolin 5 ~ 10 parts, natural perfume material 4 ~ 8 parts, carborundum 2 ~ 6 parts.
A kind of rubber dehumidizer formula the most according to claim 1, it is characterised in that by the following raw material according to weight portion
Composition: calcium carbonate 30 ~ 38 parts, Kaolin 5 ~ 8 parts, natural perfume material 4 ~ 6 parts, carborundum 2 ~ 4 parts.
A kind of rubber dehumidizer formula the most according to claim 1, it is characterised in that by the following raw material according to weight portion
Composition: calcium carbonate 35 parts, Kaolin 8 parts, natural perfume material 6 parts, carborundum 4 parts.
4. the preparation method of a kind of rubber dehumidizer as described in claim 1-3 is arbitrary, it is characterised in that by following step
Rapid composition:
(1) calcium carbonate is put into calcining furnace calcining, and calcium carbonate can generate calcium oxide and carbon dioxide through fully calcined;
(2) take out after calcium to be oxidized cooling, add Kaolin, carborundum and natural perfume material and be sufficiently mixed stirring;
(3) mixture is put into extruder extrude;
(4) after molding, vanning seals.